| HS Code | 322644 |
| Density | 0.958 g/cm³ |
| Melt Index | 0.15 g/10 min |
| Tensile Strength At Yield | 27 MPa |
| Tensile Strength At Break | 33 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 1.2 GPa |
| Notched Izod Impact | 0.4 J/cm |
| Hardness Shore D | 66 |
| Vicat Softening Point | 126 °C |
| Heat Deflection Temperature At 0 46 Mpa | 75 °C |
| Brittleness Temperature | -70 °C |
| Environmental Stress Crack Resistance | >1000 h |
| Thermal Conductivity | 0.45 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2e-4 cm/cm/°C |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >1e15 ohm·cm |
As an accredited Chevron Phillips Marlex® C100 Polyethylene; Enhanced factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® C100 Polyethylene; Enhanced is supplied in 25 kg (55 lb) multiwall paper bags, palletized; bulk trucks/railcars available. |
| Container Loading (20′ FCL) | Loaded into 20′ FCL: 25 kg bags of Chevron Phillips Marlex® C100 Polyethylene; Enhanced, palletized, stretch-wrapped, and secured for shipment. |
| Shipping | Chevron Phillips Marlex® C100 Polyethylene; Enhanced is shipped as a non-hazardous, non-regulated solid resin in bags, sacks, or bulk containers. Keep containers closed, dry, and protected from heat, moisture, and contamination. Follow applicable DOT, IMO, IATA, and local transport regulations. Avoid dust generation and spills. |
| Storage | Store Chevron Phillips Marlex® C100 Polyethylene; Enhanced in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers closed to prevent contamination and moisture pickup. Avoid dust generation and accumulation; ground equipment to control static. Segregate from strong oxidizers. Protect from UV exposure and follow local regulations. |
| Shelf Life | Chevron Phillips Marlex® C100 Polyethylene; Enhanced: stable indefinitely when stored cool, dry, and away from sunlight, heat, and moisture. |
When Chevron Phillips Marlex C100 Enhanced is introduced on a flat-die geomembrane extrusion line, the operating envelope is determined primarily by melt-temperature stability and drawdown behavior between the die lip and the embossing nip. In typical production-scale equipment—single-screw extruder with barrier feed section, L/D 30:1 to 33:1, die width 2,500 mm to 4,000 mm, three-roll stack with one textured steel roll—the melt temperature is maintained at 210–230°C, with barrel zones set at 180°C/200°C/210°C/215°C. Die head pressure is held in the range of 80–120 bar, and the die gap is set at 1.8–2.5 times the target sheet thickness to compensate for drawdown. The addition of texture via a roughened steel roll requires the roll surface temperature to remain within 40–90°C; below this range, residual stress in the polymer surface produces edge curl and local microcracking after slitting, while above 95°C the embossed texture relaxes and partially erases the surface profile. The resin is blended with carbon black masterbatch before extrusion because geomembrane specifications require a minimum carbon black content of 2.0–3.0 wt% and carbon black dispersion meeting GRI-GM13 guidelines; the dispersion quality is checked according to ASTM D5596-94(2016). Tensile yield strength is measured under ASTM D638-14 Type IV or ISO 527-2:2012; dart impact resistance for sheet above 1.5 mm is typically characterized using ASTM D1709-21 or ISO 7765-1:1988, while environmental stress crack resistance is evaluated under ASTM D1693-15e1 Condition C.
The compounding recipe for a 100 kg batch of textured geomembrane stock is controlled within narrow limits: 96.0–97.5 wt% virgin C100 Enhanced, 2.0–3.0 wt% carbon black LLDPE/HDPE masterbatch, 0.5–1.0 wt% processing aid masterbatch, and 0.5–1.5 wt% UV stabilizer masterbatch. The lower addition limit of carbon black is driven by weathering resistance, and the upper limit is constrained by a measurable reduction in elongation at break due to filler loading.
| Component | Addition ratio | Control standard or method |
|---|---|---|
| Virgin C100 Enhanced | 96.0–97.5 wt% | ISO 1183-1:2019 density; ISO 1133-1:2022 melt flow assurance |
| Carbon black masterbatch | 2.0–3.0 wt% | ASTM D5596-94(2016) dispersion; GRI-GM13 carbon black content |
| UV stabilizer masterbatch | 0.5–1.5 wt% | ISO 4892-2:2013 xenon weathering |
| Processing aid masterbatch | 0.5–1.0 wt% | Extruder head pressure stability; no direct ASTM equivalent |
The downstream manufacturing sequence includes pre-drying of any regrind at 80°C for 4–6 h when stored at relative humidity above 60%, gravimetric metering of edge trim regrind at 15–30 wt%, flat-die extrusion, three-roll texturing, beta-gauge thickness scanning, and automatic winder tension control. Closed-loop recycling of edge trim above 30 wt% is not recommended during textured sheet production because the repeated shear history of previously processed material lowers drawdown stability and can produce localized surface roughness defects. Finished products produced under this route are single-sided or double-sided textured HDPE geomembrane panels in rolls up to 7.0 m wide, used as primary landfill liner, leachate collection sump liners, secondary containment basins, pond liners, canal lining panels, and vertical cutoff wall membranes. Seam welding for these products must be qualified separately under ASTM D6392-12(2018) because the textured surface alters peel separation behavior relative to smooth sheet.
In the extrusion blow molding of UN-certified free-standing containers for acids, agricultural chemicals, and water-miscible industrial fluids, C100 Enhanced is formulated as a 100 wt% virgin stream, with internally generated regrind allowed up to 25 wt% only when the regrind comes from the same container production lot and is free of post-consumer contamination. The process uses an accumulator-type blow molding machine with clamp force between 80 kN and 250 kN, a barrier head temperature of 190–210°C, mold temperature from 15°C to 40°C, and parison programming to control wall thickness at pinch-off zones. During continuous campaigns on 30–60 L jerrican lines, the switching between colored and natural material must account for a residence-time carryover of 6–12 min; purging with a high-viscosity HDPE purge resin is required when changing from antistatic formulations to hydrocarbon-only formulations to avoid pinhole formation at the weld line. The addition ratio of a colorant masterbatch is 0.5–2.0 wt%, and an antistatic masterbatch is added only at 0.05–0.2 wt% when the package is specified for dry flammable powders under UN 1H1. Compliance testing follows 49 CFR 178.500, ADR/RID 6.1.5, and the UN drop test at -18°C with a pack group dependence of 1.2 m for Packing Group II. Finished product types include 5–60 L jerricans, 25–220 L open-head drums, intermediate bulk container inner bottles, and screw-cap containers for laboratory waste disposal. Post-consumer recycled material is excluded from UN-certified packagings unless the complete design passes performance tests under ADR/RID 6.1.5.2.4 and 49 CFR 178.500.
Pipe extrusion of C100 Enhanced is performed on grooved-feed single-screw extruders with L/D 30:1 to 36:1 and barrel zone set points 200°C/210°C/220°C/215°C; melt temperature at the adapter is held at 210–230°C. For solid-wall pipe from Ø20 mm to Ø630 mm, the die land pressure is maintained between 150 bar and 350 bar, depending on pipe dimension and line speed. Vacuum calibration tanks are set initially at 30°C, with cooling water progression from 20°C to 60°C to control sag without residual thermal stress. The critical processing conflict is sag at large diameters above 400 mm; if the melt temperature exceeds 235°C, the pipe can lose concentricity in the calibration sleeve, and derating may occur even when the formulation is unchanged. Conversely, if the melt temperature drops below 195°C, the resin may show melt fracture at the die lip, producing visible ridges and reducing the apparent density uniformity around the circumference.
For industrial non-pressure and pressure pipe trials, the blend is 95.0–98.0 wt% C100 Enhanced, 2.0–3.0 wt% carbon black masterbatch for outdoor service, 0.0–0.5 wt% processing aid masterbatch, and 0.0–1.0 wt% antioxidant masterbatch only when extended high-temperature hydrostatic testing is specified. Recycled clean in-house pipe regrind is introduced at 10–20 wt%; higher fractions up to 30 wt% are used only for corrugated drainage pipe. All proportions are gravimetric and tied to the extruder throughput; a twin-screw side feeder is not normally required because the formulation is unfilled. Compliance of the extrudate is verified before any commercial pressure rating is assigned; no PE pressure rating is assigned to the finished pipe without a complete linear stress rupture evaluation.
| Declaration | Test method | Condition or clause |
|---|---|---|
| Hydrostatic design basis | ISO 1167-1:2006 | 20°C and 80°C internal water test |
| Oxidation induction time | ISO 11357-6:2018 | 200°C oxygen atmosphere |
| Melt flow assurance | ISO 1133-1:2022 | 190°C/2.16 kg |
| Density | ISO 1183-1:2019 | Immersion method at 23°C |
| Environmental stress crack resistance | ASTM D1693-15e1 | Condition C, 10% Igepal CO-630 |
| Carbon black dispersion | ISO 18553:2023 | Microscope rating chart |
Downstream pipe production includes die-head tooling matched to the final diameter, vacuum spray cooling, laser diameter gaging, and in-line marking. The extrudate is cut into 6 m, 12 m, or coil lengths depending on OD and wall thickness. Finished product types include mining slurry transfer lines, dredge pipeline sleeves, industrial process water pipe, subsoil drainage pipe, cable ducting, and corrugated road culvert segments. For buried outdoor service, the combination of 2.0–3.0 wt% carbon black and the resin stabilization package contributes to long-term weathering resistance, but local ultraviolet exposure conditions must be validated under ISO 4892-2:2013 when the pipe is installed above ground for extended periods.
Reciprocating screw injection molding lines converting C100 Enhanced into returnable transport packaging operate with a clamp force range of 1,500–6,000 kN; the shot weight is maintained between 30% and 70% of barrel capacity to limit residence time to 4–6 min at a maximum cylinder temperature of 230°C. Barrel temperature profile from hopper to nozzle is 180°C/190°C/210°C/220°C; injection pressure ranges from 800 bar to 1,400 bar, with hold pressure at 60–80% of injection pressure for 3–8 s, back pressure 5–15 bar, and mold surface temperature 15–40°C. For thin-wall crates weighing 3–8 kg, fast injection speeds above 200 mm/s reduce weld-line depth at the handle apertures and corner pillars, but increase shear heating; the screw speed is limited to 80–120 rpm to avoid molecular weight degradation at the check ring. The formulation is 100 parts C100 Enhanced, 0.1–0.5 wt% internal release agent masterbatch, 0.5–2.0 wt% colorant masterbatch, and 2.0–5.0 wt% elastomer-modifier masterbatch only for freezer-distribution crates or sub-zero storage racks. In-house regrind from sprues and rejected parts is incorporated at 20–40 wt%, provided the regrind is dried at 80°C for 4 h and screened through a 6 mm sieve; post-consumer recycled material is excluded from food-contact crates but may be added at 25 wt% for industrial dunnage if tested under ISO 8611-1:2021. Finished products include stackable crates, perforated dunnage sheets, pallet feet, agricultural trays, and industrial battery containment trays. Mechanical acceptance is verified under ASTM D256-10 for Izod impact, ISO 527-2:2012 for tensile properties, and ISO 180:2023 for notched Charpy impact. At mold temperatures above 60°C, cycle time increases beyond 75 s for a 5 kg crate; at mold temperatures below 10°C, weld-line impact strength falls due to quench-induced skin solidification before the melt front has fully coalesced.
In monofilament extrusion for outdoor woven geotextile and agricultural netting, C100 Enhanced is first compounded with 4.0 wt% carbon black masterbatch and 1.0–2.0 wt% HALS UV stabilizer masterbatch; the melt is then fed to a single-screw extruder with L/D 26:1 to 30:1, a melt pump set to 40–80 rpm, and a multi-hole spinneret with hole diameters from 0.6 mm to 1.2 mm. The extrudate is quenched in a two-stage water bath maintained at 25–40°C, then stretched in a hot air oven at 85–100°C with a draw ratio of 6:1 to 10:1; a final annealing stage at 100–110°C reduces shrinkage. The lower water quench temperature at 25°C produces higher drawability but increases line breaks at startup; above 40°C, the monofilament surface remains too soft and can stick to the first godet. The manufacturing route includes precision winding on 6-speed godets at 120–180 m/min; tension is controlled within ±5 mN/tex to prevent denier variation and periodic thin spots that would later become weak points in the woven fabric.
Woven fabrics made from the monofilament are supplied as silt fencing, ground cover, windbreak mesh, anti-hail netting, and construction safety scaffolding netting. Quality assurance for the woven fabric uses ISO 10319:2015 for tensile strength and elongation, EN 12224:2000 for weathering resistance, and ISO 4892-2:2013 for xenon exposure. Published data for final UV retention in agricultural netting made from this exact grade is limited; weathering trials should be run according to ISO 4892-2:2013 for the specific denier and weave structure before commercial release. Finished monofilament denier ranges from 150 tex to 700 tex, depending on spinneret hole diameter and draw ratio. A processing boundary is the line speed beyond 180 m/min, where tension oscillations at the winder can initiate surface fibrillation in outdoor-grade filaments; below 120 m/min, throughput becomes uneconomical and the residence time in the hot air oven may degrade surface stabilizers.
Thermoformed heavy-gauge sheet for agricultural machinery guards and automotive underbody liners is extruded from C100 Enhanced at a nominal caliper of 2.0–6.0 mm on a single-screw extruder with L/D 30:1, barrel zone temperatures from 180°C to 220°C, and a three-roll polish stack set at 70–90°C to reduce sheet waviness. The sheet is then reheated in a quartz or halogen oven to a surface temperature of 130–160°C, transferred to a vacuum forming station with a forming pressure of -0.08 MPa to -0.02 MPa, and cooled in the mold at 20–40°C until the core temperature falls below 70°C. Draw ratios at the deepest cavities are limited to 1:1.5; higher draw ratios produce excessive thinning at corners and a localized drop in dart impact measured under ISO 6603-2:2023 at -20°C. The compound recipe is 100 parts C100 Enhanced, 0.5–2.0 wt% colorant masterbatch, 0.5–1.5 wt% UV stabilizer masterbatch for outdoor components, and 20–50 wt% in-house sheet edge trim regrind; mixing is via gravimetric dosing at the extruder throat. The resulting formed parts include tractor roof shells, engine side panels, fender extensions, underbody shields, and chemical spray tank covers. Compliance standards for end-use parts include ASTM D790-17 for flexural modulus, ASTM D648-18 for heat deflection temperature at 0.455 MPa, and ISO 3795:1989/FMVSS 302 for horizontal flammability where vehicle interior applications are specified. A processing boundary is the thermoforming oven residence time: above 240 s at 160°C, surface oxidation can produce yellowing and a measurable fall in elongation at break; below 120 s, the core remains below forming temperature and spring-back after demolding is observed.
Competitive Chevron Phillips Marlex® C100 Polyethylene; Enhanced prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® C100 Polyethylene; Enhanced is a high-density polyethylene resin supplied in pellet form for extrusion blow moulding, injection blow moulding, and selected profile or sheet extrusion. The polymer is produced in a continuous slurry-loop train. Its nominal density is 0.954 g/cm³ when measured according to ASTM D1505-20, and its nominal mass-flow rate is 0.80 g/10 min at 190 °C under 2.16 kg load when measured according to ASTM D1238-20. This fractional melt-flow position is characteristic of blow-moulding high-density polyethylene and differentiates the grade from high-flow injection-moulding resins, which typically possess mass-flow rates above 8 g/10 min.
The “Enhanced” designation is associated with a controlled additive package and reduced lot-to-lot variability in melt flow and comonomer distribution. In production-scale accumulator blow-moulding lines with extruder diameters of 80–120 mm, clamp force of 50–150 ton, and L/D ratios of 24:1–30:1, the resin is typically processed at melt temperatures of 200–230 °C. Die-head set points are maintained at 200–220 °C, while mould cooling temperatures are kept at 15–30 °C. Published data for this specific configuration is limited; the ranges represent the general operating envelope for fractional-melt-flow blow-moulding HDPE and should be confirmed by line trials.
Aggressive liquid formulations—such as emulsifiable agricultural concentrates, mineral spirits, surfactants, and hypochlorite-based oxidising agents—promote environmental stress cracking in container sidewalls and pinch-off welds. The Enhanced designation is normally selected when acceptance testing requires long F50 times under ASTM D1693-15 Condition B at 50 °C in 100% Igepal CO-630. The molecular architecture of the Enhanced grade provides a higher molecular-weight tail and more uniform comonomer placement, which improves crack resistance in the intercrystalline tie-chain network. Nevertheless, published public datasheet values for the Enhanced designation are limited; batch certificate data must be compared with container qualification limits before release.
Mechanical properties of the blow-moulded wall are typically in the range of 26–28 MPa tensile yield stress when measured by ASTM D638-14 and 1.15–1.25 GPa flexural modulus when measured by ASTM D790-17. These values are intermediate for blow-moulding HDPE and provide top-load strength without excessive brittleness at the handle pinch region. The lower density of 0.954 g/cm³ relative to injection-grade HDPE reduces crystallinity slightly, which contributes to stress-crack resistance while maintaining adequate stiffness.
Container qualifications for industrial liquid packaging frequently include top-load testing at 23 °C and drop-impact testing after preconditioning at -18 °C. C100 Enhanced is evaluated in bottles of 1–5 L capacity with wall thickness of 0.8–1.5 mm. Failure modes observed on production lines are pinch-off delamination, handle-web thinning, and radial wall thinning opposite the flash line. When regrind content exceeds 25%, melt-pressure variability and gel-particle formation can increase; parison programming must be adjusted to compensate for the degraded fraction.
High-flow HDPE injection-moulding grades are characterised by mass-flow rates of 8–20 g/10 min under ASTM D1238-20. These resins provide low pressure drop and long flow lengths during mould filling, but their low melt strength allows excessive sag when an unsupported parison is extruded. Marlex C100 Enhanced has a fractional mass-flow rate of 0.80 g/10 min, reflecting a higher average molecular weight. This increases both shear viscosity and extensional viscosity at low deformation rates, which slows parison sag and strengthens pinch-off welds. In injection-blow moulding, the same viscosity requires higher melt temperatures and longer injection times; the grade is therefore more appropriate for small preforms and thick-wall containers than for thin-wall vials with flow-length-to-wall-thickness ratios above 150:1.
Compared with high-load-melt-index film grades tested at 190 °C under 21.6 kg, C100 Enhanced is less shear-thinning. Film grades with high-load melt indices of 5–15 g/10 min are optimised for high-throughput cast or blown film, but they can exhibit excessive die swell and parison curl in blow moulding. Die swell of C100 Enhanced is controlled in practice by die bushings sized at 70–85% of the final container diameter. Capillary rheometry of fractional-melt blow-moulding HDPE at 190 °C typically shows a melt viscosity of 2,000–4,000 Pa·s at 100 s⁻¹ and 300–600 Pa·s at 1,000 s⁻¹. The power-law index is generally 0.4–0.6. Published data for this specific configuration is limited; these values frame the general rheological behaviour of fractional-melt HDPE rather than batch-release limits.
On a single-screw extruder with an L/D ratio of 24:1 to 30:1, a general-purpose HDPE screw with a compression ratio of 2.5:1 to 3.5:1 is acceptable for pellet feedstock. A reverse barrel profile from 180 °C at the feed throat to 210 °C at the metering zone is used to prevent premature melting and feed-bridge formation. The die head is maintained at 205–220 °C. Melt temperature at the die exit is held below 230 °C to suppress oxidative chain scission and odour generation. Residence time above 230 °C is not to exceed 5 min; extended holds require purging with a higher-melt-flow HDPE of 2 g/10 min at full temperature before shutdown.
Zone set points of 180 °C, 190 °C, 195 °C, and 200 °C from feed to metering are common for a 90 mm accumulator-head extruder processing C100 Enhanced at 45 kg/h. The die head is set at 210 °C, and accumulator fill time is adjusted so that shot weight is achieved before the parison begins to sag. Blow air pressure is set at 0.6–0.8 MPa. Mould cooling water at 10–20 °C gives a cycle time of 40–90 s for 1–5 L containers with wall thickness 0.8–1.5 mm. The cooling time constant increases with the square of wall thickness; heavier containers require active internal cooling or extended blow time.
Parison programming through a diverging die gap from 2 mm to 8 mm is used to correct wall distribution. The fractional melt flow of C100 Enhanced supports programmed parisons over a free hang length of 400–600 mm, but hang length depends on melt temperature, die swell, shot size, and ambient air speed. On continuous shuttle or wheel machines, the extruder is often operated at higher throughput with a longer die land to reduce melt fracture; die land length is typically 15–25 times the die gap.
The following comparative set is not a specification; values are typical published data and must be verified against current supplier documentation and certificate of analysis.
| Property | Test method | Marlex C100 Enhanced | General-purpose HDPE blow moulding range |
|---|---|---|---|
| Density | ASTM D1505-20 | 0.954 g/cm³ | 0.945–0.965 g/cm³ |
| Mass-flow rate | ASTM D1238-20 | 0.80 g/10 min | 0.20–2.0 g/10 min |
| Tensile yield stress | ASTM D638-14 | 27 MPa | 22–31 MPa |
| Flexural modulus | ASTM D790-17 | 1.20 GPa | 0.90–1.50 GPa |
| Shore D hardness | ASTM D2240-15 | 65 | 60–70 |
| Vicat softening temperature | ASTM D1525-17 | 125 °C | 120–130 °C |
| ESCR, Condition B | ASTM D1693-15 | Published datasheet value limited; batch certificate required | Varies by comonomer package |
The base resin falls within the olefin polymer category described in 21 CFR 177.1520(c) when used unmodified and under the intended-use conditions stated by the supplier. Food-contact suitability of the finished container must be verified on the actual formulation because colour concentrates, regrind, and processing aids can alter compliance. For European supply, registration under REACH Regulation (EC) No 1907/2006 is the responsibility of the manufacturer or importer. Assessment against Directive 2011/65/EU for RoHS substances—lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE—requires laboratory verification on the final formulation; the base resin is not formulated with these substances as intentional additives.
Moisture absorption is low, and pre-drying is not required for pellet stock stored below 60% relative humidity. When storage at higher relative humidity has occurred, surface condensation is removed with a hopper dryer at 70 °C for 1 h. The resin is not recommended for prolonged contact with strong oxidising acids or chlorinated solvents at elevated temperatures, as these conditions can accelerate stress cracking or oxidative degradation. Processing above 260 °C is not recommended because off-gassing and viscosity loss may occur. Equipment should be purged of PVC or fluoropolymer residues before changeover because acid gas generation can corrode tool steel.
Incoming resin assessment for extrusion blow moulding typically includes MFR by ASTM D1238-20, density by ASTM D1505-20, and visual pellet inspection. Batch-to-batch variability of the Enhanced designation is controlled to a narrower band than standard C100; however, the exact band is defined in the supplier’s certificate of analysis. When adding colour concentrate, the converter determines the threshold for masterbatch of 2–4 wt% and validates melt-pressure stability before production.
For injection-blow-moulded multilayer barrier containers, C100 Enhanced is used as the structural outer layer because its melt strength supports the preform during transfer from injection core to blow mould. The injection unit is operated with a rear zone of 180 °C, centre 200 °C, front 210 °C, and nozzle 215 °C. Injection pressure is typically 80–120 MPa, and preform surface temperature at transfer is controlled between 105 °C and 115 °C to prevent sticking and crystallisation haze. Published data for this specific configuration is limited; tool-specific trials are required.
In sheet extrusion for deep-draw thermoforming, C100 Enhanced is run at a die temperature of 200–215 °C with chill-roll temperatures of 70–90 °C. The fractional melt-flow provides high melt strength for thick sheet and reduces sag in the draw gap. The typical sheet thickness range is 2–6 mm, and vacuum-forming conditions require sheet surface temperatures of 130–145 °C.