Chevron Phillips Marlex 7308fk Polyethylene Lldpe

Chevron Phillips Marlex® 7308FK Polyethylene; LLDPE

    • Product Name: Chevron Phillips Marlex® 7308FK Polyethylene; LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 644549
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.930 g/cm3
    Melt Index 0.8 g/10 min (190°C/2.16 kg)
    Melting Point 125 °C
    Vicat Softening Point 108 °C
    Tensile Strength At Yield 12 MPa
    Tensile Strength At Break 24 MPa
    Elongation At Break 800%
    Flexural Modulus 550 MPa
    Hardness Shore D 55
    Brittleness Temperature < -70 °C
    Environmental Stress Crack Resistance > 1000 h
    Thermal Expansion Coefficient 1.5e-4 /°C
    Thermal Conductivity 0.35 W/m·K
    Specific Heat Capacity 2.0 J/g·°C
    Water Absorption < 0.01%

    As an accredited Chevron Phillips Marlex® 7308FK Polyethylene; LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg (55 lb) polyethylene-lined multiwall paper bags, palletized and stretch-wrapped; bulk truck or railcar options may be available.
    Container Loading (20′ FCL) 20′ FCL loading for Chevron Phillips Marlex® 7308FK LLDPE: 25 kg bags, approximately 20–22 metric tons per container.
    Shipping Chevron Phillips Marlex® 7308FK LLDPE is a non-hazardous solid resin. It is typically shipped in 25 kg bags, supersacks, bulk trucks, or railcars. No special hazard class is assigned. Keep containers dry, cool, and closed, away from ignition sources and direct sunlight. Follow the manufacturer’s SDS and applicable transport regulations.
    Storage Store Chevron Phillips Marlex® 7308FK Polyethylene (LLDPE) in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers closed to prevent moisture and contamination. Avoid dust accumulation and static discharge; use grounding where required. Maintain clean, labeled storage, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Stable under normal storage conditions; no specific shelf life, but keep cool, dry, away from direct sunlight and ignition sources.
    Application of Chevron Phillips Marlex® 7308FK Polyethylene; LLDPE

    High-stalk tubular film extrusion of Marlex 7308FK at a die gap of 1.6–2.0 mm and a blow-up ratio of 2.3:1–2.8:1 is the standard monolayer route for hygiene overwrap and tissue bundling. The addition ratio is 100 wt% Marlex 7308FK in monolayer constructions; when bubble instability occurs on lines with stalk heights above 8 die diameters, up to 20 wt% high-pressure LDPE with melt index 0.25–0.5 g/10 min is introduced to increase melt tension without reducing dart impact below the specified acceptance floor. Compliance for direct food-contact overwrap is governed by FDA 21 CFR 177.1520(c) for olefin polymers and by EU Regulation (EU) No 10/2011 Annex I, with specific migration of hexene-derived oligomers verified under EN 1186-14 migration testing at 40 °C for 10 days. The production process employs a grooved-feed extruder with L/D 30:1, screen pack 60/80/100 mesh, and die temperature set between 190 °C and 215 °C to avoid surface oxidation while maintaining melt pressure below 550 bar; a dual-lip air ring with internal bubble cooling is configured to balance frost line height at 55–65% of stalk height. Terminal finished product types include lightweight produce bags, tissue-spiral bundling film, and textile drape overwrap at 18–35 µm nominal thickness. On high-output lines above 350 kg/h, gauge band formation associated with port-line die deflection is controlled by reducing die gap to 1.4 mm and increasing die temperature uniformity to ±1 °C across the circumference.

    What Limits Chill-Roll Output When Marlex 7308FK Is Drawn Down to 12 µm on Cast Film Lines?

    Cast-film palletization film based on Marlex 7308FK is processed at a melt temperature of 205–230 °C through a flat die with lip gap 0.8–1.2 mm onto a chill roll controlled at 24–28 °C. The formulation addition ratio for machine-grade stretch film is 93–96 wt% Marlex 7308FK, 3–5 wt% metallocene LLDPE with density 0.902–0.908 g/cm³, and 0.5–1.2 wt% polyisobutylene-based cling additive in a letdown concentrate; hand-grade film replaces the metallocene with 5–8 wt% lower-MI LLDPE to reduce force-to-stretch. When draw-down to 12–15 µm is performed, the primary process bottleneck is not melt delivery but edge-neck-in and draw resonance, which are controlled by reducing chill-roll speed differential and maintaining air gap at 100–160 mm. Compliance for pallet wrap is evaluated under ASTM D5748-19 for puncture resistance, ASTM D5458-95(2020) for cling, and ISO 527-3 for tensile elongation; EU food-contact packaging variants require EU Regulation (EU) No 10/2011 compliance. Downstream production employs an extruder with L/D 30:1, barrier screw, and deckle width 2.4–3.2 m, with target frost-free chill roll after 3–5 mm of web contact. Terminal products include pre-stretched machine film at 8–12 µm, coreless hand wrap, and agricultural bale-securing film. Draw resonance onset on wide lines is typically observed when the film thickness drops below 9 µm and the melt temperature exceeds 232 °C, at which point edge instability propagates toward the centerline and produces alternating thick-thin bands measured by online capacitance gauges.

    Sealant Skin Coextrusion with Biaxially Oriented Polypropylene Substrates

    Three-layer cast coextrusion positions Marlex 7308FK as the heat-sealant skin on biaxially oriented polypropylene lamination webs. The addition ratio for the sealant layer is 100 wt% Marlex 7308FK or 70–80 wt% with 20–30 wt% plastomer at density 0.902 g/cm³ to lower seal initiation temperature from 105 °C to 88–95 °C for high-speed vertical form-fill-seal machines. The skin layer is maintained at 12–20% of total film thickness, with core polypropylene homopolymer at 60–70% and tie resin at 8–10%. Compliance for food-contact laminates is verified under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with total migration below 10 mg/dm² when tested according to EN 1186-1. Downstream processing uses a three-extruder cast line with die temperature 205–225 °C, air gap 80–120 mm, and chill roll temperature 18–22 °C to suppress post-crystallization haze; corona treatment elevates surface tension from 31 dyn/cm to 38–42 dyn/cm before lamination. Finished goods include biscuit wrappers, powdered beverage sachets, and frozen vegetable pouches requiring seal-through-contamination resistance. Seal strength on contaminated jaw faces is maintained only when the skin layer remains above 15 µm; below that gauge, sealant thinning over core-layer gauge variation produces channel defects and increases oxygen transmission above 60 cm³/m²·day·atm under ASTM D3985-17.

    In heavy-duty liner extrusion for bulk chemical packaging, a grooved-feed single-screw extruder with screw diameter 75 mm and L/D 30:1 delivers melt at 190–210 °C through a die gap of 2.0–2.4 mm to a bubble with blow-up ratio 2.0:1–2.6:1. The addition ratio in the dry blend is 70 wt% Marlex 7308FK and 30 wt% LDPE film resin with melt index 0.25–0.4 g/10 min; this composition raises low-temperature dart impact on 100 µm film above 200 g under ASTM D1709-16a while maintaining tear propagation resistance above 12 N under ASTM D1922-15. Compliance for flexible intermediate bulk container liners references ISO 21898:2004 for packaging containment and, where food-grade contents are packed, FDA 21 CFR 177.1520(c). The production process requires melt pressure at the breaker plate to remain below 600 bar; pressure spikes above 620 bar on extruders with worn grooved bushings cause feed port melt-back and require liner replacement at 10,000–12,000 h intervals. Terminal products include 200–500 µm FIBC liners, mineral concentrate liners, and oil-absorbent pouch liners. Batch-to-batch variance in film blocking is reduced by maintaining the outer bubble surface temperature below 35 °C at the collapsion nip; operator feedback from production-scale lines indicates that blocking-related roll telescoping increases sharply when the nip temperature exceeds 38 °C during summer operations.

    Oxygen Ingress at the Bale-Fold Crease in Agricultural Silage Film

    For round-bale silage wrapping, Marlex 7308FK is processed at a melt temperature of 195–215 °C with UV stabilizer masterbatch addition at 3–5 wt% because the base resin is supplied without a light-stabilizer package. The masterbatch carrier is an LLDPE with melt index 2.0–4.0 g/10 min, and the final addition ratio is 95–97 wt% Marlex 7308FK to 3–5 wt% UV masterbatch; carbon black pigmentation at 1.5–2.5 wt% is added only for opaque silage covers exposed to high-UV regions. Compliance is set by EN 13207:2018 for thermoplastic silage films and by ISO 527-3 for tensile modulus in machine direction after 1,500 h of accelerated weathering. Blown-film processing uses die gap 1.8–2.2 mm, blow-up ratio 2.8:1–3.2:1, and dual-lip air ring to produce 25–40 µm film with machine-direction elongation above 500%. The folding crease in round-bale wrapping is the primary failure initiation point; oxygen ingress at the crease increases from 0.4 cm³/m²·day·atm on flat film to 1.1–1.8 cm³/m²·day·atm after 50 mechanical fold cycles when measured under ASTM D3985-17. Terminal finished goods include bale wrap, silo bag liner, and clamp silage cover. On production-scale calendering stacks, film with thickness variation greater than ±3 µm across the web creates inconsistent stretch at the bale edge and produces localized whitening at the fold line after 24 h of outdoor exposure.

    When Extrusion Coating onto 40 g/m² Kraft Paper Replaces LDPE Skin Layers

    On extrusion coating lines handling 40 g/m² kraft paper and aluminum foil substrates, Marlex 7308FK is processed at melt temperatures of 260–300 °C, with die gap 0.6–0.8 mm and air gap 150–250 mm to maximize adhesion before the chill-roll nip. The addition ratio for the coating layer is 100 wt% Marlex 7308FK when adhesion to metallic foil is required; for paper substrates, 15–20 wt% high-pressure LDPE is added to reduce neck-in and improve fiber tear under high-speed web tension. Compliance for coated food-contact papers follows FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with chloroform-soluble extractives tested under 21 CFR 177.1520(d) not exceeding 5.5% at 121 °C for 2 h. Process conditions require a cooling roll temperature of 10–15 °C and substrate pre-treatment via corona to 38–44 dyn/cm; line speed is limited to 120–180 m/min because higher speeds produce interfacial voids at the paper-fiber boundary. Terminal products include release liner base papers, aseptic carton barrier layers, and foil-based pharmaceutical strip packaging. Melt curtain instability occurs when the air-gap melt temperature drops below 255 °C at line speeds above 160 m/min, producing edge wave and intermittent coating voids that are detectable with online pinhole cameras positioned before the chill-roll nip.

    Free Quote

    Competitive Chevron Phillips Marlex® 7308FK Polyethylene; LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® 7308FK Polyethylene is identified as a linear low-density polyethylene (LLDPE) resin produced with a butene comonomer and formulated with a slip and antiblock additive package. The product is supplied as pellets and is positioned for cast film extrusion, thin-gauge stretch film, and selected extrusion coating applications. The nominal density is 0.918 g/cm³ when tested according to ASTM D1505; the nominal melt index is 8.0 g/10 min when determined at 190°C under a 2.16 kg load in accordance with ASTM D1238 and ISO 1133-1. These values place Marlex 7308FK in the high-melt-index segment of butene LLDPE film resins. The short relaxation time and low shear viscosity reduce extruder head pressure during high-speed cast film production but also require tighter control over melt curtain stability and draw resonance than fractional-melt-index grades. The additive package in the pellet contributes to surface slip and antiblocking after migration to the film surface; this distinguishes the grade from unmodified LLDPE resins that require external slip masterbatch additions.

    Nominal Physical Properties and Standardised Test Data

    The primary published nominal values are listed in Table 1. Density is controlled to 0.918 g/cm³, which places the resin in the low-crystallinity region of linear polyethylene. Melt index is controlled to 8.0 g/10 min. The combination is selected for low melt-temperature processing and high throughput in slot-die cast film equipment. Where certification is required, film tensile properties are evaluated under ASTM D882, dart impact under ASTM D1709, Elmendorf tear under ASTM D1922, optical haze under ASTM D1003, and kinetic coefficient of friction under ASTM D1894.

    Table 1. Nominal published values for Marlex® 7308FK
    PropertyNominal ValueTest Method
    Density0.918 g/cm³ASTM D1505
    Melt index8.0 g/10 minASTM D1238 / ISO 1133-1
    Comonomer typeButeneSupplier specification
    Additive packageSlip and antiblockSupplier specification
    Physical formPelletSupplier specification

    The molecular architecture of 7308FK is typical of Ziegler-Natta butene LLDPE: a broad molecular weight distribution combined with short-chain branching concentrated in the low-molecular-weight fraction. This structure gives pronounced shear thinning in high-shear zones such as screw mixers, but it also limits the extensional viscosity plateau required for vertical melt curtain stability. The branch length of butene is shorter than that of hexene or octene LLDPE; therefore the tie-chain density across crystallites is lower at equivalent density, and the film undergoes lower puncture propagation resistance and higher directional tear anisotropy. The slip and antiblock formulation partially offsets surface defects by reducing roll blocking, but it does not alter the intrinsic comonomer limitation.

    What Processing Limits Govern High-Output Cast Film Lines?

    Extrusion of Marlex® 7308FK on cast film lines is governed by the relationship between melt index, head pressure, and melt temperature. At melt index 8.0 g/10 min, the resin enters the die with lower shear viscosity than blown film LLDPE grades of 1.0–2.0 g/10 min. In practice, barrel temperature profiles commonly start with a feed throat water setting of 30–40°C, progress through compression zones in the range of 190–240°C, and hold the adapter and die at 240–260°C. The resin should not be held at melt temperatures above 280°C for extended periods; oxygen ingress from recycled edge trim accelerates gel formation. A screen pack of 40–60 mesh is typically installed to protect the die from carbonized gels. Single-screw extruders with 30:1 to 40:1 L/D ratios and double-flight feed sections are suitable; published data for this specific configuration is limited, and start-up trials should map head pressure versus screw speed before maximum line speed is set.

    Within cast film operations, no internal bubble pressure control is required. The melt curtain exits a coat-hanger slot die onto a chill roll maintained at 18–35°C. The rapid quench lowers spherulite growth and yields film with lower haze than equivalent blown film. Edge trim recycling at 10–25 wt% is common on production lines; the slip and antiblock additives in reclaimed fluff can shift surface roughness if the trim fraction is not homogenized through a gravimetric blender. The high melt index allows a larger proportion of edge trim to be reintroduced without exceeding the extruder pressure limit, but overfeeding low-bulk-density fluff can cause feed throat bridging unless a crammer feeder is used.

    When Slot-Die Edge Instability and Draw Resonance Are Evaluated

    Marlex® 7308FK has lower melt strength than fractional-melt-index polyethylenes because of its high melt index and butene branched structure. Under increasing take-off speed, the draw-down ratio—defined as the ratio of die lip width to final film gauge—controls melt curtain stability. Draw resonance typically appears as periodic thickness bands in the machine direction when the draw-down ratio exceeds the critical value for the resin's extensional viscosity. For high-MI butene LLDPE, this threshold is lower than for fractional-melt-index grades and decreases as melt temperature increases because extensional viscosity falls. Corrective measures include reducing the air-gap distance, increasing the die lip opening, lowering chill-roll speed relative to melt output, or adding 5–15 wt% high-pressure LDPE with long-chain branching. The LDPE addition introduces extensional hardening but reduces yield strength and changes the seal initiation temperature. The exact draw resonance limit for Marlex® 7308FK depends on die geometry, melt temperature, and film gauge; published data for this specific configuration is limited.

    Surface Additive Migration Continues to Shift Coefficient of Friction During Storage

    Slip additives in Marlex® 7308FK are migratory amides that bloom to the film surface over time and reduce coefficient of friction from an initial unbloomed value to an equilibrium value after storage. Because migration kinetics depend on film crystallinity and ambient temperature, coefficient of friction measured by ASTM D1894 immediately after extrusion may be higher than after 24–72 h of storage at 23°C. Low ambient temperatures slow migration, leading to higher unwinding forces on pallet wrapping lines. In high-speed stretch wrapping, this can produce intermittent film breakage. Converters that process film during cold storage should condition rolls at 20–25°C for at least 24 h before use. Antiblock particles in the formulation also contribute to surface roughness; film haze measured by ASTM D1003 is thickness-dependent and is influenced by the particle size distribution of the antiblock component. Published data for this specific configuration is limited.

    Typical uses of Marlex® 7308FK include thin-gauge cast stretch film for pallet unitization, over-wrap film, and multi-layer cast film tie layers where high melt flow improves layer distribution. In pallet stretch film, the resin is often blended with metallocene LLDPE to balance dart impact and tear propagation; the high melt index of 7308FK allows a larger fraction of recycled edge trim to be incorporated without exceeding extruder pressure limits. The material can be processed at thicknesses down to 10 μm, where the lower melt strength is offset by rapid quench and support from adjacent layers. Stretch wrapping machines commonly operate at pre-stretch ratios of 150–250%; films based on butene LLDPE are more prone to stress relaxation than films containing octene or metallocene LLDPE, so the final retention force is lower unless the film is blended.

    Across the broader LLDPE resin family, the technical separation arises primarily from comonomer length and molecular weight distribution. Hexene LLDPE grades at equivalent density typically provide higher dart impact and improved Elmendorf tear balance because the longer hexene branches increase tie-chain density. Metallocene LLDPE grades provide superior optical properties and lower extractables because of their narrow molecular weight distribution and uniform comonomer incorporation; however, their narrow distribution can increase melt pressure and melt fracture sensitivity at equivalent melt index. Marlex 7308FK, with broad molecular weight distribution and slip/antiblock formulation, is positioned for high-speed cast film where processing ease and surface slip are prioritized over ultimate tear resistance. Table 2 presents generic comparative ranges, not lot-release data for specific commercial grades; product-specific values should be taken from the relevant supplier certificate.

    Table 2. Comparative technical boundaries for LLDPE film resin families
    ParameterMarlex® 7308FK Butene LLDPEHexene LLDPE Cast Film GradeMetallocene LLDPE Cast Film Grade
    Nominal density0.918 g/cm³0.917–0.920 g/cm³0.912–0.918 g/cm³
    Nominal melt index range8.0 g/10 min2.5–3.5 g/10 min1.0–4.0 g/10 min
    Molecular weight distributionBroad, Ziegler-NattaBroad, Ziegler-NattaNarrow, single-site
    Dart impact per ASTM D1709ModerateHigher at equivalent gaugeHigher at equivalent gauge
    Elmendorf tear per ASTM D1922Directionally anisotropicImproved balanceImproved balance
    Optical haze per ASTM D1003Low to moderateLowLowest for given density
    Additive packageSlip and antiblockUnmodified or tailoredUnmodified or tailored

    Interfacial flow instabilities become the dominant concern when Marlex® 7308FK is coextruded into a skin/core/skin structure with a high-viscosity metallocene resin. If the high shear viscosity mismatch at the feedblock is too large, film quality defects such as nonuniform layer thickness or wood-grain surface patterns may appear. Coextrusion feedblocks with adjustable layer thickness and separate melt-temperature control are recommended when the viscosity ratio exceeds 2:1. Polyethylene to polyethylene adhesion in the melt is generally high, but the slip additive in 7308FK can bloom to the interface after solidification, which may reduce lamination bond strength in subsequent thermal lamination operations if the lamination temperature is below 120°C. Surface treatment by corona discharge at 38–42 dyn/cm is used before printing or metallization, and the slip additive can limit the achievable wetting tension if allowed to bloom before treatment.

    Incoming quality control for Marlex® 7308FK is based on melt index and density as primary lot-release values. The converter should record lot-specific melt index and slip additive concentration because batch-to-batch variation in additive feed can shift coefficient of friction performance without changing density or melt flow rate. In a production environment, if a new lot has a melt index at the upper end of the supplier's specification, the extruder screw speed needed to maintain target output may decrease; if the melt index is at the lower end, head pressure and melt temperature may increase. The absence of a standard test for additive surface concentration makes it necessary to track the time after extrusion at which the coefficient of friction reaches equilibrium. This is a production-scale failure mode: film may pass in-line inspection but later exhibit excessive blocking or insufficient unwind slip after storage.

    Pellets kept in an unheated warehouse and then transferred to a heated production area present a condensation risk. Although LLDPE is not hygroscopic, moisture on cold pellet surfaces can introduce steam into the extruder and create surface defects if the resin is moved directly into processing in cold weather. A minimum conditioning period of 12 h in the production hall is recommended, and storage temperatures should remain below 50°C to reduce additive loss or pellet agglomeration.

    Food-contact evaluation of Marlex® 7308FK follows olefin polymer provisions under 21 CFR 177.1520 and EU Regulation No 10/2011 when the finished article meets overall migration limits, typically 10 mg/dm². Users must verify condition-of-use restrictions for fatty foods and for retort or microwave applications because slip additive migration and oxidative by-products can exceed specific migration limits if the article is exposed to temperatures above the intended service temperature. The resin is not intended for medical implant applications. Combustion off-gases include carbon monoxide and carbon dioxide; processing ventilation must be provided. The safety data sheet, not this narrative, governs storage, handling, and disposal.

    Top