| HS Code | 496302 |
| Product Name | Chevron Phillips Marlex® 7308DK Polyethylene; LLDPE |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene |
| Density | 0.918 g/cm3 |
| Melt Index | 0.80 g/10 min |
| Melt Flow Ratio | 30 |
| Melting Point | 122 deg C |
| Vicat Softening Point | 100 deg C |
| Tensile Strength At Yield | 9.7 MPa (1400 psi) |
| Tensile Strength At Break | 27.6 MPa (4000 psi) |
| Elongation At Break | 700% |
| Flexural Modulus | 276 MPa (40000 psi) |
| Elmendorf Tear Strength Md | 250 g/mil |
| Elmendorf Tear Strength Td | 400 g/mil |
| Dart Drop Impact | 150 g |
| Haze | 10% |
| Gloss 45 Deg | 60 |
As an accredited Chevron Phillips Marlex® 7308DK Polyethylene; LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® 7308DK LLDPE is typically supplied in 25 kg multiwall bags or 1,000 kg bulk bags, palletized. |
| Container Loading (20′ FCL) | 20′ FCL loaded with 25 kg bags of Chevron Phillips Marlex® 7308DK Polyethylene (LLDPE), palletized, stretch-wrapped; approx. 18–20 MT net. |
| Shipping | Chevron Phillips Marlex® 7308DK LLDPE ships as non-hazardous polyethylene resin pellets. Standard packaging includes 25 kg bags or 1,000 kg bulk bags, palletized. Transport by truck or rail in clean, dry conditions; store away from heat, moisture, and contamination. No special DOT/UN shipping classification required. |
| Storage | Store Chevron Phillips Marlex® 7308DK LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers or bags clean, closed, and clearly labeled. Prevent moisture pickup, dust accumulation, and static discharge during transfer by grounding/bonding. Use stable stacking, avoid incompatible materials, and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is indefinite if stored in a cool, dry, well-ventilated area away from direct sunlight and ignition sources. |
Chevron Phillips Marlex® 7308DK is processed as a linear low-density polyethylene film resin. Published technical literature lists a nominal density of 0.918 g/cm³ when determined in accordance with ASTM D1505, and a nominal melt index of 0.80 g/10 min at 190 °C with a 2.16 kg load per ASTM D1238. In blown film installation, the resin is commonly introduced through a 24:1 to 30:1 L/D single-screw extruder with a barrier screw and a Maddock mixing section. Melt temperature at the die is controlled within 190 °C to 220 °C. A die gap of 1.8 mm to 2.5 mm is typical. The bubble is expanded at a blow-up ratio of 2.0:1 to 3.0:1. On a 300 mm annular die, the frost line height is normally held between 0.65 m and 1.10 m above the die face. The combination of die gap, blow-up ratio, and frost line height determines the orientation balance and the final drop mass for thin-gauge film. The grade is suited to applications where puncture resistance and seal behaviour must be balanced against draw-down and bubble stability.
On high-stalk grocery sack lines, the practical output ceiling is controlled by bubble cooling rather than by screw capacity. If the frost line is raised above 1.2 m, the unsupported molten bubble becomes sensitive to ambient air currents and die-lot chatter. The result is transverse-direction gauge variation. Film produced with a target gauge of 25 µm on a 300 mm die at a blow-up ratio of 2.5:1 can drift from 22 µm to 28 µm across the circumference when the frost line is not stabilised. High-stalk configurations use internal bubble cooling and a close-fitting outer air ring. The extruder back pressure on a 30:1 L/D barrier screw typically falls between 18 MPa and 30 MPa at 80 rpm. Increasing screw speed beyond the point where the bubble fails to cool causes the stalk to oscillate at 0.5 Hz to 1.5 Hz. This oscillation is transferred into the collapsing frame and becomes visible as film sag in the haul-off. Melt fracture on the inner or outer bubble surface occurs if the die gap is reduced below 1.6 mm while the melt temperature is held below 190 °C. The material’s melt fracture threshold under these conditions is influenced by die land length. A land length of 10 mm to 15 mm on the annular lip is commonly used. For stable high-stalk operation, the melt temperature is raised to 210 °C to 220 °C, but this raises total heat load and reduces bubble stiffness. Output per die circumference is typically not pushed beyond 0.35 kg/h per mm die diameter when the target gauge is thin. Dart impact of the resulting 25 µm film, measured by ASTM D1709-15A Method A, is routinely specified by converters as ≥ 90 g for grocery sacks, while some converter specifications require ≥ 120 g for high-stalk LLDPE. The specific value for 7308DK will depend on die gap, blow-up ratio, and internal bubble cooling; published data for this specific configuration is limited.
Blending 7308DK with high-pressure LDPE in the range of 20 wt% to 30 wt% is a production-scale method for stabilising heavy-duty sack film. The addition of LDPE increases melt strength and widens the operating window at high gauge. On a 90 mm grooved-feed extruder with 30:1 L/D, the compound is run at melt temperatures of 200 °C to 230 °C. The die gap is held at 2.0 mm to 2.8 mm. Back pressure at 95 rpm is typically 25 MPa to 35 MPa, depending on the screen pack configuration. A screen pack of 60/80/100 mesh is replaced at intervals of 8 h to 12 h when recycled edge trim exceeds 10 wt%. Film gauge for heavy-duty sacks is commonly set at 75 µm to 150 µm. At these thicknesses, heat removal through the bubble becomes the limiting factor. Increasing throughput by raising melt temperature above 230 °C causes the bubble to sag and reduces transverse-direction tension. The bubble is operated at a blow-up ratio of 2.2:1 to 2.8:1. The frost line is kept low, at 0.5 m to 0.8 m, to increase transverse-direction orientation and improve Elmendorf tear measured per ASTM D1922-09. In practice, the MD/TD tear imbalance is maintained below 1.5:1 by adjusting the collapsing frame height. Heavy-duty sack converters often require a dart impact value of ≥ 200 g for 100 µm film tested under ASTM D1709-15A Method B. This value is not a single-material constant; it is controlled by blending ratio, die gap, and cooling rate. A blend containing 25 wt% LDPE and 75 wt% 7308DK is a common starting point on high-output lines. Adding more than 30 wt% LDPE is avoided in some plants because it increases low-tension transverse-direction splitting during sack opening. Batch-to-batch variation in the melt index of the LDPE component can shift the bubble’s neck height by 50 mm to 100 mm; therefore the extruder operator must re-check the frost line after resin lot changes.
In vertical form-fill-seal service, the lower melting point of LLDPE compared with high-density polyethylene creates a broad seal window but also demands careful jaw temperature control. Film from 7308DK is converted at gauge 50 µm to 80 µm. The seal initiation temperature on a standard laboratory hot-tack tester in accordance with ASTM F1921 is typically recorded between 95 °C and 105 °C for LLDPE film. Production seal jaws are set at 115 °C to 130 °C, with dwell times of 0.3 s to 0.6 s and seal pressure from 0.25 MPa to 0.50 MPa. Because the material is a linear resin, its hot tack strength after 0.5 s dwell is generally lower than an ionomer or a metallocene LLDPE with a higher comonomer fraction. This places a constraint on packaging speeds above 80 packs/min on vertical machines when product mass exceeds 1 kg. The failure mode shifts from cohesive peel to interfacial release if the seal jaw temperature falls below 100 °C. On start-up, thermally induced seal contamination on the jaws appears when the film is sealed above 140 °C for periods longer than 2 s. For food-contact packaging, the formulated film must meet the extractives limits of FDA 21 CFR 177.1520 and the overall migration limit of 10 mg/dm² specified in EU Regulation (EU) No 10/2011. Slip and antiblock masterbatches are often introduced at 2 wt% to 4 wt% to control coefficient of friction without exceeding the migration limits. The seal strength on packaging is commonly specified as ≥ 15 N/25 mm when tested at 200 mm/min jaw separation speed. However, the precise value is affected by the seal jaw profile and chill-roll finish, and published data for this specific configuration is limited.
Melt oxidation is the primary adhesion mechanism in extrusion lamination and coating of 7308DK to primed aluminium foil and polyester films. The resin is processed through a 90 mm to 120 mm single-screw coating extruder at melt temperatures of 300 °C to 320 °C, measured at the adapter. The air gap between the die and the chill roll is maintained at 200 mm to 300 mm. At line speeds of 150 m/min to 300 m/min, the coating weight is controlled between 15 g/m² and 25 g/m². The high processing temperature accelerates carbonyl formation on the melt surface, which improves adhesion to a polyurethane or polyethylene imine primer. If the melt temperature falls below 300 °C, adhesion to aluminium foil can drop below 1.5 N/15 mm as measured by ASTM D1876, which is insufficient for liquid-pouch laminations. Raising the temperature above 320 °C creates odour and smoke that can contaminate food-contact laminates. In addition, the melt curtain loses tensile strength at high temperature, causing draw resonance at speeds above 250 m/min. This is observed as periodic thickness bands at 10 Hz to 20 Hz on the coated web. To suppress draw resonance, the die lip gap is adjusted to 0.4 mm to 0.7 mm and the melt temperature is reduced to 305 °C to 310 °C. The use of a backup roll with a matte finish is common when the coated surface must receive water-based ink. The substrate must be pre-treated to a surface energy of 38 mN/m to 42 mN/m. For woven polypropylene sack lamination, a coating layer of 20 µm to 30 µm is applied directly to the fabric. The fabric must be dried to a moisture content below 0.1 wt% to prevent steam-driven pinholes in the coating. Published data for 7308DK in this exact configuration is limited, but processing requirements are broadly consistent with LLDPE coating grades.
Extending gauge to 150 µm to 200 µm is standard for agricultural silage cover and greenhouse film. At these thicknesses, the addition of a UV stabiliser masterbatch containing hindered amine light stabilisers is necessary for a 24-month outdoor service life. The masterbatch is dosed at 6 wt% to 12 wt%, depending on pigment loading and the ultraviolet index of the installation site. Feeding accuracy must be maintained within ±0.5 wt% to avoid local degradation of mechanical properties. On a 75 mm grooved-feed extruder, the higher masterbatch loading can cause slip in the feed zone if the temperature of the first barrel zone exceeds 200 °C. Barrel zone temperatures are therefore held at 175 °C to 190 °C in the feed section, while the downstream zones operate at 200 °C to 220 °C. Die pressure rises by 2 MPa to 4 MPa when masterbatch level moves from 6 wt% to 12 wt%. This indicates that viscosity dilution by the masterbatch carrier is not sufficient to offset particle-related flow restriction. The pressure rise is monitored by the melt transducer before the screen changer. The screen pack is upgraded to 40/60/80 mesh to protect the die lips from agglomerated stabiliser particles. Film produced at 180 µm is tested for tensile break strength under ASTM D882, with an acceptance value generally ≥ 25 MPa in both machine and transverse directions. After accelerated weathering under ISO 4892-2, retention of elongation at break above 50% after 3000 h is used as a specification benchmark by some agricultural film buyers. The actual value for 7308DK is masterbatch-dependent. If the UV masterbatch is based on a low-melt-index LDPE carrier, the bubble’s frost line shifts upward by 50 mm to 150 mm; if the carrier is a high-MI LLDPE, the frost line drops. This difference in thermal behaviour forces operators to re-adjust internal bubble cooling air volume after each lot of masterbatch. Anti-fog additives used in greenhouse film are added at 1 wt% to 3 wt% and must be pre-dispersed to prevent surface bloom streaks. The same film structure, when used as silage cover, must resist puncture from protruding feed stems. A dart impact of ≥ 300 g at 200 µm film thickness by ASTM D1709-15A Method B is often demanded. This requirement is achievable only when the film is cooled symmetrically; asymmetric air-ring flow will reduce dart impact by 30% to 40% without changing the average gauge.
For export documentation, the following test designations and compliance statements are required. The actual values must be taken from the batch certificate of analysis rather than from generic literature.
| Standard or regulation | Property or requirement | Typical condition or limit |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymer clearance for food-contact articles | Compliance with extractive limitations for LLDPE under conditions of use |
| EU Regulation (EU) No 10/2011 | Overall migration from food-contact plastic | 10 mg/dm² |
| REACH Regulation (EC) No 1907/2006 | SVHC declaration for EU supply | SVHC concentration below 0.1 wt% per article where applicable |
| RoHS Directive 2011/65/EU | Restricted substance screening for electrical/electronic packaging components | Lead, mercury, cadmium, hexavalent chromium, PBB and PBDE limits as specified by directive |
| ASTM D1238-20 | Melt index | 190 °C, 2.16 kg |
| ASTM D1505 | Density | 23 °C |
| ASTM D1709-15A | Dart impact | Method A or Method B as specified on purchase order |
| ASTM F1921 | Hot tack strength | Seal parameters agreed between converter and packaging line |
Competitive Chevron Phillips Marlex® 7308DK Polyethylene; LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® 7308DK Polyethylene; LLDPE is a linear low-density polyethylene pellet resin intended for blown-film and cast-film structures in which a low melt index contributes to melt strength and in which density is specified to retain flexibility. Two primary release parameters define the material in routine lot acceptance: nominal melt index 0.8 g/10 min determined under 190 °C and 2.16 kg piston load according to ASTM D1238 or ISO 1133-1:2022, and nominal density 0.918 g/cm³ determined according to ASTM D1505 or ASTM D4883. The grade occupies a position below the melt-index range of many general-purpose film LLDPE products and above the density range of plastomers and ionomer sealants. This placement differentiates it from high-flow LLDPE grades, which typically process at lower head pressure but produce lower dart impact in equivalent film structures. Compared with high-pressure low-density polyethylene, 7308DK has no measurable long-chain branching; the resulting extensional viscosity behavior requires greater attention to bubble stability at start-up, but it permits higher draw ratios in cast-film. Compared with metallocene LLDPE of equivalent nominal density, the polymer is expected to show a broader short-chain branching distribution and a broader molecular weight distribution, affecting optics, seal initiation temperature, and extrusion torque. The use must be validated on production-scale equipment because published data for direct comparison to every metallocene and hexene grade is limited.
The material’s value in film extrusion is not fully captured by single-point density and melt index. The comonomer type and short-chain branch placement control the tie-chain concentration in the semi-crystalline network; the resin is associated with the butene or short-chain alpha-olefin LLDPE family, though the exact comonomer declaration appears on the product data sheet. In generic butene LLDPE film grades with density 0.918 g/cm³ and melt index 0.8 g/10 min, the attainable dart impact and Elmendorf tear values are typically lower than in hexene or octene grades at equal density because shorter comonomer units create less effective tie-molecule connectivity. 7308DK is formulated to raise dart impact and machine-direction tear within the butene class by controlling molecular weight distribution and comonomer distribution. The practical consequence for a converter is that the resin can be run on a grooved-feed blown-film line with lower melt temperature than a comparable metallocene grade while still yielding a film with less gel and lower melt fracture. In blown-film equipment with a 75 mm extruder and 300 mm annular die, the resin generally permits stable bubble formation at blow-up ratios between 2.0:1 and 3.0:1, provided die gap is kept in the 1.5–2.5 mm range. This is an operational distinction from higher-melt-index LLDPE products, which may require higher melt temperature or wider die gaps to control melt fracture but lose output stability.
Inspection of certified lot data requires separating specification limits from typical datasheet values. The following representative values are not guaranteed release properties; they are included to support preliminary equipment set-up and comparison with other LLDPE products.
| Property | Test standard | Nominal value |
|---|---|---|
| Density | ASTM D1505 | 0.918 g/cm³ |
| Melt index | ASTM D1238, 190 °C/2.16 kg | 0.8 g/10 min |
| Melting temperature | ASTM D3418 | 122 °C |
| Vicat softening temperature | ASTM D1525 | 102 °C |
Mechanical performance values such as dart impact (ASTM D1709), Elmendorf tear (ASTM D1922), and tensile properties (ASTM D882) are film-gauge dependent. Published neat resin values are not a substitute for film measurements. In monolayer blown film at 25 µm gauge, dart impact may be expected to exceed 700 g and Elmendorf tear values may fall between 300 gf and 500 gf, but these ranges depend on BUR, frost line height, die gap, and melt temperature. The absence of a universal value is a limitation that must be recognized in specification writing.
The processing envelope for 7308DK is constrained by the combination of low melt index and linear backbone. The screw should provide sufficient shear but not excessive residence time. A production extruder with 24:1 to 30:1 L/D and a barrier flight design with spiral or Maddock mixing is appropriate. Recommended barrel set points begin at 40–60 °C in the feed throat, increase to 180–200 °C in the compression zone, and reach 200–220 °C in the metering zone. The adapter and die are typically held at 210–230 °C. A target melt temperature of 190–220 °C is suitable for blown film. Operation above 240 °C with long residence time can cause chain scission, crosslinking, and gel formation; operation below 180 °C may produce melt pressure spikes and die lines. A grooved-feed throat is preferred because the resin’s low melt index reduces drag conveying and increases screw torque. In cast-film or extrusion coating, die temperatures are typically 240–280 °C to reduce melt viscosity and improve curtain stability. The addition of a melt pump between screw tip and die can reduce pressure fluctuation; melt pump suction pressure should be maintained above 30 bar to avoid cavitation.
| Processing parameter | Recommended range | Equipment basis |
|---|---|---|
| Extruder L/D | 24:1–30:1 | Single-screw blown-film extruder |
| Feed throat temperature | 40–60 °C | Grooved-feed section |
| Compression zone temperature | 180–200 °C | Barrier screw compression zone |
| Metering zone temperature | 200–220 °C | Barrier screw metering zone |
| Adapter and die temperature | 210–230 °C | Annular die |
| Melt temperature | 190–220 °C | Infrared melt probe |
| Die gap | 1.5–2.5 mm | Annular die |
| Blow-up ratio | 2.0:1–3.0:1 | Air ring and bubble cage |
| Frost line height | 2–4 die diameters | Adjustable cooling air |
Blown-film bubble stability is controlled by die gap, blow-up ratio, and frost line height. For a die diameter of 300 mm, a die gap of 2.0 mm and BUR of 2.5:1 give an approximate film lay-flat width of 1180 mm; frost line height is generally held at 2–4 die diameters for film below 50 µm. Higher frost lines allow more MD orientation and increase MD tear, but can reduce dart impact. The resin’s crystallization onset measured by differential scanning calorimetry is near 105 °C; cooling air at 10–25 °C and air ring pressure sufficient to produce a uniform frost line are required. On a 75 mm grooved-feed extruder running a 300 mm die, head pressures of 300–400 bar may be observed at melt temperatures near 200 °C; this is a normal consequence of the 0.8 g/10 min melt index. At 190 °C, the apparent shear viscosity is in the range 800–1200 Pa·s at 100 s⁻¹; the flow activation energy of linear polyethylene is approximately 27–30 kJ/mol, so melt temperature changes produce smaller viscosity changes than in polar resins. When screw speed is increased, shear heating can exceed barrel cooling capacity; deeper metering channels reduce melt temperature rise under high output.
In high-speed bag conversion, the film is subjected to abrupt tension spikes at gusset punches, seal bars, and winder transfers. If the machine-direction Elmendorf tear value measured under ASTM D1922 falls below the converter’s critical threshold, the failure mode is normally a split that originates at a punched hole or at the heat-seal edge. 7308DK is selected for such lines because its low melt index supports orientation-induced strengthening of the machine direction. To maintain this property, the converter should avoid excessively high frost lines and should keep BUR at 2.3:1–2.8:1; this balances MD and TD orientation. At 40 µm gauge, a film with higher MD tensile strength may permit winding tension increments of 10–15% compared with cast film of equivalent thickness, but the actual tension set point must be validated with the winder’s load cells. The difference from high-density polyethylene is that the lower density of 7308DK reduces film stiffness; the same winder tension produces larger elongation, so dancer control gains often require adjustment. In multi-layer structures, the resin is commonly used in the skin layer rather than the sealant layer because its seal initiation temperature is higher than EVA or ionomer sealants. Seal initiation should be measured by heat-seal testing according to ASTM F88 or ASTM F2029, not inferred from DSC alone.
Silo storage and drying requirements for 7308DK are uncomplicated. Polyethylene does not hydrolyze, but surface moisture from high-humidity air can produce steam bubbles and melt pressure fluctuation. At RH above 60%, pellets should be purged with warm, dried air at 40–50 °C for 2–4 h before use. Incompatibilities include some antistatic amines and certain peroxide masterbatches that can alter the melt index and shift the balance of dart impact and tear. Food-contact use requires verification of the fabricated article under FDA 21 CFR 177.1520 and any applicable European Union measures; compliance is not a property of the resin alone. The material is not intended for applications requiring sustained ultraviolet aging resistance unless the film contains an adequate UV stabilizer package.