Chevron Phillips Marlex 7120x Hexene Linear Low Density Polyethylene Blown And Cast Film

Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film

    • Product Name: Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 901516
    Productname Chevron Phillips Marlex 7120X
    Polymertype Hexene Linear Low Density Polyethylene
    Comonomer 1-Hexene
    Recommendedprocess Blown and Cast Film
    Density 0.918 g/cm³
    Meltindex 1.0 g/10 min (190°C/2.16 kg)
    Meltingpoint 124 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyieldmd 10.3 MPa
    Tensilestrengthatyieldtd 10.3 MPa
    Tensilestrengthatbreakmd 27.6 MPa
    Tensilestrengthatbreaktd 24.1 MPa
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Elmendorftearmd 300 g
    Elmendorfteartd 500 g
    Dartdropimpact 120 g
    Haze 12%
    Gloss45degree 50%
    Coefficientoffriction 0.2

    As an accredited Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Marlex 7120X Hexene LLDPE is supplied in 25 kg bags or 1,000 kg bulk bags, palletized for shipping.
    Container Loading (20′ FCL) 20′ FCL: palletized 25kg bags of Chevron Phillips Marlex® 7120X hexene LLDPE, blown/cast film; shrink-wrapped, dry, secured, approx. 18–20 MT.
    Shipping Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film, is generally shipped as non-hazardous resin pellets in 25-kg bags or 1,000-kg bulk bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Store and transport cool, dry, clean, away from moisture, contamination, and direct sunlight.
    Storage Store Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene in a cool, dry, well-ventilated area. Keep containers closed and away from direct sunlight, heat, sparks, flames, and oxidizing agents. Prevent moisture, contamination, and dust accumulation. Use appropriate grounding when handling. Maintain clean, labeled containers. Observe local regulations and the manufacturer’s SDS for safe storage and shelf life.
    Shelf Life Shelf life is indefinite if stored in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources.
    Application of Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film

    What Limits Load Retention in Cast Pallet Unitization Film?

    Cast pallet stretch film production with Marlex® 7120X is run on high-speed cast lines where chill roll temperature and melt profile govern gauge uniformity and cling stability. On a five-layer cast coextrusion line with die width of 2,400–2,800 mm and chill roll setpoint of 18–24°C, the skin layers are formulated with 85–100 wt% Marlex® 7120X, 0–10 wt% LDPE, and 0.5–2.5 wt% polyisobutylene-based cling additive masterbatch. If cling additive concentration exceeds 2.5 wt%, unwind force under ASTM D5458-18 rises above 3.0 N/cm and roll blocking increases in warehouse storage at ambient temperatures above 30°C; below 0.5 wt%, load shift during transit exceeds the retention window required by automated palletization. Melt temperatures are held at 210–245°C on cast lines running at 300–600 m/min; excursions above 250°C degrade the polyisobutylene cling species and reduce cling force by more than 15% after 48 h of roll aging. Chill roll temperature below 12°C raises quench-related surface haze under ASTM D1003-13, while temperature above 30°C slows crystallization and increases blocking. Puncture resistance under ASTM D5748-19 and tensile properties under ISO 527-3:2018 are used for incoming film qualification, while edge trim at 8–12% of web width is reintroduced into the core layer at 0–15 wt% without measurable puncture loss. Terminal product types include hand wrap film, machine stretch wrap, and pre-stretched pallet wrap used in logistics and distribution.

    Layer positionMarlex® 7120X proportionCo-additive windowMeasured change under standard
    Skin85–100 wt%Cling masterbatch 0.5–2.5 wt%; LDPE 0–10 wt%Cling force 1.5–3.0 N/cm under ASTM D5458-18
    Core100 wt% plus reclaimed trim 0–15 wt%No cling additivePuncture reduction <5% at 15 wt% reclaim under ASTM D5748-19
    Skin85–100 wt%Same as first skin layerGauge band deviation ±1.0 µm at 20 µm nominal

    On blown film lines equipped with oscillating haul-off units and internal bubble cooling, hexene LLDPE silage wrap is processed at blow-up ratios of 2.2–2.8:1, die diameters of 250–400 mm, and melt temperatures of 195–225°C. Multilayer structures containing 96–99 wt% Marlex® 7120X with 0.3–0.8 wt% hindered amine light stabilizer masterbatch and 0.2–0.5 wt% polymer processing aid are used for round bale wrap. Film thickness commonly ranges from 25–40 µm; tear propagation resistance measured according to ISO 6383-2:1983 is required to remain above the minimum values set in EN 13206:2017 for thermoplastic films used in agriculture. The processing aid loading above 0.5 wt% reduces die lip deposit on the 300 mm die but can lower cling in a coextruded tack layer, which is limited to 5–10 wt% of total thickness. UV stabilization packages are validated by ISO 4892-2:2021 accelerated weathering followed by residual elongation at break under ISO 527-3:2018. Field failure modes such as punctures at bale corners and splitting along the machine direction are monitored because they are more sensitive to film orientation than to thickness alone. Terminal product types include round bale silage film, pit sealing sheets, and greenhouse tunnel films where tear resistance and UV retention are specified for seasonal exposure.

    Form-Fill-Seal Food Contact Compliance and Seal Integrity

    For high-speed form-fill-seal converters, Marlex® 7120X is configured as three-layer blown film or five-layer cast film with sealant webs comprising 70–100 wt% Marlex® 7120X, 0–20 wt% LDPE to modify seal initiation, and 0.5–2.0 wt% slip/antiblock masterbatch. Seal strength is measured under ASTM F88/F88M-21; hot tack performance is measured under ASTM F1921-18 to avoid seal pop-open at high fill speeds. The film surface is corona-treated to 38–42 mN/m inline before lamination or printing. Food contact compliance is maintained under FDA 21 CFR 177.1520(c) for olefin polymers and Commission Regulation (EU) No 10/2011 for plastic materials intended to contact food, with overall migration below 10 mg/dm². Frozen food packaging qualification adds dart impact testing under ASTM D1709-16a Method B at -18°C; films that develop microcracking at this temperature are rejected because seal and barrier continuity fail after transportation vibration testing. Terminal product types include frozen vegetable bags, cereal liner films, snack packaging, and liquid pouch stock.

    Standard or regulationCited clause or test methodParameterAcceptance window
    FDA 21 CFR177.1520(c)Olefin polymer clearance for food contactComplies with specified food types and conditions of use
    Commission Regulation (EU) No 10/2011Annex I and overall migrationOverall migration< 10 mg/dm²
    ASTM F88/F88M-21Seal strengthPeel seal strengthApplication-specific; liquid pouches commonly > 15 N/25 mm
    ASTM F1921-18Hot tackHot tack force at seal temperatureSeal initiation window 10–15°C wider than LDPE reference in blend trials

    Where high bubble stability and dart impact above 1,000 g at 200 µm gauge are required, industrial sack liners and FIBC films use monolayer or coextruded blown film formulations based on 65–90 wt% Marlex® 7120X, 10–30 wt% LDPE or mLLDPE, and 0–5 wt% carbon black or antistatic masterbatch. The compounds are extruded through die gaps of 1.8–2.5 mm at BUR of 3.0–4.0:1 and melt temperatures of 180–220°C. Dart impact is measured under ASTM D1709-16a, Elmendorf tear under ASTM D1922-15, and secant modulus under ISO 527-3:2018 for converter specifications. Carbon black masterbatch addition above 5 wt% reduces bubble stability and can produce melt fracture on single-screw lines with L/D 24:1; lines with L/D 30:1 or barrier screws are used to maintain output without adding processing aids. Reclaimed edge trim is maintained below 10 wt% because reclaim streams with higher gel formation reduce dart impact at welded seams. Terminal product types include flexible intermediate bulk container liners, chemical sack liners, and industrial inner liners for bulk packaging.

    When 7120X Replaces LDPE in Coextruded Surface Protection Film

    In applications requiring controlled peel adhesion from polished metal and rigid polymer panels, Marlex® 7120X is used in the carrier layer of coextruded cast surface protection film. The carrier formulation contains 90–100 wt% Marlex® 7120X, while the coextruded or coated pressure-sensitive adhesive layer contains an ethylene-vinyl acetate or thermoplastic elastomer component at 2–10 wt% of total film weight. Peel adhesion is measured under ASTM D3330/D3330M-04 Method A and is typically maintained between 0.5–1.5 N/cm for non-marring removal from polished aluminum and acrylic. The cast line includes a 2,000 mm die, polished chill roll at 20–25°C, and line speed of 80–180 m/min. Capacitance-based thickness scanning is used to maintain gauge uniformity at ±1 µm; deviations beyond this range produce adhesive transfer and inconsistent unwind tension. Industrial assembly film compliance references REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU; food contact is not claimed for this construction. Terminal product types include protective masking for stainless steel panels, pre-coated aluminum building sheets, and rigid PVC profiles.

    After incorporation of calcium carbonate masterbatch to yield 40–60 wt% filler loading in the final compound, the hexene LLDPE substrate is cast and subsequently stretched in the machine direction at draw ratios of 2.0–3.5:1 and oven temperatures of 60–80°C on a cast film line fitted with an in-line machine-direction orientation unit. Water vapour transmission rate is measured under ASTM E96/E96M-22; tensile properties are measured under ISO 527-3:2018. For hygiene backsheet laminates, calcium carbonate dispersion below 8 µm top-cut and average particle diameter of 1.5–2.0 µm are required to prevent pinhole formation at 25 g/m² basis weight. Screen pack blockage occurs when dispersion quality degrades or when reclaim containing gel is added above 10 wt%. Cytotoxicity testing under ISO 10993-5:2009 is applied when the laminate is intended for medical drapes, although published data for this specific resin in medical laminates is limited. Terminal product types include diaper backsheets, breathable laminate films for underpads, and personal protective garment films.

    Free Quote

    Competitive Chevron Phillips Marlex® 7120X Hexene Linear Low Density Polyethylene, Blown and Cast Film prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® 7120X is a hexene linear low density polyethylene specified for blown and cast film extrusion. The resin carries a nominal density of 0.912 g/cm³ when tested under ASTM D1505 and a nominal melt index of 2.0 g/10 min when tested under ASTM D1238 at 190 °C/2.16 kg. The hexene comonomer introduces butyl short-chain branches along the linear backbone; this molecular structure produces a lower-density film resin without the melt strength characteristics of an equivalent melt-index LDPE. In blown film converting, the grade is used in monolayer and coextruded structures where tear resistance, dart impact, and low-temperature flexibility are required. In cast film converting, the same melt-flow class permits stable web formation at higher line speed when extruder, chill roll, and air gap parameters are held within the specified operating envelope.

    PropertyTest methodNominal value
    DensityASTM D15050.912 g/cm³
    Melt indexASTM D12382.0 g/10 min at 190 °C/2.16 kg
    ComonomerSupplier specificationHexene
    FormVisual inspectionCylindrical pellets

    For incoming lot verification, a two-point melt index test under ASTM D1238 at 2.16 kg and 21.6 kg is often used to monitor lot-to-lot rheological consistency. The melt index ratio of this class of hexene LLDPE is generally above 25, although a lot-specific upper limit is not a fixed resin specification. Capillary rheometry on a twin-bore instrument can be used to map apparent shear viscosity at 190 °C, 210 °C, and 230 °C; the apparent viscosity declines sharply between 100 s⁻¹ and 1000 s⁻¹, which supports stable flow in narrow die gaps. Published data for this specific configuration is limited, so converter validation remains necessary for any narrow-window application.

    Mechanical, optical, and tear values of the converted film are not fixed resin constants. Dart drop impact, puncture resistance, and tensile properties are determined after film formation and are strongly influenced by blow-up ratio, frost line height, cooling rate, die gap, and downstream orientation. For this reason, comparisons with other products should be based on films produced under matched conditions rather than on pellet data alone.

    What Distinguishes a Hexene Copolymer from Butene-Based Linear Low Density Grades?

    At equivalent density and melt index, butene-based LLDPE grades introduce ethyl short-chain branches, whereas hexene-based grades introduce butyl short-chain branches. The longer branch in Marlex® 7120X disrupts the regularity of the orthorhombic crystal lattice more effectively while still permitting tie-chain formation between lamellae. This structural difference is the primary reason why film made from this resin tends to show higher dart drop impact under ASTM D1709 and higher Elmendorf tear under ASTM D1922 than many butene copolymers. On production lines, the replacement of a butene LLDPE with Marlex® 7120X can allow gauge reduction of 10–20 % while maintaining puncture resistance; the actual downgauging limit must be confirmed on the target blown film line because air ring configuration, die gap, and melt temperature profile alter orientation and cooling history.

    Compared with metallocene LLDPE grades of similar density, the broader molecular weight distribution of Marlex® 7120X contributes to greater shear thinning and can reduce motor load in grooved-feed extruders. Metallocene grades typically provide narrower molecular weight distribution, lower extractables, and higher gloss under ASTM D2457, but they may exhibit lower melt strength and less stability in tall-stalk blown film. Compared with LDPE of similar melt index, Marlex® 7120X typically provides higher dart impact under ASTM D1709 and higher tensile strength under ASTM D882, but lower melt strength and more limited bubble stability in high-stalk configurations.

    On blown film lines equipped with 50–65 mm single-screw extruders and 24:1 to 30:1 L/D ratios, the following starting ranges are used for this density and 2.0 g/10 min melt index class. The values are not grade-specific guarantees; each line must be optimized based on screw design, die diameter, air ring type, and film thickness.

    Process variableBlown film starting rangeCast film starting range
    Barrel zone 1 temperature160–180 °C180–200 °C
    Adapter and die temperature200–220 °C210–240 °C
    Melt temperature190–220 °C210–240 °C
    Die gap1.0–2.0 mm0.4–0.8 mm
    Chill roll temperatureNot applicable15–28 °C
    Blow-up ratio2.0:1–2.5:1Not applicable

    Internal bubble cooling systems on high-output blown film lines may require a slightly higher blow-up ratio to stabilize the less stiff bubble of a 0.912 g/cm³ resin. Frost line heights in the range of 10–35 cm are common, but taller frost lines reduce film clarity because a slower quench allows lamellar crystals more time to grow. External air rings with soft lip air are often selected for LLDPE to prevent bubble flutter. Grooved-feed extruders improve throughput with this material because pre-drying is not required.

    When the Resin Is Down-Gauged Below 25 µm

    Below 25 µm, the processing window narrows. Melt fracture, web carrying capacity, and gauge variability become the principal limitations. The 2.0 g/10 min melt index supports adequate shear thinning in thin die gaps, but addition of a fluoropolymer processing aid at 200–500 ppm may be required if surface melt fracture appears as sharkskin at high extruder speed. Die pressure should be monitored because excessive pressure in a 1.0 mm gap can exceed the drive limit of smaller extruders. In cast film, the air gap and die-to-chill roll distance should be minimized to control neck-in and draw resonance. Draw ratios above 10:1 can induce periodic thickness variation unless the chill roll speed is ramped gradually and the melt temperature is held near 230 °C. Under such conditions, film properties must be rechecked using ASTM D1709, ASTM D1922, and ASTM D882, because downgauging alters machine-direction and transverse-direction orientation.

    Cast film produced from Marlex® 7120X is frequently used in monolayer structures and coextruded sealing skins because rapid chill roll quenching produces low haze and high clarity. The chill roll temperature range of 15–28 °C maintains a surface finish determined by the roll texture. If the chill roll temperature is too low under humid ambient conditions, condensation may form on the web path before winding. If the chill roll temperature is too high, blocking may occur at the winder. The die gap should be matched to the final film thickness, and line speed must be synchronized with the chill roll drive to avoid wrinkles. Cast film processes require precise tension control in the secondary treater and winder but do not require the internal bubble air control used in blown film.

    Optical Quality, Haze, and Antiblock Loading

    Film haze in Marlex® 7120X is influenced less by the base resin than by processing rate and additive package. Blown films made without antiblock can show haze below 5 % under ASTM D1003 at 50 µm, but this value is a conversion-dependent result and not a resin guarantee. Gloss measured under ASTM D2457 is generally higher for cast film than for blown film because the chill roll quench reduces surface roughness. When an antiblock concentrate is added at 2–5 wt%, the blocking force measured under ASTM D3354 decreases, while haze increases as a function of antiblock particle size and loading. Slip agents such as erucamide or oleamide are incorporated only when the end use requires a coefficient of friction below the base resin value. Migratory slip additives should be validated because bloom is time-dependent and can alter downstream printing, lamination, and seal strength.

    Blending with LDPE is common on blown film lines to improve bubble stability and widen the operating temperature range. A blend of 70–90 wt% Marlex® 7120X with 10–30 wt% LDPE lowers melt strength variation during bubble inflation and can permit a more forgiving frost line height. The blend also shifts seal initiation temperature, measurable by differential scanning calorimetry, because the LDPE component broadens the melting range. In coextruded structures, the resin is used in skin and core layers where sealing performance and toughness are required; adjacent layers should be selected to avoid a melt index mismatch exceeding 0.5–1.0 MI units. The resin is not a retort-grade material for high-temperature hot-fill or retort structures, and the entire polyolefin structure must be assessed for such applications.

    Recycled Content Above 30 wt% Is Not Recommended Without Line-Specific Validation

    Marlex® 7120X does not require drying before processing. If pellets are stored below the dew point, condensation on pellet surfaces can introduce visible moisture streaks in the film; therefore, silo and hopper surfaces should be maintained above the ambient dew point or purging should continue until the film clears. The resin should be protected from prolonged direct sunlight because ultraviolet exposure can degrade the pellet surface and increase gel formation. Short-term melt temperature excursions above 240 °C are typically tolerated, but sustained melt temperatures above 260 °C can initiate oxidative chain scission and gel generation. If the line is stopped, the resin should be purged with a lower melt index LDPE to prevent carbonized material in the die. Clean recycled edge trim and film scrap can be reintroduced at levels up to 20–30 wt% if the regrind is free of contamination and has not undergone repeated thermal cycles. Higher regrind fractions reduce dart impact and can increase gel counts in thin film. For food-contact use, the converter must verify that the formulation and any recycled content comply with FDA 21 CFR 177.1520 and, for European Union markets, EU Regulation No 10/2011. The supplier should be consulted for specific REACH and food-contact documentation.

    Top