| HS Code | 720864 |
| Product Name | Chevron Phillips Marlex® 7109M LLDPE Blown Film Resin |
| Manufacturer | Chevron Phillips Chemical Company LP |
| Brand | Marlex |
| Grade | 7109M |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Melt Index 190 C 2 16 Kg | 0.9 g/10 min |
| Density | 0.918 g/cm³ |
| Melting Point | 121 °C |
| Vicat Softening Point | 93 °C |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Break Md | 27.6 MPa |
| Tensile Strength At Break Td | 24.1 MPa |
| Elongation At Break Md | 600 % |
| Elongation At Break Td | 700 % |
| Dart Drop Impact F50 | 120 g |
| Elmendorf Tear Strength Md | 250 g/mil |
| Elmendorf Tear Strength Td | 400 g/mil |
| Haze | 14 % |
| Gloss 45 | 55 % |
| Coefficient Of Friction | 0.2 |
| Slip | Medium |
| Antiblock | Medium |
| Recommended Processing | Blown Film Extrusion |
| Recommended Film Thickness | 1 mil (25.4 µm) |
As an accredited Chevron Phillips Marlex® 7109M LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 50 lb (22.7 kg) polyethylene bags, palletized and stretch-wrapped; bulk truck or railcar shipments also available. |
| Container Loading (20′ FCL) | 20′ FCL loading: Chevron Phillips Marlex® 7109M LLDPE Blown Film Resin, 25 kg bags, palletized, shrink-wrapped, secured for ocean transport. |
| Shipping | Chevron Phillips Marlex® 7109M LLDPE Blown Film Resin is non-hazardous and not regulated for transport. It typically ships in 25 kg polyethylene bags on pallets, 1,000 kg bulk bags, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from ignition sources and direct sunlight. |
| Storage | Store Marlex® 7109M LLDPE Blown Film Resin in a cool, dry, well-ventilated warehouse at ambient temperature. Keep original containers sealed, palletized, and away from direct sunlight, heat, ignition sources, and oxidizing agents. Protect from moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking; follow first-in, first-out inventory practices. Clean up spilled pellets promptly to prevent slipping hazards. |
| Shelf Life | Two years from manufacture when stored unopened in original packaging in a dry, clean, well-ventilated area below 50°C, away from sunlight. |
Blown film structures qualifying under FDA 21 CFR 177.1520(c) for direct food contact and EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² have been produced with Marlex® 7109M as the dominant sealant-layer resin. In a three-layer A/B/C food packaging web, the sealant layer is typically compounded with 80–100 wt% Marlex® 7109M, 3–5 wt% synthetic silica anti-block masterbatch, 0.5–1.0 wt% erucamide slip masterbatch, and 0.3–0.8 wt% fluoroelastomer processing aid; the core layer contains 50–70 wt% Marlex® 7109M with recovered edge trim and fractional-melt LDPE, while the outer skin contains 20–40 wt% Marlex® 7109M blended with a lower-melt-index LDPE to reduce die lip fouling. The blown film line used for such structures typically employs a single-screw extruder of 45–75 mm screw diameter and 30:1 L/D, spiral mandrel die of 250–400 mm diameter, die gap 1.8–2.5 mm, blow-up ratio 2.2:1–2.8:1, melt temperature 190–230 °C, and frost line height 6–10 die diameters; online thickness control maintains variation within ±2%. Migration compliance under EU 10/2011 is verified using food simulant A (10% ethanol), B (3% acetic acid), and D2 (vegetable oil) under the intended time–temperature condition. The finished webs are converted into frozen vegetable bags, dry-food pouches, bakery film, and cereal box liners, where seal initiation at 100–110 °C and hot-tack strength above 1.8 N/25 mm under ASTM F1921 are required. Direct contact with high-fat foods above 100 °C is not recommended without supplemental fatty-food migration testing. Use of slip additive above 1.5 wt% is avoided because the resultant bloom reduces surface tension below 36 dyn/cm and interferes with print adhesion.
When substituting Marlex® 7109M for LDPE in an elastic stretch hood formulation, machine-direction orientation is governed by blow-up ratio, frost line position, and melt temperature. The resin is typically blended at 60–80 wt% with 20–40 wt% of a lower-density ULDPE or metallocene LLDPE having density 0.902–0.912 g/cm³, while slip and anti-block masterbatches are added at 0.5–1.0 wt% and 1–3 wt% respectively. The high-stalk process is run on a single-screw extruder with 30:1 L/D, die diameter 300–400 mm, die gap 1.5–2.0 mm, melt temperature 195–215 °C, and blow-up ratio 4.0:1–5.0:1. Stalk height is maintained at 18–25 die diameters to obtain sufficient machine-direction orientation; at blow-up ratios above 4.5:1, bubble flapping is observed unless air ring velocity is held at 12–18 m/s and frost line is kept below 20 die diameters. Elastic recovery is measured under ASTM D5459; a typical target is not less than 85% recovery after 200% elongation. For pallet unitization of chemical sacks, antistatic masterbatch at 0.5–1.5 wt% is incorporated to keep surface resistivity below 10^12 Ω/sq under ASTM D257; distribution testing is often governed by ASTM D4169 Assurance Level II truck and rail profiles. The film is converted into stretch hoods for palletized petrochemical resin bags, construction blocks, beverage crates, and white goods.
On production lines with internal bubble cooling, the main limitation is not melt fracture but stalk resonance; when the stalk length exceeds 25 die diameters, gauge bands develop at 1–2 Hz frequency. Reducing die gap to 1.2 mm increases melt pressure to 320–380 bar and may exceed the extruder drive limit. Published data for this specific configuration is limited beyond 4.5:1 blow-up ratio. The finished stretch hood is not used in direct food contact unless tested under EU Regulation 10/2011.
For 25 kg petrochemical sacks and FIBC liner webs, Marlex® 7109M is coextruded in a three-layer structure in which the outer layer carries puncture resistance, the core contains recovered trim, and the inner layer provides seal strength. The outer layer is compounded with 60–70 wt% Marlex® 7109M and 30–40 wt% fractional-melt LDPE; the core layer uses 60–80 wt% Marlex® 7109M with 20–40 wt% reclaimed edge trim; the inner seal layer uses 80–100 wt% Marlex® 7109M with 0.5–1.0 wt% slip masterbatch. The line is operated with die gap 2.0–2.4 mm, blow-up ratio 2.0:1–2.5:1, melt temperature 200–230 °C, and internal bubble cooling; screw diameter 65–90 mm and 30:1 L/D are typical. Film performance is tested under ASTM D1709 Method A, ASTM D1922 Elmendorf tear, ASTM D882 tensile, and ASTM F88 seal strength; industrial packaging acceptance often specifies dart impact not less than 150 g at 100 µm and MD tear not less than 3.5 N.
| Layer | Marlex® 7109M loading | Co-resin/additive | Test method | Typical target |
|---|---|---|---|---|
| Outer puncture skin | 60–70 wt% | LDPE 30–40 wt% | ASTM D5748 | puncture resistance ≥ 45 N |
| Core | 60–80 wt% | Recovered trim 20–40 wt% | ASTM D1922 | MD tear ≥ 3.5 N |
| Inner seal layer | 80–100 wt% | LDPE 0–20 wt%, slip 0.5–1.0 wt% | ASTM F88 | seal strength ≥ 12 N/25 mm |
The formed webs are converted into FIBC liners, chemical shipping sack inners, mineral and fertilizer bag liners, and bulk polymer packaging. At an inner-layer Marlex® 7109M loading above 80 wt%, seal strength is stable at 12–15 N/25 mm, but blocking becomes measurable at ambient temperatures above 35 °C unless anti-block is increased to 3–5 wt%. Downstream converters should verify that the reclaimed trim fraction does not exceed 40 wt%, because gel counts above 0.5 mm become visible in the outer layer and reduce puncture propagation resistance under ASTM D5748.
The service life of round-bale silage wrap and greenhouse cover film is limited by UV stabilizer migration and processing-induced gel formation. In a three-layer agricultural film, the outer UV-stabilized skin contains 65–75 wt% Marlex® 7109M, 20–25 wt% LDPE, and 5–10 wt% UV masterbatch based on HALS and UVA; the core layer contains 50–70 wt% Marlex® 7109M and 30–50 wt% recycled silage film; the cling inner layer contains 70–80 wt% Marlex® 7109M and 20–30 wt% EVA with vinyl acetate content 9–18%. The blown film line is operated at melt temperature 180–210 °C, die gap 1.5–2.0 mm, blow-up ratio 2.5:1–3.0:1, and frost line 5–8 die diameters on a 250–350 mm die with 30:1 L/D extruders. Processing above 220 °C volatilizes the HALS component and produces die-lip oxidation that detaches as amber specks in the finished web; below 175 °C, melt pressure exceeds 350 bar and limits throughput to below 200 kg/h. UV resistance is assessed under ISO 4892-2 or ASTM G154; for silage wrap, the film must retain tensile elongation at break above 300% after 1,500 hours of accelerated weathering. Compliance with EN 13206:2017 covering thermoplastic films for agricultural and horticultural use may be specified by EU buyers. The finished stocks include round silage bale wrap, silage pit covers, greenhouse cover films, and low-tunnel films.
In hot-fill lamination webs, seal integrity is governed by seal initiation temperature, hot-tack force, and the interaction between the sealant web and the laminated substrate. A lamination sealant film for hot-fill stand-up pouches and condiment sachets is formulated with 55–75 wt% Marlex® 7109M, 15–25 wt% fractional-melt LDPE, and 10–20 wt% metallocene LLDPE to shift seal initiation to 100–105 °C while maintaining hot-tack strength above 2.0 N/25 mm at 110 °C under ASTM F1921. Anti-block masterbatch is added at 3–5 wt%, slip masterbatch at 0.5–1.0 wt%, and fluoroelastomer processing aid at 0.3–0.8 wt%. The sealant film is blown with a die gap of 1.8–2.2 mm, blow-up ratio 2.0:1–2.5:1, melt temperature 200–220 °C, and then corona-treated to 38–42 dyn/cm on the lamination side. Lamination to polyester or biaxially oriented polypropylene is performed with 2.0–3.5 g/m² solventless adhesive; extrusion lamination may use an LDPE tie layer of 15–20 µm. The resulting duplex or triplex laminates are converted into hot-fill spout pouches, retortable lidding, and portion packs. Compliance is governed by FDA 21 CFR 177.1520 and EU Regulation 10/2011; specific migration tests for primary aromatic amines from the adhesive are mandatory under EU 10/2011 and are not a function of the polyethylene layer. If the mLLDPE fraction exceeds 20 wt%, the coefficient of friction increases above 0.6 and blocking may occur on high-humidity packaging lines unless anti-block is increased above 5 wt%, which in turn reduces clarity and increases haze above 10%.
After one-sided corona treatment above 50 dyn/cm is applied, a single-layer blown Marlex® 7109M carrier web is used for surface protection of stainless steel panels, aluminum profiles, glass sheets, and high-pressure laminates. The formulation contains 70–85 wt% Marlex® 7109M, 15–30 wt% LDPE for bubble stability, and 1–2 wt% slip masterbatch if roll unwind forces must remain below 30 g/25 mm under ASTM D3330. The film is blown on a 45–65 mm extruder with 28:1–30:1 L/D, die gap 1.2–1.8 mm, blow-up ratio 2.0:1–2.5:1, melt temperature 180–210 °C, and a dual-lip air ring to minimize gauge variation below ±2%. After one-sided corona treatment to 50–56 dyn/cm, a water-based acrylic pressure-sensitive adhesive is applied at 5–15 g/m² dry coat weight and dried in a tunnel at 80–100 °C. The finished protection film is tested for 180° peel adhesion on stainless steel under ASTM D3330 and for wetting tension under ASTM D2578; peel adhesion values outside 0.5–2.5 N/25 mm are rejected because excessive adhesion causes residue transfer after outdoor ageing. The carrier film does not require food-contact compliance, but heavy-metal restrictions under REACH 1907/2006 Annex XVII apply to the adhesive and film pigments.
Competitive Chevron Phillips Marlex® 7109M LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® 7109M is a linear low-density polyethylene blown-film extrusion resin supplied in pellet form. Supplier-published nominal values place the melt index at 0.90 g/10 min measured under ASTM D1238 at 190°C with a 2.16 kg load and the density at 0.918 g/cm³ measured under ASTM D1505. The grade is positioned as a general-purpose film resin for blown-film structures in which downgauging, tear resistance, and acceptable optical performance must be balanced. Typical application categories in supplier literature include industrial liners, heavy-duty sacks, consumer trash bags, garment overwrap, and general packaging film. The suffix M in the grade designation is associated with a film-grade additive package, commonly containing medium slip and antiblock additives; the exact additive loading must be confirmed from the certificate of analysis because it affects coefficient of friction, blocking, corona treatment retention, and food-contact declarations. The product is intended for blown-film extrusion and is not designed for injection molding or rotational molding.
As a butene-copolymer LLDPE, the resin carries a heterogeneous short-chain branch distribution. That molecular architecture provides broader melting and crystallization transitions than metallocene LLDPE and contributes more bubble stability than a metallocene film resin of comparable melt index. The same structural feature also reduces dart impact and Elmendorf tear relative to hexene or octene LLDPE grades of equal density and melt index. For applications requiring haze below 5%, a metallocene LLDPE or an LDPE-rich blend may be required because butene Ziegler-Natta LLDPE films of this density typically exhibit haze in the 5–8% range. The density of 0.918 g/cm³ selects a crystallinity level that supports toughness and clarity while retaining enough modulus for film-handling stiffness.
In blown-film evaluation, the resin is typically characterized at 25 µm gauge after extrusion through a spiral mandrel die with a die gap of 1.5 mm and a blow-up ratio of 2.5:1. The following ranges consolidate supplier-published representative film data and are not specification limits. Commercial values shift with frost line height, screw shear history, die geometry, and additive masterbatch addition. Mechanical tests are conducted on specimens conditioned at 23°C and 50% RH.
| Property | Test method | Typical range at 25 µm |
|---|---|---|
| Melt index | ASTM D1238 | 0.90 g/10 min |
| Density | ASTM D1505 | 0.918 g/cm³ |
| Haze | ASTM D1003 | 5–8% |
| Gloss at 45° | ASTM D2457 | 70–80 |
| Dart impact, F50 | ASTM D1709 Method A | 110–150 g |
| Elmendorf tear, MD | ASTM D1922 | 200–280 gf |
| Elmendorf tear, TD | ASTM D1922 | 300–420 gf |
| Secant modulus, MD at 1% strain | ASTM D882 | 150–180 MPa |
| Secant modulus, TD at 1% strain | ASTM D882 | 165–195 MPa |
| Tensile yield strength, MD | ASTM D882 | 9.0–11.0 MPa |
| Tensile yield strength, TD | ASTM D882 | 8.5–10.5 MPa |
| Elongation at break, MD | ASTM D882 | 450–550% |
| Elongation at break, TD | ASTM D882 | 600–700% |
The property window defined by 0.918 g/cm³ density and 0.90 g/10 min melt index balances extruder output against bubble strength. Higher melt index grades flow more readily but exhibit lower melt strength and reduced dart impact; lower melt index grades improve toughness and melt strength but require higher extruder torque and can limit output on smaller lines. Density below 0.925 g/cm³ preserves impact resistance and clarity, while density above 0.930 g/cm³ raises modulus and barrier but reduces film toughness and sealing performance.
On dedicated blown-film lines using 65 mm or 75 mm single-screw extruders with 30:1 L/D barrier screws and spiral mandrel dies of 200–400 mm, melt temperatures are normally held between 190°C and 230°C. The lower portion of this range preserves bubble stability and reduces oxidative degradation; the upper portion is used on high-output lines and in coextrusion where layer adhesion requires higher melt temperature. Die temperature should be maintained within 5°C of the adapter temperature to avoid surface flow defects. A die gap of 1.5–2.0 mm is preferable to 1.0 mm when producing film below 25 µm, because narrower gaps can generate shear stress sufficient for melt fracture. Blow-up ratios from 2.0:1 to 3.5:1 are used; lower ratios reduce transverse direction tear, and higher ratios may degrade bubble stability under air turbulence. Frost line height should be set between 200 mm and 400 mm on mid-scale lines to balance haze and blocking. Pellet surface moisture from condensation is a practical defect source; if pellets are stored below 10°C and exposed to humid air, surface moisture should be removed with dehumidified air at 50–60°C for 2–4 h before extrusion. Bulk pre-drying is not required for polyethylene resin in the absence of visible surface condensation.
LLDPE of this class has lower melt strength than high-pressure LDPE because of the absence of long-chain branching. Bubble stability is therefore managed primarily through die design, air-ring uniformity, and frost line control. On production-scale lines with 75 mm extruders, die pressure at 100 kg/h is generally higher than for LDPE of equal melt index by 10–30%, depending on screw design and temperature profile. At 190°C and an apparent shear rate of 100 s⁻¹, LLDPE grades with 0.90 g/10 min melt index typically exhibit an apparent viscosity of 900–1100 Pa·s; high-pressure LDPE of equivalent melt index may be 20–30% lower. This difference explains the higher torque and melt temperature observed when converting from LDPE to LLDPE on the same equipment. Barrier screws with 24:1 to 30:1 L/D and mixing heads promote melting, but grooved-feed sections can raise melt temperature by 5–10°C at constant screw speed.
Batch-to-batch variation in melt index for Ziegler-Natta LLDPE can be ±0.05 g/10 min, and density can vary ±0.001 g/cm³. These small shifts may alter dart impact by 5–10% in thin film. Converters should monitor melt flow rate and density per lot and adjust barrel temperatures or blow-up ratio rather than assuming constant film properties. Field failure modes on 65–90 mm monolayer lines include bubble chatter from air-ring turbulence, shark-skin melt fracture from excessive shear stress at low die gap, and blocking of collapsed film from high frost line and low air flow. Screen packs of 40–80 mesh are typical for these lines to protect the die from conveying fines and carbonized gels.
Thermal stability is adequate for normal blown-film extrusion. Sustained melt temperatures above 260°C or excessive residence time can generate oxidative degradation products and gels. Purge and changeover procedures should use a compatible polyolefin with similar melt index; abrupt switching from high-viscosity HDPE to this LLDPE can create feed-block bridging if the feed section temperature is too low. The resin should not be exposed to strong oxidizing agents. Recycled polypropylene contamination should be kept below approximately 3–5 wt% to avoid brittle domains and visible gel-like defects in film. Maximum continuous service temperature for unstressed polyethylene film is approximately 90–110°C; applications involving hot-fill, retort, or sterilization above 100°C are outside the intended use of the product.
Comparative evaluations between Marlex® 7109M and high-pressure LDPE typically show that the LLDPE film has higher tensile strength, higher dart impact, and higher Elmendorf tear at equal gauge. The linear resin also has lower water-vapour transmission at equivalent thickness, although the exact barrier improvement is grade-specific and must be measured under ASTM F1249 or ASTM E96. In downgauging trials, a 25 µm LLDPE film can often match the dart impact and tensile strength of a 30–35 µm LDPE film. However, the change in film stiffness and bag feel must be assessed on the specific packaging line. Published data for this specific configuration is limited, so film qualifications should include ASTM D1709 dart impact, ASTM D1922 tear, and ASTM D882 tensile tests on samples collected from the actual line.
| Resin class | Melt strength | Dart impact and tear at equal gauge | Optical clarity | Extrusion pressure at equal output | Seal initiation temperature |
|---|---|---|---|---|---|
| Marlex® 7109M butene LLDPE | Moderate | Moderate | Moderate haze | Higher than LDPE | Moderate |
| High-pressure LDPE | High | Lower | Good clarity | Lower | Lower |
| Hexene LLDPE | Moderate | High | Moderate haze | Similar to butene LLDPE | Moderate |
| Metallocene LLDPE | Low | High to very high | Low haze | Higher than Ziegler-Natta LLDPE | Lower |
The choice of Marlex® 7109M over high-pressure LDPE is usually driven by mechanical downgauging and puncture resistance. The choice of hexene LLDPE over 7109M is driven by improved dart impact and tear at equal density; the choice of metallocene LLDPE is driven by lower haze and lower seal initiation on high-speed packaging. The broader molecular weight distribution of 7109M relative to metallocene grades provides processing advantages but can raise seal initiation temperature by 5–15°C and reduce hot-tack strength. These differences should be quantified on the target line because additive package and film gauge alter the absolute values.
Untreated polyethylene film surfaces generally show a wetting tension of 31–32 mN/m by ASTM D2578. Corona or plasma treatment to 38–42 mN/m is required before printing, coating, or laminating. The medium slip/antiblock package can reduce treatment retention because slip additives migrate to the film surface and may mask polar oxidation sites. Inline treatment immediately before the printing deck is therefore preferred over offline treatment. Treated film held for more than 30 days may decay below 36 mN/m, especially in warm storage. Heat sealing is typically performed at 115–130°C with 0.2–0.5 s dwell; seal initiation temperature is approximately 105–115°C for LLDPE of this density, and is commonly measured under ASTM F1921 or ASTM F2029. On high-speed vertical form-fill-seal lines with seal dwells below 0.2 s, hot-tack requirements may necessitate blending with mLLDPE or LDPE.
Food-contact status depends on the fabricated article, additives, and possible coatings. The base olefin polymer is generally covered under FDA 21 CFR 177.1520(c) when used in accordance with the regulation’s specifications for density, extractives, and end-use temperature. European Union food-contact compliance is evaluated under Regulation (EU) No 10/2011 and its amendments; a supplier Declaration of Compliance should be obtained for the specific grade and batch before commercial use. For electrical and electronic equipment, unreinforced polyolefin resins are normally within the heavy-metal restrictions of Directive 2011/65/EU, but the converter must verify this through supplier certificates. REACH registration obligations are managed by the manufacturer or importer; a Safety Data Sheet compiled under Regulation (EC) No 1907/2006 should be consulted for handling and disposal.
Published data for this specific configuration is limited for certain specialized applications such as irradiation-crosslinked film, ultra-thin stretch film below 10 µm, and direct food-contact packaging with high-temperature sterilization. In such cases, inline qualification on the intended equipment is required before specification. The resin is not recommended for processing on cast-film lines without adequate plastication because typical LLDPE viscosity can exceed the design limits of low-torque cast-film extruders.