    Specifications
    HS Code 125431
    Product Name Chevron Phillips Marlex 7109FJ Polyethylene Film Grade LLDPE Hexene Copolymer
    Manufacturer Chevron Phillips Chemical Company
    Brand Marlex
    Grade 7109FJ
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Application Film Grade
    Form Pellets
    Melt Index 0.9 g/10 min
    Density 0.918 g/cm³
    Melting Point 124 °C
    Vicat Softening Point 103 °C
    Tensile Strength At Yield 11 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 700%
    Dart Drop Impact 150 g
    Elmendorf Tear Strength 300 g
    Haze 12%
    Gloss 65%
    Coefficient Of Friction 0.2

    As an accredited Chevron Phillips Marlex® 7109FJ Polyethylene Film Grade LLDPE Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Marlex® 7109FJ LLDPE is packaged in 25 kg (55.1 lb) polyethylene bags, palletized, with bulk quantities available.
    Container Loading (20′ FCL) 20′ FCL: 25 kg bags, palletized, approximately 18–20 metric tons net of Marlex® 7109FJ LLDPE hexene copolymer film resin.
    Shipping Marlex® 7109FJ LLDPE hexene copolymer ships as non-hazardous polyethylene pellets in 25-kg bags, bulk boxes, or bulk trucks/railcars. Keep dry, away from heat, moisture, and contamination. Not DOT/IMDG/IATA regulated; no special hazard labels required. Use standard dry freight and handle per SDS. Store indoors; avoid prolonged UV exposure.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep containers or bags closed and palletized off the floor to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain moderate temperatures and protect from prolonged UV exposure. Follow SDS and local regulations for safe handling and housekeeping.
    Shelf Life No specific shelf life; stable when stored in original, unopened packaging in a cool, dry, ventilated area away from direct sunlight and heat.
    Application of Chevron Phillips Marlex® 7109FJ Polyethylene Film Grade LLDPE Hexene Copolymer

    On cast stretch film lines built with 75 mm to 125 mm single-screw extruders, 150–250 mesh screen packs, a gear pump for melt pressure control, and 2,500 mm to 3,500 mm slot dies, Chevron Phillips Marlex® 7109FJ hexene copolymer LLDPE is loaded into the core layer at 60–80 wt% of the total film structure to increase puncture propagation resistance and elongation at break in pre-stretched machine film. The skin layers on these lines are typically formulated with 10–20 wt% metallocene or butene LLDPE for cling performance and 0.5–2.0 wt% polyisobutylene-based cling masterbatch; the exact cling additive loading is adjusted using ASTM D5458-95 so that unwinding force remains between 2.0 N and 4.5 N per 100 mm width after 24 h of roll storage at 23±2°C. Melt temperature at the die exit is maintained within 240–275°C, and the chill roll temperature is held at 15–25°C with a draw ratio of 60:1 to 80:1; excursions above 275°C lead to oxidation-induced gel formation in the hexene copolymer chain, while temperatures below 230°C produce visible melt fracture and edge instability at line speeds above 400 m/min. Downstream, the cast film is either machine-wrapped directly or converted into pre-stretched hand rolls; terminal product types include 12–23 μm machine stretch film for rotary arm wrappers, 8–15 μm pre-stretched hand film, and 20–30 μm heavy-duty cast film for open-edge coil wrapping. Compliance documentation for industrial stretch film shipments is anchored to REACH Regulation (EC) No 1907/2006, the Packaging and Packaging Waste Directive 94/62/EC, and ISO 18601:2013 for packaging and the environment. Puncture resistance is conditioned under ASTM D4332 and tested per ASTM D5748; published values for 20 μm cast stretch film containing 60–80 wt% hexene LLDPE core generally fall between 0.8 J/cm and 1.5 J/cm, but published data for this specific configuration is limited and should be verified on the production line.

    What Are the Seal Strength Boundaries When Die Gap Falls Below 0.8 mm in Frozen-Food Blown Film?

    In three-layer blown film lines with 50 mm to 80 mm grooved-feed extruders and 250 mm to 400 mm spiral-mandrel dies, hexene LLDPE is processed at 185–220°C melt temperature, a blow-up ratio of 2.5:1 to 3.5:1, and a die gap of 0.8 mm to 1.5 mm; reducing die gap below 0.8 mm increases shear rate above 300 s⁻¹ in the die lip and elevates barrel pressure to 280–320 bar, which shifts melt fracture onset to lower line speed and narrows the heat-seal plateau at 120–150°C. The formulation for food-contact frozen-food film is 90–97 wt% hexene LLDPE, 2–5 wt% white pigment masterbatch, and 1–3 wt% of an erucamide/silica slip-antiblock masterbatch; the slip agent migrates to the film surface over 24–72 h and reduces coefficient of friction measured per ASTM D1894 from 0.65–0.80 initial to 0.20–0.35 after aging, but slip masterbatch above 3 wt% suppresses heat-seal strength below 2.0 N/15 mm per ASTM F88-21 at 130°C seal bar temperature. Downstream production runs include form-fill-seal machines with single-jaw impulse sealing at 0.3–0.5 MPa seal pressure and 0.5–1.5 s dwell, producing pillow packs for frozen vegetables, ice cream sleeves, and bagged fresh-cut produce stored at -25°C to 4°C. Food-contact compliance is documented through FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation No 10/2011 with overall migration below 10 mg/dm² per BS EN 1186-1; the resin lot must also comply with the supplier's current REACH registration and 21 CFR 177.1520(b) extractives limits. Pre-drying is not normally required, but resin stored at relative humidity above 60% without sealed silo blanketing may require 2–4 h at 80°C to prevent surface moisture streaking and gel-like defects during blown film extrusion.

    Food-contact compliance checklist for three-layer LLDPE blown film at 2.5:1–3.5:1 BUR
    RequirementTest methodAcceptance criterion
    FDA olefin polymer food-contact authorization21 CFR 177.1520(c)Resin identity and conditions of use B–H
    EU plastic food-contact materialEU Regulation No 10/2011Overall migration ≤ 10 mg/dm²
    Overall migration in finished filmBS EN 1186-1≤ 10 mg/dm²
    Melt flow rate verificationISO 1133-1:2022Supplier datasheet tolerance ±0.1 g/10 min
    Heat-seal strength after form-fill-sealASTM F88-21≥ 2.0 N/15 mm at 130°C

    When Hexene LLDPE Replaces Butene LLDPE in a Three-Layer Extrusion Lamination Structure

    In a tandem extrusion lamination line with a 90 mm to 120 mm extruder, an air gap of 150 mm to 250 mm, and a counter-rotating chill roll at 15–20°C, hexene LLDPE is used as the sealant web at 70–90 wt% of the seal layer, with 10–20 wt% LDPE to increase melt elongation stability and 3–6 wt% maleic anhydride-grafted LLDPE tie layer in the adjacent adhesive layer. Melt temperature is held at 240–260°C at the die exit, and corona treatment of the outer sealant surface to 38–42 dyne/cm is performed in-line before adhesive lamination; failure to maintain dyne level above 36 dyne/cm results in incomplete ester-based adhesive wetting and delamination at the ply interface on three-side-sealed pouches. The downstream process includes extrusion coating onto aluminium foil, biaxially oriented polyester, or paper at line speeds of 120–250 m/min, followed by slitting into reels for flexographic and rotogravure lamination; final film thickness of the sealant layer is typically 20–35 μm. Compliance for food-contact laminates is established under FDA 21 CFR 177.1520 and EU Regulation No 10/2011, with the overall migration of the finished laminate tested per BS EN 1186-1 and not exceeding 10 mg/dm²; if the structure contains aluminium foil, the foil layer is not part of the polyethylene compliance assessment but the adjacent sealant remains subject to the same migration limits. Terminal product types include stand-up pouches for dry snacks, liquid detergent spouted pouches, coffee valve bags, and single-serve sugar sachets. Operational boundary: the sealant layer is not recommended for retort pouches above 100°C, because hexene LLDPE heat-seal strength decays above 110°C and the seal interface can undergo partial melting during post-sterilisation cooling at 0.2–0.3 MPa platen pressure.

    UV-Stabilized Silage Wrap Extrusion Parameters and Round Bale Cover Performance

    On mono-layer or two-layer blown film lines with 70 mm to 90 mm extruders, 250 mm to 350 mm dies, and internal bubble cooling systems, hexene LLDPE is formulated at 100 wt% virgin resin with 2–4 wt% carbon black masterbatch or 4–6 wt% HALS-based UV stabilizer masterbatch for outdoor storage; higher carbon black loading above 4 wt% increases melt viscosity and reduces annual output by 5–10% on lines without enlarged motor capacity. Extrusion uses a blow-up ratio of 3.0:1 to 4.0:1, a die gap of 1.0 mm to 2.0 mm, and melt temperature 190–220°C; film thickness is set between 25 μm and 75 μm depending on bale diameter and storage duration. The downstream process involves winding on cardboard cores at 30–60 m/min and then being pulled by manual or tractor-mounted wrappers to 50–70% elongation during bale wrapping; puncture and tear resistance are monitored using EN 13206:2017 for thermoplastic stretch films for silage bales, and tensile elongation at break is measured per ISO 527-3 on 25 mm wide strips. Terminal products include round bale silage wrap film, greenhouse cover film with 12–24-month UV resistance, and mulching film for vegetable beds. Compliance for agricultural films is covered by REACH Regulation (EC) No 1907/2006, the Packaging and Packaging Waste Directive 94/62/EC where applicable, and EN 13206:2017 for silage bale wraps; the resin must not contain heavy metals above the limits of EU Directive 94/62/EC Article 11. Operational boundary: film stored outdoors before use should be consumed within 12–24 months depending on UV stabilizer package; exposure to copper-based fungicides in silage pit liners may accelerate oxidative degradation of the film surface.

    Three-layer blown film sack lines with 70 mm to 90 mm extruders, 300 mm to 400 mm spiral dies, and reverse lip air rings process hexene LLDPE in heavy-duty industrial sacks at 70–85 wt% of the total structure, with 15–25 wt% LDPE for melt strength and up to 5 wt% fluoropolymer process aid masterbatch during high-speed campaigns above 80 kg/h per extruder. The internal layer may contain 10–20 wt% clean post-industrial reclaim, but not post-consumer recyclate, when the sack is used for non-food industrial fillers such as polycarbonate resin granules or fertilizer prills; the use of reclaimed material is documented under ISO 18604:2013 and is prohibited in food-contact structures. Extrusion parameters include a die gap of 1.2 mm to 2.2 mm, blow-up ratio 2.5:1 to 3.5:1, and melt temperature 210–240°C, with frost line height held at 6–10 times die diameter to balance machine-direction tear resistance and drop impact. The film is then gusseted, surface-printed with flexographic inks, and converted on bag-making machines into open-mouth or valve sacks with 100–120 μm wall thickness; seam sealing is performed by hot-air or impulse welding at 140–160°C. Terminal product types include 25 kg fertilizer sacks, 20–50 kg resin pellet bags, ice melt salt bags, and construction aggregate sacks. Compliance documentation for these non-food sacks includes REACH Regulation (EC) No 1907/2006, Packaging and Packaging Waste Directive 94/62/EC, and ISO 18601:2013; if the sack is shipped under dangerous goods transport codes, the testing authority assesses drop, stack, and tear resistance per the applicable UN packing group method.

    Sealant Web for Non-Aseptic Medical Device Pouches Operates Within a Narrow Slip Agent Window

    On a cast film line with a 50 mm to 70 mm extruder and a 500 mm to 800 mm slot die, hexene LLDPE is used as the sealant web in medical device pouches at 100 wt% virgin resin, with erucamide slip agent controlled to 0.2–0.5 wt% through a pre-dispersed masterbatch; exceeding 0.5 wt% reduces the seal initiation temperature below 90°C and creates unintended seal transfer on Tyvek or medical paper at 110–130°C platen temperatures. Melt temperature is kept at 200–230°C, the chill roll at 18–25°C, and the web thickness at 25–40 μm; in-line corona treatment to 38–42 dyne/cm is required before printing or lamination. Downstream production involves heat-seal coating onto uncoated Tyvek or medical grade paper on a form-fill-seal machine, followed by ethylene oxide or gamma sterilization; seal strength is tested per ASTM F88-21 and must remain above 1.5 N/15 mm after sterilization. Compliance for medical device packaging is established under ISO 11607-1:2019 for packaging for terminally sterilized medical devices, ISO 10993-5 for cytotoxicity of the final packaging material, and EU Medical Device Regulation 2017/745; the resin must also meet REACH Regulation (EC) No 1907/2006. Terminal product types include surgical instrument pouches, tubing sets, catheter packs, and sterile barrier lidding for non-aseptic device trays. Operational boundary: this grade is not approved for aseptic processing in pharmaceutical fill-finish lines, and published data for this specific configuration is limited; validation with the sterilizer type and pouch material supplier is required before release.

    Free Quote

    Competitive Chevron Phillips Marlex® 7109FJ Polyethylene Film Grade LLDPE Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® 7109FJ Polyethylene Film Grade LLDPE Hexene Copolymer is a linear low-density polyethylene resin polymerized with hexene-1 as the comonomer. Supplier-published nominal values list density at 0.918 g/cm³ when measured by ASTM D1505 and melt index at 1.0 g/10 min when determined at 190°C under 2.16 kg load per ASTM D1238. The hexene-1 comonomer generates butyl short-chain branches along the polymer backbone. These branches shorten the average crystallizable ethylene sequence and increase tie-chain probability between adjacent lamellar crystallites, affecting tear, dart impact, and seal behavior in oriented film. The grade is normally directed to blown-film structures in the gauge range 12 µm to 75 µm.

    Nominal specification data used in commercial lot acceptance appear below.

    Nominal resin property set for 7109FJ
    PropertyTest methodNominal value
    DensityASTM D1505 / ISO 1183-10.918 g/cm³
    Melt flow rateASTM D1238 / ISO 1133-1:20221.0 g/10 min

    Actual lot certificates may vary from nominal values. Incoming inspection using the cited test methods is advisable to detect contamination, regrind level, or moisture exposure. The resin is supplied as pellets; pneumatic conveying should include dust-removal filters to avoid micro-fines accumulation at the hopper screen. If the material is stored outdoors in silos, temperature cycles may create condensation on the pellet surface; this surface moisture can be carried into the melt and generate steam at the die lip.

    What Extrusion Conditions Preserve Bubble Stability in Air-Quenched LLDPE Film?

    On air-quenched blown-film lines, die lip gap is usually set between 1.8 mm and 2.5 mm. Melt temperature at the adapter and die is commonly held between 200°C and 230°C. At sustained temperatures above 230°C, the stabilizer package may be consumed more rapidly, and oxidized gel particles may become visible if residence time exceeds 5 min. At melt temperatures below 200°C, viscosity can rise enough to increase die pressure and reduce throughput on high-output grooved-feed extruders. Blow-up ratio is typically maintained from 2.0:1 to 3.0:1. A BUR below 1.8:1 may under-orient the transverse direction, while a BUR above 3.5:1 can induce bubble flutter and gauge bands unless the air ring provides dual-lip velocity control. Frost-line height is typically set at 1.5 times to 4.0 times die diameter. Extruder L/D ratios used for this resin generally fall between 24:1 and 30:1; shorter screws may require lower output rates to prevent unmelted resin from reaching the die lip.

    Die wall shear stress is a practical control variable for surface quality. For linear low-density polyethylene, sharkskin melt fracture is often observed when wall shear stress approaches 0.14 MPa. Increasing die lip gap, raising die temperature within the stated window, or reducing output lowers shear stress. Purging after shutdown is commonly performed with a low-melt-index LDPE or a commercial purge grade because the linear resin has a narrower thermal-oxidative processing window than high-pressure LDPE. Pre-drying is not generally required when silo storage is dry. If condensation occurs on cold pellets moved into a warm extrusion hall, steam can form at the die and produce pinholes; a desiccant hopper dryer at 60°C to 80°C for 2 h to 4 h is used when the relative humidity exceeds 60%. Screen packs of 60/80/120 mesh are typical for film lines; pressure drop across the screen pack should be monitored and changed before the pressure reaches a line-specific maximum.

    In coextruded structures, 7109FJ may be used as a core layer with a lower-density metallocene skin for seal initiation or as a bulk layer beneath an EVA sealant. Layer-thickness ratio and die-lip gap must be matched to the resin’s melt elasticity; large differences in melt strength between layers can produce interfacial instability and optical distortion. Corona treatment for printing or lamination is typically adjusted to a target surface energy of 38 mN/m to 42 mN/m; decay is monitored by wetting-tension fluids using ASTM D2578. The base film may require slip and antiblock masterbatches; kinetic coefficient of friction is measured by ASTM D1894 and should be specified for the converter’s winding and bag-making equipment rather than assumed from pellet data.

    Hexene Short-Chain Branching and the Resulting Tear/Toughness Offset Relative to Butene-Grade Resins

    At matched density and melt index, hexene-1 copolymerized LLDPE differs from butene-1 LLDPE in short-chain branch length. Butene contributes ethyl branches; hexene contributes butyl branches. The longer branch interrupts crystallizable ethylene sequences more efficiently and can increase tie-chain formation. Comparative film testing should include ASTM D1709 dart impact, ASTM D1922 Elmendorf tear, and ASTM D5748 puncture resistance. Published comparative data for this specific configuration is limited; side-by-side evaluation on the target line is required because die gap, blow-up ratio, frost-line height, and cooling rate alter crystalline orientation and tie-chain density. The general trend reported for Ziegler-Natta hexene LLDPE is that dart impact and tear balance improve relative to butene copolymers at 25 µm gauge, but the magnitude is line-specific.

    Compared with high-pressure LDPE, 7109FJ has little or no long-chain branching. Melt strength is lower, but thin-gauge drawdown is improved. When bubble stability is marginal on a given line, blending 10 wt% to 30 wt% of a fractional-melt LDPE can raise melt tension and widen the processing window. Such blending may shift seal initiation temperature upward, so heat-seal strength should be checked by ASTM F88 and hot tack by ASTM F1921 before a blend ratio is fixed. Compared with metallocene LLDPE of similar density, the product may exhibit broader molecular weight distribution and lower gloss; optical comparisons should be made using ASTM D1003 haze and ASTM D2457 gloss after stabilizing the film at 23°C ± 2°C and 50% ± 10% relative humidity.

    When Direct Food Contact Regulatory Limits Narrow the Use Envelope

    Food-contact suitability is a function of the finished package and its conversion history, not the pellet alone. Supplier documentation typically references FDA 21 CFR 177.1520(c) for olefin polymers intended for direct food contact. In the European Union, the final film must meet Commission Regulation 10/2011, including overall migration limits specified in Annex II and simulant assignment according to Annex III. The overall migration limit is 10 mg/dm², expressed as 60 mg/kg for infant food contact. Fatty food simulants and pasteurization conditions may require additional migration testing because low-molecular-weight oligomers can migrate at elevated temperature. Compliance with RoHS Directive 2011/65/EU and REACH Regulation 1907/2006 should be confirmed through the supplier’s product safety certificate for the exact packaging article. The base resin is not weather-stabilized; outdoor film requires a UV-stabilized masterbatch or a coextruded UV-protective skin layer. Differential scanning calorimetry per ASTM D3418 typically places the principal melting peak for LLDPE of this density near 122°C to 126°C. The melting peak is not a continuous-service limit; deformation under load should be validated by ASTM D648 or ASTM D1525.

    Compliance checks for the finished film can be organized into a simple matrix.

    Finished-film compliance and test matrix
    AttributeStandard or regulationTypical control basis
    Overall migrationEU 10/2011 Annex II10 mg/dm² or 60 mg/kg
    Olefin polymer food contactFDA 21 CFR 177.1520(c)Conditional on thickness and food type
    Hexane extractablesASTM D5227Lot-specific certificate value
    Dart impactASTM D1709To be established on 25 µm film
    Elmendorf tearASTM D1922To be established on 25 µm film

    On vertical or horizontal form-fill-seal packaging machines, finished film seal performance is controlled by seal-bar temperature, dwell time, and sealing pressure. Heat-seal strength is measured on 25 mm wide strips per ASTM F88; hot-tack strength is measured per ASTM F1921. If a converter changes from a butene-based LLDPE to this hexene grade, the seal initiation temperature may allow a lower seal-bar set point, but the actual offset must be determined on the packaging machine because film thickness, corona treatment, and coextruded layer composition alter the seal response. The resin is commonly used in heavy-duty sacks, frozen-food packaging, industrial liners, and collation shrink film. In these applications, film gauge is typically monitored on-line by capacitance or beta gauge; a total thickness tolerance of ±5% at 25 µm nominal gauge is a common starting target for converter quality agreements. Final film properties should be tested after 40 h to 72 h of conditioning at 23°C ± 2°C and 50% ± 10% relative humidity according to ASTM D618, because polyethylene film properties change with post-crystallization.

    Observed production-scale failure modes include bubble instability during hot summer shifts, die-lip buildup, gauge bands caused by uneven air-ring flow, and seal-strength drift attributable to excessive regrind. These are controlled by limiting regrind to 20 wt% to 30 wt% in critical film structures unless validation demonstrates otherwise, by maintaining die-lip cleanliness, and by monitoring melt-pressure variation before the screen changer.