| HS Code | 688694 |
| Product Name | Chevron Phillips Marlex 7109 LLDPE Blown Film Resin |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Physical Form | Pellets |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.9 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield Md | 1400 psi |
| Tensile Strength At Yield Td | 1300 psi |
| Tensile Strength At Break Md | 4500 psi |
| Tensile Strength At Break Td | 4000 psi |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Elmendorf Tear Strength Md | 250 g/mil |
| Elmendorf Tear Strength Td | 500 g/mil |
| Dart Drop Impact | 150 g |
| Haze | 12% |
| Gloss 45 | 60 |
| Coefficient Of Friction | 0.2 |
| Low Temperature Brittleness | < -70 °C |
| 1 Secant Modulus Md | 25000 psi |
| 1 Secant Modulus Td | 30000 psi |
| Puncture Resistance | 8 ft-lb/in |
| Heat Seal Initiation Temperature | 110 °C |
As an accredited Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin comes in 50 lb (22.7 kg) multiwall paper bags, 35 bags per pallet. |
| Container Loading (20′ FCL) | Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin: 20′ FCL loads 12.5 MT palletized—10 pallets, 25 kg bags, 50 bags/pallet. |
| Shipping | Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin is shipped as non-hazardous, solid resin pellets. Standard packaging includes 25 kg bags, stretch-wrapped pallets, or bulk octabins. Transport by truck, rail, or ocean container under normal conditions. Keep dry, avoid excessive heat, and handle according to supplier guidelines. Not DOT/IMDG/IATA regulated. |
| Storage | Store Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin in original, closed containers in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, sparks, flames, moisture, dust, and physical damage. Avoid strong oxidizing agents. Do not overstack; use first-in, first-out rotation. Keep away from food, drink, and incompatible materials. Follow the manufacturer’s SDS. Maintain recommended storage temperature and humidity. |
| Shelf Life | Shelf life is typically 12 months from manufacture when stored in original unopened packaging, dry, below 50°C, away from sunlight. |
In heavy-duty industrial sack conversion, Marlex® 7109 is processed as a monolayer or three-layer A/B/A structure at total film thicknesses from 100 µm to 220 µm. Grade certification supplied with the resin typically lists a nominal density of 0.918 g/cm³ according to ASTM D1505 and a nominal melt index of 1.0 g/10 min according to ASTM D1238 at 190°C and 2.16 kg. The terminal products are 25 kg, 40 kg, and 50 kg sacks for resin pellets, cementitious dry mixes, fertilizers, and industrial salts. On a 70 mm single-screw extruder with a 26:1 L/D barrier screw and a Maddock mixing tip, the melt temperature window is held at 190°C to 215°C at the die, while adapter and die zones are maintained within ±5°C of the target to avoid localized melt fracture. A die gap of 1.8 mm to 2.5 mm is used with a blow-up ratio from 2.2:1 to 3.2:1 and a frost line height of 5 to 8 die diameters. At line speeds above 45 m/min, bubble respiration at the collapsing frame is stabilized by adding 10 wt% to 20 wt% of LDPE with a melt index of 0.25 g/10 min to 0.8 g/10 min as measured by ASTM D1238. Without that LDPE addition, the low melt tension of the LLDPE phase allows gauge banding of ±12% to ±18% around the circumference, which is outside the ±5% to ±8% tolerance demanded by automatic sack indexers.
For aggressive dry product exposure, a formulation containing 2 wt% to 4 wt% carbon black masterbatch with a 45% to 50% carbon black loading, 1 wt% to 3 wt% silica-based anti-block masterbatch, and 500 ppm to 1,500 ppm erucamide slip additive is typical. The erucamide addition creates a coefficient of friction target of 0.25 to 0.45 as measured by ASTM D1894-14 after 24 h ageing. Polymer processing aid is added at 300 ppm to 800 ppm to suppress melt fracture in the die land. The seal initiation temperature of the 7109-rich layer is in the range of 105°C to 115°C under a 0.4 MPa seal bar pressure and 0.5 s dwell. Seal strength is targeted at 10 N/15 mm to 16 N/15 mm when tested according to ASTM F88/F88M-21. For dimensional stability, the film is gusseted to 90 mm to 150 mm and converted on a bottom/back sealer at 40 to 60 sacks per minute. The critical limitation is hot-tack performance: 7109 exhibits a relatively narrow hot-tack plateau, and packaging lines with fill temperatures above 60°C require a 5 wt% to 10 wt% plastomer or EVA blend to prevent seal creep during drop loading. No pre-drying is required for the resin itself because polyethylene is non-hydroscopic, but condensation on cold pellets transferred from outdoor silos at relative humidity above 75% can create surface moisture defects. Therefore, hopper heating at 50°C to 60°C is applied when ambient dew point approaches pellet temperature.
Agricultural silage wrapping specifications rarely rely on a single dart impact value because film failure occurs by slow puncture during bale compression and retraction. Marlex® 7109 is used in 25 µm to 45 µm blown structures as the stiffening layer in a three-layer coextrusion with metallocene-catalyzed LLDPE skins to lift dart impact above 600 g at 30 µm, measured by ASTM D1709-16a Method A. Total gauge variation must remain within ±8% because bale wrapping over round bales of 1.2 m to 1.5 m diameter exerts intense local stress at the film overlap. A typical layer distribution is 15% to 25% metallocene LLDPE in the outer surfaces and 50% to 70% Marlex® 7109 in the core. Tack is generated by 1 wt% to 3 wt% polyisobutene concentrate of 20% active content, while ultraviolet stabilization is provided by 0.5 wt% to 1.0 wt% HALS masterbatch and 0.2 wt% to 0.5 wt% antioxidant. The bubble is run at a blow-up ratio of 2.0:1 to 3.0:1 with a die gap of 1.5 mm to 2.0 mm and a melt temperature of 195°C to 215°C. During conversion to 750 mm rolls, edge trim generated by slitting 2,000 mm layflat is recycled at up to 20 wt%. Regrind levels above this threshold reduce tear propagation resistance by 15% to 25% because of gel formation and loss of the high-molecular-weight fraction during reprocessing.
Compliance for silage wrap is defined by EN 13207:2018, which requires minimum total thickness and specifies elongation at break after ageing. Under that standard, films must demonstrate at least 400% elongation at break in both machine and transverse directions, tested according to ISO 527-3. The 7109-containing structure typically exceeds that threshold at 25 µm, but aged films stored for more than 18 months under high UV irradiance can fall below the limit if the HALS concentration drops below 0.5 wt%. The terminal product is wrapped in 2 to 4 layers on round bales and 6 to 8 layers on square bales. Field loss is reported when the film contains more than 5 wt% inorganic anti-block filler because that filler has a disproportionate effect on slow puncture energy under ISO 7765-1:2020.
Blown drum liners produced from Marlex® 7109 at 100 µm to 250 µm are specified for dry-flowable chemical powders, pigments, and oil-contaminated metal swarf. The failure mode that controls conversion yield is not the seal initiation temperature but the retention of seal strength after the liner is filled and stored for 30 days at 40°C with a fill head adjacent to the seal. On a multi-layer blown line with an internal bubble cooling die of 200 mm diameter and die gap of 2.0 mm to 2.5 mm, the liner is run at a blow-up ratio of 1.8:1 to 2.5:1 to minimize transverse direction curl. Drop impact resistance after a 1.8 m fall at −20°C is specified at 12 kg to 16 kg for a 125 µm structure when tested according to ASTM D2463-15. That value degrades by 20% to 30% if extruder backpressure exceeds 250 bar and resin shear history generates micro-gels. To preserve seal integrity, the seal layer blend is formulated with 70 wt% 7109, 20 wt% LDPE, and 10 wt% EVA with a vinyl acetate content of 9% to 12%. The EVA lowers hot-tack initiation to 85°C and widens the sealing window from 100°C to 150°C.
The seal strength target is 20 N/15 mm to 25 N/15 mm according to ASTM F88/F88M-21, but powders with particle sizes below 10 µm can migrate to the seal area and reduce strength by 30% to 40% if the liner is filled at a drop height exceeding 2.0 m. The corrective measure on the packaging line is to reduce fill head velocity and to hold the liner mouth with vacuum-assisted opening rather than air-jet blowing. For food-contact liners, the olefin polymer is covered by FDA 21 CFR 177.1520(c) under conditions of use C through G, and EU Regulation (EU) No 10/2011 Annex I applies with an overall migration limit of 10 mg/dm². If the liner is used for retort or hot-fill above 80°C, the converter must switch to a liner grade with a higher Vicat softening point because 7109 loses dimensional stability above that threshold.
| Application matrix | Terminal product | Governing standard or clause | Measured property | Operational boundary |
|---|---|---|---|---|
| Heavy-duty industrial sacks | 25–50 kg sacks | ASTM D1709-16a | Dart impact at 100 µm | Fill temperature above 60°C requires hot-tack modifier |
| Agricultural silage wrap | Silage bales | EN 13207:2018; ISO 527-3 | Elongation at break above 400% | Regrind above 20 wt% lowers tear resistance |
| Blown drum liners | Chemical drum liners | FDA 21 CFR 177.1520(c); EU No 10/2011 Annex I | Overall migration limit 10 mg/dm² | Service above 80°C not permitted for 7109 |
| Surface protection films | Substrate protection films | ASTM D7310-20 | Gel count below 5 per 0.1 m² above 100 µm gel size | Regrind above 15 wt% raises gel count |
| Stretch-hood palletizing | Pallet hoods | ASTM D1922-15e1 | Edge tear retention | Load limit 600–800 kg at 100 µm |
| Frozen food packaging | Frozen food bags | FDA 21 CFR 177.1520(c) | Drop failure below 5% at −30°C and 1.0 m | Sharp ice-crystal puncture limited in monolayer structures |
Surface protection films for polycarbonate sheet, stainless steel skid plates, and pre-painted aluminium are converted from Marlex® 7109 as the core layer in a three-layer structure with a total thickness of 40 µm to 80 µm. A typical skin/core/skin distribution is 15/70/15 by weight. The core provides stiffness and tear resistance, while polyolefin elastomer skins provide controlled adhesion from 0.05 N/25 mm to 0.50 N/25 mm as measured by ASTM D3330/D3330M-21 Method A. The conversion line is a 90 mm main extruder with a 30:1 L/D screw and a 120 mm annular die; melt temperature is held at 200°C to 220°C, and the die gap is 1.2 mm to 1.8 mm. The blow-up ratio is set at 2.2:1 to 2.8:1 because the three-layer melt curtain must be collapsed without blocking on polished surfaces. Because the film is stretched over polished metal and optical substrates, any inclusion above 80 µm produces a visible defect. Filtration through a screen pack of 60/80/100 mesh is used, but for optical-grade products the screen pack is replaced with a 100/120/150 mesh stack and the backpressure limit is set at 300 bar. Above that limit, the screen pack is changed every 4 h to 6 h rather than risk bypass leakage through the screen changer.
Gel counts are evaluated by ASTM D7310-20 on a 40 µm sample, with a target of fewer than 5 gels per 0.1 m² for gel size greater than 100 µm. If regrind from edge trim exceeds 15 wt%, the gel count rises above that target because the polyolefin core undergoes shear-induced degradation in the reclaim extruder. The terminal product is wound on 1,500 mm to 2,500 mm rolls and die-cut to customer-specific widths; edge smoothness is critical because a serrated slit edge triggers propagation when the film is peeled at a 180° angle. For adhesion to high-energy substrates, corona treatment of the skin layer to 38 dyn/cm to 42 dyn/cm is applied in-line, but the core 7109 remains untreated and is not rated for direct food-contact lamination unless covered by a functional barrier. Published data for the long-term outdoor weathering of this specific three-layer configuration is limited, and converters must conduct their own QUV ageing according to ASTM G154-23 before replacing a PVC-based surface protection film on outdoor profiles.
Stretch-hood palletizing produces an 80 µm to 150 µm blown film hood that is stretched by 60% to 80% in the transverse direction before being released over a loaded pallet. Marlex® 7109 is combined with 20 wt% to 30 wt% LDPE and 10 wt% to 20 wt% metallocene-catalyzed LLDPE to achieve the necessary balance between extensional viscosity and tear propagation resistance. The blow-up ratio is run at 2.5:1 to 3.5:1. The process conflict arises at the film fold edges: after an automatic gusset is introduced, machine-direction tear resistance drops by 20% to 35% compared with the center web, as measured by ASTM D1922-15e1. On a line producing 1,200 mm layflat, edge tear is controlled by maintaining a frost line height of 7 to 9 die diameters and by running a dual-lip air ring with a chilled lower lip at 12°C to 15°C. This produces a more uniform transverse quench and reduces edge gauge thinning to below 10%.
The film is sealed on a vertical form-fill-seal unit with a hot-bar temperature of 140°C to 160°C and a seal pressure of 0.3 MPa to 0.5 MPa. Seal strength is measured at 15 N/15 mm to 20 N/15 mm according to ASTM F88/F88M-21. The 7109-containing formulation provides a dart impact of 350 g to 500 g at 100 µm by ASTM D1709-16a, but the addition of metallocene LLDPE raises dart impact by 20% to 35% while reducing modulus. That trade-off limits the stacking load on a pallet to 600 kg to 800 kg when a 100 µm hood is used; above this load, side gusset creep and film puncture at the pallet corners are observed. The terminal application is the replacement of shrink wrap for non-ventilated pallets carrying bagged cement, paper reams, and beverage cans. For outdoor storage, the film is UV-stabilized with 0.5 wt% HALS, but the product is not specified for exposure beyond 12 months because the low-density polyethylene matrix loses impact resistance after extended UV exposure.
At frozen-food forming temperatures below −25°C, the selection of a blown film grade with stable bubble geometry and low stress-whitening is dictated by line-surge behavior on vertical form-fill-seal machines. Marlex® 7109 is converted at 20 µm to 60 µm in laminates and monolayers for frozen vegetables, seafood, and ice-saturated poultry bags. A formulation for a 30 µm monolayer includes 1 wt% to 2 wt% silica anti-block and 500 ppm erucamide slip. The blown film process set includes a melt temperature of 195°C to 210°C, a blow-up ratio of 2.0:1 to 2.8:1, and a die gap of 1.5 mm to 2.0 mm. The terminal bags are run at 60 to 120 bags per minute on vertical form-fill-seal lines with a seal jaw temperature of 125°C to 145°C. Low-temperature drop impact is evaluated by freezing the filled bag for 24 h at −30°C and conducting a 1.0 m drop test; the failure rate is specified below 5%. Thicker films above 50 µm show lower stress-whitening and higher drop survival.
The selection of 7109 for this use is limited to applications where the package is not subject to sharp-edge puncture from ice crystals. In a monolayer structure, dart impact at −30°C is typically 30% to 40% lower than at 23°C, and the film should be downgauged only after line trials confirm seal integrity on vertical form-fill-seal machines. Compliance for direct frozen-food contact is governed by FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011 Annex I, with any added slip or anti-block masterbatch requiring its own specific migration assessment. The film is corona-treated to 36 dyn/cm to 40 dyn/cm for flexographic printing, but surface treatment decays within 30 days under high-humidity storage above 70% relative humidity; therefore, in-line treatment immediately before printing is required.
Competitive Chevron Phillips Marlex® 7109 LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Marlex® 7109 is a linear low-density polyethylene blown film resin based on an ethylene-alpha-olefin copolymer. The model designation 7109 places the material in the blown film segment of the Marlex® linear polyethylene portfolio. The grade is intended for tubular blown film conversion on single-screw extrusion lines and is supplied as pelletized resin. Two primary identity parameters define the grade: density under ASTM D1505/ISO 1183 and melt mass-flow rate under ASTM D1238/ISO 1133 at 190°C/2.16 kg. Published typical values for Marlex® 7109 are 0.918 g/cm³ for density and 1.0 g/10 min for melt mass-flow rate. These values are typical properties rather than purchase specifications; the lot-level certificate of analysis is the controlling document because reactor conditions, neutralization additives, and finishing operations can shift the actual values.
The alpha-olefin comonomer introduces short-chain branching that reduces crystallinity relative to high-density polyethylene and lowers density and modulus. The polymer backbone is linear, meaning the resin lacks the long-chain branching found in autoclave and tubular high-pressure low-density polyethylene. This structural difference controls melt elasticity, die swell, shear thinning, and the resulting film tensile and impact response.
Because the resin is linear, blown film processing requires tighter bubble control than high-pressure LDPE. On grooved-feed single-screw extruders with L/D ratios of 24:1 to 30:1, the melt is more viscous at high shear and does not shear-thin as rapidly as LDPE. This produces higher backpressure at equivalent output and requires a barrier screw or a Maddock-type mixing section to complete additive dispersion. Die gaps from 1.8 mm to 2.5 mm are typical. A die gap below 1.5 mm increases shear stress at the die lip and promotes sharkskin melt fracture, while a die gap above 2.5 mm reduces transverse-direction orientation and shifts tear balance.
Bubble stability is controlled by the interaction of melt temperature, die-gap diameter, blow-up ratio, frost-line height, and air-ring velocity. For Marlex® 7109, a die-exit melt temperature of 190°C to 230°C is common on air-cooled lines. Below 180°C, the resin develops high die pressure and surface melt fracture because the linear molecules do not shear-thin as strongly as branched LDPE. Sustained operation above 245°C can initiate oxidative chain scission and crosslinking; the resulting gel particles appear in film as fish-eye defects and are observable under dark-field or polarized-light inspection.
Blow-up ratios in the range 2.0:1 to 2.8:1 provide a workable balance between machine-direction and transverse-direction orientation. At blow-up ratios above 3.0:1, helical instability and bubble flutter can appear unless the line has a high-efficiency dual-lip air ring, internal bubble cooling, and a stabilizer cage with low-friction surfaces. Below 1.8:1, transverse-direction tear and dart impact may decline and machine-direction stiffness may increase.
Frost-line height is typically maintained between 5 and 8 die diameters. A frost line below 4 die diameters freezes orientation before molecular relaxation and can raise film haze measured under ASTM D1003, while reducing dart impact measured under ASTM D1709. A frost line above 10 die diameters produces a tall bubble that is more sensitive to ambient air currents, tower drafts, and gauge-band variation.
At the same screw speed and die diameter, backpressure is generally higher than that of a high-pressure LDPE of the same melt index. The screw drive current should be monitored against the extruder nameplate rating. On water-cooled grooved-feed liners, feed-section temperatures between 50°C and 80°C are used to prevent pellet slip and feed-throat bridging. The resin is not hygroscopic, so pre-drying is not routinely required; however, condensation from cold-to-warm transfer at relative humidity above 70% can create surface defects in film thicker than 80 µm.
Production-scale failures often involve die-lip buildup, screw surging, and bubble oscillation. Die-lip buildup in linear polyethylenes is associated with low-molecular-weight fractions and oxidized material migrating to the lip; it appears as longitudinal haze bands. Periodic purging with a high-melt-index LDPE or a commercial purge compound helps remove this material. Screw surging is observed when feed-throat temperatures exceed 80°C and pellets stick to the feed throat, reducing feed consistency; maintaining designed feed-throat water flow prevents this. Bubble oscillation at frequencies between 0.5 Hz and 2 Hz can be reduced by lowering air-ring velocity or raising melt temperature slightly within the allowed range.
Application screening uses dart impact resistance under ASTM D1709, Elmendorf tear resistance under ASTM D1922, tensile properties under ASTM D882, haze under ASTM D1003, and coefficient of friction under ASTM D1894. Because blown film is anisotropic, tear strength must be reported in both machine and transverse directions. Dart impact measurements are affected by gauge uniformity and conditioning; comparisons are valid only when thickness is identical and the same test method variant is used.
The coefficient of friction after slip-agent migration is measured under ASTM D1894 after conditioning at 23°C and 50% RH for 24 h. Slip-agent migration kinetics in semicrystalline polyethylene depend on crystallinity, temperature, and film thickness. Films containing migratory slip additives should be tested after the intended aging period rather than immediately after extrusion; immediate readings can overstate the final coefficient of friction.
The performance profile of Marlex® 7109 is governed by the interaction between comonomer short-chain branching and the tie-molecule population in oriented film. When the film is blown at a 2.5:1 blow-up ratio and a frost-line height of 6 die diameters, the orientation created in the transverse and machine directions changes tensile yield, elongation at break, and tear propagation. Tensile testing under ASTM D882 is used to compare grades after conditioning at standard conditions. The resin typically exhibits higher elongation at break and higher dart impact energy than high-pressure LDPE of comparable density when tested under the same conditions, but these benefits are gauge-dependent and are not guaranteed without a certificate of analysis.
Elmendorf tear strength under ASTM D1922 is highly direction-dependent in LLDPE blown films. Transverse-direction tear is usually greater than machine-direction tear because the crystals are preferentially oriented along the machine direction, leaving fewer load-bearing tie chains across the transverse axis. The ratio of transverse-direction to machine-direction tear depends on blow-up ratio and frost-line height. Processors should specify both directions when writing film specifications.
Dart impact resistance under ASTM D1709 Method A is measured on a clamped specimen subjected to a hemispherical striker. The measured dart impact energy rises with film thickness but not linearly; gauge uniformity, gels, and contamination can create premature failure. On production lines, discrepancies between supplier typical values and plant data are commonly caused by differences in die gap, melt temperature, frost line, and stabilization additives.
In comparative testing, the dart impact advantage of LLDPE over LDPE is associated with a more uniform comonomer distribution and a higher tie-molecule concentration. Rapid quenching from a low frost line can reduce spherulite size and alter the tie-molecule network; this is one reason why identical resin can give different dart impact values on different lines. No single laboratory value under ASTM D1709 should be used as the sole acceptance criterion without specifying film gauge and orientation conditions.
| Characteristic | Test or observation method | High-pressure LDPE | Metallocene LLDPE |
|---|---|---|---|
| Melt strength | Extensional bubble stability | Higher | Lower to comparable |
| Dart impact at 25 µm | ASTM D1709 | Lower | Higher |
| Elmendorf tear | ASTM D1922 | Lower | Higher |
| Film haze | ASTM D1003 | Comparable | Lower |
| Extruder torque at equal melt index | Screw drive amperage | Lower | Comparable to higher |
Compared with high-density polyethylene film, Marlex® 7109 has lower density, lower modulus, and lower yield strength, but it usually displays higher Elmendorf tear and dart impact at similar gauge. The trade-off appears because the lower crystallinity of LLDPE permits more tie-molecule formation during orientation, while HDPE's higher crystallinity raises stiffness and reduces energy absorption before fracture. Moisture vapor and oxygen barrier are not primary selection properties for LLDPE; where barrier is required, a coextruded film with HDPE or EVOH layers is used. Published data for Marlex® 7109 in specific coextruded barrier configurations is limited; layer-specific permeation values must be generated on the target structure.
Coextruded film structures often place high-pressure LDPE in the skin layers to improve bubble stability, heat-seal behavior, and surface gloss. Marlex® 7109 is then assigned to a core layer when the structure requires higher dart impact energy and higher tear resistance without increasing total film density. In a three-layer line with a feedblock or annular spiral mandrel, the viscosity ratio between the LLDPE core and the LDPE skins must be kept within the die design window. If the linear resin's viscosity is too high relative to the skins, interfacial instability appears as wavy internal layers; if its viscosity is too low, it may migrate toward the outer layers and reduce the intended surface modification.
Die lip temperatures in coextrusion are generally limited to 230°C to 240°C. At die temperatures above 245°C, thermal degradation products of the resin may deposit at the die lip and create crystallization lines. The line should be purged with a lower-viscosity LDPE before shutdown because the linear resin does not drop in viscosity as rapidly with shear and can remain stagnant in the spiral channels and adapter area.
Without antiblock, low-density polyethylene film can block during winding because of the low glass transition and surface adhesion. The coefficient of friction measured under ASTM D1894 and blocking force under ASTM D3354 are used to evaluate this behavior. If the resin does not contain antiblock, the converter must add a masterbatch and verify dispersion.
Food-contact compliance for the base resin is normally evaluated under 21 CFR 177.1520(c) as an olefin polymer, but the finished film must meet the conditions of use in 21 CFR 176.170(c) and any additive-specific limitations. The converter is responsible for verifying that colorants, slip agents, antiblock masterbatches, or other additives do not change the regulatory status. For the European Union, the supplier safety data sheet and REACH registration number provide the applicable compliance path. RoHS restrictions do not normally apply to unfilled polyolefin resin; however, post-added pigments and processing aids may contain restricted substances and require separate verification.
Operational boundaries include a maximum melt temperature of 245°C and a recommended hold time of less than 5 min at that temperature. Regrind levels above 30% may alter film haze and dart impact; the effect should be measured under ASTM D1003 and ASTM D1709 at the intended gauge. Additive packages containing high levels of free amines or strong bases should not be assumed compatible without a compounding trial because acid-base interactions can alter phenolic antioxidant retention. The resin is not intended for continuous service above 80°C, for medical implant applications, or for radiation sterilization without separate validation. Surface treatments such as corona discharge should be applied at low power density initially and evaluated for dyne level attainment because the low density and additive package can influence treatment decay.