Chevron Phillips Marlex 7105d Polyethylene Film Grade Lldpe Hexene Copolymer

Chevron Phillips Marlex® 7105D Polyethylene Film Grade LLDPE Hexene Copolymer

    • Product Name: Chevron Phillips Marlex® 7105D Polyethylene Film Grade LLDPE Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 398544
    Density 0.918 g/cm3
    Melt Index 0.5 g/10 min
    Tensile Strength At Yield 12.1 MPa
    Tensile Strength At Break 27.6 MPa
    Elongation At Break 700 %
    Flexural Modulus 0.276 GPa
    Vicat Softening Point 100 °C
    Melting Point 124 °C
    Haze 14 %
    Gloss 65 %
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Coefficient Of Friction 0.2

    As an accredited Chevron Phillips Marlex® 7105D Polyethylene Film Grade LLDPE Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg (55.1 lb) polyethylene bags, 40 bags per 1,000 kg pallet; bulk options available.
    Container Loading (20′ FCL) Chevron Phillips Marlex® 7105D film grade LLDPE hexene copolymer: 20′ FCL, 25 kg bags, palletized, shrink-wrapped, securely loaded for export.
    Shipping Chevron Phillips Marlex® 7105D is shipped as solid polyethylene pellets in 25 kg bags, 1,000 kg bulk bags, or palletized boxes. Transport in clean, dry, covered trucks or railcars. Not classified as dangerous goods; protect from moisture, heat, and contamination. Keep sealed until use.
    Storage Store Chevron Phillips Marlex® 7105D in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed and labeled to prevent moisture, dust, and contamination. Protect pallets from physical damage. Maintain ambient warehouse temperatures, avoid prolonged UV exposure, and follow the manufacturer’s SDS for safe handling and storage.
    Shelf Life Marlex® 7105D has no specific shelf life; store cool, dry, sealed, and away from direct sunlight for stability.
    Application of Chevron Phillips Marlex® 7105D Polyethylene Film Grade LLDPE Hexene Copolymer

    When Chevron Phillips Marlex® 7105D is converted into heavy-duty drum and can liners on high-stalk blown film equipment, the processing window is defined not by a single melt temperature value but by the interaction among die gap, bubble cooling configuration, and frost line position. The resin is run through a grooved-feed extruder with a barrier screw and a 25:1 to 30:1 L/D ratio, using a die gap of 1.8–2.5 mm and a blow-up ratio between 2.8:1 and 3.5:1. Melt temperature at the adapter is maintained between 204 °C and 227 °C; sustained operation above 232 °C raises gel formation probability and reduces retained dart impact. Barrel profiles typically move from a feed zone at 40–60 °C through 180–190 °C in zone 1, 200–210 °C in zone 2, and 210–220 °C at the adapter, while screen packs configured at 20/40/60 mesh keep contaminants from entering the die. Internal bubble cooling is preferred because high-stalk hexene LLDPE bubbles exhibit low melt strength at the die lip and require controlled expansion; frost line height is held between 8 and 12 die diameters. Pre-drying is not normally required when storage relative humidity remains below 60%; if surface condensation is observed, a desiccant hopper at 60 °C for 4 h removes adsorbed moisture. Additive dosing for industrial liner formulations includes 2.0–3.0 wt% of a carbon black masterbatch for opacity and UV screening, 300–800 ppm of a fluoropolymer processing aid to delay melt fracture, 500–1,000 ppm erucamide slip where automated liner insertion is specified, and 1,500–2,500 ppm synthetic silica antiblock. At these addition levels, converter specifications for a 100 µm liner commonly require dart drop impact exceeding 350 g under ASTM D1709 and Elmendorf tear retention above 6 N/mm measured to ASTM D5748; published data for this specific configuration is limited, so qualification on the exact film line is required. Finished articles are used as 55-gallon drum liners, construction debris bags, and contaminated waste liners, where puncture propagation resistance and machine-direction tear determine service life. Regulatory compliance for heavy-duty industrial liners is evaluated against REACH Annex XVII restrictions, RoHS heavy-metal limits, and EU Packaging Directive 94/62/EC summation limits for lead, cadmium, mercury, and hexavalent chromium.

    How Does UV Stabilizer Dispersion Limit Outdoor Exposure in Agricultural Silage Covers?

    Agricultural silage covers and bunker clamps produced from this resin require an additive package that survives both initial compounding and repeated flexing at sub-zero temperatures. The base polymer is dry-blended with 0.20–0.60 wt% of a high-molecular-mass hindered amine light stabilizer, 0.10–0.30 wt% of a benzotriazole or benzophenone UV absorber, and—for black silage film—2.0–2.5 wt% carbon black masterbatch. The stabilizer package is incorporated through a gravimetric dosing unit at the extruder throat rather than precompounded, because residence time distribution in a 24:1 single-screw extruder can locally degrade some HALS chemistries if melt temperature exceeds 210 °C. Blown film lines should operate at a blow-up ratio of 2.8:1 to 3.2:1, a die gap of 2.0–2.5 mm, and a melt temperature of 190–210 °C. Internal bubble cooling is used to keep gauge variation below ±5% on 150 µm covers. Film is evaluated using ISO 527-3 for tensile yield and elongation, ASTM D1709 for dart impact, ASTM D3895 for oxidative induction time at 200 °C, and ISO 4892-2 for accelerated xenon-arc weathering. A common acceptance criterion for silage covers is retention of at least 50% of initial elongation after 1,500 h xenon-arc exposure. The terminal products are bunker silo covers, clamp films, and temporary silage bags used in dairy and forage operations.

    Test standardParameterProduction gate for silage covers
    ISO 527-3Tensile elongation at breakReport baseline before weathering
    ASTM D1709Dart drop impact, 150 µm≥ 500 g typical converter minimum
    ASTM D3895Oxidative induction time at 200 °C≥ 20 min
    ISO 4892-2Elongation retention after 1,500 h≥ 50% of initial

    On side-gusseted freezer bags converted from blown tubular film, the critical failure mode is fold-line puncture after filling at -25 °C and subsequent stacking, not room-temperature dart impact. The film is run at 50–75 µm gauge, with a blow-up ratio of 2.0:1 to 2.5:1 to balance low-temperature tear resistance with transverse direction strength. The heat-seal operation on side-weld bag equipment uses seal-bar temperatures of 115–135 °C, dwell times of 0.4–0.8 s, and jaw pressures of 2.0–3.5 bar; seal initiation is depressed by the hexene comonomer but shifts upward when erucamide slip exceeds 800 ppm because of migration to the seal interface. Additive loadings for freezer-grade film are therefore limited to 500–800 ppm erucamide and 1,500–3,000 ppm synthetic silica antiblock. Food-contact compliance is assessed under FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 with overall migration below 10 mg/dm² under OM2 conditions. Film converted for frozen vegetables, seafood, and poultry packaging is also tested to ASTM D1709 method B at -18 °C for low-temperature dart impact and to ASTM F88 for seal strength; a typical acceptance limit is 12 N/25 mm for a 50 µm film. Production lines running this grade often observe seal-bar fouling after 48–72 h continuous operation if slip levels are too high; cleaning cycles should not be extended beyond 72 h for automated frozen food packaging.

    When Pre-Stretch Ratios Exceed 200% in Blown Stretch Film

    Blown stretch film produced from hexene LLDPE of this class enters a different mechanical regime when powered pre-stretch carriages apply ratios above 200%. At these extension levels, the strain-hardening response of the film becomes the primary control on load retention and pallet unitization. The base resin is blended with 1.0–2.0 wt% polyisobutylene cling agent or a comparable low-molecular-weight tackifier; cling is measured as 50–150 g force under ASTM D5458 and must be rechecked after 24 h because migration continues after winding. Machine film gauge is typically 18–30 µm, and the blown film process uses a die gap of 0.8–1.2 mm, a blow-up ratio of 3.5:1 to 4.5:1, and melt temperature of 220–235 °C. Melt temperature above 240 °C reduces cling consistency and increases gel streaks. Puncture propagation resistance is measured by ASTM D5748, tensile properties by ASTM D882, and pre-stretch retention by filming a palletized load at 250% stretch and measuring residual film force. Hexene comonomer provides measurably higher dart impact and tear resistance than butene LLDPE at equivalent gauge, which allows downgauging to 18 µm without breaching ASTM D1709 minimums. The terminal product is used for hand wrap and powered machine pallet wrapping in distribution warehouses. Operational boundaries include ambient temperature above 15 °C during slitting and winding; below this temperature, cling transfer to the backside of the film becomes uneven, producing telescoped rolls on high-speed unwind.

    Form-Fill-Seal Sealant Web Hot Tack and Product-Weight Tolerance

    Conversions on vertical form-fill-seal lines impose a narrow hot tack window because the seal must hold the product drop weight before cooling. Film produced from the resin is commonly blended with 20–30 wt% of a high-pressure LDPE to stabilize the bubble and broaden the sealing range. The sealant web is run at 50–100 µm gauge with a blow-up ratio of 2.2:1 to 2.8:1 and a die gap of 1.5–2.0 mm. Hot tack is measured under ASTM F1921; seal strength is measured under ASTM F88; seal initiation temperature is reported as the temperature at which 8.8 N/25 mm seal strength is reached. For high-speed VFFS equipment running 60–80 bags per minute, a hot tack force of 4 N/25 mm at 120 °C and 0.3 s dwell is a common production gate. Slip and antiblock must be tightly capped: erucamide slip is held below 800 ppm because higher levels migrate to the seal surface and increase seal initiation temperature by 3–5 °C; synthetic silica antiblock is maintained at 1,000–2,000 ppm to limit blocking without creating microvoids. The final structures include gusseted pet food bags, dry-mix pouches, and heavy-duty product sacks. Food-contact status is governed by FDA 21 CFR 177.1520 and EU 10/2011; converter-specific declarations are required for multi-layer structures containing LDPE or color concentrates.

    Coextruded pouch conversion exposes sealant layer defects not visible in flat film

    During three-layer coextrusion for non-retort pouch structures, the resin is placed as the sealant skin at 15–25% of total film thickness, typically opposite a stiff outer skin and a barrier core. The die gap is set at 2.3 mm, and melt temperature for the sealant layer is maintained at 210–225 °C. Because the sealant layer is the last surface to solidify at the nip, interfacial instability appears as pock marks or die lines only after lamination or pouch formation. The film is converted into pouches for dry beverage mixes, pet food, and powdered ingredients; seal integrity is checked after filling by vacuum leak testing to ASTM D3078, and seal strength is evaluated to ASTM F88 with a minimum of 14 N/25 mm for a 60 µm structure. Regulatory compliance for direct food contact is determined by FDA 21 CFR 177.1520(c) specifications for olefin polymers and by EU 10/2011 overall migration testing under OM2 conditions. Incompatibility with high-acid or alcohol-containing filling conditions should be reviewed because hexene LLDPE sealant layers can show environmental stress cracking in aggressive surfactants; published data for this specific configuration is limited, and pouch converters should run storage stability panels at 40 °C for 12 weeks before commercial release.

    Free Quote

    Competitive Chevron Phillips Marlex® 7105D Polyethylene Film Grade LLDPE Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Marlex® 7105D is a linear low-density polyethylene film resin produced with 1-hexene as the comonomer. The material is classified as an ethylene-hexene copolymer and differs from butene-copolymer LLDPE of similar nominal density and melt index by the length of the short-chain branch introduced during polymerization. The resin is supplied as pellets and is specified for tubular blown-film extrusion where gage reduction, dart impact resistance, and tear propagation resistance are evaluated simultaneously on formed film. Nominal supplier-published values include a melt index of 1.0 g/10 min at 190 °C/2.16 kg and a density of 0.918 g/cm³. Those values are classification properties and incoming quality-control references, not direct film performance guarantees. Film tensile, tear, impact, and optical characteristics are fabricated-structure properties and must be determined using ASTM D882, ASTM D1922, ASTM D1709, ASTM D5748, ASTM D1003, and ASTM D2457 on film produced under defined extrusion parameters. In comparison with LDPE film resins of the same nominal density, Marlex® 7105D typically exhibits higher tensile strength at break and higher puncture propagation resistance when measured on conditioned film; however, its melt strength in a molten bubble is lower, which narrows the bubble-stability window on certain high-stalk lines. In comparison with HDPE film grades, the 0.918 g/cm³ density produces a lower secant modulus and usually improves low-temperature impact resistance while reducing moisture-barrier performance.

    The designation “film grade” reflects molecular architecture and rheological balance intended for blown-film extrusion rather than injection molding or blow molding. The selection of hexene rather than butene is technically significant because hexene incorporation creates a longer side branch than butene incorporation. This does not materially increase melt entanglement, but it alters lamellar chain folding and can affect the population of stress-transmitting tie molecules in semicrystalline film. The resulting film-physics changes must still be demonstrated by standard mechanical tests because comonomer type alone does not define a fixed property outcome.

    Which standard test methods fix the specification envelope for Marlex® 7105D?

    Incoming resin control for Marlex® 7105D is based primarily on ASTM D1238 and ASTM D1505. Melt index is determined by extruding the molten polymer through a standardized die under a 2.16 kg load at 190 °C; the result is reported as grams of polymer discharged in 10 min. Density is measured by density gradient column under ASTM D1505. A supporting thermal property is peak melting temperature by differential scanning calorimetry under ASTM D3418. For this density class, the peak melting endotherm is commonly near 122 °C, but the value depends on comonomer distribution and thermal history and is not a universal specification. The following table consolidates the principal resin-level parameters.

    PropertyTest methodNominal value
    Melt indexASTM D1238, 190 °C/2.16 kg1.0 g/10 min
    DensityASTM D15050.918 g/cm³
    Peak melting temperatureASTM D3418122 °C

    Film mechanical values are deliberately excluded from the specification table because they cannot be defined independently of extrusion history. ASTM D882 requires conditioned film specimens of controlled thickness. ASTM D1922 and ASTM D1709 require film samples and are sensitive to die gap, blow-up ratio, frost line height, melt temperature, and film gauge. The same resin lot processed at a 1.0 mm die gap and 2.0:1 blow-up ratio will produce a different tear balance from film produced at a 2.5 mm die gap and 2.8:1 blow-up ratio. Any comparison between Marlex® 7105D and another LLDPE grade should therefore be made on film produced on the same line configuration and conditioned at 23 °C ± 2 °C and 50 % ± 10 % RH according to ASTM D618 or the conditioning clause of the relevant test method.

    A direct comparison of comonomer types requires separation of density, melt index, molecular weight distribution, and fabrication history. At equivalent density and melt index, a hexene-copolymer LLDPE differs from a butene-copolymer LLDPE chiefly in branch length: hexene contributes a butyl branch, while butene contributes an ethyl branch. The longer branch does not increase chain entanglement in the melt; it influences the way polymer chains fold into lamellae and the number of tie molecules formed between crystalline regions. Because tie molecules are a primary factor in high-speed puncture and dart impact resistance, the architecture can shift the balance measured by ASTM D1709 and ASTM D5748. Octene-based LLDPE carries a hexyl branch and can offer further toughness at equivalent density, but it may require different seal-barrier trade-offs and is generally evaluated when a butene or hexene grade cannot meet target values. Published data for the specific comparison between Marlex® 7105D and any particular butene or octene grade on a specific production line is limited; therefore, a site trial on the intended film line is required before quantitative film property claims are made.

    Metallocene-catalyzed LLDPE grades generally exhibit a narrower molecular weight distribution and lower melt strength than this conventional Ziegler-Natta hexene grade. That difference can produce better optics and lower seal initiation temperature in mLLDPE, but it may reduce bubble stability on older blown-film lines without internal bubble cooling. Marlex® 7105D is not a metallocene grade; its broader processing window on standard single-screw and multilayer blown-film equipment is a key point of comparison when evaluating replacement of butene-copolymer LLDPE in heavy-duty film structures.

    Processing window and bubble stability on high-stalk blown-film lines

    Tubular blown-film extrusion of Marlex® 7105D requires control of melt temperature, die lip temperature, blow-up ratio, frost line height, and film gauge. Typical starting conditions on a 60 mm single-screw extruder with a 24:1 L/D barrier screw and a 250 mm annular die are a barrel temperature profile from 170 °C at the feed throat to 195–210 °C at the die, a die gap of 1.5–2.5 mm, and a blow-up ratio of 2.0:1–2.5:1. The 1.0 g/10 min melt index indicates a moderate-molecular-weight resin that does not generally produce excessive screw torque in single-layer or multilayer film lines. If the melt temperature is too low, the resin may exhibit sharkskin melt fracture at the die lip; if it is too high, bubble cooling demand increases and the frost line may become unstable. The frost line height for a low-stalk bubble is generally held in the range of 3–8 die diameters, while high-stalk operation may require 10–14 die diameters. High-stalk processing increases machine-direction orientation and may improve tensile strength at the expense of transverse-direction tear, which is quantified by ASTM D1922.

    The addition of processing aids is not universally required. If thin-gauge film below 20 µm is produced on a die gap of 1.0 mm or smaller, melt fracture can be suppressed by increasing the die lip temperature to 210–220 °C or by adding fluoropolymer processing aid at a concentration determined by the processing aid supplier. The effect of processing aid should be verified by measuring film haze per ASTM D1003 and by gel count per ASTM D6290, because an over-concentration can create plate-out on the die lip or reduce film clarity. For high-output lines with internal bubble cooling, the cooling air temperature should be maintained below 15 °C to reduce blocking at the collapsing frames, particularly at film gauges above 50 µm.

    When Marlex® 7105D replaces a butene-based LLDPE in three-layer coextrusion equipment

    The substitution should be evaluated on the basis of rheology, not solely on density and melt index. A three-layer line with 70 mm extruders, 30:1 L/D barrier screws, and a 400 mm rotating die with 1.8 mm die gap will not necessarily run the hexene resin at the same screw speeds, melt temperatures, or frost line settings as a butene grade. The first observable change is often a shift in extruder pressure and motor load because the molecular weight distribution and shear-thinning behavior may differ. A capillary rheometry screening under 190 °C and 210 °C in accordance with ASTM D3835 is recommended before the trial to identify differences in apparent viscosity between 100 s⁻¹ and 1000 s⁻¹. If the hexene grade shows higher melt viscosity at low shear rates, bubble instability may appear at high blow-up ratios. Reducing the blow-up ratio to 2.2:1 and moving the frost line downward usually stabilizes the bubble. Conversely, if the grade shows lower viscosity at high shear rates, die lip temperature may be increased to 205–215 °C to prevent sharkskin.

    Film dart impact and tear should be measured after each process adjustment using ASTM D1709 and ASTM D1922, with samples taken from both machine-direction and transverse-direction film. Because comonomer type influences seal initiation, heat-seal curves should be generated according to ASTM F1921 or ASTM F88 if the film is used in a form-fill-seal operation. Layer distribution is not an intrinsic resin property; it is controlled by extruder screw speed and die design. Changing from a butene grade to Marlex® 7105D may require screw speed adjustment to maintain layer thickness because melt density and specific throughput can differ.

    For food-contact evaluation, the finished film must not be certified based solely on the base resin. The olefin polymer may be covered under FDA 21 CFR §177.1520, but the applicable paragraph (c) density and maximum extractable fraction conditions must be verified against the actual lot. In the European Union, plastic food-contact materials must comply with Commission Regulation (EU) No 10/2011, including overall migration limits of 10 mg/dm² when tested with food simulants under EN 1186. Specific migration testing is governed by EN 13130 and depends on the additives and colorants incorporated at the converting step. The base polyethylene is not a formulated food-contact article; therefore, the converter is responsible for final compliance. For industrial packaging not intended for food, a regulatory data sheet and REACH confirmation should be requested from the supplier. The resin does not contain intentionally added heavy metals or phthalates; RoHS screening is generally not applicable to raw polyolefin resin but may be required for finished electronic packaging.

    Marlex® 7105D is optimized for blown film. It is not intended for injection molding, sheet extrusion, or rotational molding, where melt elasticity and molecular weight requirements differ. Polymer melt temperature should remain below 260 °C; prolonged hold-up at high temperature can generate gels and degrade film appearance. If the resin is stored under high humidity and visible moisture is present, drying at 70–80 °C for 2 h is common practice; dry pellets do not require pre-drying. The material should not be exposed to strong oxidizing agents, aromatic or chlorinated solvents, or outdoor ultraviolet radiation without a stabilizer package. Film intended for outdoor service requires addition of UV stabilizers via masterbatch; the base resin as supplied may not contain sufficient UV stabilization for multi-year agricultural or construction films. Any such formulation should be tested for retained tensile properties after accelerated weathering according to ASTM D4329 or ISO 4892-2.

    Top