| HS Code | 190659 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Hexene-1 |
| Grade | Film Grade |
| Melt Index | 1.0 g/10 min |
| Density | 0.918 g/cm³ |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 31.0 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 241 MPa |
| Dart Drop Impact | 110 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 350 g |
| Haze | 8% |
| Gloss | 60% |
| Coefficient Of Friction | 0.2 |
As an accredited Chevron Phillips Marlex® 7105 Film Grade LLDPE Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Marlex® 7105 is supplied in 25 kg (55 lb) polyethylene bags, palletized; also available in bulk trucks or railcars. |
| Container Loading (20′ FCL) | 20′ FCL: 25 kg bags, approximately 18–20 MT net, loose loaded, subject to container weight and volume limits. |
| Shipping | Chevron Phillips Marlex® 7105 Film Grade LLDPE Hexene Copolymer ships as a non-hazardous solid resin in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Store cool and dry, away from heat, moisture, and direct sunlight. No DOT placards required. |
| Storage | Store Marlex® 7105 LLDPE in its original, sealed packaging in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, ignition sources, moisture, and contaminants. Maintain ambient temperature and avoid prolonged UV exposure. Protect bags/pellets from sharp objects, crushing, and excessive stacking. Use first-in, first-out stock rotation to preserve product quality. Ensure containers remain closed when not in use. |
| Shelf Life | No specific shelf life; stable under normal storage in unopened original packaging, away from heat, moisture, and direct sunlight. |
Blown film converted into 50 kg chemical shipping sacks and construction rubble bags subjects the seal and body web to different failure modes: dart impact on the unsupported web against filled rigid granules, and Elmendorf tear propagation at folds and gusset seams. Marlex® 7105 is characterized by a nominal density of 0.918 g/cm³ under ASTM D1505 and a melt flow index of 1.0 g/10 min at 190°C/2.16 kg under ASTM D1238, a combination that retains the hexene comonomer’s higher dart impact and tear initiation resistance at downgauged 125–200 µm thicknesses. Industrial sack formulation typically uses 70–85 wt% Marlex® 7105, 15–30 wt% low-density polyethylene homopolymer with melt index 0.25–2.0 g/10 min for bubble stability and heat-seal latitude, and up to 10 wt% calcium carbonate masterbatch only when opacity is required. The blown film line is usually a single-screw grooved-feed extruder with 30:1 L/D and a barrier screw, feeding a spiral mandrel die of 200–300 mm diameter through a screen pack of 80–120 mesh; die gap is held at 2.0–2.5 mm to avoid sharkskin and melt fracture with a low-melt-index hexene copolymer. Melt temperatures at the die lip are 205–215°C, blow-up ratio 2.0:1–2.5:1, and frost line height 750–900 mm, producing output of 160–220 kg/h on a 65 mm extruder. If film line operators reduce die gap below 1.5 mm to improve gauge control, surface melt fracture increases unless a fluoropolymer-based polymer processing aid is added at 200–400 ppm; this operational boundary cannot be resolved by raising melt temperature past 220°C without risk of gel formation. Compliance for dangerous goods sacks requires UN 5H2 certification under ADR/RID/IMDG where applicable, with physical testing by ASTM D1709 Method A for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D882 for tensile properties. Terminal product types include 25 kg chemical sacks, 50 kg construction rubble bags, sandbags, and insulation batt packaging, where the film must maintain seal integrity after drop cycles rather than merely meeting initial tensile yield.
Greenhouse cladding produced from Marlex® 7105 is formulated as a monolayer or three-layer blown film with a nominal thickness of 150–200 µm for multi-season installations. The resin fraction is typically 92–96 wt% after allowance for masterbatch additions; stabilizer concentrates are added at 4–8 wt%, with hindered amine light stabilizer active content of 0.20–0.60 wt% against UV degradation, anti-fog concentrate at 1.0–2.5 wt%, and silica-based anti-block at 0.3–0.8 wt% to prevent film layers from blocking on the roll. Processing is performed on a three-layer blown film line with die diameter 250 mm, die gap 1.8–2.2 mm, blow-up ratio 2.5:1–3.0:1, and frost line height 900–1100 mm; die lip temperature is maintained at 190–210°C to limit degradation of the stabilizer package. The key production conflict is that sulfur-containing pesticide sprays and fumigants can deactivate certain hindered amine chemistries; film service life in greenhouse rose or tomato houses is therefore evaluated under EN 13206:2017 for thermoplastic films used in agriculture and horticulture, with artificial weathering and tensile retention testing after exposure. Published weathering data for this specific resin with sulfur-resistant N-alkoxy hindered amine stabilizers are limited; converter validation under EN 13206:2017 therefore requires a site-specific installation trial rather than relying on laboratory-only UV exposure. The terminal products are greenhouse cladding, low tunnel covers, silage stretch wrap, and silage clamp sheets. In sulfur-rich environments, a N-alkoxy hindered amine stabilizer is specified, and exposure to acidified sulfur residues must be monitored by measuring retained elongation in accordance with ISO 527-3. Addition of the anti-fog package above 2.5 wt% is not recommended because migration to the film surface can accelerate contact blocking under high tunnel humidity.
Frozen food packaging films made from Marlex® 7105 are usually monolayer blown structures of 40–80 µm, designed to survive impact at air temperatures as low as −35°C in spiral freezers without puncturing on particulate frozen product. The formulation addition ratio is 85–100 wt% Marlex® 7105, with 0–15 wt% LDPE homopolymer added when increased melt strength and hot tack are needed for vertical form-fill-seal conversion. Slip and anti-block masterbatch is metered at 0.5–1.0 wt%, and fluoropolymer processing aid at 200–400 ppm when die gap is below 2.0 mm. Extrusion is carried out on a 50–75 mm single-screw extruder with 24:1–30:1 L/D barrier screw, spiral mandrel die gap 1.5–2.0 mm, blow-up ratio 2.2:1–2.8:1, and melt temperature 195–215°C. The film is subsequently corona-treated to 38–42 dyn/cm for print or lamination adhesion. Food-contact compliance rests on FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011, with overall migration limited to 10 mg/dm² under Article 12. Terminal finished products include IQF vegetable pouches, frozen fruit bags, meat block packaging, and ice bags. A specific operational boundary is that film destined for direct food contact must not use slip additives that are outside the positive list; pre-drying is not normally required, but hopper moisture condensation above 60% RH should be managed with dry-air purging to prevent surface defects. Corona treatment above 42 dyn/cm accelerates surface oxidation and can reduce heat-seal strength on vertical form-fill-seal lines.
In municipal and institutional refuse sack extrusion, the economic target is down-gauging to 60–80 µm while retaining tear propagation resistance at side seams after wet-waste compaction. Marlex® 7105 is normally let down with 10–20 wt% post-industrial reclaim or low-density polyethylene homopolymer, giving a final film with dart impact values controlled under ASTM D1709 Method A and Elmendorf tear under ASTM D1922. The use of filler masterbatch above 5 wt% is generally excluded because calcium carbonate reduces Elmendorf tear and puncture resistance disproportionately at thin gauges. A 75 mm grooved-feed extruder with 30:1 L/D, screen changer with 80 mesh pack, and 1.8–2.3 mm die gap is operated at blow-up ratio 2.0:1–2.5:1 and output 250–300 kg/h; internal bubble cooling is required above 220 kg/h to prevent blocking and to stabilize frost line height at 800–1000 mm. Compliance testing for sacks used in municipal collections follows EN 13592 for household waste sack types and test methods, alongside tensile property measurement per ASTM D882. Terminal product types include 60–100 µm wheeled bin liners, hospital compactor sacks, and wet-waste liners for food service operations. Processing limitation: reclaim streams with high levels of polyethylene terephthalate contamination must be filtered below 100 µm particle size to prevent die lines and tear initiation at contaminant particles.
Compliance matrix for the six downstream applications is consolidated below to align converter specifications with the relevant test method designations and regulatory references.
| Application | Standard or regulation | Test condition / endpoint |
|---|---|---|
| Heavy-duty shipping sacks | UN 5H2, ASTM D1709 Method A, ASTM D1922, ASTM D882 | Dart impact F50, Elmendorf tear propagation, tensile properties at 23°C |
| Agricultural greenhouse and silage film | EN 13206:2017, ISO 527-3 | Artificial weathering, retained tensile elongation, sulfur-pesticide exposure validation |
| Frozen food packaging | FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011 Article 12 | Overall migration limit 10 mg/dm², frozen-food contact at −35°C |
| Institutional refuse sacks | EN 13592, ASTM D1709, ASTM D1922, ASTM D882 | Wet-waste compaction tear resistance, dart impact after downgauging |
| Stand-up pouch sealant web | FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011, ASTM F88 | Seal strength, flex-crack resistance at −20°C, migration limits |
| Fresh-cut produce bags | ASTM D3985, ASTM F2476, FDA 21 CFR 177.1520 | Oxygen transmission rate, carbon dioxide transmission rate, direct produce contact |
Stand-up pouch laminates for frozen or refrigerated liquid and dry products use a blown film sealant web based on Marlex® 7105 to provide low-temperature flex-crack resistance and seal integrity through contaminated seal areas. In a three-layer laminate construction of oriented polyester or biaxially oriented polypropylene, the sealant web is 20–25 wt% of the total structure and is produced from 100 wt% Marlex® 7105 with 0.5–1.0 wt% anti-block masterbatch. The film is extruded on a 50 mm extruder with 24:1 L/D, die gap 1.5–2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 195–215°C. Corona treatment to 38–42 dyn/cm is applied before adhesive lamination to the printed web. Seal strength is verified under ASTM F88, and food-contact status is maintained under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011, with migration limits assessed for the final laminate. Terminal product types include stand-up pouches for frozen fruit, liquid detergent refill pouches with abrupt geometry at the bottom gusset, and dry powder beverage packs. The operational boundary is that heat-seal initiation temperature of Marlex® 7105 is near 100–110°C; converters running horizontal form-fill-seal lines must re-verify seal jaw pressure and dwell after changing from a lower-melt-index LDPE sealant because the hexene copolymer exhibits a narrower hot tack window at high seal temperatures above 130°C.
Fresh-cut produce bags require a combination of carbon dioxide transmission relative to oxygen transmission, low haze from anti-fog condensation control, and resistance to tear initiation from sharp vegetable edges. Marlex® 7105 is used at 100 wt% resin fraction with 1.0–2.0 wt% food-grade anti-fog concentrate and 0.5–1.0 wt% slip/anti-block masterbatch. The film is produced on a 40–65 mm extruder with 24:1–30:1 L/D, die gap 1.5–2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 190–210°C. Because gas transmission is thickness-dependent, the gauge is held at 25–40 µm and verified with ASTM D3985 for oxygen transmission rate and ASTM F2476 for carbon dioxide transmission rate, rather than relying on filler loading. Mechanical perforation by macro-perforation or micro-perforation is used to set modified atmosphere exchange rates; additive-based permeability adjustment is not used because it creates seasonal variability in cold storage. Compliance is under FDA 21 CFR 177.1520 for direct contact with washed or raw produce and EU Regulation (EU) No 10/2011. Terminal product types include single-use salad bags, spinach bags, shredded cabbage pouches, and perforated vegetable bags for cold chain distribution. An operational boundary is that corona treatment should be limited to the outer surface only; inner surface corona can reduce anti-fog efficacy and increase seal initiation variability. Anti-fog masterbatch addition above 2.0 wt% is unnecessary and can create visible streaking at film edges after slitting.
Competitive Chevron Phillips Marlex® 7105 Film Grade LLDPE Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Chemical Marlex® 7105 is a hexene-copolymer linear low density polyethylene supplied as pellets for blown and cast film extrusion. Nominal solid-state density is 0.918 g/cm³ when measured under ASTM D1505-18, and nominal melt index is 0.5 g/10 min at 190 °C with a 2.16 kg load under ASTM D1238-20. The resin is used in industrial liners, heavy-duty sacks, frozen food packaging, and coextruded sealant webs. Because the incorporated comonomer is 1-hexene, the material contains butyl side branches that disrupt crystal regularity more than the ethyl branches of butene-copolymer LLDPE. This structural difference produces a higher population of tie molecules at equivalent density and melt index, which affects dart impact, tear propagation, and down-gauging behavior. Converters replacing a butene-copolymer LLDPE in an existing structure should revalidate die gap and frost-line height rather than assuming identical extrusion conditions.
The longer butyl branches increase interlamellar tie-chain concentration. Measurements are normally made with ASTM D1709-16a for free-falling dart impact and ASTM D1922-23 for Elmendorf tear. The effect is most pronounced in film below 50 µm, where local stress concentration dominates failure. No universal film value is published for this resin; converter film certificates of analysis must be generated under fixed die geometry, melt temperature, and cooling rate to permit comparison against butene-based LLDPE.
On a monolayer line equipped with a 90 mm single-screw extruder having a 30:1 L/D ratio and a barrier feed screw, stable extrusion is commonly maintained at a melt temperature of 193 °C to 221 °C. Feed-throat barrel zones are set between 177 °C and 204 °C; adapter and die zones are held at 204 °C to 216 °C. Melt temperatures above 260 °C promote oxidative gel formation and die-lip deposits. Shear stress at the die lip governs sharkskin melt fracture. With a narrow die gap of 1.0 mm, moderate screw speeds can exceed the critical shear stress for the resin; a fluoropolymer processing aid masterbatch at 400 ppm to 800 ppm is commonly added to delay the onset of melt fracture. Screen-pack pressure oscillations increase when post-industrial reclaim exceeds 15 wt%, especially if the reclaim contains label adhesive or ink binder. In that condition, screen-pack fouling rather than screw recovery becomes the limiting output factor.
Bubble stability is controlled by internal bubble cooling, air-ring geometry, and frost-line height. Blow-up ratios from 2.0:1 to 2.5:1 typically support balanced machine-direction and transverse-direction tear. Frost-line heights of 2 to 3 die diameters stabilize the neutral bubble on conventional air rings; higher frost lines increase transverse-direction orientation and can produce gage bands. On older air-ring systems without internal bubble cooling, bubble sway and edge weave appear when melt temperature falls below 193 °C. Adding up to 20 wt% high-pressure LDPE raises melt strength and dampens oscillation, but it reduces dart impact and tear values relative to the neat hexene-copolymer film. For maximum toughness, LDPE addition is therefore an operational remedy rather than a preferred formulation.
In cast film conversion, die gaps of 0.5 mm to 0.8 mm and melt temperatures from 232 °C to 260 °C are common for this density class. Higher melt temperatures relax melt memory and improve optical clarity, but they consume antioxidant and may generate gels near the die lip. On a 75 mm extruder with a 40:1 L/D, output is often limited by chill-roll heat removal rather than screw recovery. Chill-roll temperature is commonly held at 15 °C to 25 °C to reduce post-extrusion crystallization and haze. Draw resonance is observed when the draw ratio exceeds the critical value for the die-to-roll gap; lowering melt temperature or reducing chill-roll speed can stabilize the web.
When Marlex 7105 is used as a sealant skin in a three-layer blown film structure, the sealant layer typically occupies 20% to 30% of total film thickness. Seal initiation measured under ASTM F1921-23 generally falls below that of LDPE films, and seal strength under ASTM F88/F88M-23 remains stable over a broader jaw-temperature interval. The broader melting range and lower residual crystallinity in the seal region reduce edge-seal failures on vertical form-fill-seal machines running above 60 packages/min. Converter qualification should include seal-strength tests at 5 °C increments across the jaw setpoint range because published hot-tack data for this specific resin is limited.
The following matrix summarizes standard methods used for incoming resin and film lot acceptance. Values listed as “certificate required” are not specification limits; they must be obtained from the supplier or from a fixed film line.
| Property | Test method | Unit | Nominal value or control |
|---|---|---|---|
| Melt flow rate | ASTM D1238-20 | g/10 min | 0.5 |
| Solid-state density | ASTM D1505-18 | g/cm³ | 0.918 |
| Dart impact on 25 µm film | ASTM D1709-16a Method A | g | Certificate required |
| Elmendorf tear MD/TD | ASTM D1922-23 | gf | Certificate required |
| Secant modulus at 1% strain | ASTM D882-18 | MPa | Certificate required |
| Gloss at 60° | ASTM D2457-21 | GU | Certificate required |
Compared with a butene-copolymer LLDPE of equivalent density and melt index, hexene-copolymer LLDPE generally exhibits higher dart impact and tensile energy absorption because the longer butyl comonomer branches generate more interlamellar tie chains. The difference is most visible in film below 50 µm. Machine-direction and transverse-direction tear are not uniformly improved; orientation state depends on blow-up ratio, die gap, and frost-line height. A butene-LLDPE film that fails by puncture at equal thickness may still show similar tensile break strength, so dart impact and Elmendorf tear rather than elongation at break should control the substitution decision.
Relative to high-pressure LDPE film resins, Marlex 7105 has lower melt strength and less extensional hardening. Unsupported bubble configurations without internal bubble cooling are therefore more difficult to run. In coextruded structures, LDPE is frequently used as a core or skin layer to stabilize the bubble, while the hexene-LLDPE layer provides toughness or seal performance. For extrusion coating, shrink film, or foaming where melt extension is critical, an LDPE or a high-LDPE blend is generally preferred.
In heavy-duty sack production, film thicknesses from 100 µm to 200 µm are common. The limiting failure mode is often dart impact at side gussets or tear propagation from a puncture. Converters changing from a butene-copolymer LLDPE to Marlex 7105 may observe lower puncture failure rates at equal thickness, but downgauging trials require actual bag drop and field verification because published data for this specific resin under filled-sack conditions is limited. The reduction in gauge that can be achieved is machine-dependent and cannot be stated as a universal percentage.
Marlex 7105 is a conventional broad-molecular-weight-distribution LLDPE. Compared with metallocene-catalyzed LLDPE, this gives higher melt strength on older blown film lines and lower die-lip shear stress at the same output, but also higher haze and potentially higher extractables. For transparent packaging requiring haze below 5% at 25 µm and gloss above 70 GU at 60° under ASTM D2457-21, a metallocene-catalyzed LLDPE may be more suitable. For heavy-duty industrial film above 75 µm, optical clarity is usually secondary to toughness and process stability; the conventional hexene-copolymer structure of Marlex 7105 is often retained.
A converter retrofitting a 50 mm extruder with a 1.2 mm die gap may find Marlex 7105 easier to process than a narrow-distribution metallocene resin because the shear-thinning response of the broader distribution reduces die-lip shear stress. In contrast, high-speed cast film with tight gage uniformity may favor metallocene resins because narrower composition distribution reduces draw resonance. The choice therefore depends on the extrusion line, chill-roll or air-ring capacity, and final film specification rather than on resin class hierarchy.
Drying is not normally required because polyethylene has negligible equilibrium moisture absorption. If cold pellets are moved into a warm, humid extrusion bay with relative humidity above 60%, surface condensation can introduce moisture into the feed throat. When condensate is visible, a hopper dryer set at 65 °C for 2 h is sufficient. Hopper temperatures above 80 °C can soften pellet surfaces and cause bridging. Conveying lines should be dedicated or purged before product changes; uncontrolled mixing with butene-copolymer LLDPE or LDPE will shift tear balance and seal performance unpredictably.
For film blocking control, antiblock masterbatches containing diatomaceous earth or talc are typically used at 1,000 ppm to 5,000 ppm. Calcium carbonate antiblock above 2,000 ppm may increase haze and reduce dart impact, with the exact threshold depending on particle size distribution. Slip agents such as erucamide migrate to the surface over 24 h to 72 h after extrusion, as tracked by coefficient of friction under ASTM D1894-14. Seal strength and print adhesion can change during this migration interval; seal testing should be timed after the migration window to avoid misleading low seal-strength readings. Erucamide addition must be balanced because excessive slip-agent bloom can reduce seal strength at elevated jaw temperatures.
For food-contact films, the converter must obtain the supplier’s compliance letter for FDA 21 CFR 177.1520 covering olefin polymers. End-use limitations and extractives restrictions apply to the final film rather than the neat resin. In the European Union, the film must meet the overall migration limit of 10 mg/dm² under EU Regulation (EU) No 10/2011, with testing in food simulants appropriate to the intended food type. Packaging applications are also subject to Directive 94/62/EC, which limits the sum of cadmium, mercury, lead, and hexavalent chromium to 100 ppm by weight. Documentation should be retained by the converter to support due diligence during food-safety and packaging-enforcement audits.