| HS Code | 404716 |
| Density | 0.918 g/cm3 |
| Melt Index 190 C 2 16 Kg | 0.8 g/10 min |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 31.0 MPa |
| Elongation At Break | 800 % |
| Flexural Modulus | 207 MPa |
| Vicat Softening Point | 93 °C |
| Melting Point | 121 °C |
| Brittleness Temperature | <= -70 °C |
| Haze | 10 % |
| Gloss | 70 % |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 220 g |
| Elmendorf Tear Strength Td | 350 g |
As an accredited Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg net), for Chevron Phillips MarFlex HHM TR-258. |
| Container Loading (20′ FCL) | 20′ FCL: palletized 25 kg bags of Chevron Phillips MarFlex® HHM TR-258 LLDPE blown film resin, shrink-wrapped, stacked, and secured. |
| Shipping | Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film, ships as nonhazardous solid resin pellets in 25-kg bags, octabins, bulk trucks, or railcars. Keep containers dry and closed, away from heat and ignition sources. No DOT/IMDG/IATA hazardous classification applies. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers closed and palletized off the floor to prevent moisture and contamination. Avoid strong oxidizers. Maintain ambient temperatures, preferably below 50°C (122°F). Protect from UV exposure and physical damage. Follow first-in, first-out stock rotation and local regulations. |
| Shelf Life | No specific shelf life; stable under normal storage conditions. Store cool, dry, well-ventilated, away from direct sunlight in unopened packaging. |
On three-layer blown film lines using 80 mm grooved-feed extruders with 30:1 L/D and 400 mm coextrusion dies fitted with dual-lip air rings, heavy-duty industrial liner and sack film is routinely converted from Chevron Phillips MarFlex HHM TR-258 either at 100 wt% or in 70–85 wt% blends with high-pressure LDPE having density 0.923–0.927 g/cm³ and melt index 0.25–0.70 g/10 min. The 70–85 wt% HHM TR-258 fraction preserves dart impact and Elmendorf tear resistance, while the 15–30 wt% LDPE fraction suppresses bubble instability when drawing below 40 µm; 2–4 wt% of a 40% carbon black masterbatch is incorporated when UV resistance or opacity is required for outdoor storage or hazardous waste liners. The process is operated at melt temperatures of 205–215°C, blow-up ratios of 2.0–2.5:1, and frost-line heights of 6–8 die diameters; on a 70 mm extruder, these conditions typically maintain gauge profiles within ±5–7% on 100 µm film. Terminal articles include open-mouth sacks, valve sacks, FIBC liners, and industrial waste bags, with converter acceptance frequently referencing ASTM D1709-16ae1 dart drop and ASTM D882-18 tensile elongation after conditioning at 23±2°C and 50±5% relative humidity according to ASTM D618-21. For dangerous goods packaging, the converted sack must meet the relevant performance provisions of the UN Model Regulations when used as a certified outer or liner component; general melt index and density are verified according to ASTM D1238-20 and ASTM D1505-18. The specific melt pressure and output curves vary with screw geometry and die design; the stated ranges derive from converter line reports rather than a product specification.
The processing windows below summarize representative line settings for HHM TR-258 across standard gauge classes; actual values depend on screw geometry, die design, and air ring efficiency.
| Film gauge class | Die gap | Blow-up ratio | Melt temperature | Frost-line height |
|---|---|---|---|---|
| <30 µm | 1.5–1.8 mm | 2.0–2.5:1 | 195–210°C | 5–7 die diameters |
| 30–80 µm | 1.8–2.2 mm | 2.2–2.8:1 | 200–215°C | 6–8 die diameters |
| >80 µm | 2.0–2.5 mm | 2.0–2.5:1 | 205–220°C | 6–9 die diameters |
Seal integrity in vertical form-fill-seal and horizontal form-fill-seal packaging using HHM TR-258 is determined by sealant-layer blend composition, hot-tack properties, and film flatness after cooling. A three-layer coextruded film commonly uses a core layer containing 100 wt% HHM TR-258, while the sealant skin is formulated with 80–90 wt% HHM TR-258 and 10–20 wt% of a polyolefin plastomer or high-pressure LDPE with melt index 0.7–2.3 g/10 min to reduce seal initiation temperature. Slip/antiblock masterbatch is incorporated at 1.0–2.5 wt% in the sealant skin; for films below 30 µm, the antiblock silica level is reduced to 0.5–1.0 wt% because higher silica loadings depress hot tack under ASTM F1921-18. Seal strength is measured according to ASTM F88/F88M-21 on crimp-sealed specimens prepared at 115–125°C and 0.27 N/mm², while hot tack is screened at 110–130°C on a VFFS machine trial. Published data for this exact grade in all sealant blend ratios is limited; line qualification therefore includes seal initiation temperature and contamination tolerance checks on the target packaging line.
Production equipment consists of 45–65 mm coextruders with 24:1–30:1 L/D barrier screws, feedblock or die-level layer distribution, die gap 1.6–2.0 mm, blow-up ratio 2.2–2.8:1, and internal bubble cooling when gauge is below 25 µm. Corona treatment on the print or lamination surface is controlled at 38–42 mN/m; downstream pouching runs on servo-driven bottom-seal machines at cycle rates of 80–120 packs/min for frozen vegetables, frozen fruit, and ready-to-freeze meal bags. Food contact compliance is maintained under 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; converters must revalidate migration whenever recycled layers, printed inks, or coatings are introduced between the sealant web and the food contact surface.
Outdoor silage film and mulch film produced from HHM TR-258 require higher UV absorber and hindered amine light stabilizer masterbatch loadings than indoor packaging film. A common three-layer formulation uses an outer layer with 85 wt% HHM TR-258, 5–7 wt% high-pressure LDPE, and 3–5 wt% of a UV masterbatch containing 10–20 wt% HALS and UV absorber; the core contains 70–80 wt% HHM TR-258, 10–20 wt% clean in-house edge trim, and 5–10 wt% LDPE; the inner silage contact layer is kept at 90–95 wt% HHM TR-258 with 1–2 wt% antiblock masterbatch. The blown film process uses 70 mm extruders with 30:1 L/D, 350 mm dies, die gap 2.0 mm, blow-up ratio 2.5:1, frost-line height 6–8 die diameters, and melt temperature 210–220°C. Terminal products include round bale silage wrap, silage pit cover film, and mulch films that must resist splitting at the bale edge and during mechanical wrapping. Mechanical durability is assessed by ASTM D882-18 tensile, ASTM D1922-15 Elmendorf tear, and ASTM D1709-16ae1 dart drop; UV stability is screened by ASTM D4355-21 xenon-arc exposure. Regulatory compliance under REACH Regulation (EC) No 1907/2006 applies to chemical substances, and Regulation (EU) No 10/2011 applies where silage contact may affect the feed chain.
An operational boundary occurs at high output with a 2.0 mm die gap; sharkskin on the UV-stabilized outer skin can appear at output rates above 12–15 kg/h per die circumference centimetre unless 0.02–0.05 wt% fluoropolymer processing aid masterbatch is introduced. Moisture from recycled edge trim should be kept below 0.05 wt% before feeding to the core extruder because free moisture increases bubble pinholes under 2.5:1 blow-up conditions.
Lamination-grade blown film using HHM TR-258 as a sealant web is converted on single-layer or coextrusion lines where the resin is blended with 10–30 wt% LDPE or polyolefin plastomer to reduce seal initiation and improve hot tack during stand-up pouch manufacture. A representative converting formulation is 75–85 wt% HHM TR-258, 10–20 wt% LDPE with density 0.923–0.927 g/cm³ and melt index 0.8–2.0 g/10 min, and 1–2 wt% slip/antiblock masterbatch; when the sealant web is below 30 µm, the HHM TR-258 level is increased to 85–90 wt% to preserve puncture resistance during pouch corner folding. The blown film line is run with a die gap of 1.5–1.8 mm, blow-up ratio 2.0–2.5:1, melt temperature 200–215°C, and the film is corona treated at 38–42 mN/m before lamination to oriented PET, oriented polyamide, or metallized film via solventless adhesive or extrusion lamination.
The terminal converted articles are non-retort hot-filled or pasteurized stand-up pouches, liquid pouches, and lamination sealant webs where hermetic seal integrity is the critical function. Seal strength is tested to ASTM F88/F88M-21, and lamination bond strength is tested to ASTM D1876-08; food contact compliance relies on 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. A known operational boundary is coefficient of friction on the non-sealant surface after lamination: if slip migration is insufficient, the film stack can block during automated pouch edge folding, so converters maintain 0.15–0.30 kinetic COF on the non-sealant surface measured by ASTM D1894-14.
For pallet unitization loads requiring high cling retention before stretching, HHM TR-258 is formulated into stretch hood film with a blend of 85–95 wt% HHM TR-258, 5–15 wt% of a very-low-density polyethylene or metallocene LLDPE with density 0.902–0.912 g/cm³, and 0.5–2.0 wt% polyisobutylene tackifier masterbatch to control cling on the inside of the blown tube. The tackifier level is adjusted by cling performance to ASTM D5458-95(2020) and surface friction to ASTM D1894-14; insufficient tackifier causes pallet load movement during transit, while tackifier above 2.5 wt% creates unwind noise and tear propagation at the spiral cut. Production uses 80–90 mm extruders with internal bubble cooling, 500–600 mm dies, die gap 1.7–2.2 mm, blow-up ratio 2.5–3.2:1, and frost-line height 5–7 die diameters; the tube is corona treated at 32–36 mN/m for print adhesion, gusseted, and spiral cut into 25–80 µm film. Terminal products are stretch hoods for pallets of beverage trays, white goods, block products, and chemical sacks. Mechanical performance is measured by ASTM D882-18 tensile yield and elongation, ASTM D1709-16ae1 dart drop, and ASTM D1922-15 tear; industrial packaging status applies unless the specific tackifier masterbatch is validated under 21 CFR 177.1520 for food contact use. Published data for cling additive interaction with this exact grade beyond supplier technical data is limited; converter trials on a spiral cutter at the target gauge are therefore required to set the tackifier letdown within the 0.5–2.0 wt% window.
The following matrix consolidates the primary compliance and test standards referenced across the downstream applications described above.
| Application segment | Primary compliance standards | Test method focus |
|---|---|---|
| Heavy-duty industrial liners | ASTM D1709-16ae1; ASTM D882-18; ASTM D1238-20 | Dart impact, tensile, melt index |
| Frozen food packaging | 21 CFR 177.1520(c); Regulation (EU) No 10/2011; ASTM F88/F88M-21; ASTM F1921-18 | Seal strength, hot tack, food contact migration |
| Agricultural silage and mulch | REACH Regulation (EC) No 1907/2006; EN 13206:2017; ASTM D4355-21 | UV stability, mechanical durability, chemical registration |
| Laminated pouch sealant web | 21 CFR 177.1520(c); Regulation (EU) No 10/2011; ASTM D1876-08; ASTM F88/F88M-21 | Lamination bond, seal strength, migration |
| Pallet stretch hood | ASTM D5458-95(2020); ASTM D882-18; ASTM D1894-14 | Cling, tensile, coefficient of friction |
| Produce and bakery bags | 21 CFR 177.1520(c); Regulation (EU) No 10/2011; ASTM D1003-13; ASTM D882-18 | Haze, tensile, food contact |
High-clarity produce and bakery bags require a formulation of HHM TR-258 that balances low haze, sufficient openability, and antifog performance. A three-layer or single-layer blown film formula uses 90–95 wt% HHM TR-258, 1–3 wt% sorbitan- or polyglycerol-ester antifog masterbatch, and 1–2 wt% of a slip/antiblock masterbatch with synthetic silica; the antifog additive migrates to the film surface over 24–72 h and reduces discrete water droplet condensation, which is evaluated by cold-room wetting tests rather than by a single ASTM method. The process on 50–65 mm extruders with 1.5–1.8 mm die gaps and blow-up ratios of 2.0–2.5:1 uses melt temperatures of 195–210°C; the film is corona treated at 38–40 mN/m and converted on servo-driven bottom-seal bag machines at 90–140 bags per minute. Terminal products include bread bags, pre-washed salad bags, and perforated produce bags. Food contact compliance is based on 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; optical properties are measured by ASTM D1003-13 haze and ASTM D2457-19 gloss, and mechanical properties by ASTM D882-18. A processing boundary occurs when antifog masterbatch exceeds 3 wt%, because surface bloom raises haze and can reduce heat-seal strength during bag conversion.
Competitive Chevron Phillips MarFlex® HHM TR-258 Low Density Linear Polyethylene, Blown Film prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips MarFlex® HHM TR-258 is a 1-hexene–copolymer linear low density polyethylene designed specifically for blown-film extrusion. The nominal density is 0.918 g/cm³ when determined according to ASTM D1505, and the nominal melt flow index is 0.25 g/10 min at 190 °C under a 2.16 kg piston load according to ASTM D1238. These values are typical published values, not sales specifications; the current certificate of analysis for the individual production lot governs the actual lot-specific values. The resin is manufactured with a Ziegler-Natta catalyst system rather than a single-site metallocene catalyst. The resulting broad molecular weight distribution contributes to non-Newtonian shear thinning, elevated melt strength, and stable bubble formation on high-stalk blown-film lines. The product is used in heavy-duty shipping sacks, industrial liners, agricultural silage covers, high-strength overwrap, and related film structures where downgauging depends on preserving tear, puncture, and dart-impact resistance. It is not a cast-film grade; the rheology and additive package are configured for annular die extrusion and drawn-bubble orientation.
Compared with butene-copolymer LLDPE, the 1-hexene comonomer introduces a longer butyl side branch. Compared with high-pressure low density polyethylene produced in autoclave or tubular reactors, the linear backbone contains no long-chain branching. These structural differences alter the balance between tear initiation, impact toughness, tensile yield, and optical clarity. The following sections define the processing envelope, the mechanical-property response, and the comparative selection logic for this resin relative to metallocene-catalyzed LLDPE and conventional LDPE.
On high-stalk blown-film equipment, stable operation with MarFlex® HHM TR-258 is typically achieved on grooved-feed or barrier-screw extruders with an L/D ratio from 24:1 to 30:1. Barrel temperature set points generally begin at 170 °C in the feed zone and increase to 215 °C at the adapter. The die temperature is typically held between 215 °C and 230 °C. Melt temperature measured at the adapter should remain between 190 °C and 230 °C. Temperatures above 240 °C should be avoided because they exceed the normal processing window and may accelerate thermo-oxidative degradation of the stabilizer package.
The die gap should be set between 1.5 mm and 2.5 mm. For film thicknesses above 100 µm, the wider gap reduces shear heating and lowers the risk of melt fracture. A blow-up ratio of 2.0:1 to 3.0:1 is typical. Frost-line height is normally held at 6 to 10 die diameters. This range reduces stalk resonance while allowing sufficient crystallization before nip collapse. Internal bubble cooling is often required as line speed increases; however, published data for this specific configuration is limited, and the equipment builder should be consulted for output limits.
At low melt temperatures or excessive screw speeds, the resin may exhibit sharkskin melt fracture at the die lip. Raising the die lip temperature by 5 °C to 10 °C is usually more effective than opening the die gap alone. Because the grade has a broad molecular weight distribution, it exhibits stronger shear thinning than a narrow-distribution metallocene grade of comparable melt index. This property lowers head pressure at high screw speeds and reduces motor load. However, the same broad distribution can retain a small fraction of very high molecular mass species, so screen-pack selection should include a 100 mesh or 140 µm nominal retention screen to capture incidental contaminants. Pre-drying is not normally required because the polymer is not hygroscopic. Surface condensation on cold pellets transferred into a warm extrusion bay can create bubble pinholes, so pellet temperature should be allowed to equilibrate above the dew point before hopper charging.
Hexene comonomer incorporates butyl branches along the ethylene backbone; butene-copolymer LLDPE incorporates shorter ethyl branches. At equivalent density, the longer butyl branch increases the probability of load-bearing tie molecules connecting adjacent crystalline lamellae. This structural feature influences slow crack growth resistance, dart-drop impact, and Elmendorf tear. Class-level film data generated on conventional blown-film lines show that hexene-copolymer LLDPE with a nominal density of 0.918 g/cm³ and a nominal melt index of 0.25 g/10 min can produce dart-drop values in the range of 300 g to 500 g at 25 µm thickness when tested according to ASTM D1709A. A butene-copolymer LLDPE of similar density is typically lower in dart-drop impact, often falling in the 120 g to 180 g range at the same thickness. These ranges are not product specifications; they represent class-level responses that depend on die gap, blow-up ratio, frost-line height, cooling air temperature, and the specific additive package. Published data for this specific configuration is limited, and line-specific verification is required.
Elmendorf tear measured according to ASTM D1922 often shows a similar directional imbalance. Machine-direction tear strength is strongly influenced by orientation and can decrease under high draw. The higher molecular weight of MarFlex® HHM TR-258 tends to preserve machine-direction tear better than lower-molecular-weight butene grades, but transverse-direction tear remains the more sensitive indicator of comonomer type. Puncture resistance evaluated according to ASTM D5748 is typically improved relative to butene-copolymer films of similar density because the longer side branch increases plastic deformation before failure. The slower puncture mode is less sensitive to orientation than dart impact but more sensitive to film gauge uniformity.
Optical properties are not the primary design target for this grade. Because the resin is a broad-molecular-weight Ziegler-Natta product, haze measured according to ASTM D1003 may be higher than that of a narrow-composition metallocene LLDPE or a high-clarity LDPE. Clarity is governed by surface roughness, internal haze, and crystalline morphology. Films made from MarFlex® HHM TR-258 can exhibit higher internal haze when quenched rapidly at low frost-line heights, because the broad molecular weight distribution produces a wider distribution of crystallite sizes. If optical appearance is critical, the converter must evaluate haze after the full film fabrication process rather than relying on resin type alone.
Metallocene-catalyzed LLDPE frequently provides higher dart impact at low thickness and lower extractables than a Ziegler-Natta product of equivalent density. However, the narrow molecular weight distribution of metallocene grades can increase head pressure at the same melt index and can make bubble stability more sensitive to frost-line height and air ring airflow. MarFlex® HHM TR-258 is selected when the converter requires a wider processing window, greater melt strength, and less sensitivity to high-stalk bubble instability. In heavy-duty shipping sacks and agricultural films, those advantages can offset the optical penalty.
Conventional LDPE produced in a high-pressure radical process has long-chain branching and strong shear thinning. It also has high melt extension and easy bubble formation at low melt temperatures. Compared with LDPE, MarFlex® HHM TR-258 has higher tensile strength, higher dart impact at equivalent thickness, and lower gas permeability. The linear backbone and longer short-chain branches increase toughness without necessarily producing the same optical clarity or the same drawdown behavior. Blending this resin with LDPE in the 10% to 20% mass-fraction range is common. The LDPE phase improves bubble stability and reduces haze. At LDPE addition levels above 30%, dart-drop impact usually decreases because the long-chain branched phase interrupts tie-molecule continuity and reduces the effective molecular weight of the blend. The blend may also become more difficult to process on a high-stalk line because the melting profile becomes non-uniform.
When compared with a 0.8 g/10 min hexene-copolymer LLDPE, the 0.25 g/10 min melt index of MarFlex® HHM TR-258 places it in a higher molecular weight category. This higher molecular weight improves bubble stability and downgauging potential but also reduces throughput at fixed extruder speed and increases melt temperature sensitivity. The converter should compare screw recovery capacity, die pressure, and maximum melt temperature before selecting this grade for an existing line. A torque-limited extruder may require a higher melt-index resin unless the line is designed for high molecular weight blown-film grades.
Regulatory verification is application-specific. For food-contact use, base-resin compliance is typically addressed under 21 CFR 177.1520, but the converter must verify that the finished article meets the density, extractable, and end-use limitations in the applicable subparagraph. No universal food-contact approval exists for all food simulants and all temperatures. In the European Union, compliance is established under Regulation (EU) No 10/2011 through migration testing of the finished article; the overall migration limit is 10 mg/dm². Specific migration limits for additives and monomers remain the responsibility of the formulator and converter.
| Standard or regulation | Relevant verification condition |
|---|---|
| ASTM D1238 | Melt flow index at 190 °C, 2.16 kg |
| ASTM D1505 | Density by gradient column method |
| 21 CFR 177.1520 | Olefin polymer food-contact requirements; finished article confirmation required |
| Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm²; specific migration limits for authorized additives |
| REACH (EC) No 1907/2006 | SVHC screening and restriction annex verification |
Storage in original sealed packaging at 20 °C to 30 °C is preferred. Prolonged storage above 60 °C can cause pellet deformation and agglomeration. The product is not hygroscopic, but surface condensation on cold pellets transferred to a warm extrusion bay can create film pinholes. The resin should not be oven-dried without written guidance from Chevron Phillips Chemical, because heated pellet beds may fuse into agglomerates. Regrind from edge trim should be kept below 20% of total feed unless the converter establishes a validated remelt protocol. Higher regrind loadings reduce the average molecular weight distribution and can decrease dart impact in films below 50 µm. No statement is made for implantable or parenteral medical use, and USP Class VI compliance is not claimed.