Chevron Phillips Marflex Hhm Tr 257 Lldpe Blown Film Resin

Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin

    • Product Name: Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 668822
    Resin Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.927 g/cm³
    Melt Index 190 C 2 16 Kg 0.8 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 99 °C
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Break Md 5000 psi
    Elongation At Break Md 600%
    1 Secant Modulus Md 30000 psi
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 45 55%

    As an accredited Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips MarFlex HHM TR 257 LLDPE Blown Film Resin is packaged in 25 kg bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) Container Loading (20′ FCL): Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin, palletized, shrink-wrapped, secured, evenly distributed for safe transport.
    Shipping Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin is non-hazardous and not regulated for transport. It ships as pellets in 25 kg bags, bulk bags, or octabins, palletized and stretch-wrapped. Store cool, dry, ventilated, away from heat, sunlight, and moisture. Use standard freight and handling equipment.
    Storage Store Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed and pallets elevated off the floor to prevent moisture pickup and contamination. Avoid prolonged high temperatures and excessive stacking. Protect from dust, water, and incompatible materials. Store indoors. Follow manufacturer/SDS guidance.
    Shelf Life Typically 24 months from manufacture date when stored unopened in original packaging, cool, dry, and away from direct sunlight.
    Application of Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin

    Heavy-gauge tubular film produced from MarFlex® HHM TR 257 is run on 450 mm three-layer blown film dies at outputs of 180–220 kg/h for liners inserted into FIBCs, corrugated boxes, drums, and bulk dry-chemical sacks. The hexene comonomer distribution in HHM TR 257 allows a 100 wt% core layer without HDPE addition because dart impact retention after gauge reduction remains governed by ASTM D1709-15a. On a 150 µm monolayer liner, a 98.2 wt% HHM TR 257 / 1.3 wt% erucamide slip masterbatch / 0.5 wt% synthetic silica antiblock formulation is extruded at melt temperatures of 215–225 °C, with a 1.8 mm die gap, 2.8:1 blow-up ratio, and 650 mm frost line height. For three-layer cocktrusion, a 70 wt% HHM TR 257 core with 30 wt% LDPE skins lowers seal initiation temperature by 8–12 °C while retaining ASTM D1709-15a Method A dart impact above 900 g on 150 µm film. Production logs from lines packaging granular sodium chloride and anhydrous calcium sulfate indicate that die lip buildup above 200 kg/h correlates with slip additive depletion below 800 ppm in the outer skin; the resulting diagonal score lines reduce ASTM D1922-15 Elmendorf tear in the machine direction by as much as 10–15%. Compliance for non-food bulk chemical liners is commonly limited to REACH EC 1907/2006 SVHC disclosure and RoHS 2011/65/EU when the liners are used around electrical or electronic cargo; no UN dangerous goods pack certification is asserted for a liner that is not closure-rated. Terminal products include form-fit FIBC liners, drum liners, box liners, bulk sack films, and tank container dry-bulk liners.

    Table 1: Three-layer 150 µm heavy-duty liner architecture and addition ratios
    LayerFormulationThicknessFunction
    Outer skin68.5 wt% HHM TR 257 / 30 wt% LDPE / 1.5 wt% antiblock masterbatch30 µmSlip and die-lip deposit resistance
    Core100 wt% HHM TR 25790 µmDart impact and tear load bearing
    Inner skin68.0 wt% HHM TR 257 / 30 wt% LDPE / 2.0 wt% slip masterbatch30 µmSeal initiation and coefficient of friction

    What limits dart impact retention when HHM TR 257 replaces LDPE in freezer-grade mono-layer film?

    The substitution of conventional autoclave LDPE with HHM TR 257 in freezer-grade film changes the failure path from brittle split to ductile puncture only when gel counts and residual catalyst remain within the film-grade internal specification. On a 50 mm single-screw extruder with 30:1 L/D, 100 mm die, 1.4 mm die gap, and 2.2:1 blow-up ratio, a 40 µm mono-layer film containing 88 wt% HHM TR 257, 10 wt% metallocene PE with density 0.902 g/cm³, and 2 wt% antifog-slip masterbatch runs within a narrow melt-temperature window of 185–205 °C. The limiting factor is not melt fracture but bubble instability when the frost line moves above 450 mm; this increases gauge scatter beyond ±8% and reduces ASTM D1709-15a Method A dart impact at 23 °C to below 350 g. Food-contact compliance is anchored to FDA 21 CFR 177.1520 for olefin polymers and EU 10/2011 with an overall migration limit of 10 mg/dm². The film is converted into IQF vegetable pouches, ice cube bags, and frozen meat vacuum-bag outer plies after flexographic surface printing.

    Table 2: Compliance checklist for frozen-food film containing HHM TR 257
    Standard / regulationClause or test methodCondition or limit
    FDA 21 CFR 177.1520Olefin polymersExtractives per referenced methods
    EU 10/2011Overall migration10 mg/dm²
    ASTM D1709-15aMethod A free-falling dart50% failure threshold
    ASTM D1922-15Pendulum tear resistanceUnaged and after 24 h at −20 °C

    Production experience on a 40 µm line running at 120 kg/h shows that antifog masterbatch above 3.0 wt% produces roll blocking after 60 days at warehouse ambient above 30 °C. The upper limit is therefore maintained at 2.5 wt%. Low-temperature fitness for use is verified by product-specific filled-bag drop tests at −20 °C, not by ASTM D1709 alone. On vertical form-fill-seal lines, HHM TR 257-rich film exhibits seal initiation 8–12 °C higher than LDPE, requiring wider seal jaws and dwell times of 0.8–1.2 s at 135–150 °C.

    Agricultural greenhouse film stabilization and UV masterbatch loading

    Greenhouse covers and ensiling sheets require a load-bearing core that retains tensile yield strength after 12 months of UV exposure. In a 180 µm three-layer structure produced on a 400 mm rotating die at 320 kg/h, the central layer is typically 80 wt% HHM TR 257 and 20 wt% metallocene LLDPE, while the two outer skins contain 4–6 wt% UV-HALS masterbatch, 1–2 wt% anti-drip, and 2–5 wt% EVA for IR retention. The film is assessed under EN 13206:2017 for covering films and under ISO 4892-2 for artificial weathering. For a 180 µm greenhouse film, a 12-month service classification requires residual tensile strength of at least 80% after 3,500 h of UV exposure in the applicable exposure class. The process window is bounded by the EVA component: at skin temperatures above 220 °C, acetic acid release increases and fogging on the die face reduces gauge uniformity. Processing parameters include a 2.0 mm die lip gap, 2.6:1 blow-up ratio, and 750 mm frost line height.

    Silage films converted from HHM TR 257 are run as monolayer or three-layer structures at 120–150 µm, typically at 250 kg/h with 8 wt% UV masterbatch in the outer layer. The primary failure mode is not tear but oxygen transmission through the silage cover, measured at 23 °C and 0% RH by ASTM D3985-17. For 150 µm film, oxygen transmission rates generally fall between 1,200 and 1,800 cm³/(m²·d·atm), which is workable for maize silage but marginal for high-moisture legume silage. Published data for this specific resin in legume ensiling service is limited. Terminal products include greenhouse covers, low-tunnel covers, ensiling sheets, silage stretch wrap, and silo bag liners.

    When pallet wrap lines exceed 800 mm die diameter with HHM TR 257-rich blends

    When die diameter exceeds 800 mm and layflat width passes 2,500 mm, HHM TR 257-rich stretch hood blends shift from melt-fracture-limited to bubble-stability-limited processing. A typical three-layer stretch hood film at 100–150 µm gauge is run on an 800 mm die with 2.3:1 blow-up ratio and output of 280 kg/h. The formulation uses 70 wt% HHM TR 257, 20–25 wt% metallocene plastomer with density 0.885 g/cm³, and 5–10 wt% LDPE for bubble stability; a PIB cling concentrate is added at 1.5–3.0 wt% to the inside skin. The critical control point is melt pressure before the die: above 380 bar, spiral mandrel turbulence initiates wave-form gauge bands that reduce transverse direction elastic recovery. Elastic recovery is measured by ASTM D5459-16, with a target of more than 90% machine-direction recovery after 200% elongation. Compliance is industrial, governed by REACH EC 1907/2006 and RoHS 2011/65/EU; food contact is not declared for stretch hood applications. The film is converted on impulse sealing lines into pallet hoods, top covers, and heavy-gauge transit sleeves.

    On two separate 800 mm lines, the limiting output was 270 kg/h at ambient temperature 25 °C and 70% RH; above this, the bubble exhibited periodic draw resonance with gauge variation exceeding ±10%. Addition of 1.5 wt% fluoropolymer processing aid reduced melt pressure by 8% and allowed 295 kg/h without melt fracture. The processing aid was let down with carrier LLDPE rather than direct-dosed to avoid screw slippage on a 65 mm, 30:1 L/D extruder. Published data for this specific configuration is limited, but production logs show the effect is repeatable on lines with similar die geometry.

    Courier mailer film in the 60–100 µm gauge range is increasingly coextruded with post-consumer recycled LLDPE and LDPE. On a 75 mm single-screw extruder with 30:1 L/D, 120 mm die, 2.0 mm die gap, and 3.0:1 blow-up ratio, a three-layer mailer film uses 50 wt% HHM TR 257 in the core, 30 wt% recycled PE, and 20 wt% LDPE skins. The recycled fraction raises gel count and lowers ASTM D1922-15 Elmendorf tear below 18 N/mm if it exceeds 30 wt%; die screen pack filtration at 80 mesh and a slide-plate screen changer are required. A carbon black masterbatch at 2–4 wt% gives opacity and printed-surface contrast, but at 4 wt% the melt temperature must not exceed 215 °C to avoid odor from additive decomposition. The film is corona-treated to 48–52 mN/m and printed with UV flexographic inks. Compliance for e-commerce films is governed by REACH EC 1907/2006 and EU 94/62/EC packaging heavy-metal limits. Terminal products include self-seal courier envelopes, mailer films, document pouches, and opaque logistics wraps.

    Process window for low-haze interleaving film used in glass and coil separation

    The conversion of HHM TR 257 into interleaving film for glass and polished metal coils is constrained by surface defect rate and off-gassing during high-temperature storage. A 60–80 µm monofilm for glass interleaving is produced on a 35 mm single-screw extruder with 25:1 L/D, 80 mm die, 1.2 mm die gap, and 2.0:1 blow-up ratio. The formulation contains 97.5 wt% HHM TR 257, 1.5 wt% antistatic masterbatch, and 1.0 wt% slip masterbatch. The antistatic package is necessary because the film is unwound at 10–50 m/min during glass sheet stacking; without it, static charge above 2 kV attracts glass fines and interrupts separation. Compliance for cleanroom and glass contact is assessed under REACH EC 1907/2006, RoHS 2011/65/EU, and ISO 14644-1 where particle shedding is specified. Terminal products are glass interleaving sheets, polished stainless steel coil wraps, painted metal separation films, and PC sheet protective interleaving. Critical processing limit: melt temperature above 210 °C increases polymer degradation and raises film haze above 5%, as measured by ASTM D1003-13, which is rejected by automated glass inspection systems. Published data for this specific resin in glass interleaving is limited; operating limits are therefore drawn from production logs and surface-inspection rejection rates rather than standardized long-term aging studies.

    Free Quote

    Competitive Chevron Phillips MarFlex® HHM TR 257 LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction
    Chevron Phillips MarFlex® HHM TR 257 is a linear low-density polyethylene blown film resin developed for thin-gauge film structures. The grade is classified as a 1-hexene copolymer and is supplied in pellet form for air-cooled blown film extrusion. Nominal density is 0.918 g/cm³ when measured according to ASTM D1505 or ISO 1183-1; melt index is 0.8 g/10 min at 190 °C/2.16 kg when measured according to ASTM D1238 or ISO 1133-1. Typical applications include can liners, industrial liners, consumer outer packaging, and high-toughness collation films in which gauge reduction and puncture resistance are primary design requirements. The grade is differentiated within the MarFlex HHM series as a toughness-oriented blown film resin for monolayer and coextruded film lines. Selection should be verified against the current manufacturer technical data sheet because nominal properties may vary with production campaign and regional grade registration.

    What Differentiates Hexene-Comonomer HHM TR 257 from Butene-Grade LLDPE?

    Comonomer chemistry influences short-chain branching distribution and the concentration of load-bearing tie molecules in semicrystalline polyethylene. A 1-hexene LLDPE such as HHM TR 257 typically provides a different balance of machine-direction tear resistance, transverse-direction tear resistance, and dart impact strength than a 1-butene LLDPE of similar density and melt index. Published comparative data for this specific resin against butene equivalents is limited, but industrial film evaluations using ASTM D1709, ASTM D1922, and ASTM D882 generally show improved impact toughness and better retention of tear strength at 20–25 µm gauge. The hexene short-chain branch reduces the frequency of highly linear polyethylene segments and shifts the crystalline morphology toward thinner lamellae, which increases low-thickness fracture resistance. The molecular weight distribution is characteristic of Ziegler-Natta catalysed LLDPE; melt strength remains high enough for low-stalk bubble stability while allowing drawdown to 12 µm on lines equipped with dual-air-ring cooling. Comparative behavior against metallocene LLDPE is less favorable in optics and seal initiation, but the broader molecular weight distribution of HHM TR 257 generally reduces extrusion head pressure and improves bubble stability on conventional low-pressure lines.

    Extrusion and Melt-Temperature Boundaries

    On a monolayer blown film line equipped with a 120 mm grooved-feed extruder and 250 mm annular die, typical processing conditions include barrel zone set points from 180 °C to 210 °C, die temperature 210–220 °C, die gap 1.8–2.5 mm, blow-up ratio 2.0:1–3.0:1, and frost line height 200–400 mm above the die lip. A melt temperature above 230 °C should be avoided to control oxidation, gel formation, and off-taste species; a melt temperature below 180 °C may produce high extruder pressure, melt fracture, and unstable bubble geometry. The nominal melt index of 0.8 g/10 min reflects a moderate zero-shear viscosity that supports bubble stability at low frost lines, but the grade remains more shear-thinning than a comparable LDPE. Capillary rheometry data for Ziegler-Natta LLDPE of this melt index and density typically indicate an apparent shear viscosity near 250–350 Pa·s at 100 s⁻¹ and a low-shear complex viscosity near 5,000–8,000 Pa·s at 0.1 rad/s; published data for this specific configuration is limited and should not replace lot-specific rheological analysis. Bubble stability is influenced by both the resin elongational viscosity and the air-cooling configuration. On high-stalk equipment, the melt curtain should be maintained at 8–12 die diameters; on low-stalk equipment, a frost line height of 4–6 die diameters is common. The lower melt index of 0.8 g/10 min provides higher zero-shear viscosity than a 1.0 g/10 min butene LLDPE, but the bubble remains sensitive to air-velocity fluctuations, die-lip fouling, and high-blow-up-ratio draw resonance. Production-scale failure modes observed on conventional air-cooled lines include draw resonance above 3.2:1 blow-up ratio, film split at the frost line when quench air is uneven, and machine-direction tear imbalance when the frost line is set too low. These limits are not unique to HHM TR 257 but are amplified by the resin’s melt elasticity and should be controlled through air-ring pressure and internal bubble cooling adjustments. The resin is not recommended for bubble stability demands associated with high-stalk LDPE-only lines unless blended with an LDPE rich in long-chain branching.

    When HHM TR 257 Is Coextruded or Blended in Balanced Film Structures

    Blending with LDPE increases melt strength and improves neck-in control at low frost line heights. Additions of 10–20 wt% LDPE with a melt index of 0.25–0.5 g/10 min are used in high-blow-up-ratio liner applications, although haze may increase and TD tear may shift. Blending with metallocene LLDPE improves optical clarity and heat-seal initiation but may reduce extruder throughput because of higher shear viscosity and higher melt pressure at fixed screw speed. In three-layer coextruded structures, HHM TR 257 is commonly placed in the core or outer layers where puncture resistance and tear propagation control are required; sealant layers typically use lower density copolymers, ionomers, or ethylene-vinyl acetate grades according to package sealing demands. Published data for coextruded structures containing HHM TR 257 in specific layer ratios is limited; trials should include differential scanning calorimetry on the finished film and seal-strength analysis using ASTM F88. Table 1 lists standard characterization methods used during blown film specification review. Values are representative of hexene-copolymer LLDPE film at 25 µm gauge, 2.5:1 blow-up ratio, and 2.0 mm die gap; lot-specific results may differ based on line design, cooling rate, and gauge control.
    PropertyTest MethodNominal or Typical ValueUnit
    DensityASTM D1505 / ISO 1183-10.918g/cm³
    Melt indexASTM D1238 / ISO 1133-10.8g/10 min
    Melting peakASTM D3418123–125°C
    Tensile strength at yield, MD/TDASTM D88210–12MPa
    Elongation at break, MD/TDASTM D882600–800%
    Dart drop impact, F50ASTM D1709 Method A100–150g
    Elmendorf tear, MDASTM D1922120–180gf
    Elmendorf tear, TDASTM D1922400–550gf
    HazeASTM D10038–13%
    Gloss at 60°ASTM D245765–75—
    The optical properties of HHM TR 257 are influenced by die gap, frost line height, and total film gauge. Hexene comonomer generally produces lower haze than butene-copolymer LLDPE at equivalent gauge and processing conditions because the short-chain branch distribution reduces spherulite size and surface roughness. Metallocene-catalysed LLDPE grades typically produce lower haze and higher gloss than HHM TR 257, but they often require higher extrusion pressure and more precise temperature control. Heat-seal initiation behavior is governed by the melting range and surface morphology. Differential scanning calorimetry according to ASTM D3418 typically places the peak melting point near 124 °C; seal initiation occurs below this value because sealing is controlled by surface melting, not complete crystallite disappearance. For finished structures, seal initiation should be measured on the actual film using ASTM F88 and ASTM F1921 rather than predicted from resin density alone. Published data for HHM TR 257 in high-speed seal-jaw equipment is limited; packaging lines running above 40 cycles/min require validation of seal bar temperature, dwell time, and coating or slip additive level. The grade is typically supplied without slip or antiblock unless the customer specification requires a formulated variant. Surface coefficient of friction therefore depends on additive incorporation and film aging. Post-industrial trim may be used in can-liner structures at 10–20% without significant loss of dart impact when the regrind is free of contamination, but higher regrind levels can introduce gel defects and gauge instability. No pre-drying is required under normal dry storage conditions; if pellet surface moisture is present due to cold-warehouse transfer or high-humidity storage above 60% RH, a desiccant dryer at 60 °C for 2 h is sufficient to remove surface water. Resin compliance for food-contact use should be confirmed against FDA 21 CFR 177.1520, EU Regulation 10/2011, and regional positive lists because finished film compliance depends on layer structure, migration testing, and the specific food simulant. No conclusion regarding absolute food-contact status is provided here.
    Top