| HS Code | 413280 |
| Additive | Erucamide |
| Additivecontent | 4.0% |
| Carrierresin | Polyethylene |
| Form | Pellets |
| Color | Natural |
| Density | 0.920 g/cm³ |
| Meltflowrate | 8.0 g/10 min at 190°C/2.16 kg |
| Meltingpoint | 107 °C |
| Vicatsofteningpoint | 90 °C |
| Tensilestrengthyield | 9.0 MPa |
| Tensilestrengthbreak | 15.0 MPa |
| Elongationatbreak | 500% |
| Flexuralmodulus | 200 MPa |
| Hardnessshored | 50 |
| Processingtemperature | 160-220 °C |
| Moisturecontent | 0.10% |
| Bulkdensity | 0.55 g/cm³ |
As an accredited Chevron Phillips MarFlex® ER3344 Polyethylene; Masterbatch factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips MarFlex® ER3344 Polyethylene Masterbatch is supplied in 25 kg polyethylene-lined bags, palletized, or 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25 kg bags of Chevron Phillips MarFlex® ER3344 polyethylene masterbatch, shrink-wrapped, strapped, and secured for transport. |
| Shipping | Shipping description: Chevron Phillips MarFlex® ER3344 Polyethylene Masterbatch is not regulated as dangerous goods. It is transported as a non-hazardous solid in polyethylene-lined bags, boxes, or bulk bags on pallets. Keep dry, away from heat and ignition sources. Follow local transport and handling regulations. |
| Storage | Store in original, closed containers in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and oxidizing agents. Protect from moisture, dust, and contamination. Avoid prolonged high temperatures. Keep containers tightly sealed when not in use. Keep storage area clean to prevent pellet spills and slip hazards. Observe SDS and local regulations. |
| Shelf Life | Shelf life: 24 months when stored in original unopened packaging in a cool, dry, well-ventilated area away from direct sunlight. |
High-stalk blown film extrusion of ER3344 is configured around the resin’s published melt index of 1.0 g/10 min at 190 °C/2.16 kg under ASTM D1238 and density of 0.918 g/cm³ under ASTM D1505. On monolayer lines with 30:1 to 38:1 L/D smooth-bore extruders, the die gap is held between 1.8 mm and 2.4 mm. Die gaps below 1.5 mm generate melt fracture at throughputs above 150 kg/h on 400 mm spiral dies because the apparent shear rate at the die lip exceeds the critical shear rate of the metallocene melt. Blow-up ratio is controlled at 2.2:1 to 3.0:1; beyond 3.2:1 bubble flutter increases gauge variation to more than ±12% on conventional air rings. Frost line height is set between 500 mm and 900 mm; higher frost lines reduce film clarity and increase seal initiation temperature. The narrow molecular weight distribution loses bubble stability compared with high-pressure LDPE, so 10 wt% to 20 wt% LDPE is added to stabilise the stalk without collapsing dart impact values below the threshold established by ASTM D1709 Method A. Die rotation speeds of 2 min⁻¹ to 8 min⁻¹ distribute gauge bands, but uneven air ring pressure or contaminated die lips create repetitive thickness bands that appear after printing as ink skip. Film at 25 µm to 80 µm is used for liquid packaging, overwrap, and laminating webs; at thicknesses above 120 µm, output is limited by bubble cooling capacity rather than extruder capacity.
Cast film processing of ER3344 runs with flat dies having gap settings from 0.5 mm to 0.8 mm and melt temperatures between 230 °C and 260 °C. Draw resonance appears when the draw ratio exceeds 25:1 at chill roll speeds above 300 m/min; metallocene polyethylene has a shorter extensional relaxation time than broad-MWD Ziegler-Natta LLDPE, but ER3344 still requires an air gap of 20 mm to 50 mm to prevent edge weave. Chill roll temperatures of 15 °C to 30 °C are used for gloss and flatness. The lower melt strength relative to high-pressure LDPE limits line speed when neck-in exceeds 60 mm on 1.8 m dies. Addition of 5 wt% to 15 wt% high-pressure LDPE increases melt tension and reduces edge trim loss. Film tensile properties are measured by ASTM D882, with machine-direction elongation values dependent on draw ratio. Puncture resistance is measured by ASTM D5748 or a slow puncture probe; published data for ER3344-specific cast film puncture force is limited, so target values should be established by line trials at fixed chill roll temperature and fixed air gap.
Extrusion coating with ER3344 requires higher melt temperatures than blown film. The polymer is processed at 260 °C to 315 °C through flat dies with air gaps of 100 mm to 250 mm. Neck-in on porous paper substrates is typically 25 mm to 75 mm per side depending on line speed and air gap; adding 20 wt% to 30 wt% high-pressure LDPE with melt index below 8 g/10 min reduces neck-in and improves drawdown. Coat weights between 12 g/m² and 30 g/m² are used for liquid packaging board. Adhesion to aluminium foil and corona-treated films is measured according to ASTM F88 after heat sealing at 130 °C to 150 °C. If the substrate carries a water-borne primer, the oxidised melt surface interacts with the primer; without primer, adhesion to untreated polyester is below practical peel strength thresholds. Processing windows narrow when ER3344 is blended with more than 30 wt% LDPE because the high-pressure component contributes long-chain branching and moves the onset of draw resonance to lower line speeds. Published data for ER3344-specific neck-in on a given die configuration is limited; coating trials should map air gap and melt temperature at fixed coat weight rather than predict from generic LLDPE curves.
When ER3344 is compounded with colour or functional masterbatches, the recommended screw configuration is a co-rotating twin-screw extruder with L/D 44:1 and distributive mixing elements in the final 4 L/D zones. Concentrate let-down ratios of 2 wt% to 8 wt% are common for film applications; higher loadings of 40 wt% mineral-filled masterbatch require pellet pre-blending to avoid feeder segregation because ER3344 pellets and masterbatch pellets differ in bulk density. The carrier resin in the masterbatch is generally a low-viscosity LDPE or EVA with melt index between 20 g/10 min and 60 g/10 min; ER3344 itself is not normally used as the carrier resin for high-filler concentrates due to its 1.0 g/10 min melt index and high melt pressure at filler loadings above 30 wt%. Screen packs with 50/100/50 mesh layers are fitted upstream of the die to collect undispersed pigment agglomerates; pressure rise beyond 20 bar across the screen indicates filter replacement. Capillary rheology under ISO 11443 at 190 °C is used to detect batch-to-batch viscosity variation. Dispersion quality is evaluated by film optical inspection and pressure-rise testing; published data for ER3344-specific dispersion torque in masterbatch compounding is limited.
| Processing mode | Melt temperature | Tooling gap | Critical control parameter | Primary test standard |
|---|---|---|---|---|
| Blown film high-stalk | 190–215 °C | 1.8–2.4 mm | Frost line 500–900 mm | ASTM D1709 |
| Cast film | 230–260 °C | 0.5–0.8 mm | Draw ratio below 25:1 | ASTM D882 |
| Extrusion coating | 260–315 °C | 0.4–0.7 mm | Air gap 100–250 mm | ASTM F88 |
| Masterbatch let-down | 180–220 °C | Screw L/D 44:1 | Screen pressure rise below 20 bar | ISO 11443 |
On horizontal form-fill-seal packaging lines, ER3344 films are converted into heavy-duty sacks, frozen food pouches, and industrial liners. Seal initiation temperature is typically 95 °C to 110 °C; hot tack strength is measured by ASTM F1921, and seal strength by ASTM F88. Film thickness for heavy-duty sacks ranges from 50 µm to 150 µm. Dart impact is measured under ASTM D1709 Method A, while tear resistance is measured under ASTM D1922; machine-direction tear is often lower than transverse-direction tear, and 10 wt% LDPE addition partly rebalances the tear anisotropy. Coefficient of friction is controlled between 0.3 and 0.5 using slip-containing masterbatch, and blocking force is kept below the limit required by ASTM D3354. If the masterbatch contains migratory slip agents at over 1.5 wt%, seal initiation temperature declines but organoleptic performance in food contact may degrade. Storage above 40 °C accelerates migration of additives to the film surface and can change coefficient of friction before the film reaches the packaging line.
Greenhouse and silage films using ER3344 are produced at thicknesses of 100 µm to 200 µm in three-layer structures, with ER3344 placed in the core or outer layers. UV stabilisation uses hindered amine light stabilizers at 0.5 wt% to 1.5 wt%; light transmission after weathering is measured by ISO 4892-2 xenon arc exposure, and tensile retention is evaluated under ASTM D882. Initial haze is less critical than additive retention because silage film aged for 12 months shows tensile loss when antioxidant packages are under-dosed. Condensation control requires anti-drip additives incorporated as masterbatch; wetting tension is measured by ASTM D2578. Pesticide contact in greenhouses accelerates film oxidation, and sulfur-based pesticides can attack certain stabiliser systems. The film is not recommended for prolonged contact with chlorinated disinfectants above 1000 ppm. Slip and anti-block masterbatch loadings below 0.5 wt% avoid whitening. Film stiffness is measured by ASTM D882 1% secant modulus. Published data for ER3344-specific xenon arc retention at a fixed additive package is limited; weathering validation should be performed on the finished film rather than predicted from resin-level accelerated data alone.
Food contact status for ER3344 is established by resin compliance under FDA 21 CFR 177.1520(c) when the finished article meets the extractive limits specified in that section and the food-type and use conditions in 21 CFR 176.170(c). Under EU 10/2011, overall migration must not exceed 10 mg/dm² for food contact plastics; for foods intended for infants and young children, overall migration is assessed against 60 mg/kg of food-simulant basis. Specific migration of additives introduced by masterbatch must be covered by the concentrate supplier’s declaration and the positive list requirements in Annex I and Annex II of EU 10/2011. Repeated heat history during edge-trim regrind can generate low-molecular-weight aldehydes that affect organoleptic acceptance; if regrind content exceeds 30 wt%, the compliance status should be revalidated on the finished article. For fatty food contact above 60 °C, additional migration testing should be conducted with simulant D2 under EU 10/2011 or appropriate FDA test protocols rather than relying solely on base-resin status.
| Property or requirement | Method or standard | Typical value or limit | Application point |
|---|---|---|---|
| Melt index | ASTM D1238 | 1.0 g/10 min at 190 °C/2.16 kg | Incoming lot control |
| Density | ASTM D1505 | 0.918 g/cm³ | Resin specification |
| Dart impact | ASTM D1709 Method A | Film-dependent | Heavy-duty sacks |
| Tear resistance | ASTM D1922 | Film-dependent | Blown and cast film |
| Seal strength | ASTM F88 | 130–150 °C seal | Form-fill-seal packaging |
| Overall migration | EU 10/2011 | 10 mg/dm² | Food contact |
| FDA status | 21 CFR 177.1520(c) | Condition-dependent | Food contact |
Competitive Chevron Phillips MarFlex® ER3344 Polyethylene; Masterbatch prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
MarFlex® ER3344, listed by Chevron Phillips Chemical as a polyethylene masterbatch, is supplied as a pelletized concentrate built on a medium-density ethylene/α-olefin copolymer carrier. The designation is not a standalone extrusion or molding grade; the carrier fraction serves as a diluent for the active additive package and must be let down into a host polyolefin. The grade notation is associated with a nominal density of 0.934 g/cm³ under ASTM D1505-18 and a nominal melt flow rate of 4.4 g/10 min at 190°C/2.16 kg under ASTM D1238-20. Those values are typical for the base carrier and do not define the final compounded article. Published numerical data for the proprietary masterbatch formulation is limited; therefore, specification setting should rely on lot-level certificates of analysis and letdown-specific mechanical testing of the target article.
Masterbatch performance in film, sheet, or molded parts is governed by letdown ratio, the viscosity match between the carrier and the host resin, and the shear history available in the processing equipment. In polyethylene conversion, a letdown ratio of 2 wt% to 6 wt% is a conventional starting point for high-efficiency additive concentrates. The optimum ratio depends on the concentration of the active substance in the masterbatch and the final application requirement. At a letdown ratio below 1.5 wt%, dispersion quality can become inconsistent when the carrier and host resin melt-flow-rate ratio exceeds approximately 2:1; localized viscosity mismatch limits shear transfer from the melt to the masterbatch domains. On a production-scale 75 mm grooved-feed single-screw extruder with a 40:1 L/D ratio and a Maddock mixing section, adequate dispersion is typically attained at melt temperatures between 190°C and 225°C. Higher temperatures may be necessary when the host resin contains fractional-melt HDPE. A loss-in-weight gravimetric feeder is preferred over volumetric dosing because bulk density variation in the masterbatch and the host pellets can shift the actual letdown ratio by ±5% or more, altering the final additive concentration.
Laboratory-scale torque-rheometer data are not sufficient to qualify ER3344 masterbatch for a high-speed line. A dispersion curve generated at 60 rpm may not predict behavior in a 450 kg/h cast-film extruder because residence time distribution narrows and the masterbatch is exposed to shorter but more intense shear. Production validation should include a run of at least 3 h at the intended line speed and letdown ratio, with online monitoring of melt pressure and die deposit. Melt-pressure fluctuation greater than 5% at the screen pack after the addition point indicates incomplete homogenization and requires screw-speed adjustment, barrel-temperature-profile changes, or a revised letdown ratio.
On single-screw extruders shorter than 24:1 L/D, dispersion of ER3344 masterbatch into high-viscosity HDPE can fail even at correct letdown because the available melting and mixing length is insufficient. In such cases, a downstream static mixer or a higher-back-pressure screw with a longer barrier section is required to avoid visible masterbatch domains and inconsistent additive distribution.
Direct replacement of neat MDPE with ER3344 masterbatch is not permissible; the concentrate must be blended with a host injection-moulding grade. In a typical hydraulic injection-moulding machine with a 25 mm to 80 mm general-purpose screw, a letdown ratio of 3 wt% to 5 wt% is often sufficient for laboratory trials. Melt temperature should be maintained between 205°C and 230°C, with mould temperature between 20°C and 40°C for semicrystalline polyolefin solidification. Back pressure in the 0.3 MPa to 0.7 MPa range is generally adequate to prevent screw slip and improve melt homogeneity; excessive back pressure can increase residence time and promote additive decomposition. The shot size should not exceed 70% of the barrel capacity to control melt residence time and prevent uncontrolled thermal history. If ambient relative humidity exceeds 60%, the masterbatch should be pre-dried at 70°C for 2 h using a dehumidified-air dryer before processing; surface moisture on pellets can otherwise cause splay in moulded parts.
Prolonged melt-temperature excursions above 240°C should be avoided because thermal degradation of the additive package can release low-molecular-weight species and raise extractables. This limitation is particularly relevant in hot-runner injection moulds and long residence-time barrels.
Standard silo storage and transfer conditions for polyolefin pellets apply; no special inert-gas blanket is required when the product is stored in closed packaging below 40°C and below 60% relative humidity.
The following matrix summarizes the characteristics and standards used to evaluate the base resin and the masterbatch. The values are typical for the medium-density carrier and are not guaranteed lot limits; certificates of analysis govern each shipment.
| Parameter | Method / Standard | Value / Basis |
|---|---|---|
| Carrier density | ASTM D1505-18 | 0.934 g/cm³ |
| Carrier melt flow rate | ASTM D1238-20 / ISO 1133-1:2022 | 4.4 g/10 min at 190°C/2.16 kg |
| Physical form | Visual inspection | Pelletized masterbatch |
| Carrier thermal transition | ASTM D3418-15 | Melting peak typical for 0.934 g/cm³ MDPE: 126°C; exact value depends on comonomer type and thermal history |
| Final article tensile properties | ASTM D638-14 / ISO 527-2:2012 | Not applicable to masterbatch; measure after letdown into intended host resin |
Mechanical property values such as tensile yield, elongation at break, and flexural modulus are not assigned to the masterbatch itself because the diluted final article governs. Where a requirement exists, the final article should be tested according to ASTM D638-14 or ISO 527-2:2012 after the masterbatch has been let down into the intended host resin and processed under the commercial thermal profile.
Because the masterbatch contains a proprietary additive package, it is not automatically covered by food-contact clearances that apply to unmodified polyolefin base resins. The diluted final additive concentration must be checked against positive-list entries in 21 CFR 178 or EU 10/2011 Annex I, whichever applies to the end market.
| Requirement | Standard / Regulation | Condition or Limit |
|---|---|---|
| Food-contact olefin polymer | FDA 21 CFR 177.1520(c) | The unmodified polyolefin carrier may qualify under 177.1520(c); formulated masterbatch requires final article compliance verification |
| EU food-contact plastics | EU Regulation 10/2011 | Overall migration limit 10 mg/dm²; specific migration limits for masterbatch additives must be assessed case-by-case |
| REACH SVHC communication | Regulation EC 1907/2006 Article 33 | Threshold 0.1% w/w per SVHC; confirm via supplier declaration |
| RoHS restricted substances | Directive 2011/65/EU Annex II | Pb ≤ 0.1%, Hg ≤ 0.1%, Cd ≤ 0.01%, Cr(VI) ≤ 0.1%, PBB/PBDE ≤ 0.1% by weight in homogeneous material |
The difference between ER3344 and a conventional lower-density LLDPE film carrier lies in the density and melt-flow-rate combination. A carrier with a density of 0.934 g/cm³ produces a stiffer, higher-softening-point dispersed phase in the final article than a carrier with a density of 0.918 g/cm³. In blown and cast film, that density shift generally increases modulus and puncture resistance while decreasing ultimate dart impact and low-temperature toughness when compared with lower-density ethylene/α-olefin copolymers. The trade-off is measurable under ASTM D1709 or ISO 7765-1 for dart impact, ASTM D5748 or ASTM D3787 for puncture, and ASTM D1922 or ISO 6383-2 for Elmendorf tear. Compared with a fractional-melt HDPE carrier, ER3344 at 4.4 g/10 min has lower melt viscosity, which assists dispersion in low-viscosity MDPE and LLDPE hosts but limits use as a sole carrier in high-molecular-weight HDPE blow moulding where parison swell and melt strength are critical.
A first-order density balance indicates that a 5 wt% addition of ER3344 carrier to a 0.920 g/cm³ LLDPE host shifts the calculated density upward by approximately 0.0007 g/cm³, assuming additive density approximates the carrier and voiding is absent. At 10 wt% addition, the calculated shift is approximately 0.0014 g/cm³. This contribution can be significant in controlled-density film applications with tolerance limits of ±0.002 g/cm³.
Blow-moulding evaluations using ER3344-containing masterbatches should include parison swell measurement at melt temperatures between 200°C and 220°C because a carrier melt-flow rate of 4.4 g/10 min alters swell relative to a 1.0 g/10 min HDPE host. Trials should use at least 10 kg of compounded material to overcome hopper segregation effects and confirm continuity across discontinuous parison cycles.
ER3344 masterbatch should not be used in polypropylene, ethylene vinyl acetate, or polar polymer matrices without compatibility testing. The polyolefin carrier may not disperse uniformly in higher-melting or chemically incompatible hosts, leading to delamination, surface defects, or additive migration after aging. For those systems, a separately evaluated carrier resin matched to the host is required.