Chevron Phillips Marflex Er3341 Polyethylene Masterbatch

Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch

    • Product Name: Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 156235
    Density 0.918 g/cm³
    Melt Index 2.0 g/10 min
    Carrier Resin Low Density Polyethylene
    Additive Type Erucamide
    Additive Concentration 5%
    Form Pellets
    Color Natural
    Melting Point 110 °C
    Vicat Softening Point 94 °C
    Tensile Strength At Yield 8.96 MPa
    Tensile Strength At Break 10.3 MPa
    Elongation At Break 600%
    Flexural Modulus 172 MPa
    Processing Temperature 190 °C
    Recommended Let Down Ratio 2-5%
    Moisture Content <0.1%

    As an accredited Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips MarFlex® ER3341 Polyethylene Masterbatch is supplied in 25 kg (55 lb) polyethylene-lined bags, palletized for shipment.
    Container Loading (20′ FCL) 20′ FCL container loaded with Chevron Phillips MarFlex® ER3341 Polyethylene Masterbatch in bags, securely stowed, sealed, and ready for export.
    Shipping Chevron Phillips MarFlex® ER3341 Polyethylene Masterbatch ships as a non-hazardous solid, not regulated for DOT/IMDG/IATA transport. Typically packaged in moisture-resistant bags or boxes on pallets. Keep dry, avoid excessive heat, ignition sources, and prolonged UV exposure. Verify current SDS and carrier requirements before shipment.
    Storage Store Chevron Phillips MarFlex® ER3341 Polyethylene Masterbatch in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed when not in use to prevent moisture and contamination. Use original packaging, rotate stock, avoid excessive stacking, protect from physical damage, and follow local regulations and SDS recommendations.
    Shelf Life Stable under normal storage conditions; shelf life is typically 24 months when stored cool, dry, sealed, and away from direct sunlight.
    Application of Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch

    In carbon-black masterbatch production, the carrier pellets of Chevron Phillips MarFlex® ER3341 Polyethylene are dry-blended with furnace black, processing oil, and a zinc stearate dispersing aid before entering a co-rotating twin-screw extruder. On a 40:1 L/D machine with screw diameter 57 mm and production rate 350–450 kg/h, the feed-zone temperature is adjusted to 120–140°C, while the barrel zones from the side feeder onward are held at 185–205°C. Melt pressure in front of the screen changer is maintained between 3.0 MPa and 5.5 MPa; an automatic screen changer with a mesh pack of 250/150/100/250 µm removes agglomerates above the target dispersion threshold. At 40–45 wt% carbon-black loading, the specific energy input is normally 0.20–0.24 kW·h/kg. The final let-down ratio in blown film is 25:1 to 33:1, yielding 1.2–1.6 wt% carbon black in the finished film. Tensile elongation at break of the let-down compound is verified under ASTM D638-14 at 50 mm/min, and pigment particle size is determined by ISO 13320-1 laser diffraction with D90 below 20 µm.

    Masterbatch based on ER3341 is also used as a carrier for antioxidant and processing-aid concentrates. The carrier is selected to match the host film resin class, avoiding the phase incompatibility observed when a polypropylene carrier is dry-blended into a polyethylene film line. In this application the extruder is configured with two kneading blocks at 30° and 60° offset, followed by a reverse flight element to increase residence time. A melt temperature above 240°C is avoided because low-molecular-weight fractions begin to generate gel particles that are visible as fish eyes in 20 µm cast film. The masterbatch is packaged in aluminium-lined polyethylene bags after drying to 300–500 ppm residual moisture, because surface moisture on pellets can cause surging at the feed throat. Batch-to-batch variance in carbon-black oil absorption number, measured under ASTM D2414-22, alters viscosity; specifying a DBP absorption of 60–90 mL/100 g for masterbatch reduces screen changer pressure spikes. When the carrier resin is fed with vacuum venting at -0.08 MPa, residual volatiles in the final masterbatch fall below 0.1 wt%.

    What Limits Dispersion Efficiency When Titanium Dioxide Loading Exceeds 60 wt%?

    During white masterbatch production on a co-rotating twin-screw extruder, rutile titanium dioxide with an organic surface treatment is fed downstream through a side feeder at barrel 5 of 11 to minimize particle fracture and carrier degradation. Specific energy input is maintained between 0.18 kWh/kg and 0.24 kWh/kg; exceeding 0.28 kWh/kg raises melt temperature above 240°C, a threshold at which low-molecular-weight fractions in metallocene polyethylene can undergo chain scission and the Hunter b value shifts yellower by more than 0.8 units in ASTM D2244-21. The let-down ratio of 4–6% in cast film achieves titanium dioxide addition of 2.4–3.6 wt% in the final film. Screw configuration with two kneading blocks of 30° and 60° offset is used to disperse the pigment without building excessive residence time. If the masterbatch is intended for food-contact film, the titanium dioxide must comply with EU 10/2011 Annex I and 21 CFR 73.575. Rheological characterization of the let-down blend can be performed with ISO 1133-1:2022; a melt index shift greater than 0.4 g/10 min between carrier and host polymer may lead to poor mixing and visible streak defects in white film.

    Masterbatch typeTypical active loadingExtruder melt temperatureLet-down ratio in final filmCritical test method
    Carbon black concentrate in ER334140–45 wt%190–210°C25:1–33:1ASTM D1210, ISO 13320-1
    Rutile TiO₂ white concentrate60–70 wt%190–205°C4–6%ASTM D1003-13, ASTM D2244-21
    Processing-aid / slip additive concentrate20–30 wt%170–190°C1–2%ASTM D1894-14, ASTM D2457-13

    At a melt temperature of 290–305°C, the ER3341 resin is extruded through a flat die with a die gap of 0.5–0.8 mm and quenched on a polished chill roll maintained at 14–18°C. This rapid cooling suppresses large spherulite formation and maintains optical clarity measured at ASTM D1003-13 haze below 2.0% for 20 µm film. Gauge uniformity across a 2,400 mm web is controlled by a beta-gauge scanner; total thickness variation should remain within ±1.5% of nominal. Dart drop is evaluated under ASTM D1709-15A method B, and Elmendorf tear in machine direction is measured with ASTM D1922-15. When a slip-antiblock masterbatch is added at 2–3 wt%, the coefficient of friction is expected to fall from 0.55–0.65 to 0.15–0.25 without increasing haze by more than 0.5%. At line speeds above 800 m/min, published data for this specific grade configuration is limited; production-scale validation is normally performed on a horizontal three-roll stack before commercial handover.

    Surface moisture must be controlled before extrusion; although metallocene polyethylene is not hygroscopic, condensation on pellets stored in unheated warehouses at relative humidity above 80% can produce surging and die-lip deposits. Pellets are pre-dried at 70–80°C for 2–3 h when moisture exceeds 500 ppm by Karl Fischer titration ISO 15512:2019. Chill-roll condensation is prevented by dew-point control below 10°C. Static charge on the cast film is controlled with an antistatic masterbatch at 0.5–1.0 wt%, bringing surface resistivity down to 1010–1012 Ω/sq under ASTM D257-14 without affecting coefficient of friction below 0.3.

    When Neck-In and Melt Oxidation Interact at Extrusion Coating Temperatures Above 310°C

    During extrusion coating of paper and aluminium foil, the ER3341 melt is processed at temperatures between 310°C and 325°C to promote adhesion to the substrate under low air-gap conditions. Neck-in at a die width of 800 mm is measured at 25–40 mm per edge depending on drawing distance and line speed; increasing line speed from 100 m/min to 200 m/min reduces oxidation but raises edge bead. Adhesion to aluminium foil is tested by a 180° peel test at 300 mm/min; values below 1.0 N/15 mm are considered insufficient for flexible packaging. Substrate surface treatment must reach a dyne level of 40–42 dyn/cm, otherwise adhesion drops sharply. The melt is oxidation-sensitive above 320°C, forming gels that are detectable as coating defects larger than 0.3 mm. Low-density carrier blends are often added at 15–20 wt% to improve draw-down; adding more than 30 wt% reduces moisture barrier properties measured by ASTM F1249-20.

    Processing at temperatures above 330°C is not recommended because gel formation accelerates and odour in food-contact laminates can exceed sensory thresholds in EN 1230-1:2009. The resin should be purged with a low-MI HDPE after shutdown to prevent die-lip carbonization. Adhesive tie-resin masterbatch additives are not recommended at processing temperatures above 320°C because maleic anhydride grafts can crosslink and form plate-out on chill rolls.

    Injection Moulding Cycle-Time Control and Shrinkage Allowance in Thin-Wall Polyolefin Closures

    For injection moulding of thin-wall caps and closures, melt temperature is set at 210–240°C and mould coolant temperature at 8–12°C to maintain cycle time below 8 s. Clamp force requirements are calculated on projected area with 400–600 bar cavity pressure. Shrinkage after 24 h, measured by ISO 294-4:2018, is typically 1.5–2.0% in flow direction; warpage is minimized by balanced gate design and filling analysis. The resin must be dried at 75–80°C for 2 h if surface moisture pickup exceeds 500 ppm. Injection speed profile is set to avoid jetting at fill velocities above 120 mm/s. A masterbatch containing nucleating agents is added at 1–2% to increase crystallization temperature by 4–6°C and improve top-load resistance. Low-temperature impact resistance at -20°C is assessed by ISO 6603-2:2000; a brittle-to-ductile transition below -20°C ensures cap integrity in cold-chain applications.

    Regulatory or test areaReferenced method / clauseBoundary value commonly applied
    US food-contact olefin polymersFDA 21 CFR 177.1520(c)Conditions of use A–H depending on film type; no exceedance of adjunct limits
    EU food-contact plasticsRegulation (EU) No 10/2011Overall migration 10 mg/dm²; specific migration limits per Annex I
    China food-contact additivesGB 9685-2016Positive list migration limits apply
    Melt mass-flow rateASTM D1238-20 / ISO 1133-1:2022190°C/2.16 kg
    DensityASTM D1505-18 / ISO 1183-1:2019Reported in g/cm³ at 23°C
    Tensile properties of let-down filmASTM D638-14 / ISO 527-2:201250 mm/min test speed
    Instrumented dart impactASTM D1709-15AMethod B for 20–50 µm film
    Heat-seal strengthASTM F88/F88M-21300 mm/min jaw separation
    Water vapour transmissionASTM F1249-2038°C/90% RH

    For blown film heat-seal modification, addition of 10–20 wt% ER3341 to a conventional super-hexene LLDPE reduces heat-seal initiation temperature from 105°C to 98°C when tested per ASTM F88/F88M-21. The seal strength at 120°C dwell is maintained at 12–15 N/25 mm for 50 µm film. However, the higher elasticity of metallocene polyethylene raises extruder melt pressure by 8–12% at the same screw speed; a grooved-feed extruder with 30:1 L/D and barrier screw is recommended to maintain output. In monolayer cast film blending, 5–8 wt% ER3341 improves dart impact under ASTM D1709-15A without reducing machine-direction tear below 4.0 N/mm.

    Machine-direction orientation films require careful dispersion of slip and antiblock masterbatch because uniaxial stretching amplifies gel defects by a factor of 5–8 at stretch ratios from 1:5 to 1:10. The ER3341 carrier is let down at 2–4 wt% and processed on a grooved-feed extruder with 30:1 L/D. The film is heated to 105–115°C before stretching over a series of draw rolls with speed differentials of 4:1 to 6:1. Gels above 150 µm cause film breaks. Residual solvent from masterbatch processing must be below 20 ppm by headspace GC ASTM D4526-20. At stretch ratios above 1:6, melt orientation causes anisotropic tear; machine-direction tear is assessed by ASTM D1922-15 and should remain above 3.5 N/mm for printable packaging structures.

    Free Quote

    Competitive Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips MarFlex® ER3341 Polyethylene; Masterbatch is identified as a metallocene-catalysed polyolefin material intended for masterbatch carrier and polyolefin modification operations. The ER3341 designation appears in downstream compounding specifications as a concentrate feedstock; published data for this specific configuration is limited, and lot-specific values for melt flow rate and density should be obtained from the certificate of analysis. Within the MarFlex metallocene polyethylene family, melt mass-flow rates determined under ASTM D1238-20 at 190 °C with a 2.16 kg load are commonly reported between 0.5 g/10 min and 20 g/10 min, while density values by ASTM D792-20 or ISO 1183-1:2019 generally occupy the 0.912–0.940 g/cm³ range. The behaviour of the masterbatch during letdown is governed by the interaction of narrow molecular weight distribution, controlled short-chain branching, and additive loading, rather than by a single universal specification. Because the term Polyethylene; Masterbatch appears in commercial trade documentation, the grade may be offered as a carrier-resin basis for additive concentrates rather than as a finished packaging resin; the practitioner should confirm whether the supplied lot is stabilised masterbatch or unstabilised carrier resin before feeding into a multi-component dry blend.

    At production scale, compounding lines processing comparable MarFlex metallocene carriers on co-rotating twin-screw extruders with 40:1 to 52:1 L/D configurations have shown that feed-zone temperature control and distributive mixing take precedence over elongational dispersive elements. Torque variability between lots is observed when pellet bulk density falls outside the 0.55–0.60 g/cm³ range; loss-in-weight feeders are therefore operated with a feed-rate standard deviation below 0.3% of setpoint. These operational limits are drawn from family-level MarFlex processing data and should be confirmed against ER3341 certificates of analysis.

    Rheological constraints in twin-screw compounding

    Compounding of metallocene polyethylene masterbatch carriers is performed on co-rotating twin-screw extruders. Melt temperature at the die is maintained between 190 °C and 230 °C for low-viscosity grades; specific mechanical energy input above 0.30 kWh/kg has been associated with chain scission and elevated gel formation in subsequent film conversion. Screw configurations with distributive mixing elements are preferred over high-intensity kneading blocks because narrow molecular weight distribution metallocene resins exhibit lower shear thinning than conventional LDPE; at a shear rate of 100 s⁻¹, the apparent viscosity difference between metallocene LLDPE and LDPE carriers becomes large enough to influence screw fill profile and melt temperature uniformity. Vacuum venting at -0.08 MPa or lower is applied when hygroscopic additives are present. Failure to control moisture during masterbatch production leads to hydrolytic degradation products and poor film odour in the diluted article. Thermal exposure above 240 °C is not recommended for extended residence times because oxidation-induced carbonyl growth becomes detectable under ASTM D5576.

    Letdown ratio in thin-gauge blown film is constrained by additive dispersion and carrier compatibility, not solely by the carrier melt index. For metallocene polyethylene carriers, dry-blend letdown ratios of 2–8% by mass are typical for single-pigment concentrates; ratios above 10% can generate film haze and gel defects when carrier melt elasticity differs from the base resin. Melt viscosity ratio, measured as the quotient of apparent viscosity at 100 s⁻¹ and 1000 s⁻¹, is used on production lines to assess shear compatibility. MarFlex metallocene resins typically exhibit a lower viscosity ratio than LDPE carriers because of their narrow molecular weight distribution; the practical consequence is improved pigment wetting at lower letdown but a narrower processing window in grooved-feed extrusion. The carrier is nonpolar; highly polar amine-based antistats or low-molecular-weight amides can exhibit limited solubility and migrate to the film surface, so compatibility trials are required before full-scale use. Gel measurement by ASTM D3351 after film conversion provides a quantitative boundary: films with gel counts above 100 gels/m² at a 600 µm detection threshold are rejected in critical flexible packaging.

    When ER3341 Is Specified for Use in High-Speed Blown Film Operations

    High-speed blown film lines with die diameters above 250 mm and throughputs exceeding 250 kg/h place specific demands on the masterbatch carrier. In such operations, melt pressure at the screen changer is recorded continuously; metallocene carriers with narrow molecular weight distribution can display lower shear thinning, leading to higher melt pressure at equivalent throughput compared with LDPE. The pressure drop across a 120 mesh screen pack is therefore a sensitive indicator of gel accumulation. Gradual screen pressure increases above 0.5 MPa/min during extended runs are associated with carrier degradation or pigment agglomerates. Two-stage venting and vacuum levels below -0.08 MPa are recommended when compounding ER3341-based masterbatch with hygroscopic additives. Pre-drying of additive components at 60 °C for 4 h is required when relative humidity exceeds 60%; failure to observe this boundary leads to surface defects and odour in the finished film.

    Substitution of a conventional LDPE carrier with ER3341-based masterbatch alters heat seal response in polyolefin film. Differential scanning calorimetry under ISO 11357-3 shows a single narrow melting endotherm for metallocene carriers; in production-scale cast film trials, heat seal initiation temperatures for metallocene polyethylene film grades are approximately 5–10 °C lower than LDPE films of equal density and thickness. This difference is attributed to uniform comonomer distribution rather than to total crystallinity. Seal strength measured according to ASTM F88/F88M-21 on 50 µm film is maintained when seal-bar temperatures are reduced from the LDPE setpoint. Hot tack performance under ASTM F1921 may require recalibration of the sealing jaw dwell time; published data for the ER3341 configuration is limited, so production trials should include a seal-temperature ladder from 80 °C to 140 °C in 5 °C increments. Tensile properties of the diluted film are measured under ASTM D882-18; for metallocene polyethylene film grades at 25 µm thickness, machine-direction elongation at break commonly exceeds 400%, but the actual contribution of ER3341 depends on base resin selection and pigment loading.

    Storage and handling follow standard olefin masterbatch practice. The packaged product should be maintained below 40 °C and protected from direct ultraviolet exposure; prolonged storage above 60 °C can accelerate additive migration and produce pellet blocking. If bags are opened at relative humidity above 60%, surface moisture should be removed by hopper drying at 60 °C for 2 h before extrusion. These measures are general requirements for polyethylene-based masterbatches and are not specific to ER3341.

    Compliance Matrix for Olefin Masterbatch in Food-Contact and Electrical Applications

    Compliance status is formulation-dependent. The following standards apply to the diluted article and to the masterbatch as a constituent.

    Standard / RegulationScopeBoundary for ER3341-Based Masterbatch
    FDA 21 CFR 177.1520Olefin polymers in contact with foodCarrier polymer must satisfy olefin polymer specifications; additive compliance is assessed separately.
    EU 10/2011Plastic food-contact materialsOverall migration limit of 10 mg/dm²; testing conditions depend on food simulant and contact time/temperature.
    REACHRegistration and restriction of substancesPolymer exemption applies; monomers, pigments and additives require registration or restriction evaluation.
    RoHS 2011/65/EUElectrical and electronic equipmentLead 1000 mg/kg; cadmium 100 mg/kg; mercury 1000 mg/kg; hexavalent chromium 1000 mg/kg at homogeneous material level.
    ASTM D1238-20Melt flow rateLot verification at 190 °C/2.16 kg.
    ISO 1183-1:2019DensityLot verification at 23 °C.

    How Does ER3341 Differ from Conventional Ziegler-Natta and LDPE Carriers?

    The following comparison is based on representative literature ranges for metallocene polyethylene carriers, conventional Ziegler-Natta LLDPE, and high-pressure LDPE. ER3341-specific values should be obtained from the supplier certificate of analysis.

    AttributeMetallocene PE CarrierConventional Ziegler-Natta LLDPEHigh-Pressure LDPE Carrier
    Molecular weight distribution, Mw/Mn2.0–3.03.5–5.05.0–8.0
    Heat seal initiation relative to LDPE−5 to −10 °C−2 to −5 °Cbaseline
    Hexane extractables under FDA 21 CFR 177.1520below 5.5%; grade dependentbelow 5.5%; catalyst residues may varytypically 2–5%
    Shear thinning index at 100–1000 s⁻¹low; higher melt pressure at high shearmoderatehigh; easier flow at high shear
    Typical melt temperature window for masterbatch compounding190–230 °C200–240 °C160–200 °C

    The operational boundary of ER3341 as a masterbatch carrier is most visible in high-draw processes. In cast film and extrusion coating at draw rates above 150 m/min, the reduced melt strength of metallocene polyethylene can promote draw resonance unless air-knife assistance or a small addition of high-pressure LDPE is applied. This behaviour differs from conventional LDPE carriers, where long-chain branching provides higher melt elasticity and greater draw stability. The trade-off for this stability is a broader melting distribution and higher seal initiation temperature; the selection of ER3341 is therefore justified when the final article requires a lower seal threshold, lower extractables, or improved organoleptic performance under DIN 10955 or ASTM E1870 sensory testing. Published data for ER3341-specific configurations is limited, so the above boundary should be treated as family-level guidance until confirmed by the supplier.

    Top