| HS Code | 287564 |
| Resin Type | LLDPE (Metallocene) |
| Comonomer | Hexene |
| Catalyst | Metallocene |
| Melt Index 190 C 2 16 Kg | 0.75 g/10 min |
| Density | 0.923 g/cm³ |
| Melting Point | 121 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 34.5 MPa |
| Elongation At Break | 600% |
| 1 Secant Modulus | 193 MPa |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Haze | 6% |
| Gloss | 80% |
| Coefficient Of Friction | 0.2 |
| Antiblock | Yes |
| Slip | Yes |
As an accredited Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips MarFlex® 7235B ships in 25 kg (55 lb) polyethylene-lined bags, 40 bags per pallet (1,000 kg net). |
| Container Loading (20′ FCL) | 20′ FCL: approximately 18–20 MT of 25 kg MarFlex® 7235B LLDPE resin bags, palletized or floor-loaded, per shipping requirements. |
| Shipping | MarFlex 7235B LLDPE resin is typically shipped in 25 kg multiwall bags or 1,000 kg bulk bags on pallets, stretch-wrapped, or in bulk trucks/railcars. Keep dry, clean, and away from direct sunlight, heat, and contamination. Follow local regulations for non-hazardous polymer transport. Store in a cool, dry, ventilated area. |
| Storage | Store Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed, clean, dry, and palletized. Prevent moisture pickup, contamination, and damage. Avoid excessive stacking and temperatures above 50°C. Protect from UV light and use first-in, first-out inventory. Consult the SDS for details. |
| Shelf Life | Typically 24 months from manufacture when stored unopened in original packaging in a cool, dry, well-ventilated area away from sunlight. |
On high-output cast stretch-film lines, MarFlex® 7235B is processed as the core-layer resin at 85–100 wt%, with the balance commonly split between mLLDPE or ULDPE cling modifiers and a slip/antiblock masterbatch. The resin's nominal melt index of 3.5 g/10 min tested to ASTM D1238 at 190 °C under 2.16 kg load and nominal density of 0.923 g/cm³ tested to ASTM D1505 place the grade within the drawdown envelope required for cast stretch film. A typical line uses a 90 mm single-screw extruder with L/D 30:1, a barrier-type screw, a screen pack of 60/100/60 mesh, and a slot die with gap 0.8–1.0 mm. Melt temperature at the adapter is maintained between 240 °C and 260 °C; the upper boundary is limited by gel formation and the lower boundary by higher motor torque and uneven web width. The web is quenched on a chrome-plated chill roll at 18–25 °C and then drawn in the machine direction at a die-to-winder speed ratio of 1.5:1 to 2.5:1, producing final film from 12 µm to 23 µm. Edge neck-in of 8–12% is removed as trim before in-line slitting. In pallet-wrapping service, pre-stretch settings of 150–300% are normal for A- and B-type machine wraps, with wrapping tension of 80–120 N at the load cell. Cling is preferentially placed in a thin coextruded skin layer rather than bulk-modified into the core; bulk tackifier addition above 1 wt% increases roll blocking in warehouses above 35 °C. The non-food wrapping web is not subject to FDA 21 CFR 177.1520 unless the end user places it in direct food contact; industrial acceptance is based on ASTM D5458 cling performance and ASTM D5748 protrusion puncture rather than a food-simulant extraction battery. Terminal products include pre-stretched hand wrap, extended-core machine wrap, and bundling stretch film for non-food industrial loads.
When MarFlex® 7235B is converted into 50–100 µm blown heavy-duty sack film, the critical processing limit is bubble stability rather than melt strength. A monolayer blown line is typically configured with a 75 mm extruder having a grooved feed and L/D 30:1, a 250 mm spiral mandrel die with 1.8 mm die gap, and a dual-lip air ring supplemented by internal bubble cooling. Melt temperature at the die is held between 190 °C and 210 °C; below 190 °C the frost line becomes unstable under air-ring turbulence, and above 210 °C output is increasingly limited by bubble sag. Blow-up ratios from 2.5:1 to 3.0:1 provide balanced machine-direction and transverse-direction tear, while operation above 3.5:1 raises the frequency of gauge bands because the bubble radius changes with minor fluctuations in room-air velocity. Frost-line height is set at 4–6 die diameters, and internal bubble cooling is adjusted to hold neck-height consistency at ±10%. Fluoropolymer processing-aid masterbatch at 200–400 ppm suppresses spiral-mandrel weld-line haze and die-lip melt fracture. Antiblock masterbatch based on silica or calcium carbonate at 3–6% prevents sack blocking in unit loads stacked above 200 kg. Elmendorf tear tested to ASTM D1922 is specified at 25–40 gf in the transverse direction for 80 µm film, and dart impact to ASTM D1709 Method A is normally specified for sacks exposed to sharp-edged demolition waste. Incorporation of post-consumer recycled LLDPE above 30 wt% destabilizes the secondary bubble and increases gel-induced web breaks; a filtration pack below 100 µm is required when the recycled fraction exceeds 20 wt%. For EU packaging waste, EU 94/62/EC heavy-metal concentration limits apply to the finished sack, with combined lead, cadmium, mercury and hexavalent chromium below 100 mg/kg. Terminal products include construction waste sacks, valve sacks for granular fill, and FIBC inner liners.
Low-temperature seal integrity in quick-frozen vegetable and baked-goods packaging is achieved by using MarFlex® 7235B as a coextruded sealant layer at 8–15% of total web thickness in three- or five-layer structures. The sealant layer is carried between a core layer of LLDPE or HDPE and an outer surface layer containing slip and antiblock. Hot-tack force is measured under ASTM F1921 at 110 °C and 200 mm/min peel speed to qualify webs for vertical form-fill-seal machines running 60–100 cycles/min. Cold-seal strength is measured to ASTM F88/F88M after 24 h conditioning with a 25 mm strip width. At storage temperatures of −30 °C, the specification package shifts from dart impact to tensile impact and slow-rate puncture because film stiffening concentrates stress at package corners. Haze of the finished structure is strongly line-dependent; values below 15% tested to ASTM D1003 are attainable on high-output cast lines only if melt temperature is kept below 250 °C and die-lip buildup is controlled. The resin's olefin polymer status is addressed under FDA 21 CFR 177.1520 and EU Regulation No 10/2011, where the latter requires overall migration below 10 mg/dm² under fatty-food simulants. Erucamide slip above 800 ppm in the sealant layer is not recommended because it migrates to the seal interface and lowers hot-tack force; converters quantify this as increased leaker rates above 0.5% on high-speed pouch lines. Terminal products include spinach and berry flex-packs, bread bags, and frozen seafood pouches.
Extrusion lamination of oriented polyester or biaxially oriented polypropylene to aluminum foil or paper can use MarFlex® 7235B as a sealant web at 12–20 g/m² coating weight when the package must survive creasing and puncturing rather than display maximum clarity. The process is run on an extrusion coating line with a 65 mm extruder, L/D 30:1, a coat-hanger slot die with 0.5 mm die gap, and a matte or gloss chill roll at 15–20 °C. Melt temperature is elevated to 280–300 °C to promote oxidative adhesion to primed polyester and foil; at this temperature, residence time in the adapter and die must be limited to prevent gel streaks that appear as coating defects at 60–100 m/min. Neck-in is higher than LDPE and may reach 20–40 mm per side depending on air gap and melt temperature, so die width is oversized and edge trim is removed before winding. Adhesion above 1.5 N/25 mm to chemically primed PET is generally acceptable for dry-food pouches, but for retort or vacuum-packaging applications a coextruded tie layer containing maleic anhydride-grafted polyethylene is specified because the LLDPE layer itself contains no acid or hydroxyl functionality. Seal initiation temperatures typically fall between 95 °C and 105 °C under ASTM F88/F88M; hot-tack must be confirmed on the actual horizontal or vertical pouching line because seal-bar pressure and dwell time control the measured value. For dry-food lamination, the sealant web is covered by FDA 21 CFR 177.1520; if used for retort applications, the total food-contact structure must comply with EU Regulation No 10/2011 overall migration limits and any specific migration limits for additives. Terminal products include lidding film for powder detergent sachets, stand-up pouch sealant webs, and insulation facestock. Published data for exact adhesion values to flame-treated aluminum foil with this specific resin is limited; each converting line must run a substrate-specific adhesion study.
Blown can liners and construction temporary sheeting converted from MarFlex® 7235B are formulated with 5–15 wt% LDPE and 2–5 wt% carbon-black or TiO2 masterbatch to meet opacity and UV exposure requirements. On a 65 mm mono-layer blown film line with 2.5:1 blow-up ratio and 1.6 mm die gap, frost-line height is set at 4–6 die diameters to control blocking in films from 38 µm to 60 µm. Machine-direction tear to ASTM D1922 and slow-rate puncture to ASTM F1306 are used as primary acceptance tests, with values specified at the end-use gauge because both measurements scale with thickness. Reprocessed post-industrial LLDPE at levels above 40 wt% increases gel counts and reduces bubble stability; when this level is required, line speed must be reduced by 10–20% or melt temperature raised by 5–10 °C. Construction sheeting is accepted as temporary containment under ASTM D4397 for polyethylene sheeting for construction, industrial, and agricultural applications; opacity and UV stabilization requirements are buyer-specified. Terminal products include roll-form masonry curing covers, temporary containment sheeting, and refuse sacks with ≥20 µm side-wall thickness for 120 L containers. This application is the least demanding for optical clarity, so higher recycled content and thicker films are used; published data for exact tensile retention after outdoor exposure in this specific configuration is limited.
In collation films for bottled water and canned goods, MarFlex® 7235B is used in the core layer at 60–80% of total film thickness, with HDPE or mLLDPE skins providing slip and seal performance. Cast-film lines with three-layer feedblocks and 1,200 mm slot dies can operate at 400–600 m/min to produce 10–15 µm film, where the limiting factor is transverse gauge uniformity rather than extruder output. Machine-direction tensile yield measured under ASTM D882 at 12 µm is commonly specified at ≥10 MPa, but web tension uniformity and seal range are more practical acceptance criteria on high-speed multi-pack lines. A coefficient of friction below 0.35 is maintained by secondary slip agents in the skin layers; if slip masterbatch exceeds 5%, haze increases above 8% and seal strength measured by ASTM F88/F88M can fall below 8 N/25 mm. For bottle collation, the formed film must pass through shrink tunnels at 150–180 °C for 2–5 s without edge burn-through; LLDPE-rich webs have lower shrink force than LDPE and are therefore restricted to low-shrink bundling rather than high-shrink contour packaging. In-line corona treatment to 40–46 dyn/cm is applied before printing to ensure ink adhesion to the low-polarity surface. Collation film for packaged beverage cans is considered incidental-contact packaging; if direct food overwrap is produced, compliance with FDA 21 CFR 177.1520 and EU Regulation No 10/2011 is required. Terminal products include printed overwrap, multi-pack can bundling film, and transparent overwrap for tissue products. Published data for exact line-speed limits with in-line flexographic printing in this specific configuration is limited.
Competitive Chevron Phillips MarFlex® 7235B LLDPE Cast/Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Chemical MarFlex® 7235B is a linear low-density polyethylene resin supplied for cast and blown film conversion. The product is a metallocene-catalyzed ethylene-alpha-olefin copolymer with a nominal melt mass-flow rate of 3.5 g/10 min when determined under ASTM D1238 at 190°C/2.16 kg and a nominal density of 0.918 g/cm³ when determined under ASTM D1505. These values are typical of the grade class and are superseded by lot-specific data on the certificate of analysis. The resin is supplied in pellet form with antioxidant stabilisation for film extrusion; it is not intended for rotational moulding, injection moulding, or blow moulding. Standard silo-to-hopper pneumatic transfer is acceptable, but high-speed conveying should be adjusted to limit pellet dust and streamer generation. The material is commonly used in cast stretch film, blown film, lamination film, and selected food-contact packaging. Published data for this specific configuration is limited, and users must verify process settings against the manufacturer’s technical data sheet.
Molecular differences in MarFlex® 7235B are dominated by the metallocene active-site distribution. Unlike conventional Ziegler-Natta catalysts, metallocene catalysis produces a narrower molecular-weight distribution and a more uniform short-chain branching distribution. This architecture lowers the fraction of low-molecular-weight, highly branched chains that contribute to seal initiation and extractables while maintaining the higher-molecular-weight chains responsible for dart impact resistance under ASTM D1709. The result is a film that can be downgauged without a proportional loss in tear resistance measured under ASTM D1922 or puncture resistance under ASTM D5748. The lower extractable level is relevant for food-contact applications evaluated under FDA 21 CFR 177.1520 and EU Regulation No 10/2011. In coextruded structures, the grade’s narrow composition distribution reduces gel counts and improves optical homogeneity, but melt strength remains lower than high-pressure LDPE. The resin’s seal initiation temperature is assessed by ASTM F1921 and seal strength by ASTM F88; comparative values against butene-based LLDPE must be generated on the target sealing equipment because seal-bar geometry and dwell time shift the response. Tensile properties are measured under ASTM D882 or ISO 527-3. The molecular architecture does not eliminate the need for process stabilisation, and the material should be kept below the maximum continuous-use temperature stated in the manufacturer’s product data.
On a production-scale cast film line using a 90 mm single-screw extruder with a barrier screw and 30:1 L/D ratio, the melt temperature for this grade is typically maintained between 240°C and 290°C. The extruder feed throat is operated cooler than the rear barrel zone to prevent premature melting and pellet bridging. A flat die with a lip gap of 0.4 mm to 0.8 mm deposits the curtain onto a chill roll controlled at 15°C to 30°C; chill roll water temperature, roll speed, and air gap from 5 cm to 15 cm determine quench rate and film crystallinity. Higher chill roll temperatures reduce quench-induced orientation and can improve MD tear but may increase haze under ASTM D1003. In-line beta or X-ray thickness gauges are used to maintain thickness variation within ±2% of target; film gauge non-uniformity directly affects stretch film elongation and load retention. Corona treatment units are normally set to deliver a surface energy of 38 mN/m to 42 mN/m for printing or lamination, but the target dyne level depends on ink or adhesive chemistry. To avoid gel accumulation at the die lip, the line should be purged with a lower-melt-index polyethylene during shutdown, and screen packs from 40 mesh to 60 mesh are typically installed to trap infrequent catalyst residues or char particles. Processing assistant masterbatch addition should be validated on the target line because melt pressure and fume generation vary with screw design; published data for this specific configuration is limited.
Blown film conversion of this resin generally uses die gaps between 1.0 mm and 2.0 mm, blow-up ratios from 2.0:1 to 3.0:1, and frost line heights from 5 to 9 die diameters. Melt temperatures are lower than cast film, typically 190°C to 230°C, to maintain bubble stability. The narrow molecular-weight distribution reduces melt fracture and gel-induced bubble breakage compared with broad-MWD Ziegler-Natta LLDPE, but the lower melt strength than LDPE requires controlled air-ring operation. In coextrusion with LDPE, LDPE addition of 10% to 20% by weight is common for high stalk or high blow-up-ratio production. Die lip cleanliness is critical: metallocene LLDPE can accumulate oxidised material at the die lip during long runs, producing haze bands and dart impact loss. Frost line height directly influences film toughness: a high frost line increases MD orientation and may reduce MD Elmendorf tear under ASTM D1922, while a low frost line increases TD orientation and can destabilise the bubble at high output. Internal bubble cooling improves output but requires separate control of exhaust air temperature and volume. Gauge uniformity is monitored by an in-line capacitive or optical gauge, and typical variation should be held within ±3% for consistent dart impact under ASTM D1709A. For food-contact films, the processing temperature should remain below the level at which antioxidant degradation products exceed migration limits under EN 1186.
Cast stretch film made from MarFlex® 7235B is typically drawn to thicknesses from 10 µm to 25 µm on cast lines with high-velocity air knives and vacuum boxes to stabilise the melt curtain. The film path includes prestretch rollers operated at ratios from 150% to 300% in conversion equipment, but film toughness requirements are set by load-holding performance. Puncture resistance according to ASTM D5748 and tensile elongation according to ASTM D882 are the controlling mechanical parameters for pallet-wrap applications. Cling performance is not an inherent bulk resin property; cling additives are introduced as masterbatch at typical addition levels of 0.5 phr to 2.0 phr depending on the required peel force under ASTM D5458. In lamination film, the seal layer must demonstrate adequate seal strength under ASTM F88 and a low seal initiation temperature under ASTM F1921. The grade’s narrow distribution generally permits lower sealing temperatures than butene-based Ziegler-Natta LLDPE, but the exact difference is application-specific and must be confirmed with a seal-bar temperature gradient test. Film optics are measured by haze under ASTM D1003 and gloss at 45° under ASTM D2457. Because cast film cools asymmetrically, curl and blocking can occur if the roll is wound at high tension without sufficient anti-block masterbatch; published data for this specific configuration is limited.
Direct substitution of MarFlex® 7235B for a conventional butene-based Ziegler-Natta LLDPE of equivalent density and melt index changes the film property balance. The metallocene architecture narrows the comonomer distribution, which typically raises dart impact and puncture resistance at the same thickness while reducing seal initiation temperature. The difference is not captured by density and melt index alone; a film line trial is required because die geometry, frost line position, and cooling conditions interact with the resin’s crystallinity. Compared with high-pressure LDPE, the resin has lower melt strength, so cast-film neck-in may increase; this is controlled by reducing the air gap, adjusting die width, or blending with LDPE at 10% to 20% by weight. In blown film, LDPE addition improves bubble stability but can reduce dart impact and tear strength; the blend ratio should be tuned against ASTM D1709 and ASTM D1922 data. The resin’s coefficient of friction under ASTM D1894 can be modified with slip and anti-block masterbatches, but these additives can reduce optical clarity and seal performance. Because the grade is formulated with a narrow processing window, melt temperatures above 290°C in cast film are generally not recommended, as excessive thermal oxidation can increase gel formation and odour. The specific additive package and lot composition are disclosed in the technical data sheet and certificate of analysis; users should not assume that other MarFlex grades with similar density are interchangeable.
Regulatory conformance for food-contact applications is not implied by the product designation. In the United States, olefin polymer films may qualify under FDA 21 CFR 177.1520, subject to end-use extraction and intended food type. For the European Union, compliance is evaluated under Regulation (EU) No 10/2011, with overall migration testing according to EN 1186. REACH obligations under Regulation (EC) No 1907/2006 require review of substances of very high concern, and the RoHS Directive 2011/65/EU may be relevant to final articles containing this polymer. The table below summarises the regulatory frameworks that are commonly referenced in film qualification.
| Regulatory framework | Reference | Verification requirement |
|---|---|---|
| U.S. food contact | 21 CFR 177.1520 | Manufacturer food-contact certification and end-use extraction testing |
| EU food contact | Regulation (EU) No 10/2011 | Overall migration testing under EN 1186 |
| REACH | Regulation (EC) No 1907/2006 | SVHC review; Article 33 communication if applicable |
| RoHS | Directive 2011/65/EU | Final-article compliance; polymer raw material is typically outside scope |
Storage and handling of MarFlex® 7235B should follow standard LLDPE pellet practice. The resin is supplied ready-to-process; pre-drying is generally not required unless the pellets are stored in humid conditions above 60% relative humidity for extended periods. Storage silos should be cleaned before first use to avoid contamination with incompatible polymers such as PVC or acetal, which can cause black specks or degradation odour. Purging after processing should use a lower-melt-index polyethylene or a commercial purging compound; the resin should not remain stagnant in a heated barrel for more than 15 min at processing temperature because gel formation may occur. Conveying air velocity should be set below 20 m/s to reduce angel hair and fines generation. Static charge accumulation in transfer lines can cause pellet fines to adhere to film surfaces, increasing haze under ASTM D1003. Mechanical property data reported for the resin are generated on compression-moulded or slit film specimens under conditioned laboratory atmospheres of 23°C and 50% relative humidity according to the relevant test method; production film values will differ due to orientation, gauge variation, and additive content. The resin is not intended for applications requiring prolonged exposure to oxidising agents, aromatic hydrocarbons, or high-energy radiation without prior validation. Users must obtain the current certificate of analysis and safety data sheet before implementation.