| HS Code | 739311 |
| Product Name | Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Melt Index 190 C 2 16 Kg | 3.5 g/10 min |
| Density | 0.923 g/cm³ |
| Melting Point Dsc | 123 °C |
| Vicat Softening Point | 101 °C |
| Tensile Strength At Yield Md | 10.3 MPa |
| Tensile Strength At Yield Td | 10.0 MPa |
| Tensile Strength At Break Md | 27.6 MPa |
| Tensile Strength At Break Td | 24.1 MPa |
| Elongation At Break Md | 500 % |
| Elongation At Break Td | 700 % |
| 1 Secant Modulus Md | 193 MPa |
| 1 Secant Modulus Td | 207 MPa |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Dart Drop Impact | 100 g |
| Haze | 2.0 % |
| Gloss 45 | 85 |
| Coefficient Of Friction | 0.2 |
As an accredited Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips MarFlex® 7235 comes in 25 kg (55 lb) polyethylene bags, palletized and stretch-wrapped for secure storage and handling. |
| Container Loading (20′ FCL) | 20′ FCL loading: Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin, palletized in 25 kg bags, securely stowed for transport. |
| Shipping | Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin is shipped as non-hazardous solid pellets in bags, boxes, bulk bags, or bulk trucks/railcars. It is not regulated for transport and requires no DOT placards. Store in a cool, dry, ventilated area away from direct sunlight, heat, and ignition sources. |
| Storage | Store Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin in original, sealed packaging in a cool, dry, well-ventilated warehouse. Keep indoors on pallets, off the floor, away from direct sunlight, heat, flames, moisture, contamination, and strong oxidizers. Avoid excessive stacking; use first-in-first-out rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typically two years from manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight and heat. |
Machine-direction pre-stretch ratios above 250% on a three-layer cast pallet wrap line convert the outer cling layer into a continuously strained elastoplastic membrane, where recovery after unwinding must remain below 8% when tested at 23 °C and 50% RH according to the film supplier’s internal method aligned with ASTM D882. On a 2.75 m wide line with 75 mm/90 mm/75 mm barrier-screw extruders and a 0.60 mm slot-die lip gap, MarFlex® 7235 is metered at 72–80 wt% of the total output in the core layer, while the cling layer, itself 10–15 wt% of total throughput, carries 2.0–4.0 wt% of a polyisobutylene tackifier concentrate calculated on cling-layer mass in a lower-density metallocene polyethylene carrier; the release layer is maintained at 5–10 wt% of the total structure via a high-density polyethylene/LLDPE backside blend. Melt temperatures at the feedblock are held between 238 °C and 255 °C, and the cast roll surface is controlled at 24–30 °C with a vacuum box pressure of -0.8 kPa to -1.4 kPa relative to atmosphere to suppress pit formation. The critical process limitation is not melt stability but adhesive transfer to the secondary chill roll at pre-stretch loads exceeding 12 N/cm; this condition is monitored with an on-line tension transducer calibrated to ASTM E74 practices. Industrial compliance for pallet overwrap intended for incidental food-contact freight is verified under FDA 21 CFR 177.1520(c) for ethylene homopolymer and olefin copolymers, with end-use migration testing performed under Regulation (EU) No 10/2011 as applicable for packaging entering the European market; heavy-metal restrictions follow REACH Annex XVII, and when the film is used as packaging for electrical and electronic equipment, final equipment compliance is evaluated under RoHS Recast 2011/65/EU at the assembler level. Terminal product types include 23 µm machine-film rolls, 17 µm hand-wrap rolls, and pre-stretched film with a nominal elongation recovery of 45–60% after stress relaxation, used for pallet unitization of corrugated cartons, white goods, and ceramic tile packaging.
Vertical form-fill-seal overwrap for washed leafy greens and cut produce requires seal initiation below 95 °C and a plateau seal strength above 2.5 N/15 mm when tested under ASTM F88 at 0.4 MPa seal bar pressure and 0.5 s dwell. Formulations based on MarFlex® 7235 at 88–95 wt% are compounded with 0.05–0.15 wt% erucamide slip additive, 0.08–0.20 wt% synthetic silica antiblock, and 3–8 wt% of a high-clarity LDPE homopolymer to modify low-temperature seal ductility. The cast film is produced on a 1.9 m single-layer or 2.1 m two-layer line using extruder melt temperature 240–260 °C, die gap 0.45–0.70 mm, and a polished chill roll set at 28–32 °C with air gap kept below 140 mm to retain optical flatness. Heat-seal strength after 24 h conditioning at 23 °C and 50% RH is measured on a tensile tester per ISO 527-3 in parallel with ASTM D1003 haze values; published resin data for this grade indicates suitability for clear overwrap when a haze value below 5% at 25 µm is required, though exact values must be confirmed on the production line. Food-contact compliance is established via FDA 21 CFR 177.1520(c) food-type restrictions and EU No 10/2011 overall migration limits of 10 mg/dm² for the finished film, including surface area-to-volume correction under Regulation (EU) 2016/1416. Downstream equipment comprises VFFS and HFFS machines with temperature-controlled sealing jaws; terminal product forms are retail overwrap for leafy greens, bakery packs, and thin-gauge non-PVC cling replacement films for delicatessen line operations.
In dry-food flexible packaging converting, blown or cast sealant webs are subsequently adhesive-laminated to BOPP, metallized PET, or aluminum foil. In a cast coextrusion line with 1.2 m die width and 65 mm 24:1 L/D extruders, MarFlex® 7235 is run at 90–100 wt% of the sealant layer, with 0–10 wt% of a high-density polyethylene cut-in when the pouch specification demands higher heat-seal temperature resistance. The cast sealant web is produced at a thickness of 20–50 µm, with a chill roll temperature of 22–27 °C and a melt temperature of 235–250 °C, then wound with a 38–42 µm PET or foil web after lamination. Formulators measure hot tack on a J&B hot-tack tester in accordance with ASTM F1921 and seal strength per ASTM F88; the target hot-tack force for high-speed vertical packing typically lies above 1.5 N/25 mm at 105 °C seal bar temperature, while the ultimate heat-seal strength is not accepted below 3.5 N/15 mm. Published hot-tack data for this specific cast sealant configuration in adhesive lamination at 20 µm on foil is limited, so seal window values must be confirmed on the converter’s packaging line. Compliance for dry food packaging includes FDA 21 CFR 177.1520 and EU No 10/2011, and printing inks/adhesives are outside the resin compliance boundary and are governed separately by FDA 21 CFR 175.105 and 175.300 where applicable. Terminal products are liquid sachet and dry-product stand-up pouches, quad-seal coffee pouches, and peelable-to-nonpeelable side-seam seals for snack packaging.
Adhesive transfer and haze development in coextruded protective film are governed by the concentration of tackifying additives in the pressure-sensitive layer and the cold-flow resistance of the backing layer. In a three-layer cast film consisting of a skin adhesive layer, a core, and a release surface, MarFlex® 7235 is used in the backing layer at 85–95 wt% of that layer, the balance being a high-density polyethylene homopolymer at 5–15 wt%, while the face-side adhesive layer constitutes 10–15 wt% of the total film structure and is based on a styrenic block copolymer-rich blend; the backing layer contains 0.05–0.15 wt% of a fluoropolymer processing aid, and the release side receives 0.1–0.3 wt% of a non-migrating polysiloxane release concentrate. The line configuration is a 2.4 m width cast coextrusion with feedblock and three extruders, using melt temperatures 240–265 °C, die gap 0.50–0.75 mm, cast roll at 22–28 °C, and a downstream corona treatment unit set to 38–46 mN/m surface tension during inline silicone release coating. Peel adhesion is measured after 24 h dwell on polished stainless steel per ASTM D3330/D3330M Test Method A, with acceptable clean peel typically between 0.2 N/25 mm and 1.8 N/25 mm depending on end-use; cling force is measured at 0.3 m/min under ASTM D5458 to avoid blocking between the release and adhesive layers. Compliance for electronics protection applications requires RoHS Recast 2011/65/EU verification for restricted substances at the finished device level and REACH SVHC candidate-list screening; food-contact incidental use is evaluated under FDA 21 CFR 177.1520 only for dry, non-fatty contact and not for direct meat or dairy contact. Terminal products include polished stainless steel coil masking film, coated metal sheet protection, electronics display protection during assembly, and window extrusions with UV-stable grades for outdoor exposure up to 3 months.
For stored round bales and high-moisture forage, cast stretch film must retain puncture resistance and cling force over a 12-month outdoor aging period. A three-layer cast film with a core made from MarFlex® 7235 at 68–75 wt% of the structure is processed into 18–30 µm gauge film and pre-stretched to 55–70% of ultimate elongation on a bale wrapper. The outer skin contains 4.0–8.0 wt% of a titanium dioxide white masterbatch and 0.8–1.5 wt% of a hindered amine light stabilizer masterbatch, while the cling layer contains 1.5–3.0 wt% of a high-molecular-weight polyisobutylene tackifier additive calculated on cling-layer mass to maintain tack at 2–10 °C application temperatures. The film is produced on a 2.1 m cast line with a barrier screw 30:1 L/D, melting at 235–250 °C, and the chilled roll is held at 26–32 °C to prevent surface bloom of tackifier before winding. Puncture energy is determined under ASTM D5748, dart impact under ISO 7765-1, and tensile properties under ISO 527-3; a production-scale failure mode is pinhole formation on stubble or wire wrap, which can be reduced by increasing the film gauge above 20 µm and by controlling pre-stretch carriage tension below 18 N/50 mm. Compliance for agri-film entering the EU falls primarily under REACH, under which the polymer is exempt from registration while constituent monomers and additives require registered substances; if the film is used as a feed-contact cover, the converter must additionally verify national feed hygiene requirements under Regulation (EC) No 183/2005. A direct food-contact use would require separate evaluation under Regulation (EU) No 10/2011, but this is not the default agri-film condition. Terminal product types are 750 mm and 500 mm silage bale wrap rolls, haylage tube film, and white/green coextruded bale covers for aerobic stability management.
Non-breathable backsheet films for adult incontinence pads and underpads are cast from a three-layer die and immediately thermally bonded to a spunbond nonwoven using an embossing nip. In this configuration, MarFlex® 7235 is formulated as the outer skin and tie layer at 60–70 wt% of the finished composite film web, with 20–30 wt% of a lower-melting metallocene LLDPE in the nonwoven-facing layer to lower thermal lamination temperature to 92–105 °C and reduce nonwoven fibre compression. The remaining layer contains 3–5 wt% of a white titanium dioxide concentrate and 0.05–0.15 wt% of a phenolic-free processing stabilizer package; no CaCO3 breathable filler is added when liquid impermeability is the dominant requirement. Downstream processing is performed on a 1.6 m width cast lamination line with a mating steel/rubber embossing roll at 0.4–0.8 MPa nip pressure and unwind tension controlled by a closed-loop tension dancer. Penetration resistance is evaluated by ISO 7765-1 dart impact at -20 °C, and the laminated composite is tested for hydrostatic head per AATCC 127 or ISO 811 depending on end-use. Regulatory status for hygiene and medical surfaces is separated by end-use: non-medical absorbent hygiene products are assessed under the EU General Product Safety Directive 2001/95/EC and REACH chemical restrictions, while medical device packaging films fall under ISO 11607-1 as a sterile barrier system and require validation for seal strength according to ASTM F88 before sterilization. Terminal product types are nonwoven-backed underpads, mattress cover substrate, protective disposable bedrolls, and non-sterile barrier film used in absorbent hygiene product backsheets.
Competitive Chevron Phillips MarFlex® 7235 LLDPE Cast Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Chemical’s MarFlex® 7235 is a linear low density polyethylene cast film resin produced by copolymerization of ethylene with 1-hexene. The pelletized product carries a nominal density of 0.918 g/cm³ when measured under ASTM D1505-18 and a melt index of 3.5 g/10 min at 190°C under ASTM D1238-20. These values are supplied as typical data and not as specification limits. The resin is intended for chilled-roll cast film lines producing industrial stretch wrap, hand wrap, high-clarity overwrap, and certain food-contact films. Primary differentiation from octene- or butene-based LLDPE grades lies in the hexene comonomer; this modifies the short-chain branching distribution and the concentration of interlamellar tie molecules after quenching. The practical consequence appears in film toughness tests—particularly ASTM D1709-16a dart drop and ASTM D1922-15 tear—where hexene-copolymer films often show higher values than butene-copolymer films of the same nominal density and melt index. The resin is not supplied with slip or antiblock; those additives are incorporated as masterbatch during extrusion. Storage and handling require moisture control only when the pellet surface is exposed to relative humidity above 60%, because residual moisture can create micro-voids when the melt exceeds 240°C.
Resin selection for cast film often starts with melt index and density, but comonomer type changes the short-chain branching distribution and the probability of tie-molecule formation during quenching. In hexene-copolymer LLDPE, the longer α-olefin comonomer is incorporated into the polymer backbone with a different distribution than butene under similar polymerization conditions. This structural difference is not captured by melt index. Comparative film evaluations on chilled-roll lines have shown that hexene-based cast films often produce higher Dart drop impact under ASTM D1709-16a and higher Elmendorf tear in the transverse direction under ASTM D1922-15 than butene-based films at the same gauge. The magnitude of the difference depends on quench rate, die gap, and film gauge, and published data for this specific configuration is limited. Direct substitution of MarFlex® 7235 into an existing butene-grade formulation should therefore be accompanied by line trials measuring tear anisotropy and puncture resistance rather than relying on density or melt index equivalence.
Rheologically, the hexene backbone influences shear-thinning behavior. Melt index under ASTM D1238-20 is a single point at low shear rate; it does not predict die pressure at cast film shear rates commonly between 100 s⁻¹ and 1000 s⁻¹. Capillary rheometry at 190°C is recommended to compare pressure drop, melt fracture onset, and extruder amp load. Production-scale experience on single-screw lines indicates that replacing a butene-copolymer LLDPE of equal melt index with a hexene grade can alter die pressure and extruder torque, requiring barrel temperature profile adjustments of 5–10°C to maintain stable throughput. The exact adjustment is line-specific and depends on screw design, die width, and throughput per die inch.
On a typical cast film line with a 90 mm single-screw extruder, 30:1 L/D grooved feed section, and a 2.4 m die, MarFlex® 7235 is processed with a melt temperature of 204–260°C. The lower boundary is set by viscosity and backpressure; the upper boundary is set by oxidative degradation and gel formation. Barrel profiles typically rise from 170–190°C at the feed throat to 220–240°C at the die adapters. The die gap is commonly set between 0.5 mm and 1.0 mm, and the molten web is pinned to a chilled roll maintained at 15–25°C. Chill roll temperature below 15°C can improve optical clarity but may cause condensation when plant humidity exceeds 60%. The air gap between die lip and chill roll is a critical control variable; excessive air gap allows draw resonance, while an insufficient gap can cause polymer buildup on the die lip. Line speed is adjusted to produce film from 8 µm to 150 µm depending on the end use. For stretch wrap, the line speed often exceeds 300 m/min, which places a premium on melt stability and gauge uniformity.
Higher output can be achieved by increasing screw speed, but this raises melt temperature due to viscous dissipation. Shear heating in a barrier screw with a Maddock mixer set at 0.5 mm clearance may add 5–15°C above barrel setpoint at high screw speed. Die pressure and motor amperage must be monitored to avoid overloading the extruder drive. If melt temperature exceeds 260°C, the risk of gel formation increases, particularly in the presence of oxygen at the feed throat. An inert gas purge on the hopper is not required for routine operation but may be used when running high-temperature reclaim blends.
Industrial stretch wrap is a primary application for MarFlex® 7235. Downgauging from 20 µm to 12 µm or below intensifies the requirement for slow-rate puncture resistance, because the film must survive contact with sharp pallet corners during automatic wrapping. ASTM D5748-19 describes protrusion puncture resistance for stretch wrap film; the test measures the force required for a probe to puncture the film, and values are gauge-dependent. Hexene-copolymer LLDPE generally offers higher puncture resistance than butene-copolymer LLDPE at equivalent gauge because of its architecture, but the actual result is influenced by cast roll quench, line orientation, and additive package.
Film produced on cast lines has lower machine-direction orientation compared with blown film, but the draw ratio from die to chill roll still creates machine-direction orientation. The ratio of tensile strength in the machine direction to transverse direction is typically lower for cast film than for blown film, which improves puncture energy distribution around a protrusion. For MarFlex® 7235, the process must be controlled to avoid excessive neck-in; the draw-down distance between die exit and chill roll, the melt temperature, and the line speed determine the final balance of MD/TD tensile strength under ASTM D882-18. A high draw ratio can increase MD tensile strength but reduce TD elongation and tear resistance, which is detrimental for stretch wrap under puncture.
Cling in stretch wrap is often provided by a migratory additive such as low-molecular-weight polyisobutylene. Migration kinetics are temperature-dependent. Below 5°C, the additive may not bloom to the surface sufficiently for manual wrapper performance; above 40°C, the same additive can create blocking on the finished roll. Peel cling under ASTM D5458-16 must be measured on the target film structure after a conditioning period of at least 24 h at 23°C ± 2°C and 50% ± 5% relative humidity, because cling values drift with time. These operational boundaries are not specific to MarFlex® 7235; they arise from the additive package and film structure selected by the converter.
Gels and optical defects in cast film are often attributed to crosslinked resin particles or contaminant ingress, but the thermal history of the melt also affects gel formation. Differential scanning calorimetry under ASTM D3418-15 can be used to compare the melting peak and crystallinity of the quenched film; rapid quenching on a chill roll suppresses spherulitic growth and reduces haze. Haze measured under ASTM D1003-13 and clarity under ASTM D1746-15 are influenced by chill roll temperature, air gap, and die lip cleanliness. A chill roll temperature above 25°C may increase haze by slowing the quench rate and allowing larger crystalline aggregates. The reverse condition, a chill roll below 10°C, risks condensation and can introduce surface defects if the film is wound before the surface temperature equilibrates. Gel counts per unit area are not standardized across all converters; a common method is visual inspection with a dark-field scanner, but correlation to downstream film breaks is line-specific.
Die lip buildup can also degrade optical quality. Low-molecular-weight fractions may migrate to the die lip during extended runs, especially when melt temperature is held above 240°C for long periods. The resulting deposits can produce die lines in the film. The mitigation is not a change in resin alone but a combination of die lip coating, purge compounds, and periodic die wiping. The need for die maintenance increases when no slip or antiblock is present in the pellet because the film surface remains tacky and can carry contaminants.
MarFlex® 7235 is typically blended with a slip/antiblock masterbatch at a letdown ratio determined by the target coefficient of friction. For high-clarity cast film, the antiblock particle size must be below the film gauge to avoid visible protrusions. The coefficient of friction is measured under ASTM D1894-14 on the film surface after conditioning; a target kinetic coefficient between 0.2 and 0.4 is common for automated packaging lines, but the exact value depends on packaging machine design. Excessive antiblock increases haze under ASTM D1003-13 and reduces gloss under ASTM D2457-13. The trade-off between blocking resistance and optical quality is therefore established on the target cast line rather than from resin density or melt index alone.
| Regulatory reference | Test method or condition | Applicability boundary |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers | Food-contact use subject to end-use condition and migration limits |
| EU Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm² | Converter validation required on final film structure |
| REACH 1907/2006/EC | SVHC candidate list, Article 33 communication | No intentionally added SVHC above 0.1% w/w |
| RoHS 2011/65/EU | Heavy metal restrictions | Not applicable to packaging; relevant only for electrical/electronic equipment components |
Food-contact suitability for MarFlex® 7235 is not a single certification. The converter must validate the final film structure, including any slip, antiblock, or cling masterbatch, against the applicable national regulation. The base polyolefin resin may comply with FDA 21 CFR 177.1520 for olefin polymers; however, the presence of process aids, surface modifiers, or reclaimed material can shift the overall migration profile. Extractives testing under the intended use conditions is required before commercial use.
Compared with butene-copolymer LLDPE of 0.918 g/cm³ density and 2.0 g/10 min melt index, MarFlex® 7235 has a higher melt index intended for cast film lines operating at high throughput and moderate melt temperature. The higher melt index reduces extruder motor load but may also lower melt strength, affecting neck-in and draw resonance. Compared with octene-copolymer LLDPE, the hexene comonomer offers a different toughness profile; octene copolymers often provide higher dart drop at the same density, but at higher comonomer cost. Compared with metallocene-catalyzed LLDPE, the resin may exhibit a broader molecular weight distribution, which can be inferred from lower shear viscosity at high shear rates and higher die swell. However, published data for this specific configuration is limited; converter trials with capillary rheometry and film property testing are required to confirm any substitution effect.