Chevron Phillips Marflex 7120s Lldpe Blown Cast Film Resin

Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin

    • Product Name: Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 652813
    Polymer Type LLDPE
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melt Flow Ratio I21 I2 28
    Tensile Strength At Yield Md 1400 psi
    Tensile Strength At Yield Td 1400 psi
    Tensile Strength At Break Md 4500 psi
    Tensile Strength At Break Td 4000 psi
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Resistance Md 200 g/mil
    Elmendorf Tear Resistance Td 350 g/mil
    Dart Drop Impact 120 g/mil
    Haze 8%
    Gloss 45 70%
    Coefficient Of Friction 0.2
    Blocking 60 g
    Vicat Softening Point 100°C
    Melting Point 122°C

    As an accredited Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin is packaged in 25 kg polyethylene bags on stretch-wrapped pallets.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin, 25 kg bags on pallets; approx. 18–22 MT.
    Shipping MarFlex® 7120S LLDPE resin ships as non-hazardous solid pellets in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars. Store and transport cool, dry, and clean, away from moisture, contaminants, and direct sunlight. No dangerous-goods placarding required under DOT/IMDG/IATA.
    Storage Store MarFlex 7120S LLDPE resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original packages closed, off the floor, and protected from moisture, dirt, and contamination. Avoid prolonged excessive heat. Rotate stock first-in, first-out, and follow the supplier’s SDS and local regulations.
    Shelf Life Shelf life is approximately 24 months from manufacture when stored unopened in original packaging in a cool, dry, well-ventilated area.
    Application of Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin

    In cast stretch-film converting, MarFlex® 7120S is typically metered through a three-layer flat-die extrusion line with a 0.45–0.7 mm die gap, a 2,000–3,200 mm coat-hanger die, and an air-knife-assisted polished chill-roll stack maintained at 18–25 °C. The resin is allocated to the skin and core layers at 70–85 wt% of total throughput, with 15–30 wt% of a narrower-molecular-weight mLLDPE or an autoclave LDPE used to suppress draw resonance and reduce neck-in; a polyisobutylene cling masterbatch is dosed at 1.0–3.0 wt%, delivering an active cling additive level of 0.5–2.0 wt% in the outer layers. Melt temperature is held between 220 °C and 250 °C because lower temperatures increase die-lip build-up and higher temperatures accelerate oxidative degradation of the polyisobutylene cling component. Draw ratios may exceed 40:1 on cast lines running at 300–600 m/min, and edge trim is re-fed at a maximum of 5–8 wt% to avoid gel specks. Compliance for non-food pallet wrap is assessed under ASTM D5458-08 for cling, ASTM D5748-95(2019) for puncture resistance, ASTM D882-18 for tensile properties, and EU Directive 94/62/EC heavy-metal limits requiring lead, cadmium, mercury, and hexavalent chromium each below 100 mg/kg. Terminal formats include hand stretch film, machine stretch film, pre-stretched cast film, and tinted or printed pallet wrap for logistics identification.

    What Happens to Seal Strength When MarFlex® 7120S Is Coextruded with LDPE in Frozen-Food Webs?

    A three-layer blown-film line producing frozen-food webs coextrudes MarFlex® 7120S with LDPE at 70–85 wt% 7120S and 15–30 wt% LDPE to stabilize the bubble while preserving low-temperature dart impact. The film is processed through a 1.0–2.0 mm die gap at a blow-up ratio of 2.0–2.8, a frost-line height of 300–700 mm, and a melt temperature of 185–210 °C. Food-contact compliance is established under FDA 21 CFR §177.1520(c) for olefin polymers, with use conditions assigned under 21 CFR §176.170(c), and under EU Regulation (EU) No 10/2011 using overall migration limits of 10 mg/dm² or 60 mg/kg food simulant. Frozen aqueous foods are simulated with simulant A (10% ethanol), while fatty-frozen applications may require simulant D2. Seal strength measured by ASTM F88/F88M-21 typically remains above 2.0 N/15 mm after a 0.5 s dwell at 105–130 °C, but low-temperature seal integrity must be verified at -18 °C because under-stretched LLDPE sealant layers can display brittle peel. Dart impact is assessed under ASTM D1709 Method A, and Elmendorf tear under ASTM D1922-15. Converted products include frozen vegetable pouches, IQF poultry bags, deep-freeze seafood pouches, and ice-cream wrappers.

    Stretch Hood Logistics Film and the Sub-250 µm Tear Propagation Threshold

    When pallet-load stabilisation film is blown at thicknesses below 250 µm, transverse-direction tear propagation becomes the controlling failure mode, and MarFlex® 7120S is placed in the core layer at 50–70 wt% with 20–35 wt% C6 mLLDPE and 10–20 wt% LDPE. Cling additives are typically omitted because the film is stretched mechanically over the load rather than relying on self-adhesion; slip and antiblock masterbatch is limited to 0.05–0.2 wt% to prevent blocking during storage. The blown-film process uses a 300–600 mm die, a die gap of 1.2–2.4 mm, a blow-up ratio of 2.0–2.6, and a frost-line height of 600–1,200 mm, with internal bubble cooling maintaining air temperature at 10–15 °C. Frost-line deviation greater than ±50 mm causes uneven transverse elongation and can shift the tear-propagation threshold by more than 15%, so automated frost-line control is specified. Mechanical conformance is measured under ISO 527-3:2018 for tensile properties, ASTM D1922-15 for Elmendorf tear, ASTM D1709 Method B for high-energy dart impact, and pallet-load stability is validated under EUMOS 40509. Terminal products include stretch hoods for palletized beverage bottles, chemical drums, building-material units, and white-goods packaging.

    Because silage bale wrap must retain a cling seal after twelve months of UV exposure, MarFlex® 7120S is typically blended with LDPE at 75–90 wt% 7120S and 10–25 wt% LDPE, with a UV masterbatch added at 4–8 wt% to achieve 0.4–0.8 wt% HALS active and 1.5–2.5 wt% TiO2 or carbon black. Cling performance is generated by a polyisobutylene or long-chain polybutene masterbatch at 1.0–3.0 wt% in the outer layers. The three-layer blown-film process operates at a blow-up ratio of 2.0–3.0, a die gap of 1.0–2.0 mm, and a melt temperature of 185–220 °C; slit rolls are wound at 500 mm or 750 mm widths for round-bale wrappers. Film is supplied in thicknesses from 25 µm to 150 µm, with the 25–40 µm range used for round bales and thicker gauges used for silage bags and pit silo covers. Regulatory compliance for non-food agricultural film is evaluated under EN 13207:2018, including tensile at break, tear resistance, and accelerated UV aging under ISO 4892-2:2013; REACH SVHC communication obligations apply to the masterbatch components. Terminal products include round-bale silage wrap, silage bags, pit silo covers, and long-term forage storage liners.

    Heavy-Duty Shipping Sacks with Form-Fill-Seal Dust Containment

    Form-fill-seal shipping sacks for polymer pellet and chemical powder export specify MarFlex® 7120S at 60–80 wt% with 15–30 wt% HDPE for stiffness and 5–10 wt% LDPE for processability; slip and antiblock masterbatch is added at 0.1–0.5 wt%. The blown-film line uses a die gap of 1.5–2.5 mm, a blow-up ratio of 1.8–2.4, a melt temperature of 190–230 °C, and a screen pack of 100–150 mesh to capture oxidized gels. Conformance for industrial packaging is verified by ASTM D1709 Method B dart impact, ASTM D1922-15 tear resistance, and ISO 527-3:2018 tensile properties; dangerous-goods sacks must satisfy the performance tests assigned under the UN Model Regulations by the competent authority. Terminal products include 25 kg FFS pillow pouches, heavy-duty liners for bulk bags, valve sacks, and chemical pellet shipping sacks.

    When a Cast PP Sealant Web Is Replaced by an LLDPE Sealant Layer

    A cast lamination line that moves from a polypropylene sealant web to an LLDPE sealant layer must recalibrate heat-seal jaw temperature from a typical PP range of 135–160 °C to an LLDPE range of 105–125 °C; MarFlex® 7120S is employed at 70–90 wt% with 10–30 wt% of an ethylene-α-olefin plastomer having density 0.865–0.885 g/cm³ to lower seal initiation and improve hot tack. Slip and antiblock are maintained at 0.05–0.2 wt% to avoid seal contamination. The cast process uses a 0.45–0.7 mm die gap, a polished chill roll at 15–22 °C, and a sealant-layer thickness of 20–50 µm; corona discharge is applied to 38–42 mN/m before lamination against BOPP, PET, or aluminium foil. Seal strength is tested under ASTM F88/F88M-21, hot-tack is assessed under ASTM F1921-18, and food-contact status follows FDA 21 CFR §177.1520(c) and EU Regulation (EU) No 10/2011 with migration limits of 10 mg/dm² or 60 mg/kg. Terminal products include three-side-seal pouches, stand-up pouches, sachets, and lidding films for chilled and dry-food formats.

    Coextruded pressure-sensitive masking backings for temporary surface protection are produced by dry-blending MarFlex® 7120S with 10–25 wt% LDPE or an olefin elastomer and processing on a cast line at a melt temperature of 200–230 °C; the draw ratio is kept below 35:1 to minimize machine-direction stiffness that would increase unwinding force. Film thickness is controlled at 20–80 µm, and corona treatment to 38–44 mN/m is applied before a solvent- or water-based acrylic adhesive is coated. Peel adhesion is measured under ASTM D3330/D3330M-04 and ISO 8510-2:2007, with REACH SVHC documentation required for the adhesive and backing system. Published data for the specific combination of MarFlex® 7120S backing and high-solids acrylic adhesive is limited, so coated-roll qualification under production-scale unwind tension and aging conditions is required before shipment. Terminal products include temporary protective film for stainless steel coil, aluminium profiles, polycarbonate sheet, appliance panels, and automotive interior parts.

    Free Quote

    Competitive Chevron Phillips MarFlex® 7120S LLDPE Blown & Cast Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips MarFlex® 7120S is a linear low-density polyethylene resin produced with 1-butene comonomer and a Ziegler-Natta catalyst system, supplied as pellets for blown and cast film conversion. The nominal melt index is 1.0 g/10 min determined under ASTM D1238 at 190 °C with a 2.16 kg load, and the nominal density is 0.918 g/cm³ determined under ASTM D1505. These two material parameters define the resin’s position in the general-purpose film segment: the density provides a thermal and stiffness profile appropriate for sealable packaging webs, while the melt index permits stable extrusion on grooved-feed blown film lines and conventional cast film lines. The product is intended for monolayer and coextruded structures in which gauge uniformity, seal integrity, and balanced tear propagation are required.

    Unlike high-pressure LDPE, 7120S contains predominantly short-chain branching from butene and only minor long-chain branching from the catalyst system. The resulting melt elasticity is lower than LDPE, which reduces bubble stability but improves draw-down and thickness control in cast film. Because the grade is not a metallocene-catalysed resin, the composition distribution is wider than that of a single-site mLLDPE; this affects optical properties, seal plateau width, and extrusion viscosity.

    Storage and handling requirements follow standard polyolefin practice. Pellets should be kept in a closed hopper or silo to exclude contamination; pre-drying is unnecessary unless condensation from cold shipment into a warm production hall has wetted the pellet surface. If surface moisture exceeds 0.05 wt% by Karl Fischer titration, a desiccant-bed dryer at 60 °C for 2 h may be used, but this situation is rare for polyethylene.

    How Does Butene Short-Chain Branching Shape Dart Impact and Tear Balance in 7120S?

    The 1-butene comonomer introduces ethyl branches that reduce lamellar thickness and overall crystallinity. At a nominal density of 0.918 g/cm³, the material has a lower tie-chain population than a hexene or octene LLDPE of the same density because butene branches are shorter and less effective at connecting adjacent crystalline regions. The consequence is measured in film toughness: under ASTM D1709, butene LLDPE resins typically show lower dart drop impact values than hexene LLDPE resins at equivalent density and melt index, and under ASTM D1922, machine-direction Elmendorf tear is generally lower. Transverse-direction tear is often higher in blown film because of the orientation state produced at standard blow-up ratios of 2.0:1 to 2.5:1.

    The optical clarity of 7120S is governed by crystallite size and internal haze. Compared with LDPE at the same film gauge, the linear butene backbone can reduce large spherulitic scattering but may still show higher surface haze than a metallocene LLDPE. Haze measurements under ASTM D1003 and gloss measurements under ASTM D2457 should be expected to vary with die gap, frost line height, and chill roll polish. Published data for this exact grade across all conversion conditions is limited; film property values should be generated on the target line rather than transferred from generic LLDPE tables.

    On a 65 mm grooved-feed blown film extruder with a length-to-diameter ratio of 30:1, a 125 mm spiral mandrel die, and a 2.0 mm die gap, 7120S is typically processed with barrel set temperatures from 180 °C in the feed zone to 210 °C at the adapter, producing a melt temperature of 215 °C to 225 °C. A barrier screw with a Maddock mixing section is preferred because the narrow molecular weight distribution of LLDPE does not generate the same shear-thinning as LDPE and can leave unmelted temperature streaks if a single-flighted general-purpose screw is used. The recommended blow-up ratio is 2.2:1 to 2.5:1; frost line height is commonly set between 6 and 8 die diameters to control film optics and tear orientation. Internal bubble cooling is advised when output exceeds 45 m/min on gauges below 25 µm.

    The upper melt temperature limit of 260 °C should be observed. Prolonged residence time above this threshold increases auto-oxidation and can generate gel specks in clear film. The lower practical melt temperature is approximately 200 °C; below this, unmelted resin or high back-pressure can create motor overload on extruders without grooved feed support. Residence time in the extruder should be kept below 5 min at maximum temperature to minimize degradation.

    Rheologically, the material can be characterized by capillary rheometry under ASTM D3835 at 190 °C. The apparent shear viscosity of a 1.0 g/10 min LLDPE at 100 s⁻¹ typically falls between 800 Pa·s and 1,200 Pa·s, but the exact curve for 7120S should be taken from the supplier’s lot-specific certificate of analysis. The power-law index is less shear-thinning than LDPE, meaning that extruder pressure rises more steeply with output. This is one reason that grooved-feed extruders with barrier screws are used instead of smooth-bore LDPE screws.

    For cast film conversion, a 32:1 length-to-diameter ratio barrier screw with a 150 mm coathanger die and a polished chill roll maintained at 20 °C to 25 °C is typical. Melt temperature at the die is held between 240 °C and 260 °C to suppress melt fracture and reduce draw resonance. The air gap is kept between 10 mm and 20 mm; longer air gaps increase neck-in and edge bead instability because the low melt elasticity of butene LLDPE provides little resistance to extensional sag. At outputs above 350 kg/h, die lip build-up from oxidized low molecular weight species can limit run length more than extruder capacity. Periodic die lip cleaning and, where validated, a fluoropolymer processing aid at 200 mg/kg to 400 mg/kg are used to control this failure mode.

    Cast Film Edge Beading and Chill Roll Release Are Controlled by Density and Melt Index

    Edge beading in cast webs is influenced by melt strength, die swell, and neck-in. At a melt index of 1.0 g/10 min, 7120S exhibits less neck-in than a 2.0 g/10 min cast film grade but more than a 0.5 g/10 min high-viscosity LLDPE. Draw ratio must therefore be limited relative to fractional-melt grades; typical draw ratios for this resin in cast film are between 8:1 and 15:1, depending on die gap and air gap. Excess draw ratio produces gauge bands and edge weave because the melt cannot relax orientation before solidification on the chill roll. Published data for this specific configuration is limited; actual edge bead profiles should be mapped against die width, coat-hanger geometry, and chill roll diameter.

    Chill roll release depends on crystallinity and surface roughness. At 0.918 g/cm³, the resin has adequate crystallinity for release from a matte chill roll without external release agents in most monolayer cast webs. However, at film thicknesses below 20 µm, blocking during winder aging may occur if warm-roll temperatures exceed 30 °C. In such cases, a lower-density skin layer or an antiblock masterbatch is used.

    When 7120S Replaces LDPE in a Sealant Layer, Which Processing Parameters Shift First?

    In coextruded film, replacement of LDPE with 7120S in a sealant layer changes the viscosity ratio and melt elasticity at the layer interface. LLDPE has almost no long-chain branching and a narrower molecular weight distribution than autoclave or tubular LDPE; at equal melt index, die pressure is often lower and shear sensitivity is reduced. Interfacial wave or layer non-uniformity may appear when the adjacent layer is a high-viscosity HDPE or when the sealant layer exceeds 30% of total thickness. To restore stable flow, the sealant layer extruder set temperature is reduced by 5 °C to 10 °C, or the die gap is narrowed from 2.5 mm to 2.0 mm. Increasing the sealant layer thickness increases its channel pressure and can also reduce interfacial distortion, but this must be balanced against total structure economics.

    The seal response of 7120S is typical for a 0.918 g/cm³ butene LLDPE. Heat-seal strength measured under ASTM F88 and hot-tack measured under ASTM F1921 should be evaluated over the temperature range 95 °C to 130 °C because the seal plateau is narrower than that of a metallocene LLDPE. The resin is not recommended for retort, hot-fill, or other structures requiring sustained seal integrity above 130 °C.

    Compared with a hexene LLDPE of the same density and melt index, 7120S trades some puncture toughness and machine-direction tear resistance for easier extrusion at lower melt temperature and generally lower back pressure. The processing difference comes from butene short-chain branching, which produces a slightly broader composition distribution under Ziegler-Natta catalysis but a shorter branch length than hexene. Published side-by-side data for this exact grade is limited; comparative screening under ASTM D1709, ASTM D1922, and ASTM F88 is required before replacing a hexene grade in a qualified package.

    Against a metallocene LLDPE of equal density, the Ziegler-Natta broad molecular weight distribution of 7120S reduces dart impact and clarity under ASTM D1709 and ASTM D1003 but widens the heat-seal processing window and improves bubble stability at high-stalk configurations. The broader melting endotherm permits processing on older extrusion lines that have limited back-pressure capability.

    The distinction from LDPE is the absence of long-chain branching. 7120S provides higher tensile strength and stiffness at equal gauge but lower melt strength and less strain hardening. The loss in melt elasticity is managed by blending 10 wt% to 20 wt% LDPE in many blown film structures; the addition of LDPE improves bubble stability and optical gloss but reduces dart toughness and heat-seal strength. In cast film, LDPE is seldom required for bubble stability because the web is supported by the chill roll, but small additions can reduce draw resonance.

    Selected resin identification data
    PropertyTest methodPublished nominal value
    Melt indexASTM D1238, 190 °C/2.16 kg1.0 g/10 min
    DensityASTM D15050.918 g/cm³
    Base resin comonomerASTM D5576 / FTIR structural analysis1-butene
    Physical formVisual inspectionPellets

    The crystallization kinetics of a 0.918 g/cm³ butene LLDPE under non-isothermal differential scanning calorimetry cooling at 10 °C/min typically produce a crystallization peak between 105 °C and 110 °C. In cast film, the chill roll must remove heat quickly enough to freeze the web before spherulitic growth increases haze. A polished chill roll at 20 °C yields faster cooling than a matte roll at 30 °C; the surface finish controls both optical properties and release. These relationships explain why film optical properties are strongly line-dependent and cannot be predicted solely from resin density.

    Regulatory and compliance references applied to polyolefin film resins
    ReferenceDesignationApplication limitation
    U.S. food contact21 CFR 177.1520Olefin polymers may be used in contact with food types and conditions specified by the regulation; end-use verification is required
    EU plastic food-contact materialRegulation (EU) No 10/2011Overall migration and specific migration limits apply; compliance depends on monomer and additive composition
    REACHEC 1907/2006Substances in the resin must be registered or exempt; supplier safety data sheet remains point-of-use authority
    RoHSDirective 2011/65/EURaw resin is not in scope as an electrical or electronic equipment article; converted article heavy-metal testing is required only where the final product is in scope
    Top