| HS Code | 454725 |
| Density | 0.918 g/cm³ |
| Melt Index | 2.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield Md | 13.8 MPa |
| Tensile Strength At Yield Td | 12.4 MPa |
| Tensile Strength At Break Md | 31.0 MPa |
| Tensile Strength At Break Td | 27.6 MPa |
| Elongation At Break Md | 500 % |
| Elongation At Break Td | 700 % |
| Dart Drop Impact | 125 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 11 % |
| Gloss | 60 % |
| Coefficient Of Friction | 0.2 |
As an accredited Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin is available in 25 kg polyethylene bags and 1,000 kg bulk bags, typically palletized. |
| Container Loading (20′ FCL) | 20′ FCL: 18 MT palletized or 20 MT unpalletized of Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin. |
| Shipping | Shipped as non-hazardous LLDPE pellets in 25-kg PE bags, jumbo bags, or bulk trucks/railcars. Store cool, dry, ventilated, away from heat, sparks, and direct sunlight. Protect from moisture and contamination. Follow SDS/local rules. Use proper handling and PPE. Transport in closed, labeled containers. Avoid pellet spills; clean promptly. |
| Storage | Store MarFlex 7120 LLDPE resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers or bags closed to prevent moisture, dust, and contamination. Use first-in, first-out stock rotation. Avoid prolonged UV exposure and extreme temperatures. Maintain clean handling areas and follow the manufacturer’s safety data sheet recommendations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area. |
In heavy-duty industrial sack and flexible intermediate bulk container liner conversion, the resin is processed on mono layer blown-film lines equipped with grooved-feed extruders in the 75–120 mm diameter range and L/D ratios of 24:1–30:1. The specified density of 0.912 g/cm³ under ASTM D1505-18 and a melt index of 2.0 g/10 min under ASTM D1238-20 at 190°C/2.16 kg place the material in the hexene-comonomer linear low-density polyethylene class; this comonomer architecture suppresses excessive lamellar thickening and yields the machine-direction tear resistance that blown-film converters exploit. Die gaps of 1.6–2.0 mm, blow-up ratios of 2.2:1–2.8:1, and melt temperatures of 195–220°C are maintained on conventional spiral mandrel dies; under these conditions, sharkskin melt fracture is not observed at shear rates below 200 s⁻¹ because the critical shear stress at the die lip remains below the resin’s slip threshold. Film gauges in 80–120 µm are tested to ASTM D1709-16A for dart impact, ASTM D1922-15 for Elmendorf tear, and ASTM D5748-95(2019) for slow probe puncture; procurement specifications for FIBC liners frequently set minimum dart impact values between 350 g and 500 g for 100 µm film, machine-direction tear values above 150 g, and transverse-direction tear values above 200 g. Secant modulus at 1% elongation under ASTM D882-18 is controlled in the 140–180 MPa range for monolayer structures; where higher bending stiffness is required, dry blending with 20–30 wt% HDPE at 0.956 g/cm³ density raises secant modulus to 220–280 MPa while retaining tear propagation resistance. On production lines with 250–350 mm die diameters, frost line height is held between 3 and 5 die diameters to prevent excessive transverse-direction orientation; thickness variation measured by beta gauge after calendering and winding is specified below ±6% to avoid localized stress concentration at bag seams. Batch-to-batch variation in melt index must be limited to ±0.15 g/10 min to avoid screw speed fluctuations and backpressure shifts on gravimetric feeders.
On cast stretch film lines running at widths of 1.5–3.0 m, the resin is extruded through a coat-hanger flat die with die gap of 0.5–0.8 mm at melt temperatures of 235–260°C and quenched on a polished chrome chill roll held at 18–24°C. Draw resonance, which appears as periodic thickness bands parallel to the machine direction, is the main operational boundary; it is triggered when the film draw ratio exceeds 6:1 and melt extension viscosity drops too steeply. The density of 0.912 g/cm³ and the 2.0 g/10 min melt flow index permit stable draw ratios up to 6:1 on conventional single-screw extruders with L/D 30:1; above 6:1, it becomes necessary to increase melt temperature above 250°C or reduce air gap to below 15 mm to remove the instability. Machine-direction ultimate elongation is measured under ASTM D882-18 at 500 mm/min; fully formulated cast stretch film of this resin class typically exhibits elongation at break above 400% in machine direction and tensile strength at break above 25 MPa. Puncture resistance is evaluated with ASTM D5748-95(2019) using a 0.75-inch probe at 23°C; stretch film procurement specifications for A-grade machine film often require slow puncture force above 25 N at 20 µm gauge. Cling force is measured by ASTM D5458-17 for cast film surfaces; with a 0.5–1.5 wt% polyisobutylene tackifier or a 2–4 wt% ultra-low-density polyethylene blended into the skin layer, cling force to a standard test plate at 23°C falls between 0.5 N/cm and 1.5 N/cm after film has been aged 24 h. Line speeds on cast stretch film mono lines are run between 250 and 600 m/min; at speeds above 600 m/min, extruder backpressure can fluctuate more than 5 bar if the melt pump is not isolated from die pressure swings. Neck-in measured at the die exit increases from 2–5% of web width at 4:1 draw ratio to 8–12% at 6:1; deckle rails are set accordingly to preserve edge trim allowance.
| Parameter | Blown Film | Cast Film | Reference Method |
|---|---|---|---|
| Die gap | 1.6–2.0 mm | 0.5–0.8 mm | mechanical setting |
| Melt temperature | 195–220°C | 235–260°C | infrared pyrometer |
| Blow-up ratio | 2.2:1–2.8:1 | not applicable | — |
| Draw ratio | 10:1–15:1 | 4:1–6:1 | line speed / die gap |
| Frost line / chill roll | 3–5 die diameters above die | 18–24°C chill roll | optical surface thermometer |
| Output rate | 150–250 kg/h | 600–1,200 kg/h | gravimetric controller |
| Typical failure mode | bubble instability at BUR >3.0 | draw resonance at draw ratio >6:1 | line observation |
Agricultural silage and greenhouse cover films manufactured from this resin family require a UV stabilizer package that balances hindered amine light stabilizer loading against plate-out on the die lip. HALS 944 or HALS 622 at 0.3–0.6 wt% and a benzotriazole UV absorber at 0.1–0.3 wt% are dry-blended before film extrusion; total stabilizer loading is kept below 1.0 wt% to avoid die-lip plate-out on 8-hour run lengths. Greenhouse films are processed at 100–200 µm gauge on blown-film dies with 2.0–2.5 mm die gaps, 2.5:1–3.0:1 blow-up ratios, and melt temperatures of 200–220°C; silage cover sheet requirements push the same process toward 80–120 µm gauge with a stronger emphasis on puncture propagation resistance. Accelerated weathering is performed under ASTM G154 Cycle 1 using fluorescent UV-B 313 lamps; agricultural film specifications frequently require retention of more than 50% of original elongation after 2,000 h exposure when tested under ISO 527-3. The presence of amine-based antifog additives in greenhouse structures can compete with the HALS radical-scavenging mechanism, so additive compatibility must be verified by sequential Soxhlet extraction and retained tensile elongation testing before full production. Dart impact for 100 µm silage cover is specified above 300 g under ASTM D1709-16A; Elonmdorf tear values above 120 g in machine direction and 150 g in transverse direction under ASTM D1922-15 are used to reduce cover propagation after hail or wind abrasion. Film extrusion at 2.5:1 blow-up ratio produces a more balanced orientation profile than 3.5:1, which is chosen only when transverse stretch during bale wrapping demands higher TD extensibility; the trade-off appears as a measurable reduction in machine-direction tear strength and an increase in gauge banding across the web.
At frozen-food packing operations where fill temperatures drop to −25°C, the coefficient of friction and low-temperature puncture resistance determine whether a 50 µm blown film runs on vertical form-fill-seal equipment without jaw folding or seal-area contamination. Films fabricated from this olefin polymer are reviewed for food-contact compliance under 21 CFR 177.1520(c), which requires that the finished article meet density, melt index, and extractable fraction specifications and remain within applicable conditions of use; parallel European Union compliance is assessed under Regulation (EU) No 10/2011, with overall migration limit of 10 mg/dm² and specific migration limits for authorized monomers and additives. Erucamide slip additive at 500–1,000 ppm and synthetic amorphous silica antiblock at 1,000–3,000 ppm are used in the sealant region; kinetic coefficient of friction is measured after 72 h slip bloom under ASTM D1894-14 and is typically held between 0.10 and 0.25. Low-temperature toughness is qualified by conditioning film at −18°C for 24 h before ASTM D1709-16A dart impact; 50 µm film of this density class commonly delivers 80–150 g dart impact at −18°C, compared with 150–250 g at 23°C. Heat-seal strength is measured with ASTM F88-21 at 40 psi jaw pressure, 0.5 s dwell, and 15 mm specimen width; the seal plateau reaches 8–14 N/15 mm by 130°C, while seal initiation is observed between 85°C and 105°C. Film stored at relative humidity above 85% should be pre-dried at 20–25°C for 4 h before extrusion to prevent hydrolytic surface gel formation from condensation on pellet surfaces.
| Requirement | Standard / Regulation | Parameter | Acceptance Window / Limit |
|---|---|---|---|
| U.S. food contact | 21 CFR 177.1520(c) | olefin polymer specification | density, melt index, extractable fraction as specified |
| EU food contact | Regulation (EU) No 10/2011 | overall migration | <10 mg/dm² |
| REACH SVHC | Regulation (EC) No 1907/2006 | SVHC content per article | <0.1 wt% |
| Dart impact | ASTM D1709-16A | puncture fail mode | 80–150 g at −18°C, 50 µm |
| Coefficient of friction | ASTM D1894-14 | kinetic COF | 0.10–0.25 after 72 h slip bloom |
| Heat seal strength | ASTM F88-21 | seal plateau at 0.5 s dwell | 8–14 N/15 mm at 130°C, 40 psi |
High-speed form-fill-seal laminates demand a heat-seal layer that maintains hot-tack strength before full cooling; the resin is coextruded as a 15–25 µm sealant skin on 80–120 µm pouch backings and tested on vertical or horizontal machines. Hot-tack is evaluated under ASTM F1921-12(2018) using 25.4 mm wide specimens, 0.5 s dwell, 0.3 N/mm² seal pressure, and 200 mm/s separation speed; values of 1.5–3.0 N/25.4 mm are typical for hexene LLDPE sealant webs of this density at 105–125°C. Differential scanning calorimetry under ASTM D3418-17 shows the main melting endotherm between 120°C and 124°C; seal initiation at 85–95°C occurs because surface chains melt before full crystalline collapse, widening the operating window on pouch lines. Adhesive lamination to oriented polypropylene or polyester is performed with a polyurethane adhesive coat weight of 2.5–3.5 g/m²; interlayer adhesion is specified above 3 N/15 mm to prevent tunneling in hot-filled retort simulations. Corona treatment to 38–42 mN/m under ASTM D2578-17 is applied online to the sealant film before lamination; dyne level uniformity must remain within ±2 mN/m across the web to avoid adhesive strikethrough. Gel count is another release criterion for high-speed pouch films; gels larger than 200 µm must be fewer than 10 per m² in cast film, as detected by high-speed optical surface scanning, because a single gel in the seal area can create a leak channel through the pouch. The film’s low seal initiation temperature permits line dwell reduction of 20–50 ms on microprocessor-controlled seal jaws, but jaw temperature setpoint must not exceed 150°C because film thinning at the seal edge can reduce burst strength under ASTM F2054 by more than 25%.
When a coextruded surface protection film is produced for temporary protective masking of laminated panels, the resin functions as a backing or core layer, not as the adhesive skin; the backing must elongate uniformly without splitting while allowing corona treatment and coating. Cast film lines with 0.5 mm die gaps and chill roll temperatures of 18–22°C produce 30–60 µm backing at line speeds of 150–250 m/min; at higher line speeds, web tension must be maintained below 5 N/cm to avoid film stretching and subsequent die-cut misregistration. Secant modulus under ASTM D882-18 at 1% elongation is kept between 120 MPa and 170 MPa; this ensures that the finished protection film can be peeled manually but does not leave adhesive residue. Corona treatment to 38–42 mN/m using an atmospheric corona unit at 1.0–1.5 kW per meter of electrode coverage is applied inline before coating; surface wetting is measured with ASTM D2578-17 dyne solutions and must be uniform within ±2 mN/m across the web. Solvent-free or water-based pressure-sensitive adhesive coating weights of 3–8 g/m² are applied on a separate line; adhesion build to stainless steel under ASTM D3330/D3330M-18 Method A is controlled between 0.5 N/25 mm and 3.0 N/25 mm after 24 h dwell. At 60 µm thickness, the backing contributes tensile strength above 2.5 kN/m and elongation at break above 400%, which reduces the risk of edge tear during machine-assisted panel installation. Low gel content is critical: film gels larger than 150 µm cause visible defects in the protected surface, so melt filter screens of 100–150 µm mesh are installed at the breaker plate on cast film extruders; pressure build-up across the screen pack is monitored and screen changes are scheduled when differential pressure exceeds 35 bar.
Competitive Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips MarFlex® 7120 LLDPE Blown & Cast Film Resin is supplied as pelletized linear low-density polyethylene with a nominal density of 0.918 g/cm³ determined by ASTM D1505 and a nominal melt index of 1.0 g/10 min determined by ASTM D1238 at 190°C/2.16 kg. The grade is positioned as an ethylene-hexene copolymer, placing it in the C6-LLDPE class rather than the butene-based C4-LLDPE class. The nominal values identify the product but do not substitute for the certificate of analysis; lot-specific melt flow rate, density, and additive levels control release. Because the linear backbone lacks the long-chain branching characteristic of high-pressure LDPE, the resin shows higher melt viscosity at equivalent melt index and requires different die-gap and temperature management. For blown film, the practical constraints are die-land shear stress, bubble stability, and frost-line control. For cast film, the limiting defect is often draw resonance, which appears as machine-direction thickness oscillation when draw ratio and melt elasticity become unfavorable. The resin is not hygroscopic, but condensation may occur when cold pellets enter a high-humidity blend area at relative humidity above 60%; if surface moisture appears, drying for 2 h at 80°C removes the water without altering the polymer morphology.
Incoming quality control is usually based on melt flow rate by ASTM D1238, density by ASTM D1505, and visual pellet cleanliness. A melt flow ratio between 190°C/21.6 kg and 190°C/2.16 kg can provide a comparative index of molecular weight distribution, but the value should be used only for lot-consistency monitoring because the test is not a direct measure of film toughness. Capillary rheometry under ASTM D3835 or ISO 11443 is preferred when a converter must quantify shear viscosity before a die-gap change or a new screw design. Oxidative induction time under ASTM D3895 may be used as a screening method for antioxidant package consistency, although it does not predict long-term heat aging performance of the finished film.
At constant density and melt index, the comonomer type changes the distribution of short-chain branches and the probability of forming load-bearing tie molecules during crystallization. A hexene-based LLDPE such as MarFlex® 7120 typically develops higher dart impact strength per ASTM D1709 and higher machine-direction and transverse-direction Elmendorf tear per ASTM D1922 than an equivalent butene-based LLDPE. The benefit is most pronounced in films below 30 µm because impact failure in thin-gauge polyethylene is controlled by the network of tie molecules rather than by bulk yielding. The difference is not unlimited; orientation from blow-up ratio, frost-line height, and die gap can dominate the measured tear and impact balance. Compared with high-pressure LDPE, the linear structure of MarFlex® 7120 has fewer long-chain branches and therefore lower melt strength. In blown film, this translates into a narrower stable bubble window and higher back pressure. In the solidified film, the same structural difference generally provides higher tensile strength at break and greater puncture resistance per ASTM D5748 when compared with LDPE of similar density and melt index.
Metallocene LLDPE grades are a further comparison class. They often provide higher dart impact per ASTM D1709 and lower haze per ASTM D1003 than conventional Ziegler-Natta C6-LLDPE, but their narrower molecular weight distribution may reduce shear-thinning and increase die pressure. MarFlex® 7120 is not a metallocene resin; its behavior is consistent with a broader molecular weight distribution that supports processability on conventional single-screw blown and cast film lines. The choice between a conventional C6-LLDPE and a metallocene LLDPE should be based on the full structure, because a coextruded film with metallocene skin layers can mask the optical penalty of a conventional core while preserving processing stability.
On single-screw extruders with L/D ratios of 24:1 to 30:1, MarFlex® 7120 is typically processed with barrel temperatures from 170°C in the feed zone to 215°C–230°C at the adapter and die. The die gap for LLDPE is generally set between 1.5 mm and 2.5 mm. If the die gap is reduced below 1.0 mm or melt temperature falls below 185°C, the shear stress in the die land may exceed the critical level for this polymer and generate sharkskin melt fracture. Sharkskin appears as a periodic surface roughness perpendicular to the extrusion direction and may increase haze per ASTM D1003 and reduce printability. The critical shear rate is not a single material constant; it depends on die inlet geometry, die-metal surface roughness, die exit angle, and melt temperature. Capillary rheometry under ASTM D3835 or ISO 11443 should be performed at 190°C, 210°C, and 230°C to map the shear-thinning response before processing-window trials. If sharkskin persists, the recommended sequence is to widen the die gap, raise melt temperature in 5°C increments, reduce output, or add a fluoropolymer process aid at 200–600 ppm. Excessive process aid can produce a low-gloss film surface and should not be used to compensate for an improperly sized die gap.
Bubble stability is controlled by frost-line height, blow-up ratio, and ambient air flow. A fractional-melt LLDPE such as this grade usually begins with a blow-up ratio of 2.2:1 to 3.0:1 and a frost-line height of 5 to 8 die diameters. Below 2.0:1, transverse orientation may not balance machine-direction tear; above 3.5:1, bubble movement increases in high-draft environments. These values are starting points, not product-specific release limits. A converter moving from a 2.0 g/10 min cast-film LLDPE to MarFlex® 7120 should expect higher die pressure and should verify that the extruder thrust-bearing load and screen-pack pressure drop remain within the equipment manufacturer’s limits.
Cast film extrusion uses a flat die and chill-roll cooling instead of an internal bubble. For MarFlex® 7120, cast film trials often begin with melt temperatures from 210°C to 260°C, a die gap of 0.5 mm to 1.0 mm, and a die-to-chill-roll gap below 25 mm. The chill roll is held at 15°C to 30°C. The main instability is draw resonance, which appears as a sinusoidal gauge variation along the machine direction and is amplified by high draw ratio, low melt temperature, or a long air gap. Draw resonance initiates when melt elasticity couples with the draw ratio; published data for this specific resin configuration is limited, so the onset should be determined on the production line using a high-speed thickness scanner. Reducing the die-to-chill-roll gap, increasing melt temperature, or increasing the film basis weight can reduce the severity. Vacuum boxes and air knives are used to pin the film edges and reduce neck-in but do not eliminate the fundamental instability. In cast stretch film between 12 µm and 25 µm, power pre-stretch ratios of 150% to 300% are common; failure at high pre-stretch is often initiated by transverse-direction tear, and ASTM D5458 or ASTM D1922 is used to rank film performance.
Mono-layer and coextruded food packaging films may use the resin as a sealant or core layer. Seal initiation temperature and hot-tack performance are not resin-only properties; they must be measured on the final film under ASTM F2029 or equivalent heat-seal profile methods. Frozen food films at thicknesses below 50 µm require low-temperature impact testing; conditioned dart impact at -10°C per ASTM D1709 is a screening method for brittle failure due to orientation and crystallinity. Industrial liners and heavy-duty sacks at 75 µm to 150 µm are evaluated by slow puncture per ASTM D5748 and Elmendorf tear per ASTM D1922. For incipient gel detection, an optical scanner or camera-based gel counter is used on the production line because laboratory pellet inspection does not always detect dispersion defects.
Film property data should be generated after a stable extrusion condition is established, because orientation and thickness variation dominate mechanical performance. Tensile properties are measured under ASTM D882 or ISO 527-3 at a fixed extension rate of 500 mm/min; the reported values depend on whether the specimen is taken in the machine or transverse direction. Dart impact per ASTM D1709 is influenced by sample gauge uniformity and test temperature; a film with a thickness variation of ±5% can show a wider impact distribution than a uniform film of the same average thickness. Puncture resistance per ASTM D5748 requires a lubricated probe and a consistent clamping force to avoid edge artefacts. Haze per ASTM D1003 and gloss per ASTM D2457 are optical tests that are sensitive to die-line roughness, chill-roll texture, and anti-block addition. The converter should maintain a film property database that records extruder output, melt temperature, die gap, chill-roll temperature, and take-off speed, because these variables can shift the measured values more than a lot change in the resin.
The resin supplier may provide food-contact statements under FDA 21 CFR 177.1520 and European Union regulations, but the final film must be evaluated in the finished state. The following matrix identifies the standards framework that converters use to assemble compliance documentation.
| Standard or regulation | Relevant test or clause | Verification point |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymers | Confirm the polyethylene meets the specified density, melt index, and condition-of-use requirements for the intended food type. |
| EU Regulation (EU) No 10/2011 on plastic materials intended for food contact | EN 1186 migration testing; EN 13130 specific migration | Overall migration 10 mg/dm² of food contact surface; specific migration limits for authorized monomers and additives must be met in the final film. |
| REACH EC 1907/2006 | SVHC list and Annex XVII restrictions | Verify supplier statement for SVHC concentration below 0.1% w/w per article; assess restricted substances for the intended market. |
| RoHS 2011/65/EU | IEC 62321 screening | Applicable only to electrical and electronic equipment packaging; cadmium limit 0.01% w/w; other restricted substances 0.1% w/w. |
| ASTM D1238 / ISO 1133-1 | Melt mass-flow rate at 190°C/2.16 kg | Incoming resin quality control and lot consistency; compare against the certificate of analysis. |
Absence of a specific migration limit in a regulation does not imply that a substance is unbounded; migration must remain below the overall limit and toxicological restrictions. Food simulant selection under Regulation (EU) No 10/2011 is based on food type and contact time, and the final film must be tested at the actual thickness and with the actual food-contact layer. The resin is not sterilizable by steam autoclave at 121°C without validation, because polyethylene film may lose orientation and shrink. Sustained exposure to strong oxidizing acids, direct ultraviolet radiation, or blends containing unneutralized acid catalysts should be avoided unless the final application is explicitly validated. These limitations are common to polyolefin film and do not imply a product-specific failure; each end-use must be confirmed with the supplier’s current technical data sheet.