| HS Code | 637482 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 1.0 g/10 min |
| Tensile Strength At Yield | 11.0 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 276 MPa |
| Vicat Softening Point | 95°C |
| Melting Point | 122°C |
| Brittleness Temperature | < -70°C |
| Hardness Shore D | 50 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g/mil |
| Elmendorf Tear Strength Td | 400 g/mil |
| Film Haze | 12% |
| Film Gloss 45 | 55% |
As an accredited Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips MarFlex® 7114 LLDPE is supplied in 25 kg bags, palletized and stretch-wrapped, with bulk truck and railcar options. |
| Container Loading (20′ FCL) | Chevron Phillips MarFlex® 7114 LLDPE in a 20′ FCL: 25 kg bags, palletized, shrink-wrapped, ~20 MT net, dry container, secured. |
| Shipping | Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE is shipped as a non-hazardous solid resin in 25-kg bags, bulk bags, or bulk trucks/railcars. It is not regulated for DOT, IMDG, or IATA transport. Keep dry; avoid heat, sparks, and open flames. Store in a cool, dry, well-ventilated area. Use standard freight. |
| Storage | Store Chevron Phillips MarFlex® 7114 LLDPE at ambient temperature in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers or bags closed to prevent moisture and contamination. Avoid excessive stacking and protect from physical damage. Maintain good housekeeping; do not store near strong oxidizers. Follow local regulations and SDS recommendations. |
| Shelf Life | Stable indefinitely under recommended storage: cool, dry, sealed, away from sunlight, heat, ignition sources, and contaminants. |
On three-layer blown film lines with internal bubble cooling and annular die diameters between 250 mm and 450 mm, MarFlex 7114 is typically allocated to the core and inner plies of heavy-duty industrial liners and flexible intermediate bulk container liners. The grade’s narrow short-chain branching distribution permits a die gap reduction from 2.2 mm to 1.8 mm without raising melt pressure across a 30:1 L/D grooved-feed extruder beyond 28–35 MPa if barrel temperatures are maintained between 190°C and 220°C. Incoming resin is characterized for melt mass-flow rate according to ISO 1133-1:2022 at 190°C and 2.16 kg; deviations greater than 0.2 g/10 min from the supplier lot average can shift bubble stability. At blow-up ratios from 2.0:1 to 2.8:1, frost line heights between 600 mm and 900 mm stabilize the bubble against breath-induced oscillation in high-speed winding. Film samples at 25 µm nominal gauge produced under these conditions are characterized for dart impact according to ASTM D1709 Method A. The method uses a 38 mm diameter tup and a 0.66 m drop height, and the failure mode should be recorded as ductile rather than brittle because brittle failures indicate insufficient melt homogenization or excessive gel content. Elmendorf tear values measured in machine direction and transverse direction follow ASTM D1922. The expected MD/TD imbalance is between 1.2:1 and 1.8:1 depending on frost line height. Pre-drying is not mandatory below 60% relative humidity, but resin stored outdoors below 0°C and transferred into a warm production hall forms surface condensation. Conditioning in a silo for 24 h at 20–30°C eliminates moisture-induced flow instabilities. The primary processing boundary on these lines is not melt pressure but the onset of melt fracture at the die lip when output exceeds 0.8 kg/h per mm of die circumference. Reducing die lip temperature by 5–10°C or raising the lower die lip angle by 5° can delay sharkskin without altering film gauge.
Cast film extrusion subjects the melt to a short air gap and rapid quench on a chill roll. For a high-draw-down stretch film configuration, the flat die lip gap is typically set between 0.5 mm and 1.0 mm, and the distance from die exit to the first chill roll is held between 150 mm and 250 mm. Under these conditions, MarFlex 7114 can be drawn to final thicknesses of 12–20 µm without film breakup when the chill roll temperature is maintained at 20–30°C and the primary nip roll pressure does not exceed 0.4 MPa. The resin exhibits lower melt strength than a branched LDPE, so draw resonance may appear at draw ratios above 25:1 unless the melt curtain is stabilized by an air knife or vacuum box positioned 30–50 mm below the die exit. For machine wrap film, tackifier concentrates based on polyisobutylene or hydrogenated hydrocarbon resins are introduced at 0.5–2.0 wt%. Addition above 2.0 wt% increases unwind force without proportional cling gain, as measured by internal cling methods derived from ASTM D4649 peel test geometry. The mechanical performance of the drawn film is evaluated according to ASTM D882 tensile test Method A with a 500 mm/min crosshead speed. Machine-direction elongation at break normally exceeds 300% for films below 15 µm, but the value is highly sensitive to the primary draw ratio and edge-trim recycling rate. In cast film lines equipped with a trim-in-feed system, edge trim reintroduction should not exceed 15 wt% of total throughput because higher recycle fractions broaden residence time distribution and generate oxidized gel specks that reduce optical clarity and stretch uniformity. Melt temperature at the die must remain below 260°C to prevent thermal degradation at the edges of the coat-hanger manifold, where shear is highest and residence time longest.
Seal initiation temperature, rather than melt index, governs the use of MarFlex 7114 in frozen-food packaging sealant webs. In a three-layer coextrusion with a 10–20 µm sealant layer, the resin is coextruded between a barrier tie layer and a low-SIT outer layer. The die temperature profile is held flat between 210°C and 230°C to minimize layer-to-layer viscosity disparity. Heat-seal strength is tested according to ASTM F88/F88M with a 25.4 mm specimen width, 0.5 s dwell time, 0.28 MPa jaw pressure, and 140°C upper jaw temperature. Published data for this specific grade in frozen-food sealant constructions is limited. However, metallocene-catalyzed LLDPE sealants generally maintain a seal initiation window of 85–105°C and develop plateau seal strengths above 12 N/25.4 mm when the sealant layer is sufficiently thick and the hot-melt is not diluted by the core layer. Hot tack is evaluated according to ASTM F1921 Method J. Hot-tack values above 4 N/25.4 mm at 0.2 s dwell and 0.5 s cooling are typical for blown films under 50 µm, but these values depend on the amount of slip and antiblock additives. The addition of 5–10 wt% LDPE lowers seal initiation by approximately 3–5°C and broadens the seal window, but it decreases dart impact according to ASTM D1709. A critical operating boundary is the presence of high-slip erucamide at concentrations above 800 ppm, which blooms to the seal surface and can reduce seal strength by more than 15% after 7 days of aging at 40°C.
Agricultural silage covers and bale stretch films are subjected to slow puncture from fibrous stalk ends rather than high-speed impact alone. The relevant test is ASTM D5748 or ISO 7765-1 for puncture propagation. In a 150 µm blown coextrusion, placing MarFlex 7114 in the core layer and a lower-melt-strength LDPE in the skin layers improves transverse direction tear resistance, but the resulting machine-direction Elmendorf tear according to ASTM D1922 may fall below 20 g/µm at high blow-up ratios. Field data from commercial balers indicate that failure is rarely a clean tensile yield but a slow splitting from puncture sites at the folded bale edge. Therefore, puncture energy per unit thickness is a more reliable specification than nominal elongation at break. The die gap should be maintained at 2.0–2.4 mm, and the blow-up ratio should not exceed 2.5:1 when the film contains 10 wt% recycled edge trim, because higher blow-up ratios amplify bubble instability and create gauge bands that concentrate stress at the silage surface. The following test matrix is used to release film for agricultural service.
| Test | Standard designation | Specimen condition / measured quantity |
|---|---|---|
| Dart impact | ASTM D1709 | Method A; 38 mm tup; ductile/brittle ratio |
| Slow puncture propagation | ASTM D5748 | 250 mm diameter clamp; puncture energy per mm |
| Elmendorf tear | ASTM D1922 | MD/TD; pendulum tester; values reported in g/µm |
| Tensile properties | ASTM D882 | 500 mm/min crosshead; 50 mm gauge length |
| Secant modulus | ASTM D882 | 1% secant in MD and TD |
On vertical and horizontal form-fill-seal lines running above 80 cycles/min, the seal jaw contact time is commonly 20–40 ms. Film temperature at the interface must therefore reach the softening point before jaw pressure is released. MarFlex 7114 can be used as the sealant layer in a 60–80 µm lamination when the sealant layer is formulated with a low-SIT heat-seal additive, but the concentration must be verified by differential scanning calorimetry on the compounded pellet before extrusion. The upper seal temperature is limited by film distortion at the jaw edge. When jaw temperature exceeds 150°C, the sealant layer thins and fails cohesively. Heat-seal strength is measured after 24 h conditioning at 23°C and 50% relative humidity according to ASTM F88/F88M. Hot-tack force is measured according to ASTM F1921 at 0.2 s dwell and 0.1 s cooling. The use of polytetrafluoroethylene-coated seal jaws is required to prevent polymer buildup on heater surfaces. Production-scale troubleshooting on rotary FFS machines shows that seal failure at the back seal is often not a resin defect but an effect of film slip variability. Kinetic coefficient of friction should be monitored according to ASTM D1894 and held between 0.10 and 0.30 on the outer layer to maintain consistent film tracking through the forming collar. Slip additive levels above 1,000 ppm reduce hot-tack by blooming to the seal surface, and antiblock loadings above 3,000 ppm create surface roughness that can entrap air during the sealing dwell.
Extrusion lamination of oriented polyester to an LLDPE-based sealant web uses MarFlex 7114 in the melt curtain between the primed PET and the coextruded sealant film. The laminator die gap is set at 0.5 mm, and the air gap between die exit and nip is limited to 100–150 mm to minimize neck-in and maintain a melt thickness of 12–20 µm. Adhesion to the oriented polyester surface requires an in-line corona treatment at 42–46 mN/m, measured according to ASTM D2578 wetting tension. Peel adhesion is evaluated after 24 h conditioning at 23°C/50% RH using ASTM D1876 T-peel geometry at a crosshead speed of 127 mm/min. Destructive peel values below 2 N/15 mm typically indicate insufficient surface oxidation of the polyester, while cohesive failure within the LLDPE indicates that the melt curtain was over-oxidized by excessive air gap residence time. Laminates for medical device packaging are subject to seal integrity testing after ethylene oxide sterilization. Seal strength according to ASTM F88/F88M after conditioning at 50°C and 90% RH for 24 h should not decrease by more than 20% relative to values obtained at 23°C/50% RH. The practical boundary in this conversion is not the resin’s flow rate but the adhesion drop observed when the melt temperature falls below 270°C in the curtain. Low-temperature extrusion produces poor wet-out on the primed film and lowers peel values disproportionately to the reduction in melt temperature.
Competitive Chevron Phillips MarFlex® 7114 Polyethylene; LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Chemical MarFlex® 7114 is a linear low density polyethylene (LLDPE) film resin produced in the MarFlex loop-slurry reactor system. The product is supplied as dense pellets, typically 3 mm to 4 mm in diameter, with an antioxidant stabilization package. Current grade literature identifies a nominal density of 0.918 g/cm³ determined by ASTM D1505 and a nominal melt index of 1.0 g/10 min determined at 190 °C under a 2.16 kg load per ASTM D1238 or ISO 1133-1:2022. These values are centerline targets rather than guaranteed limits; lot-specific variation is defined by the manufacturer’s Certificate of Analysis. The grade is used in blown and cast film applications requiring higher dart impact and tear resistance than general-purpose butene copolymer LLDPE of identical density and melt index. Compared with high-pressure LDPE, MarFlex 7114 has a lower concentration of long-chain branching and lower strain-hardening melt strength; bubble stability therefore depends more strongly on die gap, air-ring velocity, and frost-line position than on extensional thickening. Compared with metallocene LLDPE of the same density, a conventional loop-slurry LLDPE may exhibit broader molecular weight distribution and wider processing latitude, but optical performance and heat-seal response must be validated on the intended coextrusion structure.
MarFlex 7114 also differs from metallocene LLDPE in molecular weight distribution and from broad-specification butene LLDPE in short-chain branching distribution. In a coextruded structure, the choice of this grade is often a response to a specific property deficit: high machine-direction tear, dart impact, or downgauging capacity. In high-toughness applications, the resin may be placed in the core layer while a lower-MI metallocene or LDPE skin provides heat-seal and optical performance. For abuse-fill applications requiring high dart impact, the opposite arrangement may be selected. These substitutions must be tested by the converter; no universal ranking can be derived from density and melt index alone.
Melt temperature and die gap are coupled variables in blown-film conversion of MarFlex 7114. A die gap between 1.2 mm and 2.5 mm is typical for monolayer and coextruded film lines. Gaps below 1.0 mm increase die-lip shear stress and may initiate sharkskin at moderate screw speeds; gaps above 2.5 mm reduce transverse-direction orientation and may destabilize the bubble when the blow-up ratio exceeds 2.5:1. Melt temperature measured at the die adaptor is normally held between 199 °C and 227 °C. Residence time at temperatures above 240 °C should be limited to less than 5 minutes; prolonged high-temperature hold times promote oxidative chain scission, long-chain branching, and gel particles that appear as defects in film thinner than 25 µm. Although the polymer is not hygroscopic, condensation on cold pellets transferred directly into a heated feed throat can produce steam pockets and irregular solids conveying.
Production-scale behavior on a 90 mm grooved-feed extruder with L/D 30:1 and a 250 mm die shows that start-up shear stress is often highest before the air ring reaches thermal equilibrium. Die-lip melt fracture and gauge bands may appear if screw speed is increased before frost-line height stabilizes. Heater-band failure or thermocouple drift above 250 °C can generate black specks and hole formation during stretching. These failure modes are common to this viscosity band of LLDPE and should be monitored by recording melt pressure, melt temperature, and frost-line position hourly. A frost-line height between 2 and 8 die diameters is typical. A frost line below 2 die diameters can quench the film too rapidly and reduce dart impact; a frost line above 8 die diameters can contribute to bubble wander and gauge variation. Air-ring cooling should be adjusted before changing die gap, because the bubble’s cooling rate and crystallinity profile control the final tear balance.
Regulatory conformance for MarFlex 7114 is governed by the finished article rather than by generic polymer approval. The resin may be used in food-contact applications if the final film meets the olefin polymer specifications of 21 CFR 177.1520 and the extractive limitations associated with the intended food type and use temperature. Masterbatch components, adhesives, and surface modifiers must be assessed separately, because they can become the controlling regulatory variable. For European food contact, compliance is evaluated under Regulation (EU) No 10/2011 as amended; converters should obtain the supplier’s Declaration of Compliance for the specific lot. RoHS substance restrictions under Directive 2011/65/EU are not typically the limiting constraint for unfilled polyethylene, but all added colorants and processing aids must be assessed. Storage should be in a clean, dry area below 40 °C and away from direct ultraviolet exposure; unstabilized outdoor storage can lead to surface oxidation and yellowing of pellets and finished film.
| Standard or Regulation | Scope | Condition or Method |
|---|---|---|
| ASTM D1505 | Plastics density by gradient technique | 23 °C |
| ASTM D1238 / ISO 1133-1:2022 | Melt mass-flow rate | 190 °C, 2.16 kg |
| ASTM D4976 | Polyethylene extrusion materials classification | Grade call-out on Certificate of Analysis |
| FDA 21 CFR 177.1520(c) | Olefin polymers for food contact | Finished-article migration testing |
| Regulation (EU) No 10/2011 | Plastic food-contact materials | Declaration of Compliance |
In 38 µm monolayer blown film, MarFlex 7114 is evaluated by ASTM D1709 for dart drop impact, ASTM D1922 for Elmendorf tear, and ASTM D882 for tensile properties. The tear balance is not isotropic. Machine-direction tear and transverse-direction tear respond in opposite directions to changes in blow-up ratio and frost-line height. A blow-up ratio between 2.0:1 and 2.5:1 is often used to generate balanced orientation; above 3.0:1, transverse-direction tear may improve while machine-direction tear decreases. Dart impact values measured at 38 µm should not be extrapolated from 50 µm data, because the thickness–impact relationship for LLDPE is nonlinear. Processors replacing a general-purpose butene LLDPE of identical density and melt index should not assume identical machine settings will yield equivalent toughness. Differences in short-chain branching distribution can shift the ductile-to-brittle transition temperature and change puncture failure mode from brittle cracking to ductile stretching. Published data for this specific configuration is limited when the film is downgauged below 25 µm; converter trials are required to establish the minimum gauge for a given packaging line.
Optical properties of MarFlex 7114 are controlled by cooling rate, die-line design, and the antiblock package. Additive-free films of 25 µm can show haze values below 5%, but the addition of diatomaceous silica antiblock increases surface roughness and haze. Gloss measured at 45° under ASTM D2457 is commonly reported between 60 and 80 for this density range, but the value is not a lot specification. Rapid quenching lowers haze by reducing spherulite size but may reduce dart impact by altering the crystalline network. Converters targeting low-haze packages must validate the optical and mechanical trade-off on the intended line.
A single-point melt index of 1.0 g/10 min is not a complete rheological specification. Converters running high-shear processes should request the high-load melt index at 21.6 kg and calculate the melt flow ratio. For many loop-slurry LLDPE grades, the melt flow ratio falls between 25 and 35, but the public grade datasheet may not list this value. A single-point melt index cannot detect lot-to-lot differences in molecular weight distribution that affect elongational viscosity, bubble stability, or hot-tack performance. Capillary rheometry at 190 °C using a 20:1 length-to-diameter die provides a more useful shear-viscosity curve for die pressure and melt fracture calculations. The power-law index for an LLDPE of this density is typically near 0.6 to 0.7 across shear rates from 100 s⁻¹ to 1,000 s⁻¹. Processors should use the actual shear-viscosity curve from the lot certificate rather than inferring shear-thinning behavior from melt index alone.
The extensional viscosity requirements of high-draw cast film and stretch-film lines differ from those in blown film. On cast film lines with draw ratios above 6:1 and chill-roll temperatures below 25 °C, the lower long-chain branching of LLDPE relative to LDPE can reduce neck-in and improve drawdown. Winding tension must be controlled to avoid blocking, because polyethylene film surfaces are not inherently tacky but the coefficient of friction depends on the slip and antiblock package. A slip agent, typically erucamide or oleamide, and a diatomaceous silica antiblock are used to control handling behavior. The processor must verify the additive concentrations before setting roll pressures, because excessive slip-agent migration to the film surface can reduce lamination bond strength. Migration kinetics in the polymer matrix are temperature-dependent; storage of finished film above 35 °C can accelerate additive bloom. Combination with certain amine-based processing stabilizers is not recommended unless specifically validated, because secondary amine structures can interact with phenolic antioxidants and reduce long-term thermal stability. Published data for specific high-draw equipment configurations is limited beyond supplier processing guidelines.
Storage stability of MarFlex 7114 is controlled primarily by the antioxidant package and ambient temperature. Supplier guidance indicates that unopened bags and bulk containers should be stored in a clean, dry area below 40 °C. Direct solar exposure for extended periods can produce surface oxidation and yellowing, even in pellet form. If the resin is held in an outdoor silo, silo surface temperatures above 50 °C may accelerate additive loss and increase the risk of gel formation during extrusion. The resin should not be left in a hot hopper overnight unless the throat is cooled and the hopper is sealed against moisture. Cross-contamination with polypropylene, PVC, or PET can cause weld-line incompatibility and film defects; purging with a compatible LLDPE or a commercial purge compound is required when changing from a high-melt-temperature resin.
Heat-seal initiation temperature of films containing MarFlex 7114 is measured by gradient seal tests or by controlled impulse sealers. The heat-seal temperature range is a function of film thickness, layer placement, and heat transfer rate. In a three-layer A/B/A structure with MarFlex 7114 in the seal layer, seal initiation may occur near 95 °C to 105 °C, but the hot-tack window depends on cooling after the seal jaws open and on the molecular weight distribution of the seal-layer resin. Typical laboratory seal conditions of 0.5 s dwell, 0.3 N/mm² jaw pressure, and 100 °C to 120 °C jaw temperature are used for evaluation; these conditions are not universal and must be mapped for the target packaging line. Slip and antiblock additives can bloom to the seal surface and reduce seal strength if additive levels exceed 1,200 ppm. Seal strength is evaluated per ASTM F88/F88M with jaw separation rates of 200 mm/min to 300 mm/min; the selected rate must be reported because LLDPE seal strength is rate-sensitive. Hot-tack strength is measured by ASTM F1921 or an equivalent instrumented method. The interaction between seal-bar coating, film thickness, and seal-layer resin should be validated at production speed.