Chevron Phillips Marflex 7109s Lldpe Blown Film Resin

Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin

    • Product Name: Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 988967
    Meltindex 0.9 g/10 min
    Density 0.918 g/cm³
    Meltflowratio 27
    Meltingpoint 121 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyieldmd 10.3 MPa (1500 psi)
    Tensilestrengthatbreakmd 24.1 MPa (3500 psi)
    Tensilestrengthatbreaktd 20.7 MPa (3000 psi)
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Elmendorftearmd 250 g
    Elmendorfteartd 400 g
    Dartdropimpact 200 g
    Haze 12%
    Gloss 60
    Coefficientoffriction 0.15

    As an accredited Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing MarFlex® 7109S LLDPE resin is supplied in 25 kg (55 lb) polyethylene bags, 40 bags per pallet, and bulk trucks or railcars.
    Container Loading (20′ FCL) 20′ FCL: Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin, 25 kg bags, palletized, shrink-wrapped; approx. 18–20 MT.
    Shipping Chevron Phillips MarFlex 7109S LLDPE Blown Film Resin is typically shipped as free-flowing pellets in 25 kg (55 lb) polyethylene bags on shrink-wrapped pallets, or in bulk trucks/railcars. It is nonhazardous under normal transport. Store in a dry, cool area away from direct sunlight, heat, and moisture; handle pallets carefully.
    Storage Store Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers/packages closed, clean, and off the ground. Protect from moisture, dust, and extreme temperatures. Avoid incompatible oxidizers. Follow first-in, first-out inventory and manufacturer SDS/local regulations. Ensure good housekeeping and minimize dust generation.
    Shelf Life Shelf life: typically 24 months from date of manufacture when stored unopened in original packaging in cool, dry, well-ventilated conditions.
    Application of Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin

    On a mono-layer municipal refuse sack line equipped with a 65 mm 30:1 L/D grooved-feed extruder and a 250 mm spiral mandrel die, MarFlex® 7109S LLDPE blown film resin is processed with a nominal density of 0.918 g/cm³ per ASTM D1505 and a melt index of 1.0 g/10 min per ASTM D1238. The resin is not hygroscopic, so pellet pre-drying is not mandatory below 60% RH; however, surface condensation on railcar pellets stored in humid bulk silos must be removed before extrusion because moisture carryover destabilizes the bubble and increases web gauge variation beyond ±8%. The blend for black kerbside sacks consists of 85 wt% MarFlex 7109S, 10 wt% LDPE having a density of 0.922 g/cm³ and a melt index of 2.0 g/10 min to reduce melt tension loss at high draw, and 5 wt% of a 40 wt% carbon black LLDPE masterbatch for opacity and ultraviolet screening. The downstream extrusion process is run at a die gap of 2.0 mm, blow-up ratio of 2.4:1 to 2.6:1, melt temperature of 205 °C to 225 °C, and frost line height of 450 mm to 550 mm from the die face. Output rates of 120–150 kg/h are stable on this configuration; raising output above 160 kg/h without internal bubble cooling decreases dart impact resistance and creates uneven frost line movement. The terminal product is a black refuse sack in the 30–80 L capacity range with wall thickness between 60 µm and 120 µm. Compliance for the sack is evaluated under EN 13592:2017, and the packaging heavy-metal sum remains below 100 mg/kg under EU Directive 94/62/EC, Article 11 and Annex II. Converter lot records show dart drop values on 80 µm film of 150–250 g using ASTM D1709-16a Method A, and Elmendorf tear of 450–700 mN in the machine direction using ASTM D1922; the lower limit corresponds to BUR above 2.7:1, where bubble instability degrades molecular orientation uniformity.

    What Limits Seal Initiation Temperature in Frozen Food Pillow Pouch Conversion?

    For frozen vegetable and fruit pillow pouches, the dominant conversion risk is not film optics but heat-seal initiation and seal-through at high throughput. In this application the addition ratio is 90 wt% MarFlex 7109S, 7 wt% LDPE of density 0.923 g/cm³ and MI 2.0 g/10 min, and 3 wt% of a slip/antiblock masterbatch with erucamide active content between 0.8 wt% and 1.2 wt% to control coefficient of friction without exceeding migration limits. The food-contact compliance boundary is defined by FDA 21 CFR 177.1520(c)(2.2) for olefin polymers with density below 0.94 g/cm³, and by EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² under Annex I and Article 12. Downstream production uses a mono-layer blown film line with a 300 mm die, 1.8 mm die gap, 2.0:1 BUR, melt temperature 200 °C to 215 °C, and downstream corona treatment to a wetting tension of 38–42 mN/m. Heat-seal initiation is verified by ASTM F88/F88M-21 using a 0.5 s dwell and 0.3 N/mm² seal pressure. A minimum seal strength of 12 N/25 mm at 125 °C is required to avoid leakers in vertical form-fill-seal runs above 60 pouches/min. Raising seal-bar temperature above 150 °C causes localized thinning at the seal transition and reduces burst performance, while running the melt below 195 °C raises die lip pressure and produces visible sharkskin. The terminal product is a 40–70 µm pillow pouch for frozen vegetables. A compliance matrix is given below.

    RegionStandard / RegulationClause / AnnexKey Limit
    United StatesFDA 21 CFR 177.1520(c)(2.2)Olefin polymer for food contact; extractive limits apply
    European UnionEU Regulation (EU) No 10/2011Article 12, Annex IOverall migration ≤ 10 mg/dm²
    People's Republic of ChinaGB 4806.7-2016Clause 4.3Total migration ≤ 10 mg/dm²

    Post-consumer recyclate dilution curves in coextruded mailer structures create a different pressure profile than mono-layer refuse sack lines. The total structure blend is 30 wt% MarFlex 7109S, 50 wt% post-consumer LLDPE lightweight scrap with a melt index between 0.8 g/10 min and 1.2 g/10 min, 15 wt% LDPE of MI 2.0 g/10 min, and 5 wt% carbon black masterbatch. The skins of a three-layer A/B/A die are enriched with virgin MarFlex 7109S, while the core carries the PCR fraction to maintain tear resistance and surface uniformity. Compliance is assessed under the US TPCH Model Legislation for packaging heavy metals, with a combined lead, cadmium, mercury, and hexavalent chromium limit of 100 mg/kg; EU Directive 94/62/EC, Article 11 and Annex II imposes the same sum limit; and REACH Regulation (EC) No 1907/2006, Annex XVII Entry 23 restricts cadmium in plastic to 0.01 wt%. Downstream production is accomplished on a three-layer coextrusion blown film line with a 450 mm die, 2.2 mm die gap, 2.4:1 BUR, melt temperature 215 °C to 235 °C, and an extruder screen pack at 40/60/100 mesh. Screen pack head pressure trends upward from 80 bar to 120 bar as recycled gels accumulate; a continuous melt filter or screen changer is required to avoid pressure spikes above 130 bar, which correlate with localized thin bands and tear initiation in the finished mailer. The terminal product is an opaque black e-commerce mailer film of 50–90 µm, with a dart impact requirement typically set at ≥200 g for 70 µm film under ASTM D1709-16a Method A.

    Melt Curtain Stability Without Internal Bubble Cooling in 15 µm Garment Film

    Garment bag film at 12–20 µm represents a thin-gauge processing boundary where MarFlex 7109S must be extruded with the die gap at 1.5 mm, a blow-up ratio of 3.0:1, and a melt temperature of 215 °C. The formulation addition ratio is 97 wt% MarFlex 7109S and 3 wt% slip/antiblock masterbatch with erucamide active content of 0.8–1.2 wt%. Dynamic coefficient of friction is measured at 0.25–0.35 per ASTM D1894, and blocking force is evaluated with a two-plate compression method to avoid web blocking during roll storage, because thin garment film stored above 35 °C can block if slip additive bloom is incomplete. The production process uses a mono-layer blown film line with a 250 mm die, output of 80–100 kg/h, frost line height 350–400 mm, and no internal bubble cooling. Without internal bubble cooling, melt curtain stability below 15 µm is sensitive to ambient air currents; plant air handlers should maintain laminar flow around the bubble. The terminal product is a garment bag, dry cleaning bag, or thin retail sleeve in the 12–20 µm range. Compliance is limited to general packaging requirements under EU Directive 94/62/EC, Article 11 and Annex II for heavy metals, and REACH Regulation (EC) No 1907/2006, Annex XVII Entry 23 for cadmium at 0.01 wt%. Operational boundary: at melt temperatures above 230 °C, slip additive degradation creates die lip plate-out; at temperatures below 195 °C, sharkskin appears at 12 µm. Ambient RH above 60% can induce surface condensation and bubble instability, but pellet pre-drying is not required.

    When a 150 µm Sub-Slab Vapor Retarder Must Meet ASTM E1745 Class A

    Sub-slab vapor retarder film made from MarFlex 7109S requires a thick-gauge blown film configuration with lower bubble stretching than thin garment film. The formulation addition ratio is 96 wt% MarFlex 7109S and 4 wt% carbon black masterbatch to provide thermal stability during concrete placement and to screen ultraviolet exposure on the job site. Compliance under ASTM E1745-17 Class A requires water vapor permeance not greater than 0.1 perm when tested per ASTM E96/E96M-16, and the 150 µm nominal thickness must be held within ±5% across the web to avoid thin sections that fail the permeance specification. The downstream process uses a heavy-gauge mono-layer blown film line with a 2.5 mm die gap, 2.0:1 BUR, melt temperature 220 °C to 240 °C, output of 140–180 kg/h, and internal bubble cooling. At thickness below 125 µm, pinhole risk increases due to carbon black dispersion defects; at BUR above 2.2:1, water vapor permeance can exceed Class A due to molecular orientation effects. The terminal product is a 150 µm sub-slab vapor retarder sheet laid beneath concrete slabs. The level of carbon black masterbatch must be controlled precisely because over-dispersion raises melt pressure and pre-filtration loading, while under-dispersion creates visible resin-rich streaks that reduce tear resistance under site traffic.

    Anti-static drum and box liners for powder packaging introduce a surface-resistivity constraint that is absent in refuse sacks and garment film. The formulation addition ratio is 88 wt% MarFlex 7109S, 8 wt% LDPE with a melt index of 0.3 g/10 min to raise puncture resistance, and 4 wt% conductive carbon black masterbatch. The conductive carbon black must produce a surface resistivity between 10⁶ Ω/sq and 10⁹ Ω/sq per IEC 60079-32-2 for packaging used in explosive atmosphere zones, while the film retains a thickness of 200–300 µm. Downstream production is run on a heavy-gauge mono-layer blown film line with a 75 mm 30:1 L/D barrier screw and Maddock mixing section to disperse conductive carbon black, a 2.5 mm die gap, 1.8:1 BUR, melt temperature 225 °C to 240 °C, and internal bubble cooling. Screen pack pressure must be monitored because conductive masterbatch can plate out on the die lip and create localized resistivity variation above 10⁹ Ω/sq. Standard carbon black masterbatch does not lower surface resistivity into the target range; only conductive grades are acceptable. The terminal product is a 200–300 µm anti-static liner for drums, boxes, or bulk powder handling containers, with puncture resistance tested by ASTM D5748 or dart impact by ASTM D1709-16a Method A as specified by the end user.

    Free Quote

    Competitive Chevron Phillips MarFlex® 7109S LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Within the linear low density polyethylene blown-film segment, Chevron Phillips MarFlex® 7109S is designated as a 1-hexene copolymer resin with a density of 0.918 g/cm³ under ASTM D1505 and a melt index of 0.9 g/10 min determined at 190°C and 2.16 kg according to ASTM D1238. The S suffix denotes a slip and antiblock additive package, which reduces film-to-film and film-to-metal friction during winding, slitting, and converting. The base resin is a Ziegler-Natta-catalyzed linear low-density polyethylene whose hexene comonomer differentiates it from butene-based LLDPE grades in the same density and melt-index envelope. This distinction is not cosmetic; the longer butyl branches introduced by 1-hexene influence tie-chain probability, crystallite thickness distribution, and the balance between tear resistance and dart impact once the resin is converted into film.

    Because the grade is targeted at blown film, its 0.9 g/10 min melt index positions it between easy-flow film grades and high-melt-strength fractional-melt resins. The result is a compromise between bubble stability at low melt strength and controlled head pressure on conventional single-screw extruders. Typical production equipment for this density and melt-index class includes smooth-bore or grooved-feed extruders with screw diameters from 40 mm to 75 mm, L/D ratios from 24:1 to 30:1, and blown-film dies with die gaps between 1.0 mm and 2.0 mm. Barrel temperature profiles are generally flat to reverse; feed throat cooling is required, with zone setpoints commonly between 160°C and 210°C and die head temperatures maintained near 200–215°C. Blow-up ratios from 2.0:1 to 2.5:1 are typical for balanced orientation, while high-stalk configurations may extend toward 3.0:1 when the line is equipped with adequate bubble stabilization.

    What Processing Envelope Is Required for Stable Bubble and Gauge Control?

    On production-scale blown-film lines, the grade exhibits the characteristic shear viscosity behavior of hexene LLDPE: shear thinning is less pronounced than high-pressure low density polyethylene, and die pressure does not fall as rapidly with increasing screw speed. Compared with a butene LLDPE of equivalent melt index, the hexene resin typically shows higher extensional viscosity and improved bubble stability at moderate blow-up ratios, but die pressure at equivalent output may be 5–15% higher on a 50 mm extruder with an L/D of 30:1. Operators frequently reduce die gap toward the lower end of the range when internal bubble cooling is not available because wider gaps increase shear heating and can reduce melt strength at the die exit. Gauge variation is minimized by holding frost line height constant and avoiding abrupt changes in cooling-air volume. Melt temperature fluctuations above ±2°C contribute to thickness bands detected by online capacitance gauges, especially at film gauges below 25 µm.

    Film properties are strongly dependent on cooling rate. A higher frost line or lower cooling-air temperature increases crystalline orientation and can raise tensile modulus while reducing clarity. A lower frost line generally improves haze and gloss but may reduce dart impact retention. For blown film, the relevant test methods include ASTM D882 for tensile properties, ASTM D1709 Method A or B for dart drop impact, ASTM D1922 for Elmendorf tear, ASTM D1003 for haze, and ASTM D2457 for gloss. Published lot-to-lot film data for this grade are typically generated on a 50–60 mm extruder at a 2.0:1 blow-up ratio and 25 µm film gauge; deviations in die gap, stalk height, or cooling configuration shift the test results and should not be interpreted as specification limits.

    In food-contact compliance evaluations, the grade falls under the olefin polymer provisions of FDA 21 CFR 177.1520, subject to extractables limitations and end-use temperature restrictions specified in the regulation. European Union food-contact use is evaluated under EU Regulation 10/2011, with overall migration and specific migration limits applicable to polyethylene. REACH and RoHS conformity is documented through supplier declarations, and the resin does not contain intentionally added per- and polyfluoroalkyl substances or phthalate plasticizers. For pharmaceutical or high-purity applications, additional notification or testing may be required because the slip and antiblock additives are not necessarily covered by all food-contact clearances in the same manner as the base polyethylene.

    Regulatory AreaStandard or RegulationApplicable Condition
    United States food contactFDA 21 CFR 177.1520Olefin polymers; end-use temperature and food-type limitations apply
    European Union food contactEU Regulation 10/2011Overall and specific migration limits for polyethylene
    Chemical registrationREACHSubstance and article obligations as applicable
    Hazardous substance restrictionRoHS Directive 2011/65/EUNo intentionally added restricted substances

    How Does Hexene Comonomer Distribution Affect Tear, Impact, and Seal Performance?

    Relative to butene LLDPE at equivalent density and melt index, the hexene comonomer introduces butyl short-chain branches rather than ethyl branches. At equal density, the longer branch length disrupts crystal packing more effectively, producing a broader interlamellar amorphous layer and a higher tie-chain probability. This architectural shift is reflected in improved dart impact and tear resistance without the density reduction that would otherwise be required in a butene-based grade. Transverse direction Elmendorf tear, measured under ASTM D1922, is often the most sensitive indicator of comonomer type because it responds to both orientation and tie-chain continuity. The resulting film is more tolerant of gauge variation in heavy-duty packaging applications, although the improvement in toughness does not automatically translate to higher stiffness.

    Compared with high-pressure low density polyethylene at equivalent melt index, the grade has lower melt strength and less pronounced strain hardening. This limits drawdown in high-stalk bubble configurations and reduces bubble stability at high blow-up ratios unless the line is equipped with internal bubble cooling or a dual-lip air ring. Blending with 10–20 wt% high-pressure LDPE is common to increase melt strength and improve bubble stability while retaining most of the toughness advantage. The blend approach also reduces die-lip buildup at high extrusion rates. However, addition of LDPE raises seal initiation temperature and can reduce dart impact, so the blend ratio becomes a processing-versus-performance tradeoff.

    Seal performance follows the standard LLDPE trend: the lower density relative to high-pressure LDPE reduces seal initiation temperature, but the hexene branch distribution also influences hot tack strength and seal strength as characterized by ASTM F88 and ASTM F1921. The slip package in the S designation migrates to the film surface and can alter heat-seal behavior if excessive levels accumulate on the sealant layer. For critical seal applications, seal strength should be verified on the final film structure rather than inferred from resin density alone, because surface additives and coextruded layers change the interfacial failure mode.

    When Internal Bubble Cooling and High-Stalk Bubbles Are Used on Converting Lines

    Internal bubble cooling changes the quenching rate and shifts the frost line upward, altering crystalline orientation and film haze. On lines equipped with internal bubble cooling, the grade can be processed at output rates 15–25% higher than on external-air-only configurations because the additional heat removal stabilizes the bubble and allows higher extrusion rates without severe gauge fluctuation. The limitation is that the internal cooling air must be filtered to 10 µm or finer to prevent surface defects, and the exhaust air temperature should remain below 50°C to avoid condensation on the bubble surface. These constraints derive from general film-line engineering practice rather than grade-specific published data, but they are relevant to the grade because surface defects can be amplified by the antiblock particles and slip additive distribution.

    On a high-speed converting line, the slip and antiblock package is intended to reduce coefficient of friction and prevent blocking during roll storage. Coefficient of friction against steel or film is typically evaluated using ASTM D1894. Antiblock particle size and distribution affect clarity; excessive antiblock levels raise haze and reduce gloss measured by ASTM D2457. The S-grade is therefore more suitable for form-fill-seal packaging and premade bags requiring consistent frictional behavior than a barefoot grade without surface additives. Film-to-film blocking tendency is assessed by room-temperature block tests under pressure; the slip package is most effective after migration to the surface, which may require 24–48 h after extrusion. Winding tension should be tapered to avoid blocking in the inner layers of large-diameter rolls.

    Differential Scanning Calorimetry and Crystallization Kinetics

    Differential scanning calorimetry of the resin under ASTM D3418 typically reveals a broad melting endotherm with a peak near 122°C and a crystallization exotherm near 105–108°C for this density class. The breadth of the melting peak reflects the heterogeneous short-chain branch distribution produced by Ziegler-Natta catalysis. The lower crystallization rate relative to high density polyethylene allows more time for lamellar development during bubble cooling; this is one reason frost line height and cooling-air temperature are critical for film optics. In laboratory film tests, haze values are frequently reported in the 10–14% range at 25 µm thickness under ASTM D1003, but published lot-to-lot variability may be wider, and film fabricated on a high-shear line can exhibit higher haze if the melt temperature exceeds the recommended range.

    In heavy-duty shipping sacks and industrial liners, the grade is selected for the combination of puncture resistance and tear propagation resistance. Puncture energy measured by ASTM D5748 or slow puncture tests is generally higher for hexene LLDPE than for butene LLDPE at the same film gauge, allowing a gauge reduction of approximately 10–15% while retaining equivalent field performance; this is a common design basis in flexible packaging. However, gauge reduction requires verification of seal strength and stiffness because secant modulus under ASTM D882 decreases with lower density and may not meet machine handling requirements on vertical form-fill-seal equipment. The lower stiffness can also cause film tracking instability on high-speed bag machines unless tension and guide alignment are adjusted.

    Regrind incorporation up to 20 wt% is generally tolerated if the regrind is dry, contaminant-free, and produced from the same film structure. Inclusion of polypropylene or polyamide contamination at levels above 1–2 wt% can cause gel-like defects, poor optical appearance, and reduced tear strength because of phase incompatibility. For critical film applications, melt filtration with screens of 80–120 mesh is recommended to remove charred particles and crosslinked gels. Pre-drying is not normally required for LLDPE because moisture absorption is low; however, in humid environments above 60% RH, surface moisture on pellets can create steam-induced defects, and a drying step at 60–70°C for 2–4 h may be applied to hopper-fed systems. Additive interactions with acid-neutralizing agents or release modifiers should be evaluated when the film is used in direct contact with aggressive agricultural chemicals or fatty foods.

    For film structures requiring low seal initiation and high hot tack, coextrusion with a lower-density sealant layer or metallocene LLDPE is often considered. The grade can serve as the core or outer layer in three-layer films; its hexene comonomer improves interlayer adhesion relative to butene LLDPE when processed with ethylene-vinyl acetate or adhesive tie layers. However, specific adhesion values depend on coextrusion die design, layer ratio, and melt temperature at the interface. Published data for this specific configuration is limited, and end users should verify the final laminate using ASTM F904 or ASTM D1876 for heat-seal strength and peel adhesion respectively.

    Top