| HS Code | 173244 |
| Melt Index | 1.0 g/10 min |
| Density | 0.918 g/cm³ |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 1500 psi |
| Tensile Strength At Break | 4000 psi |
| Elongation At Break | 700 % |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 7 % |
| Gloss | 70 % |
| Coefficient Of Friction | 0.2 |
As an accredited Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | MarFlex® 7109L is supplied in 25 kg (55 lb) bags, 40 bags per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | Container loading (20′ FCL) for Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin: palletized 25 kg bags, stretch-wrapped and secured. |
| Shipping | Chevron Phillips MarFlex 7109L LLDPE Blown Film Resin ships as non-hazardous polyethylene pellets, typically in 25 kg bags, bulk bags, or bulk trucks/railcars. Packages are palletized, stretch-wrapped, and transported in clean, dry containers at ambient temperature. Avoid moisture, sunlight, and contamination. Not DOT/IMDG regulated. |
| Storage | Store Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and open flames. Keep bags or containers tightly closed and palletized off the floor to prevent moisture pickup and contamination. Avoid excessive stacking, rough handling, incompatible materials. Use FIFO rotation and maintain normal ambient temperatures. Protect from physical damage. |
| Shelf Life | Typically 12 months from date of manufacture when stored unopened in a cool, dry, well-ventilated area away from direct sunlight. |
Blown film lines configured for heavy-duty open-mouth shipping sacks typically process MarFlex® 7109L at a melt temperature of 195–220 °C through a grooved-feed extruder with a 30:1 L/D barrier screw and a spiral mandrel die having a 1.6–2.0 mm die gap. The bubble is formed at a blow-up ratio of 2.2:1–2.8:1, with frostline height held between 7 and 9 die diameters; dual-lip air-ring airflow is set to maintain the frostline near the upper bound when gauge exceeds 180 µm. At 100% virgin operation, bubble stability is maintained on 300–400 mm annular dies at output rates of 1.2–1.8 kg/h per millimetre of die circumference. If the line pushes beyond 1.8 kg/h/mm, bubble flutter typically appears unless frostline height is extended beyond 9 die diameters and the lower air-ring lip is opened to reduce venturi-induced neck oscillation. For processors blending for melt strength, a 15–25 wt% addition of high-pressure LDPE with a melt index of 0.3–0.5 g/10 min is gravimetrically dosed with the LLDPE feed; no pre-drying is required at ambient relative humidity below 60%. High-pressure LDPE addition raises melt strength but reduces dart impact retention, so the blend ratio is fixed by the sack-drop performance specification. Sack qualification commonly follows ISO 7965-2 drop testing with the filled sack mass corresponding to the end-use fill weight, while film tensile properties are measured per ASTM D882 and dart impact per ASTM D1709 Method A. Terminal formats include gusseted open-mouth sacks, sewn or glued valve sacks, and flat or folded liners for rigid intermediate bulk containers; edge fold cracking on gusseted sacks is evaluated using ASTM D1922 tear resistance before commercial approval.
The limiting variable in frozen-food film converting is not resin density but the combined effect of slip additive surface migration and low-temperature impact retention below -20 °C. Converters running this resin typically blend 97.0–98.5 wt% MarFlex® 7109L with 1.5–3.0 wt% slip/antiblock masterbatch, corresponding to active erucamide slip at 500–1500 ppm and synthetic silica antiblock at 1000–3000 ppm depending on film gauge. The bubble is processed through a 1.2–1.5 mm die gap at a blow-up ratio of 2.0:1–2.5:1 and a frostline height of 6–8 die diameters; internal bubble cooling air is held at 15–25 °C to stabilize the frostline under high ambient humidity. Food-contact approval is established under FDA 21 CFR 177.1520(c)(3.1a) and EU Regulation No 10/2011 with the overall migration limit of 10 mg/dm² in the applicable food simulant; converters must verify that the chosen masterbatch carries equivalent compliance documentation because the base resin approval does not automatically cover additive packages. On a 350 mm annular die with 75 mm grooved-feed extruder, bubble stability is maintained at 2.4:1 BUR; production records indicate that raising slip masterbatch above 3.0 wt% reduces static coefficient of friction below 0.20 per ASTM D1894 but increases dust pickup on gusset creases. Terminal product forms include frozen vegetable pillow pouches, seafood bags, ice cube bags, and flat-bottom freezer pouches.
When silage film requires both surface cling and sustained UV resistance, 7109L is positioned in the 3-layer coextrusion core rather than the cling skin. A typical structure uses a core layer of 60–70 wt% MarFlex® 7109L and 30–40 wt% high-pressure LDPE, while the skins contain 80–85 wt% LLDPE and 15–20 wt% EVA for tack; the complete film carries a hindered amine light stabilizer masterbatch loading of 4–8 wt%, with the exact dosage indexed to the intended 12–36 month exposure period. Coextruded agricultural film is run through a 1.8–2.2 mm die gap at a blow-up ratio of 2.5:1–3.0:1, with frostline height kept between 5 and 7 die diameters to maintain transverse-direction tear resistance. Melt temperature is held at 190–210 °C; higher melt temperatures accelerate EVAc acid formation in the skin and displace cling balance. Film performance is tested against EN 13206:2017 for agricultural and horticultural covering film, with tensile properties measured per ISO 527-3 and tear resistance per ISO 6383-2. UV stabilizer packages must be selected from masterbatches whose carrier resin and actives do not destabilise the LDPE/EVA skin at the die lip. Terminal products include round bale silage wrap, silo bag film, greenhouse covering, and temporary tunnel covers.
| Sector | Primary standard | Critical test or limit | Application boundary |
|---|---|---|---|
| Heavy-duty shipping sacks | ISO 7965-2 | Filled sack drop test at end-use mass | Not a UN-certified dangerous goods packaging unless separately qualified |
| Frozen food packaging | FDA 21 CFR 177.1520(c)(3.1a); EU 10/2011 | Overall migration < 10 mg/dm² | Additive masterbatch compliance must be independently documented |
| Agricultural covering film | EN 13206:2017 | ISO 527-3 tensile; ISO 6383-2 tear | Skin-layer EVA ratio is adjusted only after UV stabilizer loading is fixed |
| Stretch hood film | ASTM D882; EUMOS 40509 | Tensile elongation and pallet-load stability | Not a substitute for heavy-duty shrink film below 50 µm on irregular loads |
| Construction vapour retarder | ASTM E96/E96M; EN 13984:2013 | Declared water vapour resistance factor | Carbon black masterbatch above 6 wt% may destabilise the bubble |
In pallet-containment stretch hood film, the resin is processed at a die gap of 1.2–1.5 mm and a blow-up ratio of 2.5:1–3.0:1 to produce transverse-direction tensile properties suitable for 50–80 µm hood gauge. A blend of 70–80 wt% MarFlex® 7109L with 20–30 wt% metallocene LLDPE is used; a fluoroelastomer polymer processing aid is added at 200–400 ppm to suppress die-lip build-up at high output. Hood film qualification follows ASTM D882 for tensile stress and elongation and ASTM D5748 for puncture resistance; pallet-load stability validation is conducted under EUMOS 40509 where the end user specifies load unit security for road transport. Terminal products include pallet hoods for glass racking, building material bundles, beverage pallets, and ceramic tile loads.
The governing process conflict in commercial can liner extrusion is the loss of bubble stability when post-industrial recyclate contains uncontrolled LDPE and trace PP fractions. A melt blend of 60–70 wt% MarFlex® 7109L and 30–40 wt% post-industrial LLDPE/LDPE recyclate is processed through a die gap of 2.0–2.5 mm at a blow-up ratio of 2.0:1–2.5:1, with melt temperature raised to 205–225 °C to homogenise the recycled fraction. A dual-lip air ring with upper-lip extension is used instead of a single-lip design because recyclate-induced melt elasticity changes require broader frostline control; a screen pack of 60/80/100 mesh is installed to remove gel particles. Output is derated by 20–30% relative to virgin operation to limit gel-induced bubble puncture. Published line-speed data for high-recyclate can liner configurations varies by recyclate source; the derate is therefore established by trial on the specific extrusion line. Recycled content claims are managed under ISO 14021; EU market access requires REACH and, where applicable, packaging derogation documentation. The resin itself does not confer compliance for recycled content; chain-of-custody certification rests with the recyclate supplier. Terminal products include commercial can liners, waste collection bags, janitorial liners, and medium-duty industrial refuse sacks.
Die-gap selection for construction vapor retarder film differs from food packaging because the gauge range extends from 150 µm to 250 µm and the film must maintain low crease sensitivity during wide-sheet conversion. A formulation of 94–96 wt% MarFlex® 7109L and 4–6 wt% carbon black masterbatch is run through a 2.0–2.5 mm die gap at a blow-up ratio near 2.0:1 and a frostline height of 4–6 die diameters; the shorter frostline is used to keep the bubble in the stabilising cage during thick-gauge startup. Moisture barrier performance is measured under ASTM E96/E96M desiccant method, and product conformity for building applications is demonstrated under EN 13984:2013 for plastic vapour control layers where the project specifies a declared water vapour resistance factor. Carbon black masterbatch above 6 wt% tends to accumulate at die lips and destabilises the bubble via radiant heat absorption; no pre-drying of the base resin is required below 60% RH. Terminal products include underslab vapour retarders, crawl space liners, temporary weather protection sheeting, and construction dust partitions.
Competitive Chevron Phillips MarFlex® 7109L LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips MarFlex® 7109L is a metallocene-catalysed linear low-density polyethylene (mLLDPE) supplied as a pelletized blown film resin. The nominal melt flow index is 0.9 g/10 min when determined at 190 °C under a 2.16 kg load in accordance with ASTM D1238 or ISO 1133. The nominal density is 0.918 g/cm³ as measured by ASTM D1505 or ISO 1183. The resin is produced with a 1-hexene comonomer and a narrow molecular weight distribution characteristic of single-site catalysis. It is indicated for blown film applications in which seal initiation, dart impact, and optical haze are controlled parameters. Published data for proprietary comonomer distribution and rheological molecular architecture are limited in public sources; lot-specific certificates should be consulted for exact values.
Because the resin is synthesized using a metallocene catalyst, comonomer placement is more uniform than that of a conventional Ziegler-Natta hexene LLDPE. The narrow molecular weight distribution and reduced high-density homopolymer fraction produce films with lower haze and a distinct sealant response. The resin is typically specified for monolayer and coextruded blown film structures where seal integrity and dart impact resistance are required at film gauges below 50 µm. The material is not a drop-in replacement for high-melt-strength autoclave LDPE in shrink film lines that require deep-draw bubble geometry; in such cases, LDPE blending or internal bubble cooling is required. It is also not recommended for injection molding or rotomolding, because the narrow molecular weight distribution and high shear sensitivity are outside the design envelope of those processes.
Bubble stability for 7109L depends on melt strength, die geometry, and air-ring configuration. On a 60 mm grooved-feed blown film extruder with an L/D of 30:1, a 250 mm spiral mandrel die, and a dual-lip air ring with internal bubble cooling, stable operation is generally reported at melt temperatures between 195 °C and 215 °C, blow-up ratios from 2.2:1 to 2.8:1, and die gaps from 1.8 mm to 2.5 mm. The narrow molecular weight distribution produces lower shear sensitivity than autoclave LDPE; therefore, excessive shear heating in deep-flight barrier screws can reduce melt viscosity and destabilize the stalk. Operators have observed bubble chatter when the frost line height exceeds 350 mm without internal bubble cooling or when melt temperature drops below 190 °C. Die lip build-up can occur after extended runs above 220 °C; purge cycles should follow the resin supplier’s recommended polyethylene purge sequence.
The resin’s critical shear rate for melt fracture is lower than that of a broad-MWD Ziegler-Natta LLDPE at equal melt index. When output is increased beyond the onset of sharkskin, a slight melt temperature increase of 5–10 °C or a die gap widening of 0.5 mm can shift the failure to a higher screw speed. Use of fluoropolymer processing aids at 300–800 ppm suppresses die lip build-up but does not alter the fundamental strain-hardening behaviour of the film.
Extruder back pressure at 80–110 kg/h output on a 60 mm grooved-feed extruder is typically 25–35 MPa before the screen changer, but line-specific values differ. A screen pack of 20/40/60 mesh or finer can reduce gels but increases shear heating. The operating window for screw speed is usually set by melt temperature rather than drive torque; therefore, the resin should not be processed above 220 °C unless purge or rapid grade transitions require it.
Film tensile properties are evaluated by ASTM D882 on 25 µm monolayer samples. Because the resin has a lower elastic modulus than HDPE and a higher yield elongation than LDPE, machine-direction and transverse-direction elongations at break typically exceed 400%; however, actual values depend on frost line height and blow-up ratio. For converter specifications, film should be conditioned at 23 ± 2 °C and 50 ± 5% relative humidity for a minimum of 40 h before destructive testing. Published data for this specific processing configuration are limited, and development trials on the target blown film line are required for precise mechanical property limits.
For vertical form-fill-seal packaging lines sealing at speeds above 80 packages/min, seal initiation behavior becomes a rate-limiting variable. Heat seal initiation temperature is evaluated according to ASTM F1921 or peel seal strength per ASTM F88 using a 0.5 s dwell and 276 kPa pressure against a selected sealant interlayer. The uniform comonomer distribution of 7109L narrows the difference between seal initiation and plateau seal strength compared with conventional Ziegler-Natta LLDPE of equivalent density and melt index. This allows a lower jaw setpoint and reduces the heat load transferred to the package content. Hot tack strength is assessed by ASTM F1921 at seal bar temperatures from 150 °C to 170 °C; published values for this specific resin are limited, so converter trials on the target packaging machine are required.
In coextruded structures, 7109L is frequently used as a sealant layer adjacent to an HDPE or polypropylene core. The sealant layer improves seal through contamination and reduces the seal bar temperature required to achieve a 10 N/15 mm peel strength. The resin’s low extractable fraction also supports organoleptic performance; hexane extractables measured by FDA 21 CFR 177.1520 protocols are typically below 2.6 wt% for the base polymer, but additives must be included in the final package assessment. In snack packaging, the low seal initiation temperature allows a reduction in jaw temperature from polypropylene-based sealants, reducing film shrinkage and distortion at high speed.
The base resin is delivered without intentionally high slip or antiblock loadings; converters typically introduce slip and antiblock masterbatches to control coefficient of friction. The coefficient of friction is tested by ASTM D1894, and target values depend on form-fill-seal machine design rather than on the base polymer. The absence of a high loading of migratory slip additive in the base resin permits a wider converting window but requires that final film specifications be qualified on the intended packaging line.
Film downgauging trials with 7109L on a 45 mm extruder with a 150 mm die and 2.0:1 blow-up ratio show that dart impact resistance and Elmendorf tear propagation can be retained at 25–38 µm gauge. Dart impact is determined according to ASTM D1709 Method A or B; tear propagation is measured by ASTM D1922 in machine and transverse directions. The hexene side-chain length and uniform comonomer placement increase tie-chain density relative to butene-based LLDPE at the same nominal density. However, transverse-direction tear in blown film can exhibit a machine-direction bias at high blow-up ratios, so the downgauging limit should be validated with package drop tests and simulated distribution trials under ISTA 6A or equivalent. Tensile properties are measured by ASTM D882; yield stress and elongation at break are geometry-dependent and should not be extrapolated from cast film data.
The puncture resistance of a 25 µm monolayer film is typically assessed by ASTM D5748 or a slow puncture probe, while field performance is validated by package drop tests under ISTA 6A. Downgauging below 40 µm requires that the load-bearing layers maintain tear propagation, not merely tensile yield. The uniform branching in 7109L increases the probability of tie-chain formation between crystallites, which improves puncture energy absorption relative to conventional butene-based LLDPE. However, the low stiffness of the resin at 0.918 g/cm³ means that unsupported heavy-duty sacks may require a stiffer coextruded core layer of HDPE or a blend with high-density resin.
Differential scanning calorimetry per ASTM D3418 on re-solidified material typically shows a broad melting interval ending near 120 °C and a crystallization exotherm near 105 °C. The exact peak positions vary with cooling rate and film orientation. These values are not direct processing setpoints; they are used to anticipate heat seal temperature and shrink behaviour in secondary operations.
Molecularly, the difference between 7109L and a conventional Ziegler-Natta hexene LLDPE lies in the comonomer composition distribution and the low-molecular-weight extractable fraction. In Ziegler-Natta resins, short-chain branching concentrates in lower-molecular-weight chains, producing a broader melting range and a weaker sealant plateau. In 7109L, the metallocene active sites place 1-hexene more evenly across the molecular weight distribution; the consequence is a narrower crystalline thickness distribution and a lower heat seal initiation temperature. The resin also exhibits fewer high-density homopolymer fractions that would otherwise raise haze in thin films. Rheologically, the narrow molecular weight distribution gives a lower shear thinning index than branched LDPE, so die pressure at a given output is lower but bubble tension and stalk stability are more sensitive to frost line height. Blending with 5–20 wt% LDPE is common when high-stalk geometry or melt strength is required.
Compared with a butene-based Ziegler-Natta LLDPE at the same nominal density, the 1-hexene comonomer produces a higher tie-chain density and lower seal initiation temperature. Butene-based resins are not directly interchangeable in formulas where film tear balance and seal-through-contamination are optimized. Conversely, 7109L lacks the long-chain branching of autoclave LDPE; thus, it has lower strain hardening during bubble expansion and may require blending with LDPE or the use of internal bubble cooling in high-stalk configurations.
Regulatory compliance for food contact use requires verification against multiple jurisdictions. The following matrix summarizes core references; it is not exhaustive.
| Reference | Scope | Test method / limit |
|---|---|---|
| US FDA 21 CFR 177.1520 | Olefin polymers for food contact | Composition or end-test |
| EU Regulation 10/2011 | Plastic materials and articles intended for food contact | Overall migration limit 10 mg/dm² |
| REACH | Chemical registration and authorization | Article-specific declaration |
| RoHS Directive 2011/65/EU | Electrical and electronic equipment | Not normally relevant to polyolefin film |
No single global statement applies to all converting jurisdictions; the converter is responsible for verifying that additives and processing aids used with 7109L comply with the destination market. Compliance declarations should be obtained from the resin supplier for the specific lot, because product stewardship documents can change after additive reformulation or production site qualification.
Incoming resin handling requires dry-air conveyance or sealed-container hopper loading if ambient relative humidity exceeds 60%. Although LLDPE is not strongly hygroscopic, surface moisture on pellets can generate surface splay and bubble pinholes at melt temperatures above 200 °C. Extruder barrel profiles typically start at 170–180 °C in the feed zone and increase to 190–210 °C at the die, but these settings must be adjusted for screw speed, back pressure, and output. The product does not require pre-drying at RH < 60%. Nitrogen purging of the hopper is recommended only for long-term storage. Avoid blending with acid-functional polymers or heavily oxidized regrind without verification, because acid groups can react with residual catalyst components and cause gel formation. Fluoropolymer processing aids at 300–800 ppm can reduce die lip build-up but must be validated for food contact compliance in the finished package.
In coextruded blown film lines, 7109L is typically assigned to the sealant or toughness layer. Layer ratios from 10% to 30% are employed depending on the total film gauge and the mechanical requirements of the outer layers. The viscosity of the resin at 0.9 g/10 min is close enough to many HDPE and LLDPE grades to maintain layer uniformity in spiral mandrel dies; however, interfacial instability can occur if the viscosity ratio between adjacent layers exceeds 2:1 at the processing shear rate. Therefore, converters should match the melt index and die pressure behaviour of the coextruded layers rather than relying solely on nominal melt index.
Optical haze is measured by ASTM D1003, and 45° gloss by ASTM D2457. In 25 µm film, the resin’s uniform comonomer distribution reduces internal haze; however, surface irregularities from die lines, melt fracture, or excessive frost line height can dominate the measured total haze. Therefore, optical specifications should be interpreted together with melt pressure and bubble stability records rather than as isolated material properties.
For liquid packaging films and stand-up pouches, the sealant layer must withstand internal product pressure and moderate flex-cracking. Flex-crack resistance is evaluated by ASTM F392 using Gelbo flex testing at 20 °C and -5 °C. The high impact strength of 7109L films supports puncture resistance in laminates, but the outer polyethylene terephthalate or oriented polyamide layer governs overall flex-crack propagation. No laboratory flex-crack test replaces filled-package transit trials.
The low extractable fraction supports organoleptic-sensitive food packaging; sensory panels are typically conducted under ISO 13302 or an internal protocol. The resin alone does not guarantee taste and odour neutrality; additive masterbatches, printing inks, and lamination adhesives can dominate taint and odour. Therefore, any organoleptic claim must be accompanied by a complete packaging system evaluation, not a material-only certificate.
For collation shrink or stretch-hood applications, the low seal initiation and controlled shrinkage can be combined with LDPE in the outer layers. Shrink tension is determined by biaxial orientation and is less influenced by the metallocene structure than by the LDPE fraction. No published data support a single recommended blend ratio for all shrink tunnels; the required shrink percentage must be mapped against tunnel temperature and residence time.