Chevron Phillips Marflex 7105fl Polyethylene Lldpe

Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE

    • Product Name: Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 865559
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 27.6 MPa
    Elongation At Break 700%
    Flexural Modulus 207 MPa
    Film Dart Drop Impact 120 g
    Film Elmendorf Tear Strength Md 250 g
    Film Elmendorf Tear Strength Td 450 g
    Film Haze 12%
    Film Gloss 45 60%
    Film Coefficient Of Friction 0.2
    Film Tensile Strength At Break Md 30.3 MPa
    Film Tensile Strength At Break Td 27.6 MPa
    Film Elongation At Break Md 500%
    Film Elongation At Break Td 700%

    As an accredited Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips MarFlex 7105FL LLDPE comes in 25 kg polyethylene-lined paper bags, 40 bags per pallet (1,000 kg net).
    Container Loading (20′ FCL) Container Loading (20′ FCL): 25 kg bags of Chevron Phillips MarFlex® 7105FL LLDPE, palletized, stretch-wrapped, and securely braced for transport.
    Shipping Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE is shipped as non-hazardous LLDPE pellets, typically in 25 kg polyethylene bags or bulk bags, palletized and stretch-wrapped. Transport in clean, dry trucks or containers. Protect from moisture, contamination, excessive heat, and UV. Not regulated for transport; follow supplier SDS and local rules.
    Storage Store Chevron Phillips MarFlex® 7105FL Polyethylene (LLDPE) in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers or bags closed, off the floor, and protected from moisture and contamination. Maintain moderate temperatures to prevent melting or degradation, and use first-in, first-out stock rotation. Ensure proper ventilation and avoid prolonged UV exposure.
    Shelf Life Shelf life: two years from manufacture when stored unopened in a cool, dry area away from sunlight and heat.
    Application of Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE

    Cast Film Optical Haze and Pre-Stretch Retention in High-Speed Pallet Wrapping

    Cast film converted from MarFlex® 7105FL is typically produced on lines equipped with a 90 mm barrier screw, L/D 30:1, compression ratio 3.0:1, and a die width of 2.0–3.0 m. For down-gauged wrap below 12 µm, the resin is melt-blended with a single-site polyethylene plastomer at 10–20 wt%, the plastomer having a density below 0.902 g/cm³. Melt temperature is held between 210 °C and 245 °C, the die gap is set at 0.6–1.0 mm, and the polished chill roll is maintained at 18–25 °C. On a 2.5 m line running at 350 m/min, screen-pack pressure above 35 MPa at constant throughput indicates gel accumulation, poor mixing, or metal fatigue in the screen changer. Machine-direction tensile elongation is measured under ASTM D882 as an indirect check on pre-stretch uniformity, while cling is tested under ASTM D5458 and puncture resistance under ASTM D5748. Turntable wrappers commonly apply 200–250% pre-stretch; at the upper limit, edge tear propagation initiates if web thickness variation exceeds ±5%. Haze values below 2.0% measured per ASTM D1003 require a clean chill roll and controlled wax pickup. Melt flow rate is verified at 190 °C/2.16 kg under ASTM D1238 or ISO 1133-1. If the grade is combined with chlorinated wax or an incompatible processing aid, cling uniformity shifts, so only saturated masterbatches are used.

    Silage wrap and greenhouse cover webs are produced on three-layer blown-film lines with die diameters of 250–350 mm, die gaps of 1.6–2.2 mm, and layflat widths of 1,500–2,500 mm. The core layer contains MarFlex® 7105FL with 0.3–0.6 wt% hindered amine light stabilizer and 0.1–0.3 wt% UV absorber concentrates; outer layers incorporate slip and antiblock concentrates at 0.5–1.5 wt%. Blow-up ratios between 2.0:1 and 2.6:1 are used to balance dart impact and tear, with frost line height kept at 8–12 die diameters. Melt temperatures above 220 °C increase gel formation from high-molecular-weight stabilizer by-products, while temperatures below 185 °C produce visible melt fracture at high output. Field failures in silage wrap below 25 µm most often appear as crease splitting after 12–18 months of UV exposure and silage acid contact; tensile elongation is checked under ISO 527-3 and dart drop under ASTM D1709. Roll geometry must maintain web thickness variation below ±5% because stacked rolls in storage develop permanent deformation at the core. Batch-to-batch variation in stabilizer dispersion can be detected as a screen pack pressure increase of 1.5–3.0 MPa over an 8 h run.

    What Seal Initiation and Hot Tack Window Are Achievable in Coextruded Food Packaging?

    The sealant webs in three-layer food packaging are usually run as a coextruded skin layer at 15–25% of total structure, paired with a polyamide or EVOH barrier core and tie layers. In such structures, the linear low-density polyethylene provides seal initiation near 100–115 °C; published data for this specific converted configuration is limited, so converters generate a seal-force curve per ASTM F88 and hot-tack values per ASTM F1921 across a 10 °C gradient before setting packaging line dwell times. On high-speed flow wrappers, a hot-tack window of 0.2–0.5 s at 0.3–0.5 N/mm seal force is common for polyethylene-based sealant webs, though actual values depend on web thickness, die-gap orientation, and additive package. Slip and antiblock additives must be selected from compliant masterbatches because overall migration above <10 mg/dm² under EU No 10/2011 can affect organoleptic testing. Pre-drying is not required unless ambient humidity exceeds 60%, at which point additive concentrates may agglomerate and create visible gels.

    ApplicationStandardCompliance or test basis
    Food contact sealant websFDA 21 CFR 177.1520Olefin polymer requirements; overall migration <10 mg/dm² per EU No 10/2011
    Silage wrap and greenhouse filmEN 13206:2017Thickness, tensile and UV retention per specified classes
    Cast stretch filmASTM D5458 / ASTM D5748Cling and puncture targets set by line design; no fixed pass/fail value
    Heavy-duty sack filmASTM D1709 / ASTM D1922Minimum dart drop and tear values per buyer specification

    Form-fill-seal lines converting heavy-duty sacks run 80–150 µm webs at fill rates of 25–35 cycles/min. On three-layer blown-film extruders, the core layer of MarFlex® 7105FL is blended with 10–20 wt% high-pressure LDPE to improve bubble stability at blow-up ratios of 1.8:1–2.0:1. Dart impact is measured per ASTM D1709, Elmendorf tear per ASTM D1922, and coefficient of friction per ASTM D1894. Web thickness variation above ±6% causes intermittent seal-bar leaks at lap seals.

    When Extrusion Lamination Lines Run Above 300 m/min on Foil and Paperboard

    At line speeds above 300 m/min, extrusion lamination of MarFlex® 7105FL onto paperboard and aluminium foil requires blending with 20–30 wt% LDPE or a low-melt-index extrusion-coating grade to control neck-in and draw resonance. Melt temperature is set between 285 °C and 315 °C; below 280 °C, adhesion to foil falls below practical peel values, while above 320 °C, smoke generation and oxidative gel formation increase. Die gaps of 0.6–1.0 mm and air gaps of 200–250 mm are employed, with internal deckles adjusted to keep edge bead below 2 mm. T-peel adhesion is measured under ASTM D1876; acceptable values are often specified between 1.5 N/15 mm and 4.0 N/15 mm depending on foil thickness and corona treatment level. When a coextruded tie layer of ethylene-acrylic acid or ethylene-methacrylic acid is required, the supplier’s recommended melt temperature and backpressure limits must be observed; published data for this specific configuration is limited. Longer air gaps above 250 mm reduce peel strength because the oxidised film surface cools below the necessary level for carboxylic acid bonding.

    Surface protection films for stainless steel sheet, painted aluminium profiles and glass are extruded at 40–80 µm using MarFlex® 7105FL blended with 5–15 wt% LDPE and a pressure-sensitive adhesive concentrate. Peel strength is adjusted between 0.5 N/25 mm and 2.0 N/25 mm per ASTM D3330. Blow-up ratios of 2.0:1–2.5:1 reduce visible gel defects that would mark polished metal surfaces.

    Free Quote

    Competitive Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips MarFlex® 7105FL Polyethylene; LLDPE is specified as an ethylene-hexene linear low-density polyethylene cast film resin. Current technical documentation lists a nominal density of 0.918 g/cm³ determined under ASTM D1505 and a melt index of 3.5 g/10 min determined under ASTM D1238 at 190 °C and 2.16 kg. The intended processing route is slot-die cast film extrusion; coextruded film structures are a secondary use. Typical application classes include monolayer and coextruded stretch wrap, industrial liners, overwrap, frozen food film, and lamination film. Relative to butene-based LLDPE of equivalent melt index, the hexene comonomer modifies short-chain branching distribution, which changes tear, dart impact, and seal initiation behaviour in thin-gauge structures. Relative to high-pressure LDPE, the linear polymer has lower melt strength and is less suited to high-stalk blown-film operations than to cast film.

    Because single-point melt index is measured at low shear, it does not describe shear-thinning response in a cast film extruder. Lot-to-lot density movement of ±0.001 g/cm³ can shift melt-phase specific volume and alter extruder throughput at constant screw speed. Production qualification therefore employs capillary rheometry or on-line melt viscosity data across the barrel residence time, rather than relying solely on melt index.

    Core specification points from current commercial documentation
    ParameterMethodPublished nominal value
    DensityASTM D15050.918 g/cm³
    Melt indexASTM D12383.5 g/10 min
    Comonomer typeManufacturer designationHexene
    Primary processManufacturer designationCast film extrusion

    Material Characterization and Standard Reference Points

    Density and melt index are not stand-alone defining properties for this grade. Incoming inspection for thin-gauge cast film often adds thermal transition measurement under ASTM D3418, Vicat softening under ASTM D1525, and oxidative induction time under ISO 11357-6. These methods identify lot shifts that may appear as chill-roll release variation, winding tension drift, or changes in film haze measured under ASTM D1003. The semicrystalline morphology of a 0.918 g/cm³ LLDPE is sensitive to quench rate; therefore, film properties are not solely a function of resin pellet data. Published data for this specific configuration is limited for direct numerical comparison across all film testing standards, so matched processing history is required during qualification.

    In slot-die extrusion of this 3.5 g/10 min grade, apparent shear viscosity at the die lip is governed more by die geometry and shear rate than by the single-point melt index. Capillary rheometry across shear rates of 100 to 1000 s-1 provides a more usable measure of die pressure response. On production-scale cast film lines, pressure transducers positioned before the screen pack and in the adapter are monitored because pressure rise is the earliest reliable indicator of gel accumulation or screen blockage.

    How Does a Melt Index of 3.5 g/10 min Interact with Cast Film Extrusion Rates?

    With a melt index of 3.5 g/10 min, this grade occupies the medium-flow segment for LLDPE cast film. On a 90 mm grooved-feed extruder with 30:1 L/D, the melt index supports high screw speed without motor torque saturation, but the relationship is not linear across the shear-rate range encountered at the die lip. At shear rates above 1000 s-1, shear-thinning reduces the apparent viscosity advantage relative to a 1.0 g/10 min LLDPE. Barrel profiles reported in cast film practice start below 45 °C in the feed throat zone, rise to 190–220 °C in compression zones, and stabilize at 240–260 °C at the adapter and die. Die lip gaps are commonly set between 0.4 mm and 0.8 mm; narrower gaps improve gauge uniformity but raise die pressure and increase sensitivity to melt-temperature non-uniformity.

    The molten density of this 0.918 g/cm³ resin is below solid density; throughput calculations based on solid density require correction. In single-layer cast film, draw-down ratios above 40:1 are used for film thickness below 20 µm. At such ratios, melt resonance and edge-bead instability become process limits. Draw resonance maps are generated by varying chill-roll speed and air gap while holding die throughput constant, because the boundary between stable drawing and resonance is equipment-specific rather than resin-specific alone.

    Slip and antiblock loadings for MarFlex 7105FL are not universal; they are supplied according to commercial agreement. In cast lamination-grade base film, the absence of migratory slip helps preserve the stability of corona-treated surfaces. Where film-to-metal friction is excessive during winding, operators adjust roll hardness and trim edge position before adding external antistat. On manufacturing lines, film coefficient of friction is tracked under ISO 8295 or ASTM D1894 because additive variation can shift unwind performance without changing melt processing behaviour.

    On High-Speed Cast Film Lines, Die Temperature Uniformity Sets the Practical Speed Limit

    High-speed cast film lines operating above 150 m/min are sensitive to melt-temperature non-uniformity and gel content. Melt temperature differences of ±2 °C across the die width can produce gauge variation outside ±2% at film thickness below 25 µm. The primary processing boundary is the upper die-temperature limit; extended residence above 260 °C increases oxidative degradation and yellowness index measured under ASTM E313. Filtration with screen packs of 40/60/100 mesh reduces cross-linked resin particles but raises head pressure as screens age. Line operators track pressure rise per hour against the screen-change threshold specified for the die pack.

    Air gaps between 100 mm and 250 mm produce stable sheet when the melt is maintained within a narrow temperature band; air gaps outside this range amplify edge-bead thickening and neck-in. Because this grade is formulated for slot-die extrusion, blown-film bubble stability is not the relevant performance window. The lower melt strength of LLDPE relative to LDPE makes the resin unsuitable for high-stalk blown-film processes without blending.

    Chill-roll temperature and surface finish are independent of melt index but strongly affect haze and seal behaviour. Cast film quenched on chill rolls maintained between 15 °C and 30 °C generally shows lower haze than film produced on warmer rolls, but excessive chilling can create condensation defects and matte bands from differential quench. Chill-roll optimization therefore uses ASTM D1003 haze measurement together with winding tension records.

    Cast film mechanical property testing for the grade uses ASTM D882 for tensile properties, ASTM D1922 for Elmendorf tear, and ASTM D1709 for dart drop. The film property values recorded in commercial qualification depend on chill-roll temperature, line speed, and gauge; comparisons between resins require matched processing history. When film is drawn to 20 µm, tensile elongation above 300% in the machine direction is commonly specified for stretch wrap. Published data for this specific configuration is limited for product-specific numerical claims beyond the resin data sheet.

    When Layer Ratio Changes in Coextruded Structures, Melting Point Mismatch Becomes Critical

    Coextrusion lines combining this LLDPE with HDPE or PP skins must manage melting point mismatches. Under ASTM D3418, the LLDPE melting peak is reported in the 120–125 °C band. HDPE skins typically require higher melt temperatures; the LLDPE core is therefore maintained near the lower end of its processing window while skin-layer extruders are operated independently. This segmented thermal profiling prevents core-layer oxidative degradation and preserves interlayer adhesion. When the LLDPE layer drops below 10% of total gauge, melt viscosity mismatch between adjacent layers can produce interfacial turbulence and local thickness variation. When the LLDPE layer exceeds 70% of total gauge, the structure approaches monolayer cast film and neat resin stability dominates.

    Improving interlayer performance in such structures often involves melt temperature offsets of 5–10 °C between layers rather than resin replacement. Manufacturing lines record layer-ratio deviations and die-temperature profile data because deviation above 1% in layer ratio can shift seal initiation temperature measured by ASTM F88. Seal strength comparisons between different LLDPE grades should be run on the same coextrusion line and with the same chill-roll history.

    Comparing Hexene LLDPE and Butene LLDPE Under Matched Cast Film Conditions

    The structural difference from butene-based LLDPE lies in the length of the short-chain branch. Hexene introduces a 4-carbon side branch, whereas butene introduces a 2-carbon branch. At equivalent density and melt index, the longer branch influences tie-molecule formation between crystalline lamellae. This difference affects Elmendorf tear and dart impact values determined under ASTM D1922 and ASTM D1709, but film values also depend on orientation and quench rate. Published data for this specific configuration is limited for direct numerical comparison; extrusion trials under matched chill-roll conditions are the accepted method for substantiating performance differences.

    Relative to high-pressure LDPE of similar density, this linear resin has a narrower molecular weight distribution and lower melt strength. In cast film, that combination supports higher draw-down but also produces greater neck-in. Blown-film lines designed for high-stalk LDPE are not directly interchangeable. Relative to metallocene LLDPE grades, this resin may exhibit different organoleptic and melt fracture behaviour; selection in taste-and-odour-critical packaging requires testing under actual film-making conditions and at the intended wound-roll age.

    Food-contact compliance for polyethylene should be verified against FDA 21 CFR 177.1520, which covers olefin polymers, and against EU Regulation No 10/2011 where applicable. These designations refer to the polymer class and do not by themselves cover additives, contaminant limits, or migration from the final fabricated article. A separate end-use compliance record is required when the film is corona-treated, laminated, or printed, because post-treatment surface chemistry may fall outside the original resin certification.

    Standards and regulatory anchors for specification and end-use evaluation
    Standard or regulationApplication in resin or film qualification
    ASTM D1505Density determination by gradient column
    ASTM D1238Melt mass-flow rate of polyethylene
    ASTM D882Tensile properties of thin plastic sheeting
    ASTM D1922Elmendorf tear resistance
    ASTM D1709Dart drop impact energy
    ASTM F88Seal strength of flexible barrier materials
    FDA 21 CFR 177.1520Olefin polymers in food-contact articles
    EU Regulation No 10/2011Plastic materials intended for food contact

    Film End-Use Specifications Require More Than a Resin Compliance Letter

    Operational boundaries for the resin include storage in dry conditions at ambient temperature below 50 °C. Extended residence time above 260 °C at the die increases yellowness index and surface oxidation. Batch-to-batch density variation should be tracked through certificate-of-analysis data because movement greater than 0.002 g/cm³ can shift draw-down characteristics on thin-gauge cast film even when melt index remains within specification. Resin performance in a final film article is inseparable from extruder configuration, layer ratios, chill-roll temperature, and winding tension; therefore, end-use qualification records must retain these processing parameters alongside the resin designation.