| HS Code | 178028 |
| Product Name | Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm³ |
| Melt Index | 1.0 g/10 min at 190°C/2.16 kg |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 27.6 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 234 MPa |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Dart Impact Strength | 100 g |
| Haze | 10 % |
| Gloss 45 Degree | 70 % |
As an accredited Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips MarFlex 7105DL LLDPE is supplied in 55 lb (25 kg) multiwall bags, with 2,200 lb boxes and bulk available. |
| Container Loading (20′ FCL) | 20′ FCL loaded with 25 kg bags of Chevron Phillips MarFlex® 7105DL LLDPE polyethylene, palletized and securely stowed for export. |
| Shipping | Shipping description: Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE is transported as non-hazardous solid pellets. Standard packaging includes 25-kg polyethylene bags, palletized and stretch-wrapped, or bulk trucks/railcars. Store dry, away from heat, moisture, and direct sunlight; keep containers closed. Handle carefully to prevent bag damage and pellet loss. No special DOT hazard classification. |
| Storage | Store Chevron Phillips MarFlex® 7105DL LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain ambient temperatures, protect from UV, and practice first-in, first-out inventory rotation. Ensure good housekeeping to prevent slipping on spilled pellets. Do not store near food or incompatible chemicals. |
| Shelf Life | Stable under normal conditions; shelf life indefinite if stored in sealed original packaging, cool, dry, well-ventilated, away from direct sunlight and heat. |
In pallet unitization cast film lines, MarFlex® 7105DL is metered as the principal hexene-copolymer linear low-density polyethylene at 70–85 wt% of total extrudate, with the remaining fraction split between a metallocene-catalyzed very-low-density polyolefin at 10–20 wt% for cling force development and an LDPE component below 10 wt% for melt curtain edge stability. The grade is processed on a 75–90 mm single-screw extruder having a 30:1 L/D barrier screw, feed zone maintained at 190–205 °C, compression zone at 220–230 °C, metering zone at 235–250 °C, and a flat die set to 245–260 °C. The die gap is held at 0.5–0.8 mm, the air gap between die exit and chill roll is adjusted within 25–80 mm, and the primary chill roll temperature is controlled at 18–24 °C to limit crystallinity-induced haze while preserving machine-direction extensibility. Production-scale field data from cast film lines indicate that condensate-induced point defects increase when the chill roll falls below 15 °C at line speeds above 450 m/min, and winder telescoping becomes measurable when film gauge variation exceeds ±3% across the web. Material lot-to-lot melt index drift greater than 0.05 g/10 min from the nominal 0.50 g/10 min value determined by ASTM D1238 at 190 °C/2.16 kg has been associated with gauge control instability and inconsistent pre-stretch behaviour. Compliance for non-food industrial stretch film is evaluated under REACH Regulation (EC) No 1907/2006, with Article 33 SVHC declarations below 0.1 wt%; mechanical acceptance uses ASTM D882 for tensile strength, ASTM D5748 for protrusion puncture resistance, ASTM D5459 for elastic recovery, and ASTM D5458 for peel cling. The downstream products are machine-grade pallet wrap at 12–35 µm and hand wrap at 15–23 µm, slit to widths of 400–500 mm and wound on 76 mm cores.
Bubble stability in frozen-food blown film coextrusion is governed by the balance between the 0.918 g/cm³ nominal density of MarFlex® 7105DL and the melt strength contributed by a high-pressure LDPE blending partner at 15–25 wt%. The resin is introduced at 75–85 wt% of the blend, with a silica-based antiblock and erucamide slip masterbatch at 2–4 wt%; the LDPE component typically has a melt index of 0.2–0.3 g/10 min by ASTM D1238 to reduce neck-in and maintain bubble geometry under an 2.0:1–2.8:1 blow-up ratio. Converters process the formulation on a 40–65 mm single-screw blown film extruder with a 25:1 L/D screw, a die gap of 1.5–2.0 mm, and a melt temperature of 190–215 °C; the frost line height is set at 600–850 mm to balance optical clarity and gauge uniformity. Film thickness for frozen food packaging is maintained at 40–80 µm. On production lines, bubble flutter increases when the LDPE fraction drops below 10 wt% at high blow-up ratios, and gel accumulation at the die lip becomes visible after 8–12 h of continuous operation if the screw wear diameter clearance exceeds 0.8 mm. Compliance is verified under FDA 21 CFR 177.1520(c), paragraphs 3.1 and 3.2 depending on food type and use conditions, and European food-contact status is assessed under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² using EN 1186-1 migration test procedures; Regulation (EC) No 1935/2004 applies to the finished article. End products include frozen vegetable bags, ice cream pouches, and freezer liners requiring seal integrity at -30 °C and low-temperature toughness evaluated by ASTM D1709 dart impact and ASTM D882 tensile testing.
| Segment | Regulation/standard | Test or control parameter | Value/range |
|---|---|---|---|
| Pallet cast stretch film | REACH (EC) No 1907/2006 | SVHC declaration | <0.1 wt% |
| Frozen-food blown film | EU 10/2011 | Overall migration | 10 mg/dm² |
| Agricultural silage wrap | EN 13206 | UV durability | ISO 4892-2 |
| Heavy-duty sack film | EU 94/62/EC | Heavy metal sum | ≤100 ppm |
| Lamination sealant web | FDA 21 CFR 177.1520(c) | Heat seal initiation | ASTM F2029 |
| Stretch hooder film | ISO 7765-1 | Dart impact | Film impact test |
Agricultural silage wrap produced from MarFlex® 7105DL is configured as a five-layer cast film with 80–88 wt% of the resin distributed across the core and tie layers, 8–12 wt% of a metallocene-catalyzed VLDPE for elongation capacity, and 2–4 wt% of a UV stabilizer masterbatch placed in the outer skin layers, while a polyisobutylene tackifier at 1–2 wt% is limited to the inner cling layer. Published data for this specific resin grade under long-term silage UV exposure is limited; converter trials typically benchmark ultraviolet resistance using ISO 4892-2 accelerated weathering and retain tensile properties under ISO 527-3. The cast film process operates with a 55–90 mm extruder, die gap 0.5–0.8 mm, air gap 30–60 mm, melt temperature 240–260 °C, and line speeds of 350–550 m/min; layer distribution of 20/20/20/20/20 is common but adjusted when UV masterbatch is present to 15/20/30/20/15 to prevent surface migration. Field observations from baling lines show that roll blocking occurs when tackifier levels exceed 2 wt% in warm storage above 35 °C, and uneven cling develops if the cast film edge trim is recycled into the core layer at more than 15 wt% of total throughput. Regulatory compliance for non-food agricultural film is usually limited to REACH (EC) No 1907/2006 and EN 13206 for mechanical and optical classification; no food-contact claim is attached to this conversion route. The terminal articles are round bale silage wraps at 25 µm thickness, 750 mm width, and roll lengths of 1500 m for application by pre-stretch bale wrappers.
A 65–75 wt% loading of MarFlex® 7105DL in heavy-duty blown sack film modifies low-temperature impact resistance and reduces resin cost relative to unimodal LLDPE, while 15–25 wt% of LDPE and 5–10 wt% of HDPE are introduced to raise melt strength and creep resistance. The blend is processed on a 50–70 mm single-screw extruder with a 28:1 L/D grooved-feed throat, die gap set to 1.6–2.4 mm, blow-up ratio held at 2.5:1, melt temperature 190–210 °C, and back pressure limited to 25–35 MPa; excessive screw speed above 120 rpm generates melt-temperature overshoot above 215 °C that reduces bubble stability and increases gels. Thickness ranges from 70–150 µm depending on sack capacity. Packaging waste and heavy-metal compliance is checked against EU 94/62/EC, with the sum of lead, cadmium, mercury, and hexavalent chromium not exceeding 100 ppm; finished sack drop performance is evaluated by ISO 7965-2, and film mechanicals by ASTM D882 and ASTM D1709. End products include valve sacks, FIBC liners, and chemical shipping sack liners in non-food service, where the film is converted on bottom-seal bag lines operating at 20–60 bags/min.
On solventless lamination lines, a cast sealant web containing 85–100 wt% MarFlex® 7105DL, 0–10 wt% LDPE, and 1–3 wt% of a slip-antiblock masterbatch is first produced as a 20–50 µm film and then corona-treated to 38–42 dyn/cm immediately before adhesive coating. The lamination nip is maintained at 70–80 °C, with curing at 35–45 °C for 24–48 h; seal-bar parameters for finished pouches are set at 115–140 °C with 0.3–0.5 s dwell and 3 bar pressure, and heat seal initiation is measured by ASTM F2029 while hot-tack is assessed by ASTM F1921. Food-contact status for the sealant layer is established under FDA 21 CFR 177.1520(c), and EU compliance is documented under Regulation (EU) No 10/2011 with migration tests specified in EN 1186-1 and good manufacturing practice under Regulation (EC) No 2023/2006. A field-reported defect mode occurs when corona treatment decays below 36 dyn/cm during reel changes, producing laminate delamination at the sealant-adhesive interface; similarly, slip additive bloom can reduce seal strength by more than 20% if the finished reel is stored above 30 °C for more than 12 weeks. The terminal formats are stand-up pouches, sachet film, and laminated pouch stock for dry foods, condiments, and non-food granulated products.
Stretch hooder film lines using MarFlex® 7105DL commonly operate at 70–85 wt% of the base resin, 10–20 wt% of a very-low-density metallocene polyolefin for corner puncture resistance, and 5–10 wt% of LDPE for extrusion stability; the blend is cast to 100–180 µm thickness and is not heat-shrunk. Equipment typically includes a 75–100 mm single-screw extruder with a 30:1 L/D screw, a 0.8–1.2 mm die gap, 18–22 °C chill roll set, and line speeds of 250–400 m/min; the molten web is drawn in the machine direction to orient the film before edge slitting for stretch hooder machines. Production bottlenecks observed on hooder lines include film break-out at the corners when orientation ratio exceeds 6:1, and gauge bands near the die lip when the die heater zones deviate by more than ±2 °C. Mechanical acceptance relies on ISO 7765-1 for dart impact, ASTM D882 for tensile modulus, and ASTM D5748 for puncture; regulatory documentation is normally limited to REACH (EC) No 1907/2006 for the European market and EU 94/62/EC when packaging waste recovery is included in customer specifications. The end products are stretch hooder films for appliance, beverage, and building-material pallet loads, consumed as pre-slit rolls on automatic hooders at 60–80% applied elongation.
Competitive Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips MarFlex® 7105DL Polyethylene; LLDPE is a linear low density polyethylene resin supplied in pellet form for cast film extrusion and selected coextruded sealant layers. The grade carries a nominal melt index of 5.0 g/10 min when measured under ASTM D1238 at 190 °C with a 2.16 kg load, and a nominal density of 0.918 g/cm³ when measured under ASTM D1505. These values position the material in the high-flow cast film segment rather than in fractional-melt blown film grades. The polymer backbone is linear, and the product is distinguished from high-pressure low density polyethylene by the absence of long-chain branching; the α-olefin comonomer distribution controls short-chain branching and therefore melt tension, quench response, and heat seal initiation. Supplier technical literature describes the product as a cast film resin with thin-gauge draw-down capability, but converter qualification is required because film properties are sensitive to die gap, chill roll temperature, and cooling roll finish. On production single-screw extruders with 30:1 L/D barrier screws, the melt index of 5.0 g/10 min reduces melt pressure and permits higher screw speed relative to fractional-melt LLDPE, but the resin must be processed within a defined temperature window to avoid gel formation and surface defects.
Incoming inspection of the resin is supported by melt index, density, and visual appearance data recorded on each certificate of analysis. Melt index under ASTM D1238 is not a direct measure of molecular weight distribution; converter laboratories may supplement it with dynamic shear measurements using a rotational rheometer equipped with parallel-plate geometry, in which complex viscosity curves are generated across angular frequencies from 0.1 rad/s to 100 rad/s. The resulting van Gurp–Palmen plot or loss tangent profile can reveal subtle lot-to-lot differences that the single-point melt index does not capture, especially when regrind is introduced. Density under ASTM D1505 is recorded on compression-moulded plaques, and its variation across campaigns is typically reported within the supplier’s specification band; accumulative variation outside that band may indicate cross-contamination or improper incoming resin handling. These measurements are part of incoming inspection but do not replace film-level testing.
| Parameter | Standard method | Representative value |
|---|---|---|
| Nominal melt index | ASTM D1238 | 5.0 g/10 min at 190 °C/2.16 kg |
| Nominal density | ASTM D1505 | 0.918 g/cm³ |
| Molecular structure | Supplier technical documentation | Linear low density polyethylene; no intentional long-chain branching |
| Pellet form | Supplier shipping specification | Free-flowing pellets |
Processing conditions are established on cast film lines equipped with barrier feed screws, melt filtration, and flexible-lip flat dies. Die gap settings are commonly held between 0.4 mm and 0.8 mm; wider die gaps are used where thicker film or higher output is required, but gap adjustment alters shear history and residence time. Melt temperature at the die is maintained from 232 °C to 260 °C, with the lower boundary set by melting and homogenisation requirements and the upper boundary set by degradation risk and gel generation. On a 65 mm single-screw extruder with a 30:1 L/D screw, melt pressure upstream of a 100-mesh screen pack is monitored; pressure variations above 10% of the nominal set point can produce gauge banding and edge bead thickness fluctuation. Chill roll temperature is controlled between 15 °C and 25 °C; the quench rate influences thermal history, freeze-line position, and optical measurements under ASTM D1003. Inadequate chill roll heat removal produces a slowly cooled surface layer that can increase haze and film blocking, whereas excessive chilling can produce surface condensation if the production room dew point exceeds the chill roll set point. High-speed cast film lines operating from 150 m/min to 300 m/min require additional attention to air knife positioning and edge-pinning systems to prevent web chatter and reduce neck-in. The linear molecular architecture of MarFlex 7105DL produces less shear thinning than high-pressure LDPE at comparable melt index; this can be measured by capillary rheometry under ASTM D3835 across apparent shear rates of 100 s⁻¹ to 1000 s⁻¹. Lower shear thinning reduces die swell and can produce flatter film profiles, but the reduced extensional viscosity may require higher melt strength in coextruded structures where draw resonance occurs. Lot-to-lot variation in melt index and density is controlled by the manufacturer within published specification limits; converters should verify certificate-of-analysis values for each production campaign.
Production records from cast film lines identify edge pinning, neck-in, and chill roll release as the most frequent processing deviations when switching from high-pressure LDPE to LLDPE. Neck-in is observed as a reduction in usable film width relative to die width; it is measured on a stable web at a given line speed and die-to-chill-roll distance. Edge pinning systems using compressed-air nozzles or electrostatic edge pinning are adjusted to reduce neck-in; typical die-to-chill roll distances are maintained below 15 mm to limit draw length and preserve film flatness. Chill roll release problems are addressed by controlling roll temperature and surface ageing; the linear polymer may show higher unwind blocking if the roll temperature is too high or the winding tension exceeds the yield stress of the film. Draw resonance can appear on thin-gauge films below 10 µm as periodic width or gauge bands across the web; changing melt temperature or die gap within the ranges already cited shifts the draw ratio. Published data for this specific product in edge-pinning and draw-resonance studies is limited, so the converter must map the stable operating envelope on the specific cast film line.
Across stretch wrap, pallet wrapping, breathable hygiene backsheet film, and packaging overwrap, commercial applications for MarFlex 7105DL center on monolayer and coextruded cast film. In stretch wrap, the grade is blended with tackifier masterbatch and optionally with lower-density polyolefin plastomers; the melt index of 5.0 g/10 min permits draw-down to thicknesses below 10 µm on high-speed cast film units. Puncture resistance is measured under ASTM D5748, and stretch force retention is measured on a laboratory stretch wrapper; published data for this specific blended configuration is limited, so converters qualify the exact formulation on their own machinery. In overwrap and envelope film, the resin is used for gauge uniformity and lower haze relative to high-pressure LDPE, with haze measured under ASTM D1003 and gloss measured under ASTM D2457 at a 45° angle. The optical response is strongly dependent on chill roll surface finish and die lip cleanliness; film produced on matte-finish chill rolls may not show the same gloss as film produced on polished rolls. Coextruded cast structures use the product in sealant layers where low-temperature sealing response is evaluated by flat-jaw heat seal testing under ASTM F88 at dwell times of 0.5 s and 1.0 s and a seal pressure of 0.3 MPa. The grade can be blended with high-pressure LDPE to adjust stiffness and heat seal initiation, but this changes quench behaviour, blocking resistance, and coefficient of friction. The coefficient of friction is measured under ASTM D1894; if the product does not contain the required slip and antiblock additives for a given application, these additives are introduced in a masterbatch at the converter. Published data for specific additive concentrations in this product is limited.
A direct substitution of MarFlex 7105DL for high-pressure LDPE on a cast film line produces measurable shifts in shear viscosity, melt tension, die swell, and heat seal initiation. Capillary rheometry under ASTM D3835 shows a more extended Newtonian plateau for the LLDPE, with a less pronounced viscosity decrease across apparent shear rates of 100 s⁻¹ to 1000 s⁻¹. The reduction in die swell relative to LDPE can improve flatness but increases neck-in if the edge-pinning system is not repositioned. Dart impact resistance is tested under ASTM D1709 using a clamped film specimen and a hemispherical dart; at equivalent gauge and chill roll conditions, LLDPE grades with narrow short-chain branching distribution generally show higher dart impact values than high-pressure LDPE, but the absolute result depends on film gauge, quench rate, and additive package. Tear propagation resistance is measured under ASTM D1922; machine-direction and transverse-direction tear data are required because LLDPE often displays an anisotropic tear pattern that differs from high-pressure LDPE. When the comparison is made to fractional-melt LLDPE of similar density, the higher melt index of MarFlex 7105DL reduces extruder head pressure and motor load but may lower tensile modulus and puncture resistance. Tensile properties are measured on conditioned specimens under ASTM D882 using a constant-rate-of-grip separation tester; secant modulus at 2% elongation is used for stiffness comparisons. The choice between 7105DL and a fractional-melt grade is therefore a process-versus-property decision: the 5.0 g/10 min melt index improves throughput on cast film equipment, whereas lower melt index grades may retain higher dart and tear strength in application. Published data for this specific configuration is limited to supplier typical property sheets and converter trial reports, so final substitution decisions are made on the converter’s own film-testing equipment.
If the grade is supplied without slip and antiblock additives, coefficient of friction and blocking behaviour are governed by the converter’s incorporation of erucamide, oleamide, silica, or talc masterbatches. Migration of slip agents to the film surface is time- and temperature-dependent; coefficient of friction is measured under ASTM D1894 after conditioning for at least 24 h at 23 °C and 50% relative humidity. Blocking force is evaluated under ASTM D3354; inadequate antiblock can produce reel blocking on production winders, especially with polished chill rolls and high winding tension. Corona treatment levels are measured by wetting tension under ASTM D2578; typical values for downstream printing and lamination fall between 38 dyn/cm and 42 dyn/cm, but the required level depends on ink, adhesive, and lamination process. The base resin does not inherently provide these surface values; converter trials are required to establish additive loadings and treatment set points.
For food-contact applications, regulatory documentation supplied with the commercial resin references FDA 21 CFR 177.1520 as an olefin polymer; compliance under this regulation is use-condition dependent and must be confirmed for the final article. For European food-contact use, final films are evaluated according to EU Regulation 10/2011 and applicable migration testing standards such as EN 1186; overall migration limits are not automatically guaranteed by resin selection because conversion aids, additives, and coextruded layers influence the final result. The resin should be stored indoors to avoid condensation; if surface moisture is observed after storage in high-humidity conditions, drying should be conducted at low temperature to prevent pellet agglomeration. Processing temperatures above 315 °C or extended residence times at high shear can cause thermal degradation, cross-link gel formation, and surface defects in cast film. Equipment purges and shutdown procedures should follow the producer’s technical bulletin. The product is not a universal drop-in replacement for all LLDPE grades; film performance is governed by the interaction of melt index, density, comonomer distribution, quench conditions, and additive package. Published data for this specific product in specialty structures remains limited, so production qualification on site is required before commercial conversion.