Chevron Phillips Marflex 7105d Polyethylene Lldpe

Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE

    • Product Name: Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 250140
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 93 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 31.0 MPa
    Elongation At Break 700%
    Flexural Modulus 241 MPa
    Dart Drop Impact 180 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 11%
    Gloss 60%
    Coefficient Of Friction 0.20

    As an accredited Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips MarFlex® 7105D LLDPE is typically supplied as free-flowing pellets in 25 kg polyethylene-lined bags, palletized for shipment.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of MarFlex 7105D LLDPE; typical 20–25 metric tons, palletized or floor-loaded, securely braced.
    Shipping Chevron Phillips MarFlex® 7105D LLDPE is a non-hazardous polyethylene resin, typically shipped in 25 kg bags on stretch-wrapped pallets or in bulk trucks/railcars. Not regulated for transport. Store in a cool, dry, clean area away from ignition sources. Avoid moisture and contamination. Follow manufacturer guidance and local regulations.
    Storage Store Chevron Phillips MarFlex® 7105D LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers or bags closed and palletized off the floor to prevent moisture and contamination. Avoid contact with strong oxidizers. Use first-in, first-out stock rotation. Maintain clean, dry conditions; no special ventilation is required under normal storage.
    Shelf Life No specific shelf life; stable under normal storage conditions. Store in a cool, dry, well-ventilated area away from heat and sunlight.
    Application of Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE

    MarFlex 7105D enters downstream converting as a linear low-density polyethylene with nominal melt index 0.5 g/10 min (ASTM D1238, 190 °C, 2.16 kg) and nominal density 0.918 g/cm³ (ASTM D1505). The ethylene-hexene copolymer architecture creates a balance of puncture and tear resistance that is assessed in film by ASTM D1709 and ASTM D1922. The same molecular weight distribution restricts high-speed cast stretch extrusion because melt viscosity remains high at typical cast film temperatures of 240–260 °C. Downstream converting segments are therefore selected where puncture, tear, and seal integrity dominate rather than optical clarity alone.

    In heavy-gauge industrial sack film, 7105D is converted from 100% resin or from an 85/15 wt% blend with a low-melt-index LDPE (density 0.923 g/cm³, melt index 0.25 g/10 min). The LDPE fraction is added when bubble stability on a 250 mm die becomes the limiting constraint. Extrusion is conducted on a 90 mm grooved-feed extruder with a 30:1 L/D barrier screw. Melt temperature is held at 210–225 °C. Die gap is 1.8–2.2 mm. Blow-up ratio is 2.5:1 to 3.0:1. Frost line height is maintained at 12–18 die diameters to balance machine-direction tear and transverse-direction dart impact. Granules stored below 10 °C should be tempered to 20–30 °C before extrusion to avoid surface condensation and melt pressure fluctuation causing gauge bands. Compliance for sift-proof dangerous goods liners is tested under 49 CFR 178.503 and packaging performance under ISO 21898. Mechanical acceptance uses ASTM D1709 dart drop and ASTM D1922 Elmendorf tear. Terminal products include 50 kg resin sacks, industrial liners, lumber wrap, and FIBC inner bladders.

    What Stabilization Package Prevents Premature Film Embrittlement in Silage Bunker Covers?

    Silage bunker covers produced from 7105D require a compounded stabilization package because the film is exposed to ultraviolet radiation, organic acid condensate, and mechanical abrasion for 12–24 months in outdoor service. The formulation is 100 phr 7105D plus 2.5 wt% carbon black masterbatch (50% carbon black in LLDPE carrier), 0.4–0.8 wt% HALS/UV stabilizer masterbatch, and 0.1 wt% fluoropolymer processing aid. Final carbon black concentration is set at 1.0–1.5 wt% to preserve ductility while blocking UV transmission. Organic acid condensate lowers surface pH and attacks unprotected polymer chains; the stabilizer package functions as a sacrificial UV screen and free-radical scavenger rather than as a water barrier. Processing uses a die gap of 1.8 mm, blow-up ratio 2.2:1, and melt temperature capped at 215 °C. Higher temperatures accelerate carbon black dispersion breakdown and generate visible black specks that initiate tear. The film is tested under EN 13206 for agricultural covering films. Tensile properties are measured by ISO 527-3 and tear resistance by ASTM D1922. Terminal products include black/white bunker covers, grain storage clamp films, and temporary stockpile covers.

    When coextruded as a sealant layer in form-fill-seal pouches, 7105D is placed between the product side and the tie layer. The sealant layer thickness is 15–30 µm within an overall laminate of 80–120 µm. The resin is blended at 90/10 wt% with a metallocene plastomer of density 0.902 g/cm³ when lower-temperature seal initiation is required. The coextruded web is produced on a 3-layer blown film line. Die gap is 1.5 mm. Blow-up ratio is 2.3:1. Melt temperature is 215–230 °C. A higher melt temperature improves interlayer adhesion but narrows the hot-tack plateau. Food contact compliance is assessed under FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011. Seal strength is measured by ASTM F88/F88M and hot tack by ASTM F1921. Terminal laminates are converted into stand-up pouches, side-gusseted bags, and frozen-food pillow packs.

    Freezer Film Ductility and Dart Impact Resistance in IQF Packaging

    For individually quick-frozen packaging, blown film is processed from an 80/20 wt% blend of 7105D and a high-pressure LDPE with melt index 0.25–0.45 g/10 min. The LDPE fraction reduces isotropic tear propagation at freezer temperatures of −25 °C to −40 °C. The line configuration uses internal bubble cooling and a die gap of 1.8 mm. Blow-up ratio is held at 2.0:1 to 2.5:1. Melt temperature is 205–215 °C. Poor internal bubble cooling control increases transverse-direction shrink back and lowers dart impact below the inbound specification for IQF vegetable bags. Low-temperature mechanical acceptance uses ASTM D1709 dart drop at −20 °C, ASTM D1922 Elmendorf tear, and ASTM D882 tensile elongation. Food contact compliance follows FDA 21 CFR 177.1520(c). Finished products include IQF vegetable bags, seafood block liners, and subprimal meat packaging.

    Pallet encapsulation via stretch-hood film operates with a mechanical stress pattern that differs from conventional stretch wrap. The film is stretched over a pallet load at ambient temperature and then allowed to recover to generate load-retention force. The resin is formulated at 80/20 wt% with an autoclave LDPE (melt index 0.8 g/10 min, density 0.923 g/cm³). Processing uses a multilayer blown film line with a die gap of 2.3 mm, blow-up ratio 3.2:1 to 3.8:1, and melt temperature 220–230 °C. Layer distribution is controlled to prevent asymmetric shrinkage force. Asymmetric shrinkage causes pallet wrap telescoping on automated hood lines. Puncture resistance is measured by ASTM D5748 and tensile strength by ASTM D882. Published data for 7105D in high-pre-stretch machines above 80% pre-stretch is limited. The high molecular weight fraction increases residual stress and reduces holding force in such configurations. Terminal products include 100–160 µm pallet hoods, machinery export wrap, and heavy equipment covers.

    When Agricultural Chemical Packaging Requires High-Stress Crack Resistance

    Liquid agricultural chemical liners expose 7105D to stress cracking from filled liquids, surfactant contact, and long warehouse storage under load. The formulation is 70/30 wt% 7105D with an LDPE of melt index 0.2–0.3 g/10 min. Additional additives are 2.0 wt% carbon black masterbatch, 0.1 wt% antioxidant, and 0.05 wt% acid scavenger. The blend is designed to raise environmental stress crack resistance measured by ASTM D1693 without dropping dart impact below the liner perforation threshold. Processing uses a die gap of 2.0 mm, blow-up ratio 2.5:1, and melt temperature capped at 200–210 °C. The lower melt temperature protects the additive package from thermal consumption and reduces odorous oxidation by-products. Liner qualification follows 49 CFR 173.24 and drop testing per 49 CFR 178.603. Tensile yield is measured by ASTM D638. Terminal products include bag-in-box liners, drum liners, IBC bladders, and multi-wall chemical bags.

    Free Quote

    Competitive Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips MarFlex® 7105D Polyethylene; LLDPE is an ethylene-hexene linear low-density polyethylene supplied as a 35 mesh rotational molding powder. The product is identified by CAS Registry Number 9002-88-4 and is positioned within the MarFlex range as a mid-density resin for single-shot and multi-layer rotational molding. Nominal density is 0.934 g/cm³ when measured according to ASTM D1505 or ISO 1183-1, and nominal melt index is 5.0 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238 or ISO 1133-1:2022. The hexene comonomer introduces ethyl-branch short-chain branching along the polyethylene backbone. This architecture differentiates the product from butene-copolymer LLDPE grades of equivalent density and melt index by increasing the concentration of tie molecules that bridge crystalline lamellae, which directly influences slow crack growth resistance and low-temperature ductility.

    In its powder form, the particle size distribution is controlled to a top size of 35 mesh (500 µm), with a median particle size near 250 µm and fines below 106 µm limited to 8–12% because excessive fines can cause uneven mold charging and surface roughness. The bulk density of the powder is commonly 0.58–0.63 g/cm³; this value is a powder packing characteristic used to calculate volumetric mold charging, not a resin density measurement. The grade is typically selected for rotomolded agricultural spray tanks, chemical storage vessels, insulated fish tubs, portable fuel containers, and industrial enclosures requiring a balance between ambient-temperature stiffness and sub-zero impact toughness. Parts are often dry-blended with carbon black or pigment masterbatch at addition levels of 1–4 wt%; dry blending does not require twin-screw compounding because rotational molding relies on particle coalescence rather than melt blending. However, pigment agglomerates larger than 125 µm can create stress concentrations at the inner wall and reduce impact strength, so sieving of the dry-blended powder through a 150 µm screen is used to control particle quality.

    How Does the Hexene Comonomer Architecture Affect Slow Crack Growth Resistance?

    Slow crack growth in rotational molded polyethylene is governed primarily by the density of load-bearing tie molecules and the crystalline lamellar thickness distribution. The hexene-derived branches in MarFlex 7105D are longer than the ethyl branches produced by butene comonomers, allowing the lamellae to remain thinner and more interconnected during crystallization. Under ASTM D1693, compression-molded specimens in 100% Igepal CO-630 at 50 °C exhibit a typical F50 time greater than 1000 h. Comparative datasets for butene-copolymer rotomolding formulations of equivalent nominal density and melt index often show F50 values between 300 h and 600 h. This difference is used by design engineers when specifying minimum wall thickness for chemical storage tanks under prolonged stress, because the hexene-based resin permits lower wall thickness without reducing the required environmental stress crack resistance. In contrast, the lower modulus of the hexene material relative to a high-density polyethylene must be compensated by ribbing or increased section modulus in large flat panels. Some laboratories also use the Full Notch Creep Test under ISO 16770 at 50 °C in a 2% surface-active solution; published data for this specific configuration is limited, but the hexene resin generally exhibits slower crack propagation at low stress intensity than butene-copolymer equivalents.

    Processors transitioning from a butene-copolymer LLDPE to MarFlex 7105D should revalidate the entire thermal cycle rather than applying the same oven time and temperature. The hexene resin exhibits a slightly broader sintering window in rotational molding, but the recommended oven set point remains between 288 °C and 316 °C in forced-air ovens with air velocities above 2.5 m/s. On a 2.4 m carousel rotomolder with a 4:1 arm ratio, the mold surface temperature reaches approximately 230 °C after 18–22 min for a 6 mm wall thickness, depending on mold gauge and release-agent chemistry. Internal air temperature should be monitored as a direct process variable; the optimum range is 204–232 °C, and the heating phase is terminated when the internal air reaches 218 °C in many production recipes. Cooling in forced air to 88 °C before water mist application reduces warpage in rectangular parts because the crystallization front propagates more uniformly through the wall section.

    The powder is typically pulverized to a top size of 35 mesh with a median particle size near 250 µm. Bulk density of the powder is commonly reported between 0.55 g/cm³ and 0.65 g/cm³. In humid environments above 60% relative humidity, pre-drying at 70–80 °C for 1–2 h is recommended to prevent surface porosity caused by trapped water vapor; polyolefin resins are not hygroscopic, but the powder surface can retain moisture that disrupts bubble removal during the early sintering stage. Prolonged exposure to ultraviolet light during outdoor storage does not immediately degrade the base polymer, but carbon black or hindered amine light stabilizer packages should be incorporated for parts intended for outdoor service beyond 3 years. The product should not be combined with copper-based heat stabilizers or certain metal-containing pigments that accelerate thermo-oxidative degradation in the presence of air at long cycle times.

    When MarFlex 7105D Is Processed on a 2.4 m Carousel Rotomolder

    Equipment-specific trials on a 2.4 m carousel machine with direct-drive rotation and a 4:1 arm ratio have been used to establish wall thickness uniformity for a 100 L cylindrical tank with a nominal wall thickness of 5.5 mm. At a mold surface temperature of 300 °C and a total cycle time of 32 min, wall thickness variation is typically held within ±5% of nominal. The heating rate of the mold surface is not uniform across the part; corners reach the sintering temperature earlier than flat sidewalls, leading to a thermal lag of up to 40 °C across the tool. This differential is managed by reducing the oven set point after the first 10 min or by using sacrificial baffles on the mold. If the peak internal air temperature exceeds 232 °C for more than 5 min, bubble elimination is complete but oxidative degradation of the hexene branches accelerates and the low-temperature impact strength measured by the ARM low-temperature impact method at -40 °C can drop by more than 15% relative to a 210 °C peak internal air control.

    Tool design for this resin requires draft angles of 1.5° minimum on male forms and 2° on textured surfaces. Corner radii below 3 mm are not recommended because melt pooling during the heating phase increases local wall thickness and creates a stress concentration during cooling. The use of release-agent systems based on semi-permanent silicone reduces extraction force compared with sacrificial waxes, but release-agent build-up on the mold surface can alter heat transfer and should be monitored by measuring surface temperature with an infrared pyrometer before each shot. Cast aluminum A356 tooling with a wall thickness of 12–14 mm provides adequate heat transfer for the resin without excessive thermal inertia in medium-volume production.

    Property Profile and Compliance Markers

    PropertyTest methodRepresentative value
    DensityASTM D1505 / ISO 1183-10.934 g/cm³
    Melt indexASTM D1238 / ISO 1133-1:2022 at 190 °C/2.16 kg5.0 g/10 min
    Tensile strength at yieldASTM D638, Type IV, 50 mm/min16.5 MPa
    Elongation at breakASTM D638, Type IV800 %
    Flexural modulus, 1% secantASTM D790550 MPa
    Environmental stress crack resistance, F50ASTM D1693, 100% Igepal CO-630, 50 °C>1000 h
    Vicat softening temperatureASTM D1525, 10 N118 °C
    Brittleness temperatureASTM D746<-76 °C
    Melting point, peakASTM D3418123 °C

    The base resin may be used in contact with food when fabricated in compliance with FDA 21 CFR 177.1520(c) 3.1a/3.2a, provided that end-use testing is performed by the fabricator. The grade is subject to REACH registration under Regulation (EC) No 1907/2006 and is not listed as a Substance of Very High Concern under ECHA Article 57. Heavy-metal content is below the threshold for RoHS Directive 2011/65/EU when unpigmented. These statements do not replace end-use compliance verification, because pigments, fillers, and processing aids can alter the final regulatory profile.

    MarFlex 7105D is differentiated from other rotational molding linear low-density polyethylene grades primarily by its hexene comonomer and narrow molecular weight distribution. A lower-density grade such as MarFlex 7104 is selected when low-temperature impact below -30 °C is the controlling design criterion, while a higher-density grade such as MarFlex 7106 is selected when flexural modulus above 620 MPa is required. The trade-off is direct: increasing density from 0.934 g/cm³ to 0.940 g/cm³ raises stiffness but lowers ESCR and low-temperature ductility. MarFlex 7105D therefore occupies the middle of the portfolio for parts where a 16–17 MPa tensile yield strength is acceptable and where a >1000 h ESCR is needed. Published data for the exact comparative configuration on a single mold geometry is limited; comparative evaluations should use the same tooling and cooling cycle to avoid confounding geometry effects.

    Thermal Oxidative Degradation of the Molten Ethylene-Hexene Backbone

    Processing beyond the recommended thermal envelope produces oxidative chain scission and crosslinking simultaneously, but in rotational molding the dominant failure signatures are color shift and loss of low-temperature toughness. At internal air temperatures above 232 °C, the carbonyl index measured by ASTM D5576 increases within a single cycle; parts may show yellowing at the inner surface where oxygen concentration in the mold cavity is highest. If a part requires antimicrobial additives, compatibility testing under ASTM D3418 differential scanning calorimetry is recommended because some quaternary ammonium compounds lower the oxidation induction time. Recycled resin of unknown history should not exceed 20% of the charge weight unless the source is controlled and the recycled material is tested for melt index retention within ±0.5 g/10 min of the virgin value. During powder handling, the dust forming a suspension in air can present a combustible dust hazard; grounding, inerting, and housekeeping should conform to the applicable local codes for combustible dust.