| HS Code | 310097 |
| Density | 0.918 g/cm³ |
| Melt Index | 0.50 g/10 min |
| Melting Point | 121 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Dart Drop Impact | 250 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 12% |
| Gloss 45 | 55 |
| Coefficient Of Friction | 0.20 |
As an accredited Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin supplied in 25-kg polyethylene bags, 55 bags per pallet, stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL loaded: 16 pallets, 880 bags x 25 kg, 22,000 kg net Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin. |
| Shipping | Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin ships as non-hazardous solid pellets, typically in 25 kg polyethylene bags on stretch-wrapped pallets or in bulk trucks/railcars. Store dry, away from heat, sunlight, and moisture. Secure loads for transport and follow the SDS and local regulations. |
| Storage | Store Dynex™ D605C3 resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original containers or bags closed and palletized to prevent contamination and moisture pickup. Avoid excessive stacking and protect from physical damage. Follow the manufacturer’s SDS and local regulations for safe storage. Use first-in, first-out stock rotation. Inspect containers regularly. |
| Shelf Life | Shelf life is typically 12 months from date of manufacture when stored unopened in original packaging in a cool, dry area. |
Washed and trimmed ready-to-eat spinach, rocket, and mixed-leaf salads are sealed on vertical form-fill-seal equipment in film webs that require a balance of tear resistance, low-haze optics, and consistent hot-tack at dwell times below 0.4 s. Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin is used as the primary body layer at 100 wt% in monolayer structures or at 80–90 wt% in the core layer of three-layer coextrusions with LDPE or metallocene LLDPE in the skin layers; antiblock is added at 0.3–0.8 wt% and slip additive at 0.05–0.15 wt% based on total layer weight. Formula addition ratios are adjusted downward when perforation equipment is used, because surface bloom from excess slip reduces hole edge cleanliness and increases smear on cutting pins. Food-contact compliance follows FDA 21 CFR 177.1520(c) 3.2(a) for olefin polymers and EU No 10/2011 with an overall migration limit of 10 mg/dm² under simulated raw fruit and vegetable contact. The downstream process uses a single-screw extruder with L/D 30:1, die gap 1.8–2.2 mm, blow-up ratio 2.0:1–2.5:1, melt temperature 190–210°C, and frost line height maintained at 4–7 times the die diameter to stabilize bubble geometry without excessive crystallinity. Micro-perforation is performed inline after haul-off using 0.5 mm pins at hole spacing of 30–50 mm in both machine and transverse directions, producing a target oxygen transmission rate of 2,000–6,000 cm³/(m²·day·bar) for respiration control in cut-leaf produce. Terminal products include 142 g, 284 g, and 454 g pillow pouches for baby spinach, mixed leaf, and broccoli florets, with seal strength validated to 1.2–1.8 N/15 mm per ASTM F88/F88M-21 and dart impact to 120–180 g per ASTM D1709A at 20–25 µm film thickness.
Industrial liners used in flexible intermediate bulk containers for carbon black, polymer granules, and non-hazardous mineral fillers must survive fill shock, pallet vibration, and truck transport without splitting. D605C3 is incorporated at 65–85 wt% with 15–35 wt% LDPE or reclaimed LLDPE to raise melt strength while retaining low-temperature ductility. The addition ratio is constrained by a documented performance cliff: when LDPE content exceeds 30 wt% and film thickness drops below 80 µm, dart impact resistance measured by ASTM D1709A falls below 400 g, and field failure rates in filled FIBC liners increase at side-seal folds. The formulation may also contain 0.5–1.0 wt% processing aid and 0.3–0.6 wt% antiblock; reclaimed material should not exceed 20 wt% unless impact performance is revalidated on the actual blowing line. Regulatory compliance for non-food industrial packaging does not require FDA clearance, but the outer FIBC system is tested under UN 13H3 or UN 13H4, and the internal liner contributes to the package performance under drop, stacking, and vibration tests according to UN 6.1.5.2. The film is produced on a high-output blown film line with die diameter 250–400 mm, die gap 2.4–3.0 mm, blow-up ratio 1.8:1–2.2:1, melt temperature 205–230°C, and throughput of 300–500 kg/h. Internal bubble cooling and oscillating haul-off are required to distribute gauge variation and prevent drumhead formation that can initiate tear propagation along the layflat edge. Terminal products include 80–120 µm layflat tube liners for FIBCs of 90 cm × 90 cm × 120 cm, as well as gusseted liners for corrugated bulk bins. Published certificate data for D605C3 in this specific down-gauged formulation is limited; the matrix below summarizes representative industrial LLDPE/LDPE blown film values rather than manufacturer-specific certification figures.
| Blend ratio D605C3/LDPE (wt%) | Film thickness (µm) | ASTM D1709A dart impact (g) | ASTM D5748 puncture (N) | ASTM D1922 tear MD (gf) |
|---|---|---|---|---|
| 80/20 | 90 | 620–700 | 85–95 | 650–720 |
| 70/30 | 80 | 520–580 | 70–78 | 580–640 |
| 60/40 | 70 | 440–490 | 58–66 | 500–560 |
The critical operational boundary on high-output extrusion is frost line control. When frost line height is below 3 times the die diameter, surface haze increases and the film develops a coarse crystalline morphology that reduces dart impact by an additional 8–12%. When the frost line is pushed above 7 times the die diameter to improve optics, bubble stability decreases under warehouse air currents, and gauge variation exceeds ±6% across the layflat, creating thin bands that fail preferentially during side-seal folding. These limits define the practical downgauging window for D605C3 in heavy-duty liner applications.
In agricultural bale wrapping and silage bag production, the film is deployed under tensile stress from bale compressors and must resist puncture from corn stalks and coarse grass stems. Three-layer black/white silage films use D605C3 in the white reflective layer at 97.5–99.0 wt% with 1.0–2.5 wt% UV masterbatch; the black layer contains 2.0–3.0 wt% carbon black masterbatch and 0.5–1.0 wt% processing aid. Titanium dioxide masterbatch is added at 6–8 wt% to the white layer to achieve opacity and solar reflectance. Compliance follows EN 13207:2018 for silage thermoplastic films and tubes, and weathering resistance is screened under ISO 4892-2 ultraviolet exposure with retained elongation measured by ISO 527-3:2018. The downstream process runs a three-layer coextrusion line with die gap 2.0–2.4 mm, blow-up ratio 2.5:1–2.8:1, melt temperature 200–220°C, and layflat width up to 1,500 mm. Film thickness is held at 25–40 µm, with the higher end specified for wrapped bales stored on rough stubble ground. Terminal products include 750 mm × 1,500 m bale wrap rolls and 1,500 mm × 50 m silage bags. The film is not an oxygen-barrier structure; silage fermentation depends on rapid oxygen consumption by aerobic bacteria after baling, and the resin’s mechanical contribution is puncture resistance, cling consistency, and UV durability over a 12–18 month storage cycle.
Flexible sterile barrier pouches for syringes, catheters, and wound care dressings use a heat-sealable film web laminated to medical-grade paper or uncoated Tyvek 1073B. D605C3 is processed as the sealant layer at 100 wt% or as 90 wt% D605C3 with 10 wt% metallocene LLDPE to widen the seal temperature range without reducing seal strength. The blown film sealant web is produced at 30–50 µm thickness with die gap 1.6–2.0 mm, blow-up ratio 2.2:1–2.5:1, melt temperature 185–200°C, and a clean-room-compatible pellet feed system to limit particulate contamination. The extruded web is then adhesive-laminated to the porous substrate at line speeds of 100–150 m/min and cured at 40–50°C for 3–5 days before slitting. This construction requires that the sealant film forms a continuous, non-porous barrier while the porous face permits sterilant ingress. Compliance is governed by ISO 11607-1:2019 for seal integrity and microbial barrier design, with material biocompatibility evaluated under ISO 10993-5:2009 for cytotoxicity and ISO 10993-10:2010 for irritation. Seal strength is measured under ASTM F88/F88M-21 with a minimum acceptable value of 1.5 N/15 mm width, and dye penetration is checked according to ASTM F1929-15 for channels along the seal. Terminal products include 90 mm × 250 mm and 110 mm × 300 mm pouches for ethylene oxide or gamma sterilization, with shelf-life stability documented by accelerated aging at 55°C for 90 days.
| Control point | Standard / method | Typical acceptance criterion |
|---|---|---|
| Heat seal strength | ASTM F88/F88M-21 | ≥1.5 N/15 mm |
| Dye penetration | ASTM F1929-15 | No channel penetration |
| Cytotoxicity | ISO 10993-5:2009 | No cytotoxic effect |
| Microbial barrier of porous face | ASTM F1608-16 | Log reduction per validated protocol |
The primary operational boundary in medical web conversion is seal-temperature drift. The seal window for a 50 µm D605C3 sealant web laminated to Tyvek 1073B typically lies between 95°C and 125°C at 0.5 s dwell. Below the lower limit, peel-mode seal strength drops below 1.0 N/15 mm, and above the upper limit the seal may distort and produce visual channel defects under ASTM F1886/F1886M-16. Fourier-transform infrared inspection of converted film is used to confirm that slip additive concentration in the sealant layer does not exceed 0.15 wt%, because migration above this level can reduce surface energy and compromise adhesive lamination to the porous substrate. Batch-to-batch variance in seal initiation is controlled by limiting melt index drift to ±0.10 g/10 min measured by ISO 1133-1:2022.
Blast-frozen vegetables, individually quick-frozen seafood, and 1–5 kg ice cube bags are filled at −10°C to −30°C ambient conditions where film must retain seal integrity after frost contamination on the seal area. D605C3 is used at 100 wt% in monolayer structures or at 85 wt% with 15 wt% LDPE to increase downstream packaging stiffness. Slip additive is added at 0.1–0.2 wt% and antiblock at 0.5–1.0 wt%. Food-contact compliance falls under FDA 21 CFR 177.1520(c). Conversion takes place on vertical form-fill-seal lines at 30–80 bags/min with melt temperature 190–210°C, blow-up ratio 2.0:1–2.5:1, and die gap 1.8–2.2 mm. Terminal products include 0.5 kg, 1 kg, 2.5 kg, and 5 kg pillow bags for frozen peas, shrimp, and ice cubes. Published data for D605C3-specific impact behavior below −30°C is limited, so conversion trials should validate dart impact under ASTM D1709B and seal strength under ASTM F88/F88M-21 before release.
Stretch hood pallet films are extruded on high-stalk blown film lines where the bubble is allowed to rise 8–12 times the die diameter before frost line, producing high machine-direction orientation and elastic recovery. D605C3 is used in the core layer at 70–85 wt% with 15–30 wt% metallocene LLDPE or LDPE, while outer skins contain slip from 0.2–0.5 wt% and antiblock from 0.5–1.0 wt% respectively. The die gap is 2.2–2.6 mm, blow-up ratio 3.5:1–4.0:1, melt temperature 195–220°C, and internal bubble cooling is used to stabilize high-stalk geometry; output rates are typically 250–320 kg/h on 250 mm die equipment. Compliance for elastic recovery and puncture follows ASTM D5459 and ASTM D5748, with a target machine-direction elastic recovery of greater than 78% at 50% stretch after 60 s relaxation. Terminal products are 900–1,200 mm layflat hoods at 60–90 µm thickness for automatic stretch hood machines securing pallets of bagged chemicals, beverage crates, and building materials. The operating boundary is that high-stalk height exceeding 12 times die diameter may induce bubble instability under high ambient air humidity, and recycled content above 15 wt% is not recommended because thickness variation above ±4% reduces on-pallet load retention and increases the frequency of hood breakage during insertion by automatic applicators.
Competitive Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Dynex™ D605C3 Enhanced LLDPE Blown Film Resin is classified as a pelletized linear low-density polyethylene for monolayer and coextruded blown film. Incoming resin acceptance is typically based on melt mass-flow rate under ASTM D1238 at 190 °C with 2.16 kg and on density under ASTM D1505 or ISO 1183-1. The grade is positioned for applications in which a conventional butene-based LLDPE fails either in dart impact, Elmendorf tear propagation, or seal-abuse resistance. Film property statements for D605C3 are meaningful only when tied to a stated blow-up ratio, die gap, frost line height, and film thickness because the same resin can produce different orientation levels on high-stalk versus low-stalk bubbles.
Lot release for this product normally reports melt mass-flow rate and density on pellets, not film property values. Film property values are fabricator-dependent and are produced on the supplier’s reference line at a specified thickness, die diameter, die gap, and blow-up ratio. Because D605C3-specific property values are not universally fixed, procurement specifications should reference the version number of the supplier’s technical data sheet and the end-use film specification. Published data for this specific configuration is limited; therefore, structural performance must be confirmed on the end-user’s line rather than inferred from a generic resin class.
| Property | Test method | Condition or reporting basis | Inspection purpose |
|---|---|---|---|
| Melt mass-flow rate | ASTM D1238 / ISO 1133-1:2022 | 190 °C, 2.16 kg | Comparison to supplier lot-release interval |
| Density | ASTM D1505 / ISO 1183-1 | 23 °C | Classification and stiffness control |
| Moisture content | ASTM D6869 or coulometric Karl Fischer | Pellets at hopper feed | Detection of porosity-causing surface water |
| Ash residue | ASTM D5630 / ISO 3451-1 | Ignition at stated temperature | Inorganic antiblock or processing aid content |
| Pellet bulk density | ASTM D1895 | 23 °C | Feed hopper and conveying behavior |
| Oxidative induction time | ASTM D3895 / ISO 11357-6 | Differential scanning calorimetry | Antioxidant package integrity after storage |
For blown film processors, the first machine-specific variable to establish is the melt temperature profile. Melt temperatures in the range 180 °C to 230 °C measured at the adapter are common starting points for enhanced LLDPE grades of this type, depending on extruder size, screw geometry, and output demand. A die gap of 1.5 mm to 2.5 mm and a blow-up ratio from 2.0:1 to 2.5:1 are frequently used for LLDPE film production. When the bubble is operated in high-stalk mode, the frost line is raised to control the point at which the film reaches full crystallinity under directional stress. These are line-setup baselines, not product-specific acceptance limits, and require adjustment against bubble stability, film property targets, and winder appearance.
At equal melt index and density, an LLDPE made with a C6 or C8 comonomer typically shows higher Elmendorf tear and dart impact than a C4-based resin because the longer side branches are more effective at coupling crystalline regions across the amorphous phase. D605C3 is supplied as an enhanced grade; if the supplier’s technical data sheet confirms a higher alpha-olefin comonomer, the resulting film may allow down-gauging relative to butene LLDPE in heavy-duty packaging, provided that the converter verifies edge-fold tear and seal strength under the intended packing line conditions. Published data for this specific configuration is limited, so down-gauging behavior should not be assumed without a trial. The comparison should include dart impact by ASTM D1709, Elmendorf tear by ASTM D1922, and tensile properties by ASTM D882, all measured on films of identical thickness and orientation history.
Replacing high-pressure LDPE with D605C3 in a blown film blend changes bubble mechanics. LDPE contributes long-chain branching and strain-hardening melt extension, whereas LLDPE contributes higher solid-state toughness but lower melt elasticity at equivalent melt temperature. Blending 10–30 wt% LDPE is a common approach to stabilize the bubble and improve optics; the exact ratio is set by the end-use specification for tear, secant modulus, and seal initiation. In comparison with metallocene LLDPE, the enhanced grade may exhibit broader molecular weight distribution and improved extrusion stability on older equipment, but may produce higher gel counts if the melt is held outside its thermal stability window for extended periods.
A die gap below 1.2 mm can raise shear stress at the lip and cause melt fracture or sharkskin on a high-output LLDPE film line. A die gap above 2.5 mm can reduce orientation and require a higher post-die draw to reach the same film thickness, altering tear balance between machine direction and transverse direction. On grooved-feed extruders with barrel length-to-diameter ratios of 30:1 to 38:1, screw speed and backpressure are balanced to avoid melt temperatures above 250 °C, above which oxidation gel counts are known to increase in LLDPE film products. Frost line height is normally adjusted between 8 and 12 die diameters for high-stalk LLDPE operation; lower frost lines reduce orientation and improve tear balance, while higher frost lines decrease haze but can destabilize the bubble if the air ring is not adjusted accordingly.
Film obtained from D605C3 should be conditioned at 23 °C and 50% relative humidity for at least 40 h before mechanical testing according to ASTM D618. Dart impact resistance is measured by ASTM D1709 method A or B, depending on the expected failure weight. Elmendorf tear is measured by ASTM D1922, and tensile properties are measured by ASTM D882 at a crosshead speed of 500 mm/min. Seal initiation temperature is typically evaluated on a laboratory heat sealer with dwell time of 0.5 s and pressure of 0.28 MPa, followed by peel testing under ASTM F88. These conditions must be reported with every property value because heat seal failure modes change from interfacial peel to tearing above the seal plateau, and comparisons without identical sealing history are invalid.
The optical performance of enhanced LLDPE is generally lower than that of LDPE or metallocene LLDPE when measured by haze under ASTM D1003 and by gloss at 60° under ASTM D2457. In coextruded structures, the outer layers may be formulated with LDPE or metallocene LLDPE to retain clarity while the core uses D605C3 for stiffness and tear resistance. Haze values are strongly affected by die gap, cooling rate, and film thickness; therefore, a haze value from a different fabrication line should not be applied to a new structure without trial verification. The product should not be processed above the supplier’s stated maximum melt temperature, and additive packages containing certain amine-based species should be screened before use because interactions with primary antioxidants can shift oxidative induction time and generate color bodies during high-temperature extrusion.
Regulatory compliance for food-contact uses, if required, must be verified against FDA 21 CFR 177.1520 for olefin polymers and the current Commission Regulation (EU) No 10/2011 and its amendments. The supplier should confirm that the grade and its additives meet the applicable positive lists for the intended food type and migration conditions. REACH registration and RoHS obligations do not apply to the polymer as supplied in every jurisdiction but may become relevant to formulated compounds or finished articles; downstream users should not infer compliance without the supplier’s written declaration for the specific grade and packaging structure.