Chevron Phillips Dynex D605a6 Enhanced Lldpe Blown Film Resin

Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin

    • Product Name: Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 843643
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 101 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Tensile Strength At Break Md 37.9 MPa
    Tensile Strength At Break Td 33.1 MPa
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 200 g
    Haze 11 %
    Gloss 45 55 %
    Coefficient Of Friction 0.2

    As an accredited Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene bags, 55 bags per pallet, totaling 1,375 kg per pallet for safe transport.
    Container Loading (20′ FCL) 20′ FCL: Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin—palletized 25 kg bags, shrink-wrapped, secured; approx. 20 MT net.
    Shipping Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin is shipped as non-hazardous, free-flowing pellets in 25-kg bags, 500–1,000-kg bulk bags, or bulk trucks/railcars. Keep containers closed, dry, and away from heat or contamination. Palletized loads are secured for truck, rail, or container transport.
    Storage Store Chevron Phillips Dynex™ D605A6 in a cool, dry, well-ventilated, indoor area in original, tightly closed containers. Keep away from direct sunlight, heat, moisture, ignition sources, and incompatible oxidizers. Protect pellets from contamination and moisture absorption. Avoid dust generation and static buildup; use grounding during handling. Maintain first-in, first-out rotation. Follow the manufacturer’s SDS and local storage regulations.
    Shelf Life Shelf life is typically 24 months from manufacture when stored unopened in original packaging, dry, below 50°C, away from direct sunlight.
    Application of Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin

    On blown-film lines producing heavy-gauge industrial liners from 80 µm to 250 µm, Dynex™ D605A6 is used as the primary LLDPE component in monolayer or two-layer structures where dart drop energy and Elmendorf tear resistance are specified by end-users. The formulation addition ratio for heavy-duty sack and liner applications typically ranges from 80–90 wt% D605A6 with 10–20 wt% of a high-pressure LDPE having a melt index of 0.25–0.5 g/10 min at 190 °C/2.16 kg and density of 0.921–0.925 g/cm³; the LDPE fraction is introduced to stabilise the bubble at high blow-up ratios, not to reduce formulation cost. Downstream production uses monolayer blown-film extrusion with a 45–75 mm grooved-feed single-screw extruder, 24:1–30:1 L/D, a Maddock or spiral mixer, and a die gap of 2.0–2.5 mm. Process parameters are commonly set to a melt temperature of 190–210 °C, die temperature of 200–215 °C, blow-up ratio of 2.5:1–3.0:1, and frost-line height of 4–8 die diameters; internal bubble cooling is used when film thickness exceeds 120 µm to remove heat from the stalk and reduce incidence of bubble sag. The critical process conflict is that raising the D605A6 fraction above 90 wt% increases dart impact energy but narrows the stable bubble window on conventional air-ring lines; bubble instability appears as width variation and edge wrinkling before film thickness deviations exceed ±5%. Conversely, increasing LDPE beyond 20 wt% improves bubble geometry but lowers machine-direction tear performance in a measurable step change. Industry compliance for heavy-duty liners intended for bulk solid transport references ISO 21898:2004 for sack drop testing, ASTM D1709-16a for dart impact, ISO 527-3 for tensile properties, and ASTM D1922 for Elmendorf tear; converters supplying UN-certified packaging may also verify leakage resistance under ASTM D3078. Terminal product types include FIBC inner liners, rigid drum liners, box liners, bulk bag liners, and heavy-gauge refuse sacks.

    What Limits Puncture Propagation Energy in Silage and Greenhouse Cover Films?

    Reducing silage cover thickness from 150 µm to 80 µm concentrates stress at bale surface irregularities and makes puncture propagation energy the controlling film property, not tensile yield. In this formulation, Dynex™ D605A6 is let down at 88–92 wt% with a UV-stabilised masterbatch at 8–12 wt%; black silage films use carbon black masterbatch, while greenhouse films use hindered amine light stabiliser packages with light-diffusing minerals. The addition ratio of UV masterbatch is confirmed by ash content and thickness-normalised UV absorbance; poor dispersion at let-down ratios above 12 wt% increases die-lip deposit formation and reduces film burst strength. Downstream production is tubular blown-film coextrusion on a 70 mm grooved-feed extruder with die gap 2.0–2.5 mm, blow-up ratio 2.2:1–3.0:1, frost-line height 3–6 die diameters, and melt temperature 190–205 °C. Wide-width covers are produced with an oscillating haul-off and edge folding; silage wrap is slit to 250 mm or 500 mm rolls for round balers. The key process constraint is that a high-stalk bubble shape reduces tear anisotropy but increases susceptibility to wind-induced bubble movement; production lines with dual-lip air rings and internal bubble cooling show flatter film thickness profiles at BUR 3.0:1. Compliance for agricultural films references EN 13206:2017 for greenhouse covers and EN 13207:2017 for silage films, with tensile testing per ISO 527-3 and tear testing per ISO 6383-2. Terminal product types include round bale silage wrap, clamp silage sheets, greenhouse light-diffusing covers, low tunnel films, and temporary silage pit covers.

    Compliance parameterStandard designationMeasurement equipment / note
    Film thicknessISO 4593Contact micrometer, 0.1 µm resolution
    Tensile propertiesISO 527-3Universal testing machine, 500 mm/min
    Tear resistanceISO 6383-2Elmendorf tear tester
    UV resistance / weatheringEN 13206 specified methodXenon arc or UV-A 340 lamps per standard

    Frozen Food Packaging Sealing Integrity at High Line Speeds

    Where vertical form-fill-seal machines cycle at 90–120 packs per minute, the sealant web is required to exhibit low seal-initiation temperature, high hot-tack strength, and resistance to puncture from sharp frozen product edges. For this application, Dynex™ D605A6 is incorporated into a three-layer coextruded film at 65–85 wt% in the core and skin layers, with 15–35 wt% of a metallocene LLDPE or LDPE-rich blend added to the skin to lower seal initiation. The exact addition ratio is adjusted against seal strength data collected on a laboratory heat-seal tester per ASTM F88 and hot-tack data per ASTM F1921; sealing temperatures below 105 °C are not targeted because low-vicat skin blends can generate blocking during roll storage. Downstream production uses a three-layer blown-film coextrusion line with 1.8–2.2 mm die gap, blow-up ratio 2.0:1–2.5:1, melt temperature 190–210 °C, and corona treatment to 38–42 dyn/cm for lamination or print adhesion. The primary failure mode on high-speed vertical form-fill-seal lines is seal contamination at the cross-seal when product dust deposits on the inner surface; converters compensate by specifying higher seal-bar pressure and verifying seal-through-contamination performance with an ASTM F88 seal-strength test on contaminated film. Food-contact compliance requires FDA 21 CFR 177.1520 for olefin polymers and Regulation (EU) No 10/2011 for EU market films, with overall migration below 10 mg/dm²; processing above 240 °C is avoided because degradation extracts can compromise organoleptic properties. Terminal product types include pillow pouches for frozen vegetables, wicketed bags for frozen seafood, side-gusset bags for frozen fruit, and printed overwrap for frozen meat.

    Compliance areaStandard designationRequired condition
    Food contact monomerFDA 21 CFR 177.1520Olefin polymers for food contact
    EU food contactRegulation (EU) No 10/2011Overall migration limit 10 mg/dm²
    GMPRegulation (EC) No 2023/2006Good manufacturing practice
    Seal strengthASTM F88Seal tester at 200 mm/min

    Because low seal-initiation temperature and high hot-tack strength govern throughput in liquid packaging, Dynex™ D605A6 is dry-blended into sealant webs at 70–85 wt% with 15–30 wt% of a lower-density metallocene LLDPE to shift the seal initiation curve downward without eliminating bubble stability. The downstream production process is two-layer or three-layer blown-film coextrusion on a 50–70 mm extruder with die gap 1.8–2.2 mm, blow-up ratio 2.3:1–2.7:1, and chilled air-ring temperature of 10–15 °C to increase melt strength; edge trim and start-up film are recycled into the core layer at ≤20 wt% to avoid pressure fluctuations and gel counts. The critical constraint is that exceeding 30 wt% metallocene LLDPE in the seal layer lowers melt strength sufficiently to cause draw resonance at high take-off speeds; published data for this specific D605A6 configuration in liquid-pouch sealant webs is limited, so pilot-line seal-curve generation is required before commercial conversion. Compliance references FDA 21 CFR 177.1520 for food-contact webs, Regulation (EU) No 10/2011 for European liquid packaging, and ASTM F2029 for heat-seal strength measurement on finished pouches. Terminal product types include bag-in-box inner liners, liquid pouch films for non-carbonated beverages, and liner films for rigid pails and intermediate bulk containers.

    When E-Commerce Mailer Films Require Puncture Resistance Without Sacrificing Down-Gauging

    E-commerce mailer films converted at 50–80 µm rely on puncture propagation resistance rather than tensile yield because the main field failure is puncture from box edges and conveyor pinch points. Dynex™ D605A6 is formulated at 75–90 wt% with 10–25 wt% recycled LLDPE from internal edge trim; post-consumer recyclate above 25 wt% is not recommended without revalidation because dart impact and Elmendorf tear can fall below distribution-centre performance thresholds. Downstream production uses a high-output single-layer blown film line with a 60 mm grooved-feed extruder, 2.0–2.5 mm die gap, blow-up ratio 2.8:1–3.2:1, and internal bubble cooling; gussetting and inline perforation or self-seal adhesive application follow the primary nip. The process conflict in down-gauging is that reducing film thickness from 80 µm to 50 µm without increasing D605A6 content decreases puncture propagation resistance below the minimum specified by ASTM D5748; conversely, adding too high a fraction of high-molecular-weight LLDPE raises extruder backpressure and can exceed the amp limit on 60 mm extruders. Compliance for e-commerce packaging is driven less by food-contact regulation and more by distribution testing under ISTA 3A and film property testing per ASTM D1709, ASTM D5748, and ASTM D882. Terminal product types include e-commerce mailer outer films, protective furniture bags, document envelopes, and padded mailer skin webs.

    In coextruded lamination sealant webs for stand-up pouches, the requirement is not tensile strength but seal-through-contamination and interlayer peel strength after solventless lamination. Dynex™ D605A6 is used in the sealant layer at 80–100 wt%; when a lower seal-initiation temperature is required, up to 20 wt% of a metallocene LLDPE with a density below 0.915 g/cm³ is added. The film is produced on a three-layer coextrusion line with a 2.0 mm die gap, blow-up ratio of 2.4:1–2.6:1, melt temperature 195–215 °C, and inline corona treatment at 40–44 dyn/cm; lamination is completed on a solventless laminator with 1.5–2.0 g/m² adhesive coat weight. The processing boundary is that 100 wt% D605A6 sealant webs show elevated seal initiation and limited hot-tack plateau compared with a mixed-skin web, so converters running pouch lines above 80 pouches per minute typically qualify the blend through ASTM F88 and ASTM F1921 before full production. Food-contact compliance references FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, with adhesion testing by ASTM F904 for lamination bond strength. Terminal product types include stand-up pouches for dry foods, pet food inner webs, and side-gusset pouch films for granular products.

    Free Quote

    Competitive Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Dynex™ D605A6 Enhanced LLDPE Blown Film Resin is a 1-hexene-based linear low-density polyethylene intended for monolayer and coextruded blown film production. The resin is identified by a nominal density of 0.926 g/cm³ when tested to ASTM D1505 or ISO 1183, and a nominal melt index of 0.6 g/10 min when tested to ASTM D1238 or ISO 1133 at 190 °C under a 2.16 kg load. These values are typical lot averages rather than contractual release limits, and the certificate of analysis governs each shipment. D605A6 differs from conventional butene-based LLDPE of equivalent melt index and density through its 1-hexene comonomer, which introduces butyl branches instead of ethyl branches and shifts the balance of impact toughness, tear propagation resistance, and low-temperature seal initiation.

    Published data for this specific configuration is limited in public documents. Converter-scale film properties should therefore be generated on the intended extrusion line and at the intended gauge, rather than transferred from laboratory cast-film or compression-molded specimens. The resin is not intended for injection molding or rotomolding. Melt temperatures below 180 °C produce excessive melt viscosity and bubble instability on conventional blown film equipment, while sustained operation above 240 °C can consume the stabilizer package and generate oxidation-induced gels.

    What Limits the Processing Window During Stalk Extrusion?

    On a 65 mm grooved-feed extruder with a 30:1 length-to-diameter ratio and a 250 mm die, D605A6 is typically run at melt temperatures between 195 °C and 225 °C. Below 190 °C, melt pressure at the screen changer rises and bubble respiration becomes more frequent unless haul-off speed is reduced. Above 235 °C, oxidative degradation can form gels at the die lip, particularly if residence time exceeds 20 min during line stoppages. A screen pack of 20/40/80 mesh is commonly used. Finer screens can raise melt temperature by shear heating, especially when the die gap is below 1.5 mm.

    The recommended die gap is 1.5 mm to 2.5 mm. A narrower die gap increases shear rate and may improve gauge uniformity, but it also increases the risk of melt fracture and local temperature rise. A frost line height of 8 to 12 die diameters is typical for a 2.5:1 blow-up ratio. Higher frost line heights reduce film haze but decrease bubble stability in low-output startup periods.

    High-speed coextrusion of a 10 µm sealant layer in a 3-layer blown film line with a 300 mm die places different demands on the resin than a 100 µm monolayer liner. At layer ratios above 30%, D605A6 contributes seal-initiation behavior and low-temperature toughness. At layer ratios below 10%, the outer high-density or polyamide layers dominate film stiffness and tear balance. The sealant layer should be extruded at 210 °C to 225 °C to minimize interfacial layer distortion; lower melt temperatures can produce melt-fracture streaks at the die lip.

    When a 2.5:1 Blow-Up Ratio Replaces a 2.0:1 Setting

    Raising the blow-up ratio from 2.0:1 to 2.5:1 at constant die gap and output increases transverse-direction orientation and tends to increase transverse-direction Elmendorf tear while decreasing machine-direction tear. The effect is not specific to D605A6; it is amplified by the resin’s molecular weight distribution and short-chain branching distribution. On a 70 mm extruder with a 300 mm die and a 2.0 mm die gap, shifting BUR from 2.0:1 to 2.5:1 without adjusting frost line height can reduce dart impact F50 by 5% to 15% because bubble strain hardening increases orientation in the amorphous phase. Machine-direction tear may drop by 10% to 25%, while transverse-direction tear may rise by 15% to 35%. These ranges are directionally representative for enhanced hexene LLDPE and should be verified on the production line because local cooling rates and die pressure vary.

    The product differs from a 0.918 g/cm³ octene-based mLLDPE in stiffness and seal initiation, not necessarily in dart impact. At equivalent film gauge, the higher density of D605A6 generates a higher secant modulus and lower gas permeability but may reduce dart impact relative to a lower-density mLLDPE. Comparison should be made with ASTM D882 for tensile modulus and ASTM D3985 for oxygen transmission rate on the same line. The resin also differs from LDPE-rich blends: LDPE contributes higher melt strength and broader bubble stability but tends to lower dart impact and raise haze under ASTM D1003.

    Nominal Property Characteristics and Test Methodology

    The table lists the primary resin properties published in the technical data sheet. They are not release specifications; the sales specification and certificate of analysis control lot acceptance.

    PropertyTypical valueTest method
    Density0.926 g/cm³ASTM D1505 / ISO 1183
    Melt index at 190 °C, 2.16 kg0.6 g/10 minASTM D1238 / ISO 1133

    Film property values such as dart impact, Elmendorf tear, tensile elongation at break, haze, and gloss are lot-dependent and line-dependent. The supplier’s certificate of analysis should be obtained for each hopper lot. Laboratory values generated on a 25 µm monolayer film at a 2.5:1 blow-up ratio should not be applied to a 100 µm coextruded structure without verification. The following test methods are typically used for product qualification.

    Film attributeTest standardTypical gauge
    Dart drop impact F50ASTM D1709A / ISO 7765-125 µm
    Elmendorf tear propagation MD/TDASTM D1922 / ISO 6383-225 µm
    Tensile strength and elongation at breakASTM D882 / ISO 527-325 µm
    HazeASTM D100325 µm
    Gloss 60°ASTM D245725 µm
    Coefficient of frictionASTM D1894 / ISO 829525 µm

    D605A6 is typically evaluated at 25 µm monolayer thickness for optical and mechanical qualification. Coextruded structures, especially those with high-density polyethylene or polyamide skins, alter tear and stiffness balances enough that monolayer values cannot be substituted for structure validation.

    Clear the Extruder with a Viscosity-Matched Transitional Resin

    During startup and shutdown, D605A6 should be purged with a polyethylene of similar melt index rather than with a high-viscosity HDPE or a low-viscosity LDPE. A purging resin with melt index between 0.5 g/10 min and 1.0 g/10 min reduces the residence time required to clear the die lip and avoid melt-fracture streaks on the next production lot. Barrel temperatures should be set at 190 °C to 210 °C for purging. Screw speed should be reduced to 20 rpm to 40 rpm on a 65 mm extruder until melt pressure stabilizes. Injection of compressed air or nitrogen through the hopper is not recommended because it can introduce moisture and particulate contamination.

    Accumulated gels after a shutdown should be removed by barrel teardown if die head pressure remains above 400 bar after purging for 20 min. Continued operation above this pressure can overheat the melt film at the screw tip and accelerate degradation. A capillary rheometer test according to ASTM D3835 at 190 °C and shear rates from 50 s⁻¹ to 1000 s⁻¹ is recommended for die design verification, especially when a custom die gap or high-output barrier screw is being evaluated.

    Food Contact Compliance and Storage Boundaries

    For food packaging, the converter should request the manufacturer’s food-contact statement and verify the finished structure against FDA 21 CFR 177.1520 or EU Regulation 10/2011, as applicable. Compliance is not conferred by the resin alone because coextruded layers, adhesives, and print primers contribute to overall migration. End-use testing for specific food simulants should follow the migration test conditions specified in the relevant regulation.

    Storage before processing should be below 30 °C and protected from ultraviolet exposure. If the resin has been exposed to relative humidity above 60% for more than 24 h, pre-drying is recommended at 60 °C to 70 °C for 4 h to 6 h using desiccant-type drying. Blown film processing is less moisture-sensitive than cast film extrusion, but surface splay can occur with high moisture uptake. D605A6 should not be dry-blended with polypropylene above 5 wt% unless the converter has evaluated interlayer adhesion and tear balance under ASTM F88 and ASTM D1922. Avoid extended contact with copper-based stabilizer systems in high-temperature storage, because copper ions can accelerate oxidative degradation of polyethylene at elevated temperatures.