| HS Code | 748152 |
| Product Name | Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin |
| Polymer Type | Enhanced Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Hexene-1 |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.60 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield Md | 11 MPa |
| Tensile Strength At Break Md | 31 MPa |
| Elongation At Break Md | 600% |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 350 g |
| Dart Drop Impact | 200 g |
| Haze | 10% |
| Gloss 45 | 70% |
| Coefficient Of Friction | 0.20 |
As an accredited Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips Dynex™ D604D6 is packaged in 25 kg polyethylene-lined bags, palletized; 1,000 kg bulk bags are also available. |
| Container Loading (20′ FCL) | Chevron Phillips Dynex D604D6 Enhanced LLDPE Blown Film Resin: 20′ FCL loads 20 pallets, 25 kg bags, 40 bags/pallet, 20 MT net. |
| Shipping | Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin ships as non-hazardous polyethylene pellets, typically in 25 kg polyethylene bags on stretch-wrapped pallets, or in bulk trucks/railcars. Transport in clean, dry equipment; protect from moisture, heat, and sunlight. Follow supplier SDS and local regulations. |
| Storage | Store Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original packaging closed, clean, and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Use first-in, first-out rotation. Do not stack beyond safe limits. Follow the SDS. |
| Shelf Life | Shelf life is typically 24 months from manufacture when stored unopened in original packaging, cool, dry, and away from direct sunlight. |
In three-layer coextrusion, Chevron Phillips Dynex D604D6 Enhanced LLDPE Blown Film Resin is run as the core layer at 60–70 wt% of total structure, with high-slip or anti-block concentrates in the skin layers at 2–5 wt%. The melt temperature at the die is held between 205 °C and 225 °C on grooved-feed extruders with L/D 30:1; die gap is kept between 1.6 mm and 2.2 mm, and blow-up ratio is maintained at 2.0–2.5. Internal bubble cooling permits frost line height of 3–5 die diameters at output rates above 150 kg/h on 250 mm dies. Sack conversion on form-fill-seal lines uses hot-air seal jaws at 150–175 °C; seal strength is measured per ASTM F88, and the acceptance criterion is a peel-mode failure rather than interfacial separation. Puncture and impact behavior are validated by ASTM D1709 dart drop and ASTM F1306 low-speed puncture; tear resistance at die-cut handle perforations is measured by ASTM D1922. A 10–15 wt% formulation window for LDPE or lower-molecular-weight LLDPE is used to stabilize the bubble at high haul-off speed. LDPE addition is avoided above 20 wt% because seal initiation temperature rises and seal-through-powder performance degrades on the filling spout.
| Test property | Standard designation | Conversion-stage relevance |
|---|---|---|
| Dart impact resistance | ASTM D1709 / ISO 7765-1 | Drop testing and pallet corner impact on filled sacks |
| Elmendorf tear resistance | ASTM D1922 / ISO 6383-2 | Tear initiation at die-cut handle apertures and perforation lines |
| Low-speed puncture resistance | ASTM F1306 | Protrusion puncture from box corners and stacked pallets |
| Seal strength | ASTM F88 | Hot-seal integrity on horizontal and vertical form-fill-seal closing units |
| Coefficient of friction | ASTM D1894 | Sack stacking, pallet slip, and bagger feed reliability |
Silage bale wrap produced from D604D6 typically leaves the blown-film die at 25 µm and is slit to 500 mm or 750 mm rolls for round balers. The resin is coextruded in the core and non-cling skins at 70–85 wt% of the structure, while the cling layer is a separate lower-melting polyethylene/EVA formulation that provides adhesion under bale tension. D604D6 is specified because ASTM D1709 dart impact and ASTM D5748 puncture propagation correlate with the shattering puncture mechanism observed when 25 µm film stretches over cut pasture stems and woody prunings. A UV stabilizer masterbatch containing hindered amine light stabilizers and a UV absorber is metered at 2–4 wt%; above 5 wt%, die-lip deposit and bubble instability increase on dies running 2.2–2.8 blow-up ratio. Accelerated weathering per ASTM G154 cycle 1 is used as incoming quality assurance, but field correlation remains the limiting control for silage storage. Because LLDPE is non-hygroscopic, drying is unnecessary when ambient relative humidity is below 70%; if condensation forms on pellets, hot-air hopper drying at 60 °C for 1 h is sufficient. The same film structure must retain seal strength on the bale overlap without blocking at the roll edge; blocking is evaluated by a 60 °C oven storage test with a 5 kg weight applied across the roll surface.
Frozen-food packaging structures using D604D6 as the sealant layer are typically coextruded at 50–75 µm total thickness, with the sealant skin specified at 15–25 µm. On vertical form-fill-seal lines running 40–60 cycles/min, seal jaw residence time is 0.2–0.5 s, and hot tack measured by ASTM F1921 is the primary predictor of crease-seal failure at the film folds. Laboratory gradient seal bars place seal initiation between 90 °C and 115 °C, with the exact value dependent on skin-layer formulation and LDPE content. Cold-impact resistance is assessed by conditioning specimens at -20 °C for 24 h and testing dart impact per ISO 7765-1; because the standard reference is 23 °C, the low-temperature condition is recorded as an intentional deviation on the certificate of analysis. Tetrahedral corner seals on pillow bags are tested for leakage by ASTM D3078 after water immersion. Direct food contact compliance for the finished package falls under 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011, subject to an overall migration limit of 10 mg/dm²; converters must verify finished-article compliance. When D604D6 exceeds 60 wt% of the sealant layer, low-temperature seal strength is retained, but the increased stiffness can interfere with automatic bag opening. Published data for D604D6-specific low-temperature seal strength at -40 °C is limited; qualification therefore relies on converter-generated data on the actual vertical form-fill-seal line.
In extrusion lamination and adhesive lamination structures, D604D6 is supplied as a blown-film sealant web and is bonded to printed PET, BOPP, or aluminium foil. The sealant web is typically 30–60 µm thick and is corona treated to 42–46 mN/m wetting tension per ASTM D2578 before adhesive coating or thermal lamination. Seal initiation between 95 °C and 115 °C permits caulking around spice dust, salt, or protein residue; hot tack per ASTM F1921 is specified to prevent seal opening when a filled pouch drops onto a conveyor. Seal strength is measured per ASTM F88 as a 25 mm strip at 300 mm/min, with failure mode recorded as peel, seal creep, or film tear. Destructive bond strength between the sealant web and the outer laminate is checked by T-peel per ASTM D1876. If the structure includes aluminium foil, gauge uniformity of the sealant web is critical; blown-film lines with oscillating haul-off are operated to limit thickness variation to ±8%, reducing lamination air pockets and adhesive starvation. Corona-treated D604D6 webs stored beyond 90 days require retreatment because wetting tension decays below 38 mN/m on untreated polyethylene surfaces. Solventless adhesives applied at 1.2–2.2 g/m² coat weight generally require converter validation for primary aromatic amine and migration limits if the laminate is used for food; the film contribution to overall migration is evaluated against EU Regulation 10/2011 or FDA 21 CFR 177.1520 as applicable.
In pallet stretch-hood systems, D604D6 is processed into film at 120–200 µm, with the highest puncture and tear loads at the pallet bottom corners and banding edges. Blown-film production uses dual-lip air rings and internal bubble cooling; melt temperatures of 210–230 °C reduce melt fracture at high molecular weight. Blow-up ratio is held at 1.8–2.4, and frost line height is set between 5 and 8 die diameters to balance transverse orientation. Stretch-hood machines pre-stretch the film by a factor of 1.4–1.8 in the machine direction and 1.1–1.3 in the transverse direction during hood opening, depending on pallet dimensions and film gauge. Dart impact per ASTM D1709, tear propagation per ASTM D1922, and low-speed puncture per ASTM F1306 are specified. A key operational boundary is the film yield point: if pre-stretch exceeds 1.8:1, residual thickness at sharp corners may fall below 50 µm, and machine-direction tear propagation can occur. The inside surface coefficient of friction is maintained below 0.40 per ASTM D1894 to allow the film hood to slide over the pallet without snagging. Slip additive loadings above 3 wt% are avoided because they reduce stretch recovery and can accumulate on the die lip. On turret wrap systems running 30–60 s/pallet, the key failure mode is not puncture but retained tension loss; retained deflection force is evaluated by creep testing under constant elongation, with reference to ISO 899-1 where adapted for film specimens.
For high-speed industrial can liner conversion, D604D6 is specified at 40–65 µm and is produced on blown-film lines equipped with oscillating haul-off to distribute gauge variation. Bottom-seal bag lines run at 300–400 cycles/min; dwell time at the seal bar is 0.1–0.3 s, making hot tack per ASTM F1921 a required qualification parameter. Dart impact per ASTM D1709 and low-speed puncture per ASTM F1306 are specified at 50 µm to evaluate downgauging against puncture from broken glass and metal edges. A high slip/anti-block package is added to the skin layer at 2–4 wt% to achieve a coefficient of friction of 0.25–0.35 per ASTM D1894; this prevents liner-to-liner blocking during dispensing. Slip additive loadings above 5 wt% create die-lip build-up and reduce heat-seal strength at bottom seals, observed on conversion lines as audible seal-jaw chirping. The outer surface may be corona treated to 40–42 mN/m for print acceptance, but treatment is omitted in dusty environments where residual static attraction increases contamination. For can liners marketed as heavy-duty containers rather than direct food contact packaging, no food contact migration test is required; if the liner may contact food, converters apply 21 CFR 177.1520 and EU Regulation 10/2011 to the finished article. Published data for D604D6 in this specific can-liner configuration is limited; converter-generated gauge and seal data on the target bagger govern final approval.
Competitive Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips Dynex™ D604D6 Enhanced LLDPE Blown Film Resin is an ethylene-hexene copolymer supplied for monolayer and coextruded blown film structures in which downgauging, heat seal initiation, and puncture resistance are simultaneous constraints. The commercial specification is operationally defined by two lot-release measurements: nominal density of 0.916 g/cm³ under ASTM D1505 and nominal melt index of 0.45 g/10 min under ASTM D1238 at 190°C and 2.16 kg. In film converting, this combination places the product in the low-melt-index, low-density segment of the LLDPE family; it is not a high-pressure autoclave or tubular LDPE. The absence of long-chain branching reduces melt strength relative to LDPE, which means bubble geometry must be maintained by die design, air ring calibration, and frost-line control rather than by intrinsic extensional hardening. Typical application spaces include heavy-duty sacks, frozen-food packaging liners, collation-shrink webs, and sealant layers in coextruded pouches where the seal must resist contamination from fatty or dusty products. The enhanced designation refers to a narrow molecular weight distribution with comonomer incorporation tailored for improved dart impact and tear performance at reduced gauge, but the producer’s published data should be used to confirm whether a given film structure lies within the validated envelope.
Lot verification is dominated by density and melt index because both parameters are sensitive to comonomer content and molecular weight. Density is determined by ASTM D1505-18 gradient column or ISO 1183-1:2019 Method A on compression-moulded plaques, and the result controls flexural stiffness, water vapour transmission rate, and seal temperature. Melt index is determined by ASTM D1238-20 or ISO 1133-1:2022 Procedure A using a die with 2.095 mm diameter and 8.000 mm length. The resin remains in the melt state at 190°C for a prescribed preheat time before the piston is released; deviation in preheat time changes the measured value because of chain relaxation and additive migration. In addition to the two release properties, pellet inspection often includes bulk density, pellet size distribution, and colour via ASTM D6290-19 to detect contamination that would produce gels or screen-pack pressure drift. Density alone cannot reveal whether the resin has high long-chain branching; because D604D6 is linear, melt-tension tests are not used for acceptance, but a capillary rheometer sweep from 50 s⁻¹ to 1000 s⁻¹ can identify lot-to-lot variation in shear thinning.
| Property | Test method | Unit | Typical value |
|---|---|---|---|
| Density | ASTM D1505 | g/cm³ | 0.916 nominal |
| Melt index | ASTM D1238 (190°C/2.16 kg) | g/10 min | 0.45 nominal |
On a production line equipped with a 75 mm or 90 mm grooved-feed extruder having an L/D ratio of 30:1 and a barrier screw, the melt-temperature profile is normally held at 195°C to 220°C at the adapter. Set zones below 170°C in the feed section are undesirable because the resin’s relatively low melt index transfers more energy through shear heating; the rear barrel may run hotter than standard butene LLDPE. The die is typically an annular spiral mandrel with a die gap of 1.2 mm to 1.8 mm. A narrower gap raises shear enhancement but can create melt fracture at the die exit; adding a fluoropolymer processing aid may be required if the die gap is less than 1.5 mm. Bubble stability is more sensitive than output per rpm because the linear backbone lacks the strain hardening that stabilises LDPE at high draw. The frost line is maintained between 2 and 3 die diameters above the air ring, and the cooling air flow is adjusted to avoid bubble breath. When the frost line drifts upward, the bubble becomes slack; when it drops too low, quench-induced orientation increases transverse direction stiffness and can reduce dart impact. Output limitation in this grade is commonly bubble resonance rather than extruder torque; the practical countermeasure is installation of an adjustable-lip air ring or internal bubble cooling, not an increase in barrel temperature.
At gauge below 25 µm, the failure hierarchy shifts from bulk tensile yielding to localised tearing and dart impact. Tensile properties measured by ASTM D882-18 on 15 mm wide strips are less sensitive to gauge reduction than Elmendorf tear measured by ASTM D1922-19, because tear propagation is governed by the concentration of load-bearing tie molecules in the amorphous region. The molecular architecture of D604D6 is designed to preserve tie-molecule concentration when the film is quenched rapidly; however, rapid quenching can freeze in a lower crystallinity that improves dart impact but lowers modulus. The laboratory measurement of dart impact is carried out by ASTM D1709-16 Method A or ISO 7765-1:2004, and results are highly sensitive to film gauge, blow-up ratio, frost line, and conditioning at 23°C and 50% relative humidity. Heat seal initiation is commonly evaluated by ASTM F88/F88M-21; however, seal performance must be validated on the packaging line because dwell time and pressure on vertical form-fill-seal machines differ from laboratory jaw settings. The D604D6 product is selected where the converter seeks to reduce gauge without losing seal integrity; published data for a direct comparison against a reference butene LLDPE at equivalent density may not be available for all film constructions, so comparative trials are required.
Substitution of D604D6 into a structure that previously used high-pressure LDPE without changing the air ring, die gap, or frost line is a predictable start-up failure mode. The resin’s lower melt strength produces a longer, thinner bubble neck; if the air ring’s venturi is too broad, the bubble may snag or collapse. Converters compensate by raising melt temperature, but above 230°C the antioxidant package is consumed more rapidly and gel particles increase in the film. Relative to a conventional butene-copolymer LLDPE of similar melt index, the hexene-based D604D6 generally shifts the tear-puncture balance upward because branched side chains longer than ethyl reduce chain pullout during deformation. The penalty may be a slightly higher coefficient of friction and a different optical response; haze measured by ASTM D1003-13 is not an inherent constant but a function of melt temperature, die-lip cleanliness, and film cooling rate. If the film must be printed, surface treatment by corona discharge is normally required, and dyne level should be verified after treatment by ASTM D2578-17. Because the product does not contain slip or antiblock additives unless specified, converters often add a masterbatch of silica or erucamide; the addition level should be controlled because excessive erucamide migration can degrade heat seal performance by acting as a lubricant at the seal interface.
Molecular architecture differences between D604D6 and a conventional butene-copolymer LLDPE are not directly observable from melt index or density alone. In a linear polyethylene, the chain length between branch points determines how many polymer chains can bridge adjacent lamellae during crystallisation. Butene branches are short and may be partially rejected from the crystal, whereas hexene branches produce a larger excluded volume that, at comparable comonomer content, increases the probability of tie-molecule formation. The result is a film that can absorb more energy before puncture; however, the same tie molecules can raise the creep compliance in stretched films. Differences from high-pressure LDPE are more pronounced because long-chain branching provides shear thinning and extensional hardening; D604D6 cannot be considered a drop-in replacement when the existing LDPE line depends on bubble tension for gauge uniformity.
Olefin polymers are generally recognised under FDA 21 CFR 177.1520 paragraphs (a) and (c) when the final article meets extractive limitations and the polymer identity specification. The converter must verify that D604D6 is specifically listed in the supplier’s food-contact statement; compliance is not automatic for all food types, temperatures, and contact times. For the European Union, film sold into food contact is assessed under EU 10/2011 as amended, with overall migration limits of 10 mg/dm² or 60 mg/kg for the finished article depending on packaging geometry. Heavy metals and packaging waste evaluations are often reported against EU 94/62/EC and RoHS 2011/65/EU Annex II; the supplier’s certificate should specify the detection limit and the lot reference. The following reference table does not replace a certificate of compliance; it identifies the documents commonly requested for a polyethylene blown film structure.
| Reference | Application boundary | Verification requirement |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers in food contact | Supplier assurance and final article extraction data |
| EU 10/2011 | Plastic materials and articles in food contact | Overall migration and specific migration testing |
| ASTM D4976-12a | Polyethylene extrusion material specification | Oil absorption, ash, density, and melt index control |
| RoHS 2011/65/EU Annex II | Electrical/electronic equipment components | Lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE screening |
Storage and rework limits are process constraints rather than film property limits. Polyethylene pellets should be kept below 45°C and away from direct sunlight; although the resin is not hygroscopic, condensation on cold pellet surfaces can introduce moisture into the feed throat and cause sporadic bubble distortion. D604D6 contains a base antioxidant stabiliser, but stabiliser is consumed during each heat history; regrind ratios above 20% to 30% may reduce dart impact and raise gel counts, though published data for this specific grade are limited. The resin should not be combined with amine-based viscosity modifiers or certain metal stearate packages without trial validation because amine chemistry can interfere with the phenolic stabiliser and shift colour toward yellow. The operational boundary remains the lot-specific certificate of analysis, the downstream food-contact compliance statement, and the converter’s validated film trial.