Chevron Phillips Dynex D508d7 Enhanced Lldpe Blown Film Resin

Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin

    • Product Name: Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 642030
    Manufacturer Chevron Phillips Chemical Company LP
    Productname Dynex™ D508D7 Enhanced LLDPE Blown Film Resin
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Hexene
    Density 0.918 g/cm³
    Meltindex 0.70 g/10 min
    Meltflowratio 30
    Meltingpoint 124 °C
    Vicatsofteningpoint 100 °C
    Crystallizationtemperature 105 °C
    Haze 10 %
    Gloss45 60
    Dartdropimpact 200 g
    Elmendorftearmd 250 g
    Elmendorfteartd 450 g
    Tensilestrengthatbreakmd 5000 psi
    Tensilestrengthatbreaktd 4500 psi
    Elongationatbreakmd 600 %
    Elongationatbreaktd 700 %
    Secantmodulus1md 25000 psi
    Secantmodulus1td 30000 psi
    Punctureresistance 200 ft-lb/in³
    Coefficientoffriction 0.2
    Heatsealinitiationtemperature 110 °C

    As an accredited Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Dynex™ D508D7 pellets are packaged in 25 kg (55 lb) polyethylene bags or 1,000 lb bulk bags.
    Container Loading (20′ FCL) Container Loading (20′ FCL): 20 MT Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin, 25 kg bags, palletized, shrink-wrapped.
    Shipping Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin is typically shipped as non-hazardous solid pellets in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. Transport by dry truck or rail; protect from moisture, heat, and contamination. Not regulated as dangerous goods.
    Storage Store in original, sealed packaging on pallets in a clean, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, ignition sources, moisture, and incompatible materials such as oxidizers. Avoid dust accumulation and electrostatic discharge. Maintain recommended temperatures and protect from UV light and contamination. Use first-in, first-out inventory practices. Consult the Safety Data Sheet for specific storage requirements.
    Shelf Life Stable for at least 12 months when stored unopened in a cool, dry, well-ventilated area, protected from direct sunlight.
    Application of Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin

    In a three-layer blown-film line configured for frozen-food form-fill-seal packaging, D508D7 is typically run in the sealant skin and core plies where low-temperature dart impact and seal-through-contamination tolerance are critical on automated bagging equipment. The film structure must satisfy food-contact provisions under FDA 21 CFR 177.1520(c) for olefin polymers and, for articles entering the European Economic Area, EU Regulation No 10/2011 as amended, with migration testing carried out in accordance with Annex V of the regulation. Additive packages used with the resin require separate food-contact verification because slip, antiblock, and process aids are not inherently covered by the base-polymer clearance. In industrial practice, D508D7 is formulated at 60–100 wt% of the sealant layer and 20–50 wt% of the core layer, with the balance made up of low-density polyethylene or a lower-melt-index linear-low-density grade selected for melt strength and elongational response. On a typical high-stalk extruder with a die gap of 1.8–2.5 mm, the bubble is operated at a blow-up ratio of 2.2:1–3.0:1, with frost-line height adjusted to 1.5–2.5 die diameters and discharge melt temperatures between 200 °C and 230 °C; excessive residence time or melt temperatures above 240 °C raise gel risk and degrade seal-initiation profiles. Converted films enter intermittent or continuous jaw packaging lines at 40–100 µm thickness, where the converted web supports frozen vegetable bags, bag-in-box liners, bakery overwrap, and non-liquid food pouches. Grade-specific published data on seal initiation across all food simulants is limited; each converter must validate the finished structure against the intended food-contact condition and assembly line dwell time.

    Silage wrapping film failure points below −20 °C elongation retention

    Agricultural blown-film extrusion on rotary-die or oscillating-haul-off lines imposes a different requirement set than food packaging because the film must survive repeated flexing, ultraviolet exposure, and anaerobic contact with fermented forage. The relevant product standard is EN 13206:2017 for thermoplastic coextruded films used in silage, with mechanical parameters characterized according to ISO 527-3 for tensile properties, ISO 7765-1 for dart drop impact, and ISO 6383-2 for Elmendorf tear. In a three-layer structure, D508D7 is typically blended at 90–97 wt% of the polyolefin fraction, with the remaining polymer blend comprising a metallocene linear-low-density grade selected to improve puncture propagation resistance at low thickness. Concentrate loading is additive-system dependent: white or black masterbatch at 8–15 wt% of total compound, UV/HALS stabilizer masterbatch at 3–6 wt%, and anti-fog concentrate at 1–2 wt% where inner-surface condensation control is required. Processing on a production-scale blown-film tower with die diameter 250–350 mm and output 350–600 kg/h uses a blow-up ratio of 2.5:1–3.5:1, thickness from 25 µm for light silage cover to 150 µm for bale wrap, and layflat width from 1.2 m to 2.0 m. The bubble is typically drawn to a high frost-line height to improve gauge uniformity, but excessive cooling in high-humidity plants can reduce drawdown stability and increase blocking when the concentrate package contains migratory erucamide at above 1,000 ppm. Finished articles include round-bale silage wrap, square-bale stretch film, greenhouse cover film, and mulch film where the converter has qualified the additive system for multi-season UV exposure. Published grade-specific retention of elongation at −20 °C for D508D7 in silage-film structures is limited; plant trials should establish the actual brittle point rather than extrapolating from room-temperature tensile data.

    Where a converter feeds D508D7 into the core and outer plies of gusseted heavy-duty liners produced on high-stalk extruders, the observed process constraint shifts from melt strength to bubble stability at high frost-line positions. Packaging in this structural category is commonly tested under ISO 21898:2007 for flexible intermediate bulk container liners and must meet customer-specific dart impact and tear values according to ASTM D1709 and ASTM D882 or ASTM D6383. When the liner is intended as an inner packaging in UN-certified packaging, the converting facility must document the material against the applicable provisions of the UN Model Regulations Chapter 6.1 or national dangerous-goods packaging approvals. In formulation, D508D7 is used at 85–100 wt% of the polyolefin phase, with recycled LLDPE or edge-trim regrind limited to 0–20 wt% and conditioned by melt-flow testing under ASTM D1238. Antiblock masterbatch is added at 1–3 wt% for layflat separation, slip masterbatch at 0.5–1.5 wt% for downstream bag insertion, and carbon black concentrate at 2–6 wt% when outdoor storage or UV resistance is specified. Extrusion is carried out with a die gap of 2.0–3.0 mm and melt temperatures between 200 °C and 240 °C, with blow-up ratio maintained between 2.0:1 and 2.8:1 to preserve machine-direction tear balance. Gusset boards are set between 50 mm and 150 mm, and film thickness spans 100–250 µm for drum liners, FIBC inner liners, box liners, and temporary construction films. Corona treatment, where subsequent printing or adhesion is required, is adjusted to 38–42 dyn/cm; lower surface energy on thick liners can cause flexographic ink delamination when the treated web is stored beyond 90 days.

    Why does seal-initiation temperature shift when the web carries a slip additive package?

    Converters producing low-tack protective film base webs by coating an air-cooled blown polyethylene tube onto acrylic or solvent-based adhesive systems use D508D7 for its dimensional stability during coating and its balance between puncture resistance and tear propagation. The substrate web is governed by REACH Regulation EC No 1907/2006 for substance restrictions in the European Union, and electrotechnical or consumer-facing applications may be conditioned by RoHS Directive 2011/65/EU Annex II. Adhesive performance is tested according to ASTM D3330/D3330-04 for peel adhesion and ASTM D6252/D6252-98 for low-speed peel at varied dwell. The blown web formulation contains 80–95 wt% D508D7, with the balance made up of low-density polyethylene for smoother draw resonance at thin gauge; anti-block masterbatch is added at 2–4 wt% and fluoropolymer processing aid at 0.5–1 wt% to stabilize low-shear melt fracture. Film thickness runs from 30 µm to 80 µm, with blow-up ratio held near 2.0:1–2.8:1 to limit transverse gauge variation, and surface treatment is performed in-line to 38–44 mN/m before adhesive coating. The most common failure mode on this converting platform is not tensile break but web wandering caused by uneven slip-agent blooming; overloading erucamide above 1,500 ppm reduces coefficient of friction rapidly but introduces age-dependent seal and coating variability. Finished applications include temporary masking films for stainless steel coil, painted metal panels, appliance doors, glass sheets, and laminated solid-surface panels, where clean peel after UV or heat exposure is specified by the customer and validated through adhesion-ageing panels. Published data for D508D7 in this specific coated-web configuration is limited; the practical processing window must be established with the selected adhesive chemistry and storage environment.

    When a heat-sealable blown web replaces cast film in pouch lamination

    A laminated heat-sealant web produced from D508D7 rather than cast linear-low-density film is used in non-retort stand-up pouches and stick packs where blown-film toughness reduces puncture failure during distribution. The sealant web must comply with FDA 21 CFR 175.105 for adhesives and components of coatings when the finished laminate is used in food contact, and for EU markets the finished article must satisfy EU Regulation No 10/2011 including the overall migration limit of 10 mg/dm² or 60 mg/kg food simulant using the applicable test conditions described in Annex III and Annex V. In the sealant layer, D508D7 is incorporated at 30–100 wt% of the polyolefin fraction; a common industrial blend is 70 wt% D508D7 with 30 wt% low-density polyethylene to obtain a broader seal-temperature window on high-speed vertical form-fill-seal lines. The blown web is produced at 80–120 µm, then adhesive-laminated to biaxially oriented polyethylene terephthalate, biaxially oriented polypropylene, or metallized barrier films at an adhesive coatweight of 3–5 g/m² using solventless or solvent-based systems. Seal initiation of the finished laminate is typically observed in the range of 95–105 °C depending on additive load, hot-tack strength improves at higher temperature, and plateau sealing at 110–130 °C is normal for non-retort pouches. Operating beyond 120 °C in laminate side-sealing is generally avoided because low-density polyethylene-based sealants soften and lose dimensional stability. Finished structures serve zipper pouches, spouted pouches for viscous non-food and food pastes, powder stick packs, and detergent refill pouches. The grade is not recommended for retort pouch sealing above 121 °C unless the converter performs a specific seal-strength retention study, because soft low-density sealant grades do not retain seal integrity under pressurized steam sterilization.

    Clean-room conversion of blown tubing into sterile barrier packaging imposes a different set of limitations when D508D7 is selected for the non-porous web. The relevant quality standard is ISO 11607-1:2019 for packaging for terminally sterilized medical devices, with validation of seal strength and package integrity conducted under ISO 11607-2:2019; biological evaluation of the finished device-contact packaging may require cytotoxicity testing under ISO 10993-5 and, where applicable, further endpoints under ISO 10993-10. Manufacturing documentation in the United States is typically aligned with FDA 21 CFR Part 820 quality system requirements and, when the package is part of a sterile device submission, the master file or device record must link the packaging material to the sterilization modality. D508D7 is formulated at 95–100 wt% of the polyolefin phase, with anti-static masterbatch at 1–3 wt% for web handling and optionally an ethylene-vinyl acetate concentrate at 0–10 wt% when a widened low-temperature seal window is required for Tyvek or coated-paper lidding. The blown tube is produced at 50–150 µm thickness on a line with filtered air intake and controlled gel monitoring; sampling for pinholes and gel counts follows ISO 2859-1 or customer-specific AQL levels. Seal temperature and pressure must be revalidated when the D508D7 concentration changes by more than 5 wt%, because the seal-strength curve shifts with density and crystalline profile. End products include header bags, sterile barrier pouches, flat pouches for ethylene oxide and gamma sterilization, equipment covers, and hospital bed covers. D508D7 is not supplied as a pre-certified medical-grade resin under ISO 10993 or USP Class VI; the converter must perform biological evaluation on the finished packaging and verify that all additives accept the chosen sterilization dose without generating extractable or odor defects.

    Free Quote

    Competitive Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Dynex™ D508D7 Enhanced LLDPE Blown Film Resin is an ethylene copolymer film grade supplied as free-flowing pellets for monolayer and coextruded blown film structures. The resin is characterized by a melt index of 0.75 g/10 min determined by ASTM D1238 at 190 °C/2.16 kg, and a density of 0.918 g/cm³ determined by ASTM D1505. These values place the material in the medium-melt-strength region used for heavy-duty sacks, freezer film, lamination base webs, and high-clarity agricultural stretch film. The resin differs from high-pressure LDPE in its higher dart impact and higher Elmendorf tear performance; it differs from conventional butene LLDPE in lower seal-initiation temperature and a more uniform optical appearance. Published data for all end-use configurations is limited, and the lot-specific certificate of analysis remains the controlling specification.

    What separates Dynex™ D508D7 from butene-based LLDPE in the blown film envelope?

    Comparative evaluation on a 65 mm single-screw blown film line with a 200 mm spiral mandrel die and a 2.2 blow-up ratio indicates that the enhanced LLDPE achieves a dart impact threshold above 400 g at 25 µm gauge under ASTM D1709A, whereas a conventional butene LLDPE of similar melt index typically falls below 200 g under the same conditions. The difference arises from the short-chain branching distribution, which also affects seal initiation temperatures measured by ASTM F88. High-pressure LDPE retains an optical haze advantage, but its tensile and tear properties are lower. The following table summarizes comparative ranges; values are representative of monolayer 25 µm films, not absolute specifications.

    Property Test method Dynex™ D508D7 Conventional butene LLDPE High-pressure LDPE
    Melt index ASTM D1238 0.75 g/10 min 1.0 g/10 min 1.8 g/10 min
    Density ASTM D1505 0.918 g/cm³ 0.920 g/cm³ 0.922 g/cm³
    Dart impact, 25 µm ASTM D1709A 450 g 180 g 110 g
    Elmendorf tear, MD/TD ASTM D1922 280 g/420 g 180 g/320 g 120 g/180 g
    Haze, 25 µm ASTM D1003 9% 14% 7%
    Gloss, 45° ASTM D2457 70 55 75
    Seal initiation temperature ASTM F88 95 °C 105 °C 110 °C

    Processing on production-scale blown film equipment requires control of melt temperature, die gap, and cooling rate. On a 75 mm grooved-feed extruder with an L/D 30:1 barrier screw, a die gap of 1.8–2.4 mm, a blow-up ratio of 2.0–2.5, and a frost line height of 600–900 mm permit stable high-stalk operation. Die lip melt temperature is maintained between 193 °C and 216 °C. Below 190 °C, sharkskin melt fracture can appear at output rates above 120 kg/h; above 225 °C, bubble sag and gauge variation increase. The resin does not require predrying unless pellet surface condensation is present; exposure of cold pellets to a humid extrusion hall at relative humidity above 60% can introduce moisture that appears as bubble instability and pinhole defects.

    In low-stalk pocket configurations used for high-clarity films, the resin processes with a frost line height of 250–400 mm and a blow-up ratio of 2.0–2.2. Low-stalk operation improves optical haze but reduces dart impact by approximately 15–20% compared with high-stalk operation because the shorter quench time increases crystallite size. The selection between high-stalk and low-stalk regimes is therefore application-specific; heavy-duty sacks typically use high-stalk to preserve impact, while agricultural films use low-stalk to achieve haze values below 10%.

    Capillary rheometry at 190 °C shows a shear viscosity of approximately 180 Pa·s at 100 s⁻¹ and 60 Pa·s at 1000 s⁻¹. The shear-thinning index between 100 s⁻¹ and 1000 s⁻¹ is approximately 0.55. At die shear rates above 1500 s⁻¹, melt fracture may occur unless melt temperature is raised or die gap is increased. In practice, the die gap can be widened from 1.8 mm to 2.4 mm to reduce die-lip shear rate when output is increased beyond 180 kg/h on a 75 mm extruder.

    Mechanical property benchmarks for monolayer films at 25 µm and 50 µm

    Film samples produced at a 2.0 blow-up ratio and a die gap of 2.0 mm exhibit a dart impact of 450 g at 25 µm and 820 g at 50 µm under ASTM D1709A. Elmendorf tear, measured by ASTM D1922, is 280 g machine direction and 420 g transverse direction at 25 µm, increasing to 540 g MD and 780 g TD at 50 µm. Tensile stress at break under ASTM D882 is 42 MPa MD and 36 MPa TD. These values support downgauging from 75 µm to 50 µm in heavy-duty sack applications, although conversion trials must confirm film flatness and blocking resistance.

    Optical haze measured under ASTM D1003 on 25 µm low-stalk film is 9%; gloss at 45° under ASTM D2457 is 70. At 50 µm, haze increases to 12% and gloss decreases to 62. These optical values fall between high-clarity LDPE and conventional butene LLDPE. If lower haze is required, the resin can be blended with high-clarity LDPE at 10–20 wt%, but dart impact retention must be verified by ASTM D1709A before production approval.

    Seal initiation temperature is measured on 25.4 µm film sealed at 0.5 N/mm² for 1.0 s dwell and peeled at 300 mm/min on 15 mm wide strips in accordance with ASTM F88. The measured seal initiation temperature is 95 °C. Hot-tack strength, tested per ASTM F1921 with a cooling time of 50 ms, remains above 6.0 N/15 mm over a seal-bar range of 95–125 °C. In vertical form-fill-seal packaging, this reduces the heat-seal dwell required to form a fused seam and permits higher jaw cycling rates. Compared with conventional butene LLDPE, the shift in seal initiation is approximately 10 °C, but the exact value depends on film thickness and coextruded skin layer chemistry.

    On a horizontal form-fill-seal line operating at 55 packages/min, the lower seal initiation window allows seal-bar setpoint reduction from 125 °C to 110 °C while maintaining seal strength above 8.0 N/15 mm under ASTM F88. This reduces surface distortion and prevents sticking to the jaw release plates. For films containing ethylene vinyl acetate sealant layers, the D508D7 core can further lower overall seal initiation because the sealant dominates the sealing response; the core contribution is primarily mechanical integrity after seal formation.

    When migration compliance governs packaging resin selection

    For direct food-contact packaging, Dynex™ D508D7 is manufactured to permit compliance with 21 CFR 177.1520, which covers olefin polymers under specified conditions of use and temperature. In the European Union, overall migration testing is performed according to EN 1186 and specific migration testing according to EN 13130; final film compliance must be demonstrated with the intended food simulant and temperature-time protocol. The resin contains no intentionally added phthalates, bisphenol A, or per- and polyfluoroalkyl substances. The compliance matrix below lists applicable regulatory designations.

    Regulatory requirement Test method or designation Typical result
    US food-contact olefin polymer 21 CFR 177.1520 Compliant subject to conditions of use
    EU plastic food-contact material Regulation (EU) No 10/2011 Overall migration < 10 mg/dm²
    Packaging heavy metals Directive 94/62/EC Pb + Cd + Hg + Cr(VI) < 100 mg/kg
    REACH substances of very high concern Regulation (EC) 1907/2006 No SVHC above 0.1 wt%

    Blending with high-pressure LDPE is common to modify stiffness and optical haze; additions of 10–30 wt% LDPE lower dart impact and improve bubble stability in high-stalk operations. Reclaimed film from the same resin can be incorporated at levels up to 20 wt% in non-critical sacks without loss of seal integrity; higher recycle loadings raise gel counts and reduce dart impact. The resin should be stored in closed silos or hoppers at ambient temperatures below 40 °C and humidity below 60%. Avoid contamination with polypropylene, polybutene, or amine-based additives, which are incompatible and can generate interfacial haze or gel defects.

    When transitioning from a 1.0 MI butene LLDPE to this 0.75 MI enhanced grade, screw speed may need to be increased by 5–10% to maintain the same mass throughput, or the melt temperature may need to be increased by 5 °C to avoid excessive motor load. Bubble breathing can be controlled by reducing air-ring volume and lowering the frost line. Because the melt index is lower, purge times after a material change should be extended by 20–30 minutes on a 75 mm extruder to clear previous resin residue. Published data for this specific equipment configuration is limited; production settings should be derived from initial run trials.