    Specifications
    HS Code 554643
    Meltindex 0.70 g/10 min
    Density 0.918 g/cm³
    Meltflowratio 30
    Meltingpoint 124 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyieldmd 1,500 psi
    Tensilestrengthatyieldtd 1,500 psi
    Tensilestrengthatbreakmd 5,500 psi
    Tensilestrengthatbreaktd 5,000 psi
    Elongationatbreakmd 650%
    Elongationatbreaktd 750%
    Elmendorftearstrengthmd 250 g
    Elmendorftearstrengthtd 350 g
    Dartdropimpact 200 g
    Haze 8%
    Gloss 75%
    Onepercentsecantmodulusmd 30,000 psi
    Onepercentsecantmodulustd 35,000 psi
    Coefficientoffriction 0.20
    Lowtemperaturebrittleness < -70 °C

    As an accredited Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Dynex™ D508A7 is packaged in 25 kg net polyethylene-lined bags, palletized and stretch-wrapped for secure transport.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin, stretch-wrapped and secured.
    Shipping Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin is shipped as solid pellets in 25 kg bags, stretch-wrapped pallets, octabins, or bulk trucks/railcars. Store under cover; avoid moisture, UV, and contamination. Keep cool, away from ignition sources. Generally non-hazardous for transport; follow local rules and SDS.
    Storage Store Chevron Phillips Dynex™ D508A7 resin in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed, off the floor, to prevent moisture, dust, and contamination. Avoid prolonged UV exposure, excessive stacking, and incompatible materials. Use first-in, first-out rotation. Consult the SDS for detailed storage and handling guidance.
    Shelf Life Typically 12 months from date of manufacture when stored unopened in a cool, dry area, away from direct sunlight.
    Application of Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin
    Extrusion of 70 µm heavy-duty shipping sacks from D508A7 on a high-stalk blown film line typically uses a barrier-flighted single-screw extruder with L/D ratio between 24:1 and 30:1. The nominal density of D508A7 is 0.918 g/cm³ per ASTM D1505, with a nominal melt index of 1.0 g/10 min per ASTM D1238. Melt temperature is held at 190–210 °C for the barrel zones, with adapter and die zones elevated only to 210–220 °C when surface melt fracture appears as a sharkskin pattern. A high-stalk bubble is preferred over a pocket bubble because the extended melt phase increases molecular orientation balance before the frost line. Die gap is set at 1.5–2.0 mm, blow-up ratio at 2.0:1–2.8:1, and frost line height at 5–8 die diameters. When bubble flutter occurs below 2.5:1, converters add 10–20 wt% branched LDPE to stabilize the bubble; however, the same addition reduces dart impact at 70 µm compared with a 100% D508A7 control structure.On a three-layer coextrusion line, D508A7 is placed in the core while the skins carry 5–10 wt% antiblock masterbatch and slip masterbatch. This construction preserves the dart impact of the core resin while preventing blocking in warm warehouse storage. At the converter, sacks filled with 25 kg of polymer granulate or mineral filler are tested under ASTM D5276 and ISO 7965-2 filled-bag drop protocols. The critical failure mode is not tensile yield but side-gusset puncture when a palletized sack strikes a sharp corner. For that reason, converters specify dart impact per ASTM D1709A above 150 g at 70 µm, and Elmendorf tear per ASTM D1922 above 300 g in the transverse direction. These are qualification specifications rather than universal material certificates. Edge trim regrind may be returned into the core at up to 10%; above this level, oxidized trim raises gel count and creates pinholes under flexographic print. Surface treatment is held at 38–42 mN/m per ASTM D2578 before solvent-based or UV ink application. Terminal products include sewn open-mouth sacks, pinch-bottom bags, and gusseted pillow sacks for fertilizers, polymer resins, and industrial minerals.

    What Limits Seal Integrity in IQF Vegetable Freezer Film?

    On vertical form-fill-seal machines running individually quick-frozen peas, broccoli florets, or berry mixes, the seal area operates in a cold ambient zone where condensed moisture and ice particles can be trapped between film plies. A blown polyethylene film in the D508A7 density class typically reaches a heat-seal initiation range near 95–110 °C, which allows the seal jaw to displace residual ice crystals without thermally overloading the film back seal. D508A7 is processed into 40–60 µm rollstock using a die gap of 1.0–1.5 mm, melt temperature of 180–200 °C, and blow-up ratio of 2.2:1–2.6:1. The lower melt temperature suppresses oxidative gel formation during long runs. The narrower die gap raises shear stress enough to homogenize the melt without creating excessive back pressure, provided the extruder screw is a barrier-flighted design with sufficient pumping capacity.European Union food-contact compliance is assessed under EU 10/2011, with an overall migration limit of 10 mg/dm² for plastic articles intended for food contact. In the United States, the film is generally supplied under FDA 21 CFR 177.1520(c) when the complete formulation is covered by the converter’s food-contact statement. The primary packaging defect in frozen applications is not cold brittleness but seal contamination leading to leakers. Converters therefore specify heat seal strength per ASTM F88 above 3.0 N/15 mm for 40 µm film sealed at 110 °C and 0.3 MPa, with dwell time of 0.5–1.0 s. Films downgauged below 40 µm require cold-temperature dart impact testing at -25 °C per ASTM D1709A, because ambient-temperature dart values do not predict puncture behavior after freezer rigidification. Terminal products include printed pillow packs for frozen blueberries, diced onions, and mixed vegetable blends.

    If Silage Bags Must Survive UV Exposure and Fermentation Acids

    Bunker silo covers and bale stretch films produced from D508A7 require a UV stabilization package added as masterbatch at the converter. For black/white coextruded silage covers, the white outer layer commonly contains 8–12 wt% titanium dioxide masterbatch and the black inner layer 2–4 wt% carbon black masterbatch. The carbon black acts as both UV absorber and light barrier to suppress mold growth at the silage surface. Processing uses a die gap of 1.5–2.0 mm, blow-up ratio of 2.0:1–3.0:1, and melt temperature of 190–210 °C. Balanced biaxial orientation is maintained because anisotropic shrinkage under field wind causes cover distortion and pullout at anchor points. Accelerated weathering for European agricultural covering films is specified under EN 13206:2017; retention of tensile elongation after 5000 h xenon-arc exposure is expected for multi-year covers, although published data for D508A7 in this exact construction are limited.Fermentation acids in silo leachate create pH values near 3.8–4.5 at the soil-film interface. Polyethylene is not degraded by these short-chain organic acids; the dominant failure risk is mechanical puncture from corn stalks, tire traffic, and animal damage. Puncture resistance is therefore measured per ASTM D5748, with acceptance limits set by converter specification rather than by a single universal standard. A 100 µm monolayer cover without a puncture-resistant core may fail at field creases that concentrate stress. For bunker covers, coextruded structures with D508A7 in the core and a carbon-black-rich inner skin provide better tear propagation resistance than monolayer films of the same gauge. Terminal products include white/black bunker covers, round bale wrap, and temporary silage clamps.High-speed form-fill-seal packaging of granular urea, polycarbonate pellets, or calcium chloride operates with vertical sealing jaws cycling at 25–40 packs per minute. At this speed, the film must carry a stable corona-treated surface through the forming collar without blocking at the corner folds and without tearing at the sealing jaw. D508A7 is processed with 1000–2000 ppm synthetic silica antiblock and 500–1000 ppm erucamide slip masterbatch; exact slip loading is adjusted to maintain a coefficient of friction per ISO 8295 between 0.20 and 0.40 for register stability. Melt temperature is maintained at 190–215 °C, die gap at 1.5–2.0 mm, and blow-up ratio at 2.0:1–2.7:1. High-speed packaging of dusty granular products introduces a seal contamination problem: product dust pushed into the seal zone reduces seal strength below the clean-film requirement. Converters therefore run dusted-seal tests using a measured amount of ground product placed into the seal area before sealing; this is a converter-specific method because no single international standard covers dusted-seal performance for all chemical packaging classes.Bags used for non-hazardous solid chemicals are qualification-tested under ASTM D5276 and ISO 7965-2 with actual fill loads. Hazardous solids may additionally require dangerous goods packaging qualification under the applicable transport regulation, such as 49 CFR Part 178 in the United States or equivalent national admissions. Specific published data for D508A7 in every UN-certified sift-proof bag configuration are limited; therefore, each construction must be qualified with the actual product and closure system. Terminal products include form-fill-seal pillow bags for fertilizer, plastic pellets, carbon black, and water-soluble salts.Blown film intended as a lamination sealant web in stand-up pouches is produced at 25–40 µm thickness with a die gap of 1.5–2.0 mm and blow-up ratio of 2.0:1–2.5:1. The film is corona-treated on the lamination side to 38–42 mN/m per ASTM D2578 and then adhesive-laminated to reverse-printed BOPET, metallized OPP, or aluminum foil. D508A7 functions as the heat-seal layer because its narrow short-chain branching distribution gives a consistent seal-strength curve across the typical jaw temperature band. The critical blown film defect in lamination is not seal initiation but gauge variation, which creates adhesive void lines after nipping. Automatic thickness control with closed-loop die bolt feedback is normally set to maintain gauge variation below ±5%.For laminated food pouches, the finished structure is evaluated under EU 10/2011 and FDA 21 CFR 177.1520(c). Specific migration testing is required because the adhesive and ink layers contribute substances in addition to the polyethylene web. For retort or hot-fill applications above 85 °C, a downgauged D508A7 sealant web may soften sufficiently to allow creep failure during depressurization; published data for this specific configuration are limited, and each pouch must be retort-tested by the converter using its own pressure-test protocol. Terminal products include dry fruit pouches, frozen seafood pouches, and valve pouches for granulated dry goods.

    Tear Propagation Resistance in Pallet Stretch Hood Film

    Stretch hood film is an A/B/A coextrusion in which D508A7 forms the core and internal skin, while the external skin contains slip and antiblock for machine handling. The film is blown at 100–150 µm using a die gap of 1.5–2.5 mm, blow-up ratio of 2.5:1–3.0:1, and melt temperature of 190–210 °C. A high blow-up ratio is selected to increase transverse-direction tear propagation resistance. Excessive machine-direction orientation produces a film that splits along the machine direction when the stretch hood frame draws the film over sharp pallet corners. Frost line height is therefore held at 8–10 die diameters to reduce machine-direction orientation and avoid split initiation.Puncture resistance is tested per ASTM D5748, and Elmendorf tear is reported per ASTM D1922. The film must retain elasticity after being stretched 40–60% by the hooder. Creep resistance at 25 °C and 35 °C is measured using load retention jigs because no single international standard fully covers pallet hood creep behavior. Operational boundary: pallet loads with protruding corner boards or exposed metal strapping require an outer layer containing 10–20 wt% high-density polyethylene or a higher-density LLDPE to increase stiffness. However, mixed-in HDPE above 20 wt% typically reduces dart impact by more than 30% in 100 µm film and is not recommended without full line trials. Terminal products include palletized bags of cement, mineral wool, and beverage containers.
    Free Quote

    Competitive Chevron Phillips Dynex™ D508A7 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Dynex™ D508A7 is classified as an enhanced linear low-density polyethylene blown film resin. The product is identified by the manufacturer as a member of the Dynex™ portfolio, where the term enhanced refers to the modification of molecular weight distribution and comonomer placement relative to conventional reference grades. The resin is intended for air-quenched blown film extrusion of monolayer and coextruded structures where the converter must balance dart impact, tear resistance, optical transmission, and seal performance. Because the technical data sheet and certificate of analysis set the release specifications, all operational decisions should use lot-specific values for melt mass-flow rate, density, and additive levels. Laboratory qualification against ASTM D1238 at 190 °C/2.16 kg, ASTM D1505 for density, and ASTM D882 for film tensile properties is common. The term enhanced is not a recognized ASTM or ISO designation; it is a commercial nomenclature that signals a shifted processing envelope and property profile. In commercial practice, this designation separates D508A7 from commodity high-pressure LDPE and from broad-MWD Ziegler-Natta LLDPE by a set of measurable extrusion responses rather than by a single structural feature.

    What Distinguishes D508A7 from Conventional Ziegler-Natta LLDPE in Melt Processing?

    The melt-processing comparison rests on molecular weight distribution and shear response. Conventional Ziegler-Natta LLDPE typically exhibits a broad molecular weight distribution, high shear thinning, and measurable melt elasticity at typical blown film shear rates; this translates to stable bubble formation but also to high extruder motor load, elevated die pressures, and a tendency toward die-lip build-up during long campaigns. Enhanced LLDPE grades are designed to narrow the distribution without sacrificing low-shear melt strength, so the resin can be drawn at lower apparent viscosity while maintaining bubble shape. On a 60 mm grooved-feed single-screw extruder with a 30:1 L/D ratio and a 200 mm spiral-mandrel die, generic enhanced LLDPE evaluations commonly report lower head pressure at equivalent output compared with a conventional α-olefin Ziegler-Natta copolymer of equal melt index and density. D508A7-specific pressure data are not independently available; a production trial with a pressure transducer mounted at the breaker plate is the accepted method for quantifying the differential. The melt flow ratio determined from ASTM D1238 condition 190 °C/21.6 kg divided by condition 190 °C/2.16 kg is a useful indirect control, but the release specification for D508A7 should be taken from the certificate of analysis.

    At high shear rates above 500 s⁻¹, conventional broad-distribution LLDPE may exhibit sharkskin melt fracture at the die land. Enhanced LLDPE is formulated to shift the onset of melt fracture toward higher shear stress, but the actual critical shear stress for D508A7 is not publicly specified. The observed film quality is therefore mapped by producing a series of screw-speed steps while holding die gap constant and measuring surface roughness against a visual standard. This approach is used because small variations in die design, die temperature uniformity, and air-ring configuration produce differences larger than the resin’s intrinsic melt-fracture threshold. The practical output ceiling on air-quenched lines is often set by bubble cooling capacity rather than extruder backpressure when the enhanced resin is used.

    For air-quenched monolayer line start-ups, the changeover procedure to D508A7 should avoid abrupt rheological transitions. A practical sequence begins with purging the extruder, adapter, and die with a viscosity-matched LLDPE at a melt temperature between 200 °C and 220 °C, followed by the introduction of D508A7 at the same screw speed and die gap. Because the grade’s shear-thinning character differs from high-pressure LDPE, initial die pressure may be higher or lower than the previous material; the operator should allow 15 min to 20 min of pressure stabilization before changing die geometry or take-off speed. Bubble stability is normally assessed at a blow-up ratio of 2.0:1 to 2.8:1 and a frost line height of 2 to 5 die diameters. If the bubble oscillates at high frost line height, reducing cooling-air ring height or lowering melt temperature in 5 °C increments is a standard corrective sequence. At ambient relative humidity above 60%, surface moisture can condense on cold pellets during warehouse transfer; a hopper dryer set at 40 °C to 60 °C for 1 h to 2 h removes surface moisture, although the resin does not require hydrolytic drying. Pellets should be stored away from direct sunlight and strong oxidizers to avoid ultraviolet degradation and oxidative stability loss.

    Compared with high-pressure LDPE, the linear backbone of D508A7-class enhanced LLDPE provides higher tensile strength and puncture resistance at equivalent film gauge, permitting some downgauging in industrial packaging. The trade-off is a different bubble geometry: high-pressure LDPE has long-chain branching that provides pronounced melt strength and stable low-flow bubble formation, while enhanced LLDPE requires more precise control of stalk height and frost line. Compared with single-site metallocene LLDPE, an enhanced Ziegler-Natta architecture may occupy a middle ground in sealing and optical behavior. Metallocene LLDPE typically offers low seal initiation temperature and high gloss but can exhibit lower melt strength and higher sensitivity to die pressure fluctuations. D508A7 is not marketed as a metallocene resin; its “enhanced” designation signals a conventional or modified Ziegler-Natta platform with improved comonomer uniformity, although the catalyst system is not disclosed in public safety data sheets. Converters may observe lower haze than broad-MWD LLDPE but not necessarily as low as a metallocene grade. The optical comparison must be made at equivalent film thickness, melt temperature, frost line height, and cooling-air flow.

    Specification Release Testing and Lot Acceptance Protocols

    Blown film qualification for this resin class rests on film property measurements rather than pellet data alone. Film specimens are conditioned at 23 °C and 50% relative humidity for at least 40 h per ASTM D618 before tensile, tear, and impact tests. A typical lot acceptance matrix includes ASTM D882 for tensile strength at break and 1% secant modulus, ASTM D1922 for Elmendorf tear, ASTM D1709 Method A or B for dart drop impact, ASTM D1003 for luminous transmittance and haze, and ASTM D2457 for 45° gloss. The values presented in Table 1 are class-typical ranges for enhanced LLDPE blown film at 25 μm thickness and are not grade-specific release limits. D508A7 lot-specific values must be compared against the manufacturer’s technical data sheet before setting internal specifications.

    Table 1. Comparative blown film property envelope for enhanced LLDPE and conventional Ziegler-Natta LLDPE at 25 μm, 2.5:1 blow-up ratio
    ParameterTest methodEnhanced LLDPE class rangeConventional Z-N LLDPE class range
    DensityASTM D1505 / ISO 1183-10.912–0.925 g/cm³0.916–0.930 g/cm³
    Melt mass-flow rateASTM D1238, 190 °C/2.16 kg0.5–2.0 g/10 min0.5–2.0 g/10 min
    Dart impact, F50ASTM D1709 Method A, 25 μm100–400 g80–250 g
    Elmendorf tear MDASTM D1922, 25 μm50–200 g40–150 g
    Elmendorf tear TDASTM D1922, 25 μm80–250 g100–250 g
    1% secant modulus MDASTM D882150–250 MPa140–220 MPa
    HazeASTM D1003, 25 μm5–15%6–18%
    Gloss 45°ASTM D245750–7540–70

    Dart impact, tear anisotropy, and hot-tack performance determine the conversion value of D508A7 in flexible packaging. Blown film tear balance is controlled by the ratio of machine-direction to transverse-direction orientation, which is set by stalk height and the take-off speed relative to melt velocity. A high-stalk process increases machine-direction orientation and transverse-direction tear, while a low-stalk process reduces machine-direction tear but may lower dart impact. The enhanced architecture of D508A7 is intended to allow stable high-stalk processing without bubble sag, although published data for this specific configuration is limited. Converter-side heat seal initiation temperature should be mapped by ASTM F1921 Method A or equivalent hot-tack evaluation; grade-specific seal data are not uniformly published, and production temperature maps remain the controlling reference. Optical performance is governed by spherulite size and surface crystalline texture; air-ring configuration and frost line height frequently influence haze more than the resin pellet itself.

    When D508A7 Is Considered for Heavy-Duty Sack and Industrial Film Converting

    When the film enters downstream bag conversion, the choice of D508A7 over a general-purpose α-olefin LLDPE is justified if oriented tear balance and dart impact remain above the converter’s specification after downgauging. Heavy-duty sack constructions often require a dart impact F50 of at least 150 g at 50 μm and machine-direction Elmendorf tear not below 50 g, measured under ASTM D1709 and ASTM D1922 respectively. The enhanced molecular architecture is intended to preserve some of these properties when the film thickness is reduced, but the actual balance depends on blow-up ratio, frost line height, die gap, and the degree of oxidation during extrusion. For industrial liners, bubble geometry should be maintained at a blow-up ratio between 2.0:1 and 2.5:1 on a die diameter of 200 mm with a neck height of 3 to 5 die diameters. Converters should not extrapolate monolayer performance to coextruded structures without sheet-level testing because the skin layers and tie resins alter the overall tear and seal response. Published multi-layer processing data for D508A7 is limited; production trials are the controlling reference.

    Regulatory positioning of polyolefin film resins is use-dependent and must be confirmed against the current safety data sheet and product stewardship bulletin. In the United States, polyethylene copolymers intended for food-contact use may be evaluated under FDA 21 CFR 177.1520(c), which establishes specifications for olefin polymers and conditions of use; the applicable paragraph depends on the final article’s end use and thickness. In the European Union, plastic materials and articles intended for food contact are framed by Regulation (EU) No 10/2011, including overall migration limits and specific migration limits for additives; compliance is assessed on the final film or component, not on the neat resin. PFAS content and other additive-related concerns should be confirmed with the manufacturer if relevant to the end market. Table 2 lists the principal compliance areas and their controlling designations.

    Table 2. Regulatory and compliance matrix for blown film resin evaluation
    AreaControlling designationEvaluation note
    US food contactFDA 21 CFR 177.1520(c)Confirm applicable use conditions and food types with the manufacturer’s compliance letter.
    EU food contactRegulation (EU) No 10/2011Overall migration testing is required on the final film or article.
    REACHRegulation (EC) No 1907/2006Polymer registration status and substance of very high concern screening should be obtained from the supply chain.
    RoHSDirective 2011/65/EUApplies only when the film is incorporated into electrical and electronic equipment; base polyolefins are not expected to exceed homogeneous material heavy metal limits, but additives and pigments require review.
    Heavy metals in packagingUS TPCH model legislation / EU Packaging Directive 94/62/ECSum of lead, cadmium, mercury, and hexavalent chromium should be confirmed below 100 ppm by test.