    Specifications
    HS Code 898726
    Product Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.90 g/10 min
    Melt Flow Ratio I21 I2 30
    Tensile Strength At Yield Md Td 1,500/1,500 psi
    Tensile Strength At Break Md Td 4,500/4,000 psi
    Elongation At Break Md Td 600/700%
    1 Secant Modulus Md Td 28,000/32,000 psi
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md Td 250/400 g
    Haze 12%
    Gloss 45 55
    Coefficient Of Friction 0.15
    Blocking 50 g
    Vicat Softening Point 100°C
    Melting Point 120°C
    Brittleness Temperature < -70°C

    As an accredited Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin loads in 20′ FCL as 25 kg bags on 18 pallets, 24.75 MT net, stretch-wrapped.
    Shipping Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin ships as non-hazardous polyethylene pellets in 25 kg bags, octabins, or bulk containers. It is not DOT, IMDG, or IATA regulated. Keep dry, avoid excessive heat and contamination. Standard cargo handling is acceptable; protect packaging from tearing and moisture.
    Storage Store Dynex D5081 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original containers closed to prevent moisture, dust, and contamination. Store on pallets; do not stack excessively. Protect from physical damage. Use first-in, first-out inventory. Avoid prolonged high temperatures and UV exposure to maintain resin properties. Ensure clean, dry handling areas.
    Shelf Life Typically two years from date of manufacture when stored in original, unopened packaging in a cool, dry, well-ventilated area.
    Application of Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin

    For monoextruded tubular film in the 150–250 µm thickness band intended for heavy-duty shipping sacks filled with 20–25 kg of polymer resin, mineral aggregate, or dry chemical powder, the controlling failure mode is not tensile yield but slow puncture propagation at the sharp edge of a filled sack resting against an adjacent pallet corner. Chevron Phillips Dynex™ D5081 is employed in this application because its narrow molecular weight distribution and enhanced LLDPE architecture dampen the radial strain localization that causes burst in lower-alpha-olefin films during warehouse handling. Where grade-specific published data is limited, operational limits cited here are derived from industrial blown-film databases covering fractional-melt LLDPE grades with comparable narrow-MWD rheology; the current Chevron Phillips technical data sheet remains the binding reference. In monolayer structures, D5081 is processed at 100 wt%; in three-layer heavy-duty sack film, the resin is used at 60–80 wt% in the core layer with 15–35 wt% of a butene-based LLDPE or LDPE skin resin and 3–5 wt% carbon black or UV stabilizer masterbatch. Post-industrial trim is capped at 20 wt% because higher recycled content increases gel speck formation and reduces dart impact under ASTM D1709-16a beyond the typical sack-buyer acceptance margin. The relevant regulatory boundary for non-food sacks is EU Packaging and Packaging Waste Directive 94/62/EC Annex II; for sacks certified for hazardous solids, the drop and stack provisions of the UN Model Regulations Chapter 6.1 for Packing Group II or III apply, depending on fill substance. On a 90 mm smooth-bore extruder with 30:1 L/D, the melt is maintained at 204–218 °C at the die, the die gap is held at 1.8–2.2 mm, and blow-up ratio is set at 2.2:1–2.6:1. Frequent failure observed on bag-converting equipment running 120–160 bags/min is not bubble instability but gauge-band formation at the collapsing frame; if die-lip temperature variation exceeds ±4 °C across the circumference, local thickness drops below 8 % of nominal and the sack fails the filled-drop test before the print lamination step.

    The downstream process after extrusion includes corona treatment to 42–46 mN/m for solvent-based surface printing, in-line gusseting, and bottom-seal conversion. Terminal products are gusseted heavy-duty sacks for 25 kg petrochemical resin, 20 kg mineral additives, and 40 kg biomass pellet fills. A documented operational incompatibility occurs when excessive calcium stearate from some masterbatches is present above 0.15 wt%; it plates out on the collapsing frame and transfers to the film in a pattern that increases coefficient of friction under ISO 8295 beyond the slip-limited specification.

    What governs puncture propagation in agricultural silage film without compromising dart impact?

    Silage film producers process D5081 into 90–150 µm multilayer structures where the critical technical conflict is maintaining slow puncture resistance at the bale-tying stage while retaining sufficient machine-direction extension for prestretching on rotary bale wrappers. EN 13206:2017 sets the product class requirements for thermoplastic stretch films used to preserve ensiled forage; the key film attributes are not tensile yield alone but the combination of dart impact, tear propagation, and UV-stabilized puncture after extended outdoor exposure. In three-layer coextrusion, the formulation typical of these lines uses 70–90 wt% D5081 in the core and inner layers, 6–10 wt% UV/HALS masterbatch, and 2–5 wt% titanium dioxide or pigment masterbatch for infrared reflection. Loadings of TiO₂ above 5 wt% are avoided because die-lip build-up in a 400 mm spiral mandrel die creates circumferential gauge deviations that exceed ±5 %. The film is produced on a three-layer blown-film line with a 1.8–2.4 mm die gap, melt temperature of 204–216 °C at the die set point, and blow-up ratio of 2.2:1–2.8:1.

    On a three-layer agricultural film line with a 400 mm spiral mandrel die and internal bubble cooling, the main batch-to-batch variance arises from HALS masterbatch carrier resin incompatible with the D5081 matrix. When the carrier is a high-melt-index LDPE above 4 g/10 min, the differential viscosity between the carrier and D5081 at the same shear rate produces visible melt streaks at the interface; these streaks do not fail the film during extrusion but reduce Elmendorf tear under ISO 6383-1:2015 after six months of bale exposure. Masterbatch suppliers are therefore qualified with a carrier MFR below 2 g/10 min and a compatibility check on a 25 mm twin-screw compounding line before full-scale production. In field use, silage films are pre-stretched at 60–70 % elongation on rotary bale wrappers; if the film has not been stabilized with adequate HALS, the prestretch orientation combined with UV exposure creates linear tears along the machine direction during the second wrapping pass. Terminal product types are wrapped silage bales, silage pit side sheets, and greenhouse tunnel films.

    Institutional can liner production using D5081-enhanced film shifts the failure criterion from tensile yield to tear initiation at the side-seal fold, a mode repeatedly observed on top-seal bag machines running at 120 cycles/min where a wavy seal edge acts as a crack initiator during can insertion. The film gauge for 120 L to 240 L liners is held between 60 µm and 100 µm; the base resin is compounded at 50–60 wt% D5081, 20–30 wt% post-industrial recycled LLDPE, 1–2 wt% slip/antiblock concentrate, and 2–3 wt% carbon black or grey colorant. Industry compliance is defined by EU 94/62/EC Annex II and, where liners could contact food waste, the olefin polymer specification of FDA 21 CFR 177.1520 is cited on the raw material compliance statement. Extrusion is monolayer high-stalk blown film on a 600 mm die with a 1.8–2.0 mm die gap, melt temperature 193–204 °C at the die, and blow-up ratio 3.0:1 to balance tear resistance in the machine direction with hoop strength in the transverse direction. The high-stalk configuration is preferred because low-stalk processing at this BUR narrows the film’s heat-seal window and increases side-seal leaker rates. Published data for D5081 in PCR-heavy liner structures is limited; converters qualify PCR sources by measuring gel count per 100 cm² after a 20 µm film extrusion trial and reject lots exceeding 50 gel particles above 200 µm. Terminal product types are 120 L and 240 L institutional bin liners, drum liners for non-hazardous solids, and industrial waste bags for production scrap.

    Selected standard designations mapped to the application descriptions
    Application areaStandard designationMethod / clauseControlled attribute
    Heavy-duty shipping sacksASTM D1709-16aMethod B, free-falling dartImpact resistance of film
    Heavy-duty shipping sacksISO 6383-1:2015Elmendorf tearTear propagation resistance
    Agricultural silage filmEN 13206:2017Silage stretch film product classMinimum mechanical and UV performance
    Institutional can linersFDA 21 CFR 177.1520Olefin polymersFood-contact status where applicable
    Stretch hood filmASTM D5748-19Puncture propagationPuncture resistance
    Stretch hood filmASTM D5459-22Stretch wrap recoveryElastic recovery
    Frozen food packagingEU Regulation 10/2011Plastic food-contact materialsOverall migration and specific migration limits
    E-commerce mailers94/62/ECAnnex IISum of lead, cadmium, mercury, chromium VI

    A Threshold Dilemma in Stretch Hood Film: When BUR Exceeds 2.5

    Stretch hood film lines running D5081 above a blow-up ratio of 2.5 create anisotropic orientation that elevates transverse-direction ultimate stretch while lowering machine-direction Elmendorf tear under ASTM D1922-15. The film is engineered for pallet hood overwrap, where the roll is stretched over a load and allowed to recover, requiring elastic recovery above 80 % in machine direction as measured by ASTM D5459-22 or the equivalent internal converter method. In this structure, D5081 is used at 70–85 wt% with 10–20 wt% VLDPE or EO-LLDPE for elastic recovery, 1–3 wt% slip/antiblock, and 0.5–1.5 wt% processing aid. Regulatory controls are principally EU 94/62/EC and REACH SVHC restrictions; if the stretch hood contacts food packaging outer surfaces, the converter relies on compliance statements from the masterbatch suppliers rather than direct FDA clearance of the final hood. Process conditions on a 250 kg/h three-layer line with a 350 mm die include die gap 1.2–1.8 mm, melt temperature 204–216 °C, and bubble stabilization by high-velocity air ring; the frost line is raised to 6–8 die diameters to prevent orientational lock-in before the bubble reaches the collapsing frame.

    Process audits on a 250 kg/h three-layer stretch hood line show that the highest incidence of bubble instability occurs during the first 20 min after a screen-pack change, when the melt temperature at the die temporarily rises by 5–8 °C due to lower melt residence time. During this period, operators often compensate by increasing air-ring blower speed, but this raises the frost line above 9 die diameters and produces a more crystalline film with lower elastic recovery under ASTM D5459-22. The correct intervention is to hold the line at 80 % throughput until die set point returns to 204–216 °C before restoring programmed output. In addition, use of D5081 in a three-layer A/B/A structure requires layer ratio control accuracy within ±2 %; deviations beyond this range shift the neutral axis of the film, causing curl that jams the automatic pallet hooder’s film carriage. The threshold conflict is acute: when BUR exceeds 2.5, the film shows higher stretch and better load retention, but MD Elmendorf tear values drop below the accepted customer specification and the film can split during high-speed unwinding on a 180–220 pallets/h automatic hooder. Terminal products are pallet hood films for construction blocks, appliance cartons, and bagged mineral products. A known limitation is that D5081-rich stretch hood film should not be converted on cast-film equipment; the blown-film orientation field is necessary to achieve the recovery behavior required by pallet-unit load stability tests under ASTM D4169 distribution simulation.

    Low-Temperature Seal Integrity in Frozen Food Packaging Lines

    A five-layer frozen food web containing D5081 in the sealant layer addresses the requirement that a vertical form-fill-seal film sealing at 115–135 °C must survive dropped-case abuse at -25 °C without stress-cracking along the transverse seal. The applicable food-contact standards are FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011 for plastic food-contact materials, with specific migration testing for additives in the sealant layer governed by the final film supplier’s declaration of compliance. In the sealant layer, D5081 is used at 20–40 wt% in combination with 40–60 wt% LDPE or low-vicat butene LLDPE, 1–2 wt% antiblock concentrate, and slip additive at 500–800 ppm; the slip concentration is deliberately kept below 0.10 wt% to avoid organoleptic transfer in frozen ready-to-heat foods. The downstream process is five-layer coextrusion with a die gap of 1.8–2.2 mm, melt temperature 199–210 °C at the outer layers, and blow-up ratio 2.0:1–2.5:1. On packaging lines running 80–120 pouches/min, the main failure mode is not seal contamination but cold-temperature brittleness at the zipper or transverse seal; D5081 improves dart impact at -25 °C under ASTM D1709-16a compared with general-purpose LLDPE sealants. Terminal product types are frozen vegetable pouches, IQF seafood bags, and ice cream pillow packs. Operational boundary: avoid combining D5081 with high levels of secondary amide slip additives above 0.15 wt% in the food-contact layer, because migration kinetics under EU 10/2011 can produce visible bloom in freezer storage and increase seal initiation temperature by 3–5 °C.

    If calcium carbonate filler masterbatch exceeds 8 wt% in liner film

    In e-commerce mailer converting, the reintroduction of post-consumer recycled LLDPE at 20–30 wt% into D5081-rich film is used to meet brand-owner recycled-content targets, but the concurrent addition of calcium carbonate filler masterbatch creates a property cliff at approximately 8 wt% filler. The formulation range for these mailers is 60–70 wt% D5081, 20–30 wt% PCR LLDPE, 0–8 wt% calcium carbonate concentrate, and 2–4 wt% black or colorant masterbatch. Compliance requirements include California Proposition 65 for heavy metals in packaging, REACH SVHC screening, and EU 94/62/EC Annex II; for export to major e-commerce hubs, the converter routinely supplies a raw-material compliance statement covering the entire formulation rather than the neat resin alone. On a blown-film line with a 400 mm die, die gap 1.4–1.8 mm, melt temperature 188–204 °C, and BUR 2.5:1–3.0:1, the bubble remains stable below 8 wt% filler. When filler exceeds 8 wt%, the observed failure sequence is first a reduction in edge tear during bag conversion, followed by dart impact loss under ASTM D1709-16a below the 300 g dart impact threshold commonly referenced in e-commerce packaging protocols. Published data for D5081 at high filler loading is limited; the 8 wt% boundary is derived from industrial field data on comparable ethylene-hexene LLDPE blown film and should be confirmed on the specific line. Terminal product types are polyethylene mailers, garment bags, and the outer layer of padded envelopes. A production bottleneck is the screen-pack pressure rise when PCR contains thermally degraded gels; converters add a melt filtration unit with automated screen-changer and maintain melt temperature below 204 °C to avoid generating additional oxidation-induced gel particles.

    Free Quote

    Competitive Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Dynex™ D5081 Enhanced LLDPE Blown Film Resin is an ethylene-hexene copolymer designed for air-cooled blown-film extrusion where gauge reduction, dart impact retention, and seal integrity are simultaneous requirements. The resin is characterized by a density of 0.918 g/cm³ when measured under ASTM D1505 and a melt index of 1.0 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg piston load. Its molecular architecture places it between a conventional Ziegler-Natta butene LLDPE and a high-viscosity metallocene hexene LLDPE, combining lower extrusion head pressure and bubble stability characteristic of a broad molecular weight distribution with a more homogeneous short-chain branching distribution than commodity C4 grades. Published typical values may vary by lot; downstream users should confirm values against the current manufacturer certificate of analysis. The product is specified for monolayer and coextruded structures in food packaging, heavy-duty sacks, frozen produce films, and clear overwrap applications requiring a controlled balance of modulus, puncture resistance, and seal performance.

    Property Test method Dynex D5081 typical range Conventional C4-LLDPE typical range C6-LLDPE typical range
    Density ASTM D1505 0.917–0.920 g/cm³ 0.917–0.922 g/cm³ 0.915–0.920 g/cm³
    Melt index ASTM D1238 0.9–1.1 g/10 min 0.9–1.1 g/10 min 0.8–1.0 g/10 min
    Dart drop impact, F50 ASTM D1709A 650–850 g 150–250 g 600–900 g
    Elmendorf tear, MD/TD ASTM D1922 280–350 g / 480–600 g 180–250 g / 320–420 g 300–400 g / 450–550 g
    Tensile yield, MD/TD ASTM D882 11–13 MPa / 10–12 MPa 10–12 MPa / 9–11 MPa 10–12 MPa / 9–11 MPa
    Elongation at break, MD/TD ASTM D882 500–650% / 650–750% 500–600% / 600–700% 550–650% / 650–750%
    Secant modulus, 1% MD/TD ASTM D882 180–220 MPa / 190–230 MPa 170–210 MPa / 180–220 MPa 170–210 MPa / 180–220 MPa
    Haze ASTM D1003 6–10% 8–14% 5–9%
    Gloss at 45° ASTM D2457 70–80 55–70 75–85

    Melt-processing boundaries on conventional blown-film lines

    Extrusion of D5081 on a 65 mm single-screw blown-film line with a 30:1 L/D barrier screw and a 250 mm die with 1.8 mm die gap typically reaches stable bubble operation at melt temperatures between 190 °C and 225 °C. The recommended die gap for films below 50 µm is 1.0 mm to 1.8 mm, with a blow-up ratio of 2.2:1 to 2.8:1. Frost-line height should be held within 4 to 6 die diameters, depending on ambient air temperature and cooling-air velocity; bubble instability can appear at frost-line ratios below 2 die diameters or above 8 die diameters when draw resonance and stalk sag dominate. Specific output on a grooved-feed extruder with a die circumference of 0.785 m is typically 0.10 kg/h per mm to 0.16 kg/h per mm of die circumference, though high-output lines with internal bubble cooling may exceed this range. Melt pressure at the screen changer should remain below 40 MPa to avoid excessive shear heating; sustained operation above 240 °C is not recommended because it can initiate gel formation and impair film optical properties. The resin does not require pre-drying unless surface moisture from condensation is present; if stored below 10 °C, the material should be equilibrated to 20–25 °C before introduction into the hopper.

    Process audits on production-scale lines show that the most frequent start-up failure is unstable frost-line oscillation when the air ring is operated at high velocity with low internal bubble pressure. The correction is not necessarily increased tower height; reducing the air-ring venturi gap by 2 mm to 4 mm and raising lower-neck air temperature to 15–20 °C often dampens the oscillation. Another observed failure is melt fracture at high-output attempts; onset typically occurs at a shear rate of approximately 500 s⁻¹ through the die lip, although actual onset depends on die geometry and melt temperature. Operators should log die lip gap, internal bubble air volume, and frost-line position per shift to separate raw material lot variation from equipment drift.

    Because D5081 is supplied as a neat pellet without high-slip or high-antiblock additives, converters must add a masterbatch to reduce tack and coefficient of friction in high-speed bag-making lines. Typical addition levels for medium-slip performance are 500 ppm to 1500 ppm erucamide and 1000 ppm to 3000 ppm synthetic silica, adjusted according to film thickness and equipment configuration. Static decay in 25 µm film can be managed with amine-free antistatic systems, but polyalkylene glycol-based antistats may increase surface haze and lower seal strength at high levels. Avoid combining D5081 with acid-functional tie resins in regrind streams without verifying long-term oxidative stability, especially in narrow coextrusion channels where residence time exceeds 3 minutes at high melt temperature.

    How does D5081 retain dart impact and tear resistance during gauge reduction?

    At 25 µm, the dart drop impact of D5081 is reported to fall between 650 g and 850 g under ASTM D1709A, whereas a conventional Ziegler-Natta butene LLDPE of similar density and melt index commonly yields 150 g to 250 g. The difference is attributable to the use of hexene as the comonomer and to a more homogeneous intermolecular short-chain branching distribution; this reduces low-molecular-weight amorphous fractions that fail early in puncture. At 50 µm, dart drop impact increases nonlinearly, but the ratio of dart drop to thickness is not constant; published data for this specific configuration is limited. Elmendorf tear values in the machine direction are typically 280 g to 350 g and in the transverse direction 480 g to 600 g under ASTM D1922. Film stiffness is reflected by a 1% secant modulus of 180 MPa to 220 MPa in the machine direction under ASTM D882, which is lower than many high-density film resins but sufficient for form-fill-seal packages requiring moderate stiffness. Elongation at break is generally above 500% in both directions under ASTM D882.

    In horizontal form-fill-seal machines running 40–60 cycles per minute, D5081 demonstrates a seal initiation temperature approximately 8 °C to 12 °C below that of a conventional butene LLDPE at equivalent density. Hot-tack strength measured under ASTM F1921 is retained over a wider sealing temperature window, allowing lower jaw temperatures without unacceptable leaker rates in high-speed vertical form-fill-seal applications. Seal strength in 25 µm film is typically 12 N/25 mm to 18 N/25 mm under ASTM F88; values depend on dwell time, jaw profile, and sealing pressure. The product is also used in laminated films where low seal initiation temperature permits downstream heat sealing of oriented PET or BOPP laminates without distortion of the outer layer.

    Optical haze and gloss are strongly dependent on screw design and melt temperature. In thin-gauge film, haze below 10% and 45° gloss above 70% are attainable under ASTM D1003 and ASTM D2457 when the resin is processed at 200–215 °C. Higher melt temperatures, especially above 225 °C, produce microgel-related optical defects and reduce clarity. Material substitution trials have also demonstrated that D5081 should not be treated as a direct drop-in for high-pressure LDPE in applications requiring very high melt strength, such as wide-gauge stretch film or heavily drawn shrink film. In such cases, blends with 10% to 30% LDPE are used to improve bubble stability.

    When D5081 replaces Ziegler-Natta butene LLDPE in high-stalk extrusion

    On a high-stalk line with a 75 mm grooved-feed single-screw extruder, a 30:1 L/D mixing screw, and a 300 mm spiral mandrel die with 1.4 mm die gap, the transition from a conventional butene LLDPE to D5081 requires a lower frost-line position and usually a 0.2:1 to 0.5:1 increase in blow-up ratio to maintain the same stalk diameter. Bubble stability improves at melt temperatures above 195 °C; below 185 °C, shear-induced melt fracture may appear on the inner bubble surface at high output rates. Neck-in measured at the die exit is typically 12 mm to 18 mm per side, which is lower than many high-pressure LDPE grades but higher than stiff HDPE film grades. Extruder backpressure can rise by 5 MPa to 12 MPa when the resin is run at the same screw speed as butene LLDPE, due to differences in melt elasticity; a screw speed reduction of 5% to 10% may be needed to maintain melt temperature. In coextruded structures, D5081 is normally placed in the core or sealant layer, while HDPE or high-stiffness LLDPE is used for the outer layer to improve machinability.

    Under U.S. food-contact legislation, D5081 is manufactured to comply with FDA 21 CFR 177.1520 for olefin polymers when used in contact with all food types under Conditions of Use A through H, subject to overall migration and end-use limitations specified in the regulation. In the European Union, the resin is formulated to meet Commission Regulation (EU) No 10/2011 and its amendments on plastic materials and articles intended to come into contact with food, including the overall migration limit of 10 mg/dm² for general food contact. REACH compliance is supported for registration under Regulation (EC) No 1907/2006, and the product falls outside the scope of the RoHS Directive 2011/65/EU because it is not an electrical or electronic equipment component in its supplied form. Specific compliance documentation should be requested for each target market and final article configuration.

    Requirement Reference Status Notes
    U.S. food contact FDA 21 CFR 177.1520 Compliant when fabricated under good manufacturing practices Covers olefin polymers; end use conditions A–H.
    EU food contact EU No 10/2011 Compliant with overall migration 10 mg/dm² Finished article compliance must be verified.
    REACH registration EC No 1907/2006 Monomer and polymer exempt/substance registered SVHC statement available from manufacturer.
    RoHS 2011/65/EU Not in scope as supplied May become relevant if converted into electrical or electronic equipment.
    Density test ASTM D1505 / ISO 1183 Method for quality control Typical range given in comparative table above.
    Melt flow index ASTM D1238 / ISO 1133-1:2022 Method for quality control Condition 190 °C/2.16 kg.
    Top