| HS Code | 191073 |
| Polymertype | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Hexene-1 |
| Meltindex | 2.0 g/10 min at 190°C/2.16 kg |
| Density | 0.918 g/cm³ |
| Meltingpoint | 123 °C |
| Vicatsofteningpoint | 96 °C |
| Tensilestrengthatyield | 10.3 MPa |
| Tensilestrengthatbreak | 25.5 MPa |
| Elongationatbreak | 600% |
| Flexuralmodulus | 200 MPa |
| Dartdropimpact | 120 g |
| Elmendorftearmd | 200 g |
| Elmendorfteartd | 350 g |
| Haze | 7% |
| Gloss | 80% |
| Coefficientoffriction | 0.2 |
| Heatsealinitiationtemperature | 100 °C |
As an accredited Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer is packaged in 25 kg polyethylene-lined bags, 40 per pallet (1,000 kg). |
| Container Loading (20′ FCL) | 20′ FCL container loaded with palletized 25kg bags of Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer, shrink-wrapped for export. |
| Shipping | Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer is a non-hazardous polyethylene resin pellet. Ship in dry, clean, closed containers, typically 25 kg bags, octabins, or bulk trucks/railcars. Not regulated for DOT, IMDG, IATA, or ADR. Protect from moisture, heat, and contamination; no special hazard labels required. |
| Storage | Store Chevron Phillips 7120T LLDPE resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and oxidizing agents. Keep original containers or bags closed to prevent moisture, dust, and contamination. Palletize securely and avoid excessive stacking. Protect from prolonged UV exposure and maintain moderate temperatures. Follow local regulations and manufacturer’s SDS for safe handling and storage. |
| Shelf Life | Shelf life is typically 24 months from date of manufacture when stored in original packaging in a cool, dry area. |
High-speed cast pallet wrap lines running 7120T at melt temperatures between 215°C and 240°C through 30:1 to 33:1 L/D barrier screws with Maddock mixing sections encounter a persistent processing conflict: the narrow-molecular-weight hexene-copolymer architecture supports high elongation, but the same chain architecture narrows the edge-pinning window at line speeds above 350 m/min. On a 2,000 mm cast die with 0.5–0.9 mm die gap and 30–70 mm air gap, edge bead thickness can increase by 2–4% when LDPE content is reduced below 10 wt%; conversely, LDPE additions above 25 wt% produce measurable reductions in ASTM D5748 puncture resistance at 20 µm. Compliance for industrial pallet wrap rests on REACH 1907/2006 Annex XVII and RoHS 2011/65/EU for additives and heavy metals; because the film is not classified as food contact, FDA 21 CFR 177.1520 is not the governing reference unless line clearance is specifically managed for food-grade production. The typical formulation splits the polymer phase as 75–88 wt% 7120T, 10–20 wt% LDPE with a melt index below 2.0 g/10 min, 1.0–2.5 phr polyisobutylene cling agent, and 0.05–0.15 phr slip/antiblock masterbatch. Downstream production on a high-speed cast line requires electrostatic pinning or air-knife edge pinning, a chrome-plated chill roll set to 18–26°C, and vacuum-box extraction at the die exit. Line speeds between 300 m/min and 500 m/min are achievable only if melt pressure after the screen changer remains below 250 bar; higher pressures indicate insufficient mixing or filter blockage. The terminal product range includes 12–35 µm machine-grade pallet wrap, pre-stretched hand film, and mini-roll wrap for bundle packaging. Thickness tolerance is checked per ASTM D882 tensile specimens cut transversally and longitudinally, with cross-web gauge variation maintained at ±2.0% or better. Pre-stretch ratios of 200–300% are common for machine wrap, while off-line pre-stretch systems can reach 350% if the film contains greater than 80 wt% 7120T. Published data for this specific configuration is limited, but line-scale observations indicate that cling retention drops below acceptable levels after 90 days of warehouse storage above 35°C.
Pre-drying of 7120T is generally unnecessary when the resin is stored in silos with moisture levels below 0.05 wt%; however, in ambient conditions above 60% RH, surface condensation on cold pellets transferred from outdoor silo lines can generate bubble faults and die-face contamination. Heavy-duty sack film produced from 7120T is typically a 3-layer coextrusion in which the core carries 70–85 wt% 7120T and the skin layers are diluted with 10–20 wt% LDPE to improve bubble stability. Carbon black masterbatch at 2–4 wt% is added for UV resistance in extended outdoor or warehouse exposure, and a fluoroelastomer PPA at 200–400 ppm is introduced to delay die-lip buildup. Compliance for non-food industrial sacks is governed by ISO 7965-2 for drop resistance, ASTM D1709 for dart impact, and REACH 1907/2006 Annex XVII for heavy-metal and additive restrictions; food contact grades, if specified, must comply with FDA 21 CFR 177.1520(c)(3.2) and EU Regulation (EU) No 10/2011 Annex I. The downstream process uses blown film extrusion with a 2.2–2.8 mm die gap, 2.2:1–3.0:1 blow-up ratio, 8–12 die-diameter frost line height, and melt temperatures between 195°C and 220°C. On a 250 mm die running at 0.8–1.2 kg/(cm·h) specific output, bubble stability improves when the outer layers contain at least 10 wt% LDPE, but dart impact at 100 µm declines when recycled LLDPE content exceeds 15 wt% of total polymer mass. The terminal products include heavy-duty shipping sacks for polymer pellets, mineral fillers, fertilizers, and petrochemical powders. These are converted on form-fill-seal lines with back-seam seal strength tested at 85–115°C seal-bar temperature. High-shear extrusion above 250°C should be avoided because oxidative gel speck formation accelerates in hexene-copolymer LLDPE at extended residence times exceeding 5 minutes.
When 7120T is coextruded with a UV-stabilised skin layer for round bale silage wrap, the critical performance criterion is not high oxygen barrier but mechanical exclusion of oxygen through sustained cling, tear resistance, and puncture resistance after outdoor weathering. The silage film structure commonly consists of 75–85 wt% 7120T in the core and 15–25 wt% total skin layers containing 6–10 wt% UV masterbatch and 3–6 wt% white or titanium dioxide masterbatch of the skin-layer mass. Compliance is evaluated under EN 13206 for agricultural covering films, ISO 527-3 for tensile elongation, ASTM D4329 for accelerated weathering exposure, and REACH 1907/2006 Annex XVII for heavy-metal restrictions in additives. The downstream production process is blown film coextrusion on a 3-layer die with 2.0–2.5 mm die gap, 1.8:1–2.2:1 blow-up ratio, melt temperatures between 200°C and 225°C, and air-ring cooling configured to maintain a frost line height above 6 die diameters. The terminal product range includes 25–30 µm round bale wrap, silage bags up to 200 µm, and silo cover sheets. Operational boundaries are defined by UV masterbatch concentration: below 6 wt% of the skin layer, failure occurs before 12 months of outdoor exposure in ASTM D4329 UVA-340 testing; above 10 wt%, machine-direction tensile strength at 200% elongation declines enough to compromise pre-stretch on round-bale wrappers. Published data for this specific 7120T configuration is limited, but film converter records indicate that carbon black-loaded silage film without sufficient dispersion can produce tear propagation at die-line weld regions after repeated bale wrapping.
| Compliance Reference | Designation | Technical Criterion |
|---|---|---|
| US FDA | 21 CFR 177.1520(c)(3.2) | Olefin polymer food-contact clearance with end-use temperature and time conditions |
| EU | (EU) No 10/2011 Annex I | Overall migration limit of 10 mg/dm² for food contact plastics |
| GMP | EC 2023/2006 | Production hygiene and traceability for food-contact film lines |
| Hot tack | ASTM F1921 | Hot seal strength of 0.2–0.5 N/mm at 95–115°C |
Frozen food packaging converters use 7120T in 3-layer or 5-layer coextruded blown film to combine low-temperature dart impact and controlled seal initiation. The sealant layer is typically 55–65 wt% 7120T, 25–35 wt% LDPE, and 5–10 wt% metallocene plastomer; the core layer uses 60–80 wt% 7120T with the balance LDPE. Film extrusion occurs through 1.8–2.4 mm die gaps at 2.0:1–2.5:1 blow-up ratio and melt temperatures of 190–220°C, followed by vertical form-fill-seal conversion with seal initiation between 95°C and 115°C. Low-temperature puncture resistance is measured by ASTM D3763 at -20°C, and dart impact is measured by ASTM D1709 Method A at -25°C. When the plastomer fraction in the sealant layer exceeds 10 wt%, cold-temperature seal strength improves but the film may block on warmed storage; below 5 wt%, seal initiation can exceed the jaw temperature window in high-speed vertical form-fill-seal operations. Terminal product types include frozen vegetable pouches, IQF seafood bags, and frozen dough bags for bakery pre-proofed products. The film must also meet organoleptic inspection under EU Regulation (EU) No 10/2011 for food packaging. Published data for 7120T in this exact formulation is limited, but film converter records indicate that the hexene comonomer provides more stable low-temperature impact than butene-copolymer LLDPE at equal density and melt index.
In coextruded temporary protective films for pre-painted aluminium coil, high-gloss appliance panels, and sanitary ware, 7120T functions as a polyolefin core that resists forming-stress whitening during coil bending and slitting. Compliance is governed primarily by REACH 1907/2006 and RoHS 2011/65/EU for heavy metals, while peel adhesion is tested after application to stainless steel or coil per ASTM D3330/D3330M and clean-removal ageing is verified at 60°C for 168 h. The formulation uses 100 phr 7120T with 0.2–0.5 phr antioxidant masterbatch in the film layer; the pressure-sensitive adhesive is applied at a coat weight of 5–15 g/m² for low-tack grades and 20–35 g/m² for high-tack grades. Corona treatment is maintained at 38–42 mN/m before adhesive application. The downstream process is cast film extrusion with a 0.5–0.8 mm die gap, chill roll temperature of 18–24°C, line speeds between 120 m/min and 300 m/min, and inline corona treatment followed by slot-die adhesive coating or lamination. Terminal products include temporary protective films for coiled metal, thermoplastic sheets, sanitary ware, and profile wrapping; the film is removed after fabrication and is not intended for food contact. Limitations include the following: adhesive systems containing ketone or aromatic solvents at high coat weights can swell the polyethylene surface and reduce peel, and storage above 40°C may increase adhesion build-up beyond clean-removal limits because low-molecular-weight tackifier migration into the LLDPE layer accelerates within 72 h.
Competitive Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips 7120T LLDPE Cast/Blown Resin, Hexene Copolymer is a linear low-density polyethylene produced by copolymerization of ethylene with a hexene comonomer. The grade is positioned for cast film and selected blown film constructions in which the higher tie-molecule population of hexene copolymerization is used to shift the balance of dart impact and Elmendorf tear relative to butene-based LLDPE. Nominal melt mass-flow rate is 2.0 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238 and ISO 1133-1:2022; nominal density is 0.918 g/cm³ according to ASTM D1505 and ISO 1183-1:2019. The base resin is typically compounded with converter-selected antiblock, slip, and processing-aid packages at the film line, which permits the same pellet to be used in cast stretch film, industrial laminating film, protective masking film, and thin-gauge blown film without a fixed additive profile.
The hexene comonomer introduces predominantly butyl short-chain branches along the polyethylene backbone. At equivalent density, a hexene copolymer can produce a broader distribution of branches that increases the probability of load-bearing tie molecules between adjacent lamellae. This molecular architecture is industrially significant because it contributes to elevated dart impact and transverse-direction tear without requiring a reduction in melt index below 2.0 g/10 min. During cast film stretching, the tie-molecule network resists puncture and film splitting at corner and radius points on spiral mandrel stretch-wrapping equipment. Published data for this specific lot configuration is limited; lot-to-lot variation in comonomer distribution should be verified by gel permeation chromatography with triple detection or by differential scanning calorimetry after annealing.
The principal difference is the length of the short-chain branch introduced by the comonomer: butene contributes ethyl branches, while hexene contributes butyl branches. In a cast film resin with a nominal density of 0.918 g/cm³, the longer butyl branch reduces the regularity of the crystalline lattice and alters the distribution of interlamellar tie molecules. This is not simply a density effect; two resins of identical density and melt index may have different dart impact values if the comonomer type differs. The practical consequence on a production line is that 7120T can be drawn to film thicknesses below 15 µm while retaining puncture resistance that is typically associated with butene-copolymer film of 25 µm. The improvement in toughness is most apparent in high-speed dart impact tests conducted under ASTM D1709 Method B and in slow puncture testing such as ASTM D5748.
The two physical properties that define the grade for incoming quality control are melt mass-flow rate and density. The melt mass-flow rate is measured at 190 °C with a 2.16 kg weight and is nominally 2.0 g/10 min; this value places the resin in the medium-flow range for cast film and allows melt temperatures to be kept lower than would be required for a 1.0 g/10 min resin. Density is measured after conditioning per ASTM D1505 or ISO 1183-1:2019 and is nominally 0.918 g/cm³. Typical certificate-of-analysis documentation includes lot-specific values for both properties; differences between supplier melt index and converter melt index are commonly observed due to moisture, thermal degradation, or calibration drift in melt indexer temperature control. The grade is also characterized by gel permeation chromatography and differential scanning calorimetry, but these methods are not normally part of a converter’s incoming inspection protocol.
Film characterization on a cast line is normally performed on 25 µm or 20 µm laboratory samples after conditioning at 23 °C and 50% relative humidity for at least 40 h according to ASTM D618. Tensile properties are measured under ASTM D882; haze under ASTM D1003; gloss at 45° under ASTM D2457; coefficient of friction under ASTM D1894; Elmendorf tear under ASTM D1922; dart impact under ASTM D1709 Method A or B. Thickness profile data from a capacitance or beta gauge should be analyzed for 2σ variation rather than average thickness alone. Frequent film breakage at a specific gauge point is usually traceable to die bolt adjustment, air gap asymmetry, or chill roll surface chatter rather than to the resin itself.
A converter replacing a butene-based LLDPE with 7120T typically observes a change in tear balance and an increase in stretch-film puncture resistance. The hexene comonomer increases the concentration of tie molecules, and this is reflected in Elmendorf tear values measured according to ASTM D1922. The resin’s 2.0 g/10 min melt flow rate is selected to maintain film tensile elongation at break, measured by ASTM D882, because an excessively high melt flow rate would reduce the molecular weight and compromise tensile strength. The degree of downgauging that is possible on a given line depends on the cast film line’s gauge control system; thickness gauges capable of measuring ±0.1 µm deviation allow film thickness to be reduced more consistently than older scanning systems. Published data for this specific formulation is limited, and converters should confirm lot-specific dart impact and tear values before reducing film gauge.
On a production-scale cast film line using a 90 mm single-screw extruder with a 30:1 L/D barrier screw, 7120T is usually processed with barrel temperatures rising from 180 °C in the feed throat to 240 °C in the metering zone. Adapter and flat-die zones are set between 240 °C and 280 °C, and the chill roll is held between 15 °C and 30 °C depending on line speed and film gauge. Air gap distance from die lip to chill roll is typically maintained at 150 mm to 300 mm to balance melt relaxation, web stability, and film flatness. Die lip build-up can occur when the resin is run without a fluoropolymer processing aid; in such cases, the die temperature should be raised by 5 °C to 10 °C before adjusting line speed. Pressure fluctuations at the melt pump are an early indicator of lot-to-lot viscosity variation and should be logged against the supplier’s melt flow rate data.
The shear viscosity of 7120T at cast film processing temperatures follows typical LLDPE behaviour: viscosity decreases with increasing shear rate, and the onset of melt fracture on a flat die occurs when wall shear stress exceeds approximately 0.14 MPa to 0.20 MPa. A fluoropolymer processing aid reduces this by coating the die metal surface, but purge times of 30 min to 60 min may be required before melt fracture is eliminated. Start-up after a material change from LDPE to 7120T should include a low-speed purge of 15 min to 20 min at 200 °C before bringing the line to target speed. These parameters are equipment-specific and are not guaranteed by the resin supplier; they are reported as industrial start-up practice.
In blown film, 7120T is processed with die gaps between 1.5 mm and 2.5 mm and blow-up ratios from 2.0:1 to 3.0:1. The bubble should be stabilized with a dual-lip air ring rather than a single-lip air ring, because the lower melt strength of LLDPE requires higher air velocity without excessive bubble flutter. Frost line height is normally held at 4 to 8 die diameters above the die exit, depending on ambient temperature and film gauge. Internal bubble cooling is recommended when output exceeds 150 kg/h on a 100 mm die; without internal cooling, the bubble becomes unstable and film thickness standard deviation increases. Extrusion melt temperatures above 260 °C are generally unnecessary and may cause oxidation-induced gel formation, which appears as lens-like defects in thin-gauge blown film.
Octene-based LLDPE introduces hexyl branches that are longer than the butyl branches of hexene, and at equal density this can produce greater dart impact and slow puncture resistance in some film formulations. Metallocene catalysed hexene copolymers may have a narrower molecular weight distribution than a conventional Ziegler-Natta grade, which reduces the amount of high-molecular-weight tail and can influence melt pressure, die swell, and seal initiation temperature. The 7120T grade is not represented as a drop-in for metallocene grades in all applications; lab-scale draw resonance studies and production-scale cast film trials are required when switching between these polymer architectures. The choice between 7120T and an octene or metallocene grade is therefore controlled by the converter’s specific balance of Elmendorf tear, tensile yield, haze, and extrusion pressure.
The base resin is normally converted with a masterbatch containing erucamide slip and synthetic silica antiblock. Migration of erucamide to the film surface follows diffusion kinetics that are temperature-dependent; at a film storage temperature of 23 °C, equilibrium coefficient of friction is often reached only after 24 h to 72 h. Higher antiblock loadings reduce blocking in roll form but increase haze; the optimum loading for a 20 µm cast film is therefore determined on the specific film line rather than from supplier pellet data. Fluoropolymer processing-aid masterbatches are used at 200 ppm to 600 ppm as active content to reduce die lip build-up and melt fracture. Combinations of 7120T with hindered amine light stabilizers are generally compatible, but excessive peroxide-based masterbatches should be avoided because they may reduce molecular weight during extended residence times.
The grade is used in packaging applications subject to regional food-contact requirements. Compliance is determined on the finished article, not solely on the pellet; the following regulatory documentation is used for the end-use declaration.
| Regulation / Standard | Scope | Test or Documentation Method |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Finished-article extraction testing under use conditions |
| EU No 10/2011 | Plastics in food contact | Specific migration testing per EN 1186 and EN 13130 |
| REACH (EC) No 1907/2006 | Registration and SVHC disclosure | Polymer exemption; substance declaration from supplier |
| RoHS Directive 2011/65/EU | Restricted substances in electrical equipment | IEC 62321 XRF screening on finished component |
Polyolefin pellets are not hygroscopic, but surface condensation is a practical source of film defects when cold pellets are loaded into a hopper under plant conditions above 60% relative humidity. If pellets are stored below dew point or moved from an unheated warehouse into a heated production area, surface moisture should be removed by a short hot-air drying step at 60 °C to 80 °C for 2 h to 4 h or by hopper throat desiccant air purging. Moisture-related defects in cast film include splay, bubble inclusion, and inconsistent melt pressure, while blown film may show pinholes and frost line oscillation. Drying beyond 4 h is not required and prolonged high-temperature residence in a desiccant dryer may accelerate additive degradation or pellet sticking. Resin from open gaylords should be protected from airborne silica dust and conveying-system fines, because fines can create gel-like defects that are difficult to distinguish from crosslinked polymer.