Chevron Phillips 7120st Lldpe Blown Film Resin Hexene Copolymer

Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer

    • Product Name: Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 292522
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Copolymer Type Hexene
    Density 0.918 g/cm3
    Melt Index 190 C 2 16 Kg 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1500 psi
    Tensile Strength At Break Md 5000 psi
    Tensile Strength At Break Td 4500 psi
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Dart Impact Strength 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 12%
    Gloss 45 60%
    Coefficient Of Friction 0.2
    Heat Seal Initiation Temperature 110 °C
    Low Temperature Brittleness < -70 °C

    As an accredited Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer is packaged in 25 kg polyethylene bags, palletized for shipment.
    Container Loading (20′ FCL) 20′ FCL container loading: Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer in 25 kg bags, palletized and shrink-wrapped.
    Shipping Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer is shipped as non-hazardous solid resin pellets in 25-kg polyethylene bags on pallets, stretch-wrapped, or in bulk lined trucks/railcars. Store in a cool, dry area away from direct sunlight, heat, and moisture. No DOT hazard classification; normal industrial handling applies.
    Storage Store 7120ST LLDPE resin in a cool, dry, well-ventilated area in sealed original bags or containers. Keep away from direct sunlight, heat, ignition sources, moisture, and oxidizing materials. Avoid dust and contamination; use first-in, first-out stock rotation. Protect pallets from ground moisture and stack safely to prevent bag damage. Prolonged UV exposure should be avoided.
    Shelf Life Product has no established shelf life; store in cool, dry, well-ventilated area away from heat, sunlight, ignition sources, and moisture.
    Application of Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer

    Rigid-container liners and heavy-duty refuse sacks converted from Chevron Phillips 7120ST are processed on grooved-feed single-screw blown film extruders with a barrier screw and 25:1 to 30:1 L/D. The nominal 0.918 g/cm³ density and 1.0 dg/min melt index of the hexene copolymer place the resin at the high-toughness end of LLDPE blown film grades. For liner gauge between 50 μm and 80 μm, the die gap is held at 1.8–2.5 mm to delay melt fracture and to preserve transverse direction tear. A blow-up ratio of 2.0:1 to 2.6:1 is maintained, with melt temperature 190–225 °C across the adapter and die. Screen packs at 40/80/100 mesh protect the die from carbonized gels and metal fines, but screen blinding above 320 bar pressure drop is the more frequent production limit than motor torque on 80–90 mm lines. Slip-antiblock packages using erucamide at 800–1200 ppm and natural silica at 2500–5000 ppm are metered at the feed throat after a dry-blend or masterbatch calibration. These additive levels are starting points, not supplier limits, because pellet humidity, regrind level and screw shear alter surface bloom. Dart impact for a 50 μm industrial liner is commonly specified at 250–400 g under ASTM D1709 Method B, while Elmendorf tear in the machine direction is quantified by ASTM D1922. The hexene branch architecture gives lower low-temperature brittleness than butene LLDPE at equal density, which is the technical rationale for selecting 7120ST for liners exposed to frozen product discharge. ESCR under ASTM D1693 Condition A at 50 °C in 100% Igepal CO-630 is the accepted predictor for detergent and chemical-containing sack liners, with many end-user specifications requiring 50% failure at 500 h or longer. Film for printed industrial liners is corona-treated inline to 38–42 mN/m and wound with edge-guide tension control to avoid bag-side dart failures caused by surface scratches.

    What Restricts Heat Seal Initiation Temperature in 7120ST/LDPE Blends?

    Heat seal initiation is dominated by the comonomer type and density rather than by melt index alone. In dry-food and bakery packaging webs, 7120ST is blended with high-pressure LDPE at 80/20 or 70/30 ratios by weight. The purpose is not only to lower seal initiation but also to improve bubble stability at high throughput and to widen the sealing window on rotary and pouch machines. Seal initiation temperature is measured by ASTM F2029, while hot tack is measured by ASTM F1921 on a J&B or equivalent hot-tack test apparatus. A 70/30 7120ST/LDPE blend commonly shifts the seal initiation point downward by 5–10 °C relative to the unblended C6 LLDPE, but published data for this exact blend is limited and must be re-established on the target extrusion line because die gap and frost line height shift seal performance. The converting run uses a die gap of 2.0 mm, melt temperature 210–230 °C, and blow-up ratio 2.0:1–2.5:1. Fluoropolymer-based processing aid at 200–500 ppm is added when surface melt fracture appears at high output. For food-contact applications, the olefin polymer layer is controlled by FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with overall migration limited to 10 mg/dm² under the assigned food simulant and contact condition. Seal jaw temperatures above 145 °C may create polyethylene smearing and transfer to the jaw face, which reduces seal uniformity and increases seal initiation variability. Regrind addition above 20 wt% is avoided for seal-critical webs because heat history and gel formation alter the seal plateau and reduce hot tack. Terminal packages include 25–50 μm pillow pouches, bread bags, biscuit overwrap and rice or pasta liners. The seal area must be free of migrating slip or antiblock agglomerates, because local surface bloom above 0.2 mg/100 cm² can prevent consistent heat transfer.

    Representative blown film formulation screening for 7120ST/LDPE food packaging webs
    Mass ratio 7120ST/LDPEMelt temperature rangeBlow-up ratioSeal initiation rangeHot tack test conditionFilm gauge
    100/0210–230 °C2.0–2.5:1108–115 °CASTM F1921 at 115 °C40–60 μm
    80/20205–225 °C2.0–2.5:1100–108 °CASTM F1921 at 110 °C40–60 μm
    70/30200–220 °C2.0–2.5:195–104 °CASTM F1921 at 105 °C40–60 μm

    The ranges are screening values for line startup and are not a release specification. Actual seal temperatures depend on die gap, frost line height, seal jaw pressure, and dwell time on the packaging machine.

    Coextruded Frozen Food Web Structures and Dart Test Methods

    Five-layer barrier film for frozen vegetables and seafood uses 7120ST in the heat-seal and outer skins, paired with an EVOH oxygen barrier core. A working structure is PE skin 12–15 μm / tie 3–4 μm / EVOH 3–5 μm / tie 3–4 μm / PE skin 12–15 μm, with total thickness 45–65 μm. The hexene copolymer contributes low-temperature film toughness after frozen distribution at -18 °C, measured by dart impact ASTM D1709 Method B and Elmendorf tear ASTM D1922. The coextrusion die is operated with PE layer melt temperature 190–220 °C and EVOH layer melt temperature 205–220 °C, because viscosity matching at the die entry is critical to avoid interfacial flow instability. 7120ST at 1.0 dg/min provides a melt viscosity closer to standard barrier grades than high-MFR LLDPE grades, but edge trim regrind should be kept below 15 wt% to avoid gel contamination and layer confusion. Blown film lines use a die gap of 1.8–2.4 mm, blow-up ratio 2.0:1–2.5:1, and a dual-lip air ring with internal bubble cooling for gauge uniformity. Food-contact compliance for the PE faces is assessed under FDA 21 CFR 177.1520(c) and EU 10/2011; the EVOH core is assessed under its own food-contact listing or national equivalent. The film is not intended for retort or hot-fill processing, and operational limits are reached above 60 °C sustained surface temperature where low-density polyethylene loses mechanical stiffness and seal creep accelerates. End-use films are converted into pillow bags, stand-up pouches and box liners for frozen vegetables, potato products and battered seafood. The primary failure mode on packaging lines is seal-area deformation caused by frost and product dust, not film puncture, when the skin layer is too thin; maintaining the skin above 12 μm is required for consistent freezer-to-boil abuse resistance.

    When High BUR Agricultural Film Demands Antiblock Packages and UV Stabilization

    Greenhouse covers, silage pit covers and agricultural lamination base webs run at high blow-up ratios from 2.5:1 to 3.0:1 to balance machine-direction and transverse-direction elongation. 7120ST is formulated with a hindered amine light stabilizer package at 0.2–0.6 wt%, a UV absorber at 0.1–0.3 wt%, and natural silica antiblock at 2000–5000 ppm; these loadings are adjusted by accelerated weathering and film surface tack requirements. The die gap is widened to 2.2–2.6 mm to maintain bubble stability at high BUR, and melt temperature is held at 200–220 °C to minimize additive decomposition. Frost line height is set between 600 mm and 1000 mm depending on cooling air temperature and line speed; a high frost line combined with high BUR increases transverse direction tear but can reduce machine direction tear and promote edge winkles. Tensile properties are quantified by ISO 527-3, tear resistance by ASTM D1922, and dart impact by ASTM D1709. Agricultural films produced from 7120ST are not food-contact materials and do not require FDA 21 CFR compliance, but the resin and additives must meet REACH registration duties and local agricultural plastic regulations where applicable. The film must be wound at low tension below 100 N/m width to avoid blocking and blocking-related surface impressions in the roll. Bubble wander becomes an operational limit above 3.0:1 on single-lip air rings, so internal bubble cooling or improved air-ring lips are used. End-product gauges range from 30 μm for row cover to 150 μm for greenhouse sheeting, with the higher-gauge film requiring additional cooling capacity or reduced output to prevent heat-induced shrinkback in the roll.

    Compliance verification matrix by terminal use for 7120ST converted film
    Terminal useRegulatory frameTest or data requirementTypical verification limit
    Dry food packagingFDA 21 CFR 177.1520(c), EU 10/2011Overall migration, organoleptic panel10 mg/dm²
    Frozen food packagingFDA 21 CFR 177.1520(c), EU 10/2011Migration under frozen conditions10 mg/dm²
    Industrial liners and sacksREACH, CLPSVHC declaration< 0.1 wt%
    Agricultural filmREACH, local agri-plastic rulesAdditive leaching, recyclability assessmentNot harmonized

    In dunnage air bag and heavy shipping sack converting, the selection of 7120ST-rich tubular film is driven by puncture propagation resistance and seal survival under rail vibration. Film for these applications is run at 75–125 μm thickness, frequently at 100% 7120ST or with 10–20 wt% high-pressure LDPE to improve bubble handling and seal flow. The die gap is set at 2.0–2.5 mm, blow-up ratio 1.8:1–2.2:1, and melt temperature 195–215 °C. A lower BUR is used to favor machine-direction tensile and reduce transverse direction stretch during bag forming. Seal strength is measured under ASTM F88, with minimum values set by bag drop and burst tests rather than by packaging appearance. Puncture resistance is evaluated by ASTM D1709 Method B for thin-gauge sections and by slow puncture methods based on end-user specifications for dunnage air bags. The hexene comonomer in 7120ST provides tensile toughness without the high-branching haze of some LDPE alternatives, but the resin is not a barrier material and is unsuitable for sustained oil contact or solvent retention. Continuous service temperature above 60 °C is outside the reliable operational range because the polymer softens and seal creep increases. Converters report that bag-side impact failures occur when film is overstretched in the transverse direction before sealing, so the bubble is collapsed with low nip pressure and edge guides are aligned to prevent gauge bands. REACH registration duties apply to the resin and additive masterbatch; no food-contact certification is assigned to this industrial film. The terminal packages are used as void-fill dunnage bags, FIBC inner liners, contamination-control liners and heavy shipping sacks for granular resins and pigments. The film surface must be clean and dry before sealing, and moisture above 0.15 wt% on regrind is removed before extrusion to prevent steam bubbles and inconsistent gauge in the finished bag.

    Free Quote

    Competitive Chevron Phillips 7120ST LLDPE Blown Film Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 7120ST is a hexene copolymer linear-low-density polyethylene blown film resin supplied in pellet form. The grade is formulated with a migratory slip agent and an antiblock package, designated by the ST suffix, for stabilized film-to-film separation and controlled coefficient of friction in converted packaging. The nominal density is 0.920 g/cm³ by ASTM D1505, and the melt index is 1.0 g/10 min by ASTM D1238 at 190 °C/2.16 kg. The resin is intended for monolayer and coextruded blown film lines producing industrial liners, heavy-duty sacks, agricultural film, and low-temperature packaging. Because the comonomer is 1-hexene rather than 1-butene, the short-chain branch length is 4 carbon atoms, which improves tie-molecule formation and low-temperature toughness at equivalent density and melt index. These features position the grade as a general-purpose LLDPE alternative to LDPE-rich film structures where downgauging and impact resistance are required; however, optical clarity is lower than a high-clarity LDPE or metallocene LLDPE grade in the same gauge.

    Representative values for Chevron Phillips 7120ST blown film at 25 µm thickness and 2.5:1 blow-up ratio. Values are not specification limits.
    Property Representative Range Test Method
    Melt index 1.0 g/10 min ASTM D1238, 190 °C/2.16 kg
    Density 0.920 g/cm³ ASTM D1505
    DSC peak melting temperature 122 °C to 125 °C ASTM D3418
    Tensile strength at break, MD/TD 42 MPa to 48 MPa / 36 MPa to 42 MPa ASTM D882
    Elongation at break, MD/TD 550% to 650% / 650% to 750% ASTM D882
    Secant modulus at 1%, MD/TD 240 MPa to 280 MPa / 260 MPa to 310 MPa ASTM D882
    Elmendorf tear, MD/TD 140 g to 200 g / 300 g to 440 g ASTM D1922
    Dart drop impact F50 110 g to 160 g ASTM D1709A
    Haze 10% to 14% ASTM D1003
    Gloss at 45° 55 to 70 ASTM D2457

    Hexene Comonomer Distribution Governs Film Toughness More Effectively Than 1-Butene

    The selection of 1-hexene as comonomer creates butyl branches rather than ethyl branches generated by 1-butene. The longer branch interferes more effectively with lamellar crystallization and allows formation of a more frequent tie-chain network between crystallites. In blown film testing under ASTM D1922, hexene grades generally show higher Elmendorf tear values than butene grades of identical 0.920 g/cm³ density and 1.0 g/10 min melt index. Published resin comparisons often report improvements of 20% to 40% in machine-direction tear and larger improvements in transverse-direction tear. Dart drop impact measured under ASTM D1709A follows a similar trend because the more entangled amorphous phase absorbs greater local strain energy before crack extension.

    Environmental stress-cracking resistance under ASTM D1693 also benefits from higher tie-molecule concentration. Lower-density butene grades can exhibit premature crack growth in the presence of surfactants and stress concentrators. Published data for the exact 7120ST formulation in direct comparator studies is limited, so end users should run lot-specific side-by-side film evaluations on the target line using ASTM D882 tensile tests and ASTM D1922 tear tests. The difference in short-chain branching also affects sealing and hot-tack response. Hexene LLDPE generally provides a lower seal initiation temperature than a butene LLDPE of comparable density; seal strength is measured under ASTM F88, and hot tack under ASTM F1921.

    Compared with metallocene-catalysed LLDPE, 7120ST is a Ziegler-Natta product with broader molecular weight distribution. The broader distribution improves bubble stability and reduces melt pressure at equivalent output, but it typically reduces peak clarity and hot-tack performance. Metallocene grades can offer superior low-temperature sealing and organoleptic properties, while 7120ST-type grades are selected where high-stalk bubble stability, tear performance, and additive package robustness govern the production decision. Relative to high-pressure LDPE, 7120ST provides higher tensile strength, puncture resistance, and Elmendorf tear at equal gauge, but it exhibits poorer shear thinning and requires wider die gaps and higher motor torque.

    On grooved-feed blown film lines with 24:1 to 30:1 L/D ratio extruders, 7120ST is processed at melt temperatures from 190 °C to 230 °C, with barrel zones typically from 170 °C to 210 °C and die temperatures from 210 °C to 230 °C. Die gaps of 1.2 mm to 2.0 mm are preferred for LLDPE; narrow gaps of 0.5 mm to 0.8 mm that run LDPE may cause sharkskin on high-output lines. Typical blow-up ratios range from 2.0:1 to 3.0:1, and frost-line heights of 3 to 5 die diameters balance machine-direction and transverse-direction property development. On a 250 mm annular die with a 1.5 mm gap, a 90 mm grooved-feed extruder running at approximately 100 kg/h may generate head pressures from 30 MPa to 45 MPa; published data for this specific equipment configuration is limited, and die pressure should be recorded on the target line.

    Because LLDPE exhibits less shear thinning than LDPE, motor torque and die pressure rise more steeply with output. A screw designed for LLDPE, with a low or moderate compression ratio and barrier flight geometry, is recommended to prevent melt-temperature override. Extended runs with inadequate screw cooling can raise melt temperature above 240 °C, leading to oxidative degradation, gel formation, and odour from slip additive decomposition. Processors typically purge with a higher-melt-index LDPE when transitions are required. 7120ST should not be left in a hot idle extruder above 220 °C for prolonged periods. Screen packs with 200 µm to 500 µm mesh retention are common for gel reduction, but fine screens increase backpressure and can worsen melt-temperature heterogeneity if the screen area is undersized.

    What Limits Stable Bubble Formation on High-Stalk Extrusion Lines When Running 7120ST at Low Melt Temperature?

    At melt temperatures below 190 °C, the frost line may rise and bubble stability can deteriorate because insufficient melt strength allows periodic breathing, helical instability, or bubble sag. The onset of sharkskin is governed by shear stress at the die lip. With LLDPE, critical shear stress is reached more readily than with LDPE at the same die gap and output. Increasing the die gap from 1.0 mm to 1.8 mm reduces shear stress and can extend the stable operating window. High-stalk configurations with a prolonged stalk height require a controlled balance between chill air, extrusion rate, and internal bubble pressure. If internal bubble pressure oscillates by more than 0.1 mbar on a 300 mm die, operators may observe frost-line vertical movement of several die diameters. An internal bubble stabilizer equipped with a low-pressure manometer is advisable.

    On high-stalk lines, the stalk is deliberately cooled below the resin crystallization onset to orient the film. With 7120ST, a frost-line height above 6 die diameters may create excessive machine-direction orientation, giving unbalanced tear and a splitty bubble. Reducing the frost line to 3 to 4 die diameters and increasing dual-lip air-ring volume typically restores balance. The broader molecular weight distribution of this Ziegler-Natta grade provides moderate melt strength compared with LDPE; however, it is not a high-melt-strength LDPE and cannot always support very high stalks run on dedicated high-stalk dies. Published film-process data for this exact grade in public literature is limited; line trials measuring film width variability, frost-line height, and melt pressure are necessary.

    Low-melt-temperature operation can also slow additive migration and increase film-to-film blocking. When extrusion is conducted below 190 °C and the film is wound warm, the slip agent may not have sufficient diffusivity to reach the film surface before winding. The result may be elevated coefficient of friction and blocking in the roll after 24 h. Winder tension and contact pressure should be reduced if the roll hardness consistently exceeds 85 Shore D equivalent indenter values. Maintain ambient storage above 20 °C for at least 24 h after winding to allow slip migration before slitting or bag conversion.

    When Slip Additive Migration Shifts Coefficient of Friction Below 0.20

    The ST additive package contains a migratory slip agent and an antiblock component. The slip agent migrates to film surfaces over time; the kinetic coefficient of friction determined under ASTM D1894 after 24 h to 48 h at 23 °C and 50% relative humidity is lower than the immediate off-line value. A freshly extruded film may show a kinetic coefficient above 0.50, dropping to 0.20 or below after ageing depending on slip agent concentration, film gauge, and storage temperature. At storage temperatures below 15 °C, migration is slower and coefficient of friction may remain elevated for several days. The antiblock component, typically synthetic silica particles, increases surface roughness slightly and prevents blocking under roll pressure; haze may rise by a measurable amount under ASTM D1003, but the trade-off is required for stable winding and bag opening.

    On high-speed form-fill-seal equipment, both static and kinetic friction should be validated because bag tracking against metal forming collars depends on the metal-to-film interface, not film-to-film only. Surface values obtained under ASTM D1894 are not directly transferable to all machine geometries, but they provide a comparative lot-acceptance method. The additive package also affects printing and lamination; the slip component can reduce surface energy. Corona treatment to 38 dyn/cm to 44 dyn/cm is commonly applied, and treated film should be tested under ASTM D2578 for wetting tension stability, because slip migration can partially mask surface energy gains. Solventless lamination may require retest after 48 h because the slip additive may alter adhesive wet-out.

    In coextruded structures, the slip and antiblock package in 7120ST contributes to the final outer surface unless the grade is buried. When used in the core layer, additive migration to the surface may still occur through the skin layers depending on skin thickness and additive compatibility. For structures with thin metallocene LLDPE skins below 10 µm, the coefficient of friction can trend downward over 72 h as slip reaches the outer surface. This migration behaviour is an operational boundary, not a defect; converter specification limits should define both kinetic and static coefficient at a fixed ageing interval, such as 48 h at 23 °C.

    Compliance Profile and Regulatory Boundary Conditions

    For food-contact packaging, the base olefin polymer is typically evaluated under 21 CFR 177.1520(c) of the Code of Federal Regulations, which covers olefin polymers. The specific end-use temperature and food type, as described in 21 CFR 176.170(c), determine the permitted use condition; polyethylene grades may be acceptable for certain aqueous, acidic, and fatty foods under defined temperature and time limits. Additive-specific clearances must be separately confirmed because migratory slip agents are not automatically covered by the base polymer clearance. Published data for the exact proprietary ST additive package is limited; therefore converters should request a regulatory compliance certificate from the resin supplier.

    In the European Union, plastics intended for food contact must comply with Regulation (EU) No 10/2011. Overall migration limits of 10 mg/dm² and specific migration limits for individual additives are evaluated using food simulants and migration test methods in the EN 1186 series. For industrial packaging outside food contact, REACH registration obligations apply to monomer and imported resin substances; the applicable substance portfolio should be verified against the current ECHA candidate list of substances of very high concern. RoHS Directive 2011/65/EU applies only to electrical and electronic equipment, not general packaging; however, where packaging is integrated into EEE, cadmium, lead, mercury, and hexavalent chromium thresholds may need to be reviewed.

    Storage before extrusion should avoid direct ultraviolet exposure and excessive heat. Polyethylene is not hygroscopic, but surface condensation on cold pellets can introduce water-induced bubble defects. Silos and hoppers should maintain resin temperatures below 50 °C to prevent additive loss or pellet agglomeration. Conveying systems with long-radius bends minimize streamers and fines that can cause melt-temperature variation and film gel formation. If regrind or post-consumer recyclate is added, melt filtration to 200 µm to 500 µm removes many contaminants and stabilizes bubble quality in non-food applications.

    Key regulatory and test references for LLDPE blown film with slip and antiblock additives.
    Reference Scope Application Condition
    21 CFR 177.1520(c) US FDA olefin polymer clearance End-use condition and food type per 21 CFR 176.170(c)
    Regulation (EU) No 10/2011 EU plastics food contact Overall migration limit 10 mg/dm²; EN 1186 series testing
    ASTM D1238 Melt index quality control 190 °C/2.16 kg
    ASTM D1505 Density 23 °C gradient column
    ASTM D1894 Film friction 23 °C, 50% RH, aged surface
    REACH Registration, notification, restrictions Verify SVHC candidate list

    In heavy-duty shipping sacks of 80 µm to 120 µm gauge, 7120ST-type LLDPE is used to replace high-pressure LDPE or blended with LDPE to improve tear and drop resistance. Dart impact under ASTM D1709A and Elmendorf tear under ASTM D1922 are common acceptance criteria. On a three-layer coextrusion line with a 250 mm annular die and 2.0:1 to 2.8:1 blow-up ratio, the resin may occupy the core or substrate layer at 40% to 70% of total thickness, while LDPE or mLLDPE skins provide sealability and optics. In agricultural silage film, puncture resistance is critical; the slower crack propagation of hexene LLDPE reduces puncture failure under contact with stalk and stored feedstock. Test methods include slow puncture by ASTM D5748 and total energy dart impact by ISO 7765-2.

    Industrial liners and can liners use the same balance of tear and processability. Blends with high-pressure LDPE are common when improved drawdown and lower torque are required; however, LDPE lowers tensile strength and Elmendorf tear. At 25 µm to 50 µm gauge, 7120ST can produce low-gel film when extruder temperatures are kept below 240 °C. Frozen food packaging demands low-temperature toughness; film conditioned at -18 °C and tested for dart impact according to ASTM D1709A shows less brittle fracture than many butene-copolymer grades at equal density. The broader relative molecular weight distribution of Ziegler-Natta LLDPE also permits post-consumer recyclate addition in non-food applications, provided that the recyclate fraction is dried and screened to 200 µm to 500 µm melt filtration to remove gels and contaminants.

    Top