Chevron Phillips 7109lt Lldpe Blown Film Resin Hexene Copolymer

Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer

    • Product Name: Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 841886
    Product Name Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Melt Flow Ratio 27
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Brittleness Temperature < -70 °C
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Break Md 5000 psi
    Tensile Strength At Break Td 4500 psi
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    1 Secant Modulus Md 25000 psi
    1 Secant Modulus Td 30000 psi
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Dart Drop Impact 200 g
    Haze 12%
    Gloss 45 55%
    Coefficient Of Friction 0.20

    As an accredited Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer is supplied in 25 kg polyethylene bags or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL container loading: Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer in 25 kg bags, palletized, shrink-wrapped, secured.
    Shipping Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer ships as non-hazardous, non-DG plastic pellets in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars. Store dry, away from heat and sunlight. Follow manufacturer handling recommendations; no special DOT hazard classification required.
    Storage Store Chevron Phillips 7109LT LLDPE Blown Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep bags or containers closed to prevent moisture, dust, and contamination. Place on pallets, not directly on floors. Avoid prolonged UV exposure and separate from strong oxidizers. Maintain clean handling areas and follow the manufacturer’s SDS.
    Shelf Life Typically 24 months from date of manufacture when stored in original unopened packaging in a cool, dry, well-ventilated area.
    Application of Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer

    On three-layer blown-film lines producing heavy-duty industrial liners and sacks, 7109LT is typically introduced in the core or outer layers at 70–90 wt% with a high-density polyethylene (HDPE) component at 5–20 wt% to elevate modulus and a carbon black masterbatch at 1–3 wt% for ultraviolet screening and opacity. The hexene comonomer structure raises Elmendorf tear resistance relative to butene-copolymer LLDPE at equivalent density and melt index; the difference becomes measurable in films above 120 μm gauge when orientation is locked in by frost-line height control. Extrusion is typically carried out on grooved-feed extruders with 25:1 to 30:1 L/D ratios, screw speeds in the 50–90 rpm range, barrel temperatures from 190°C to 230°C, and die temperature set no more than 10°C above the final adapter zone to limit melt-phase oxidation. Die gap is commonly held at 1.8–2.5 mm with a blow-up ratio of 2.0:1 to 2.8:1; narrowing the die gap below 1.5 mm can reduce dart impact strength by increasing machine-direction orientation, while widening beyond 2.8 mm can lower bubble stability and increase gauge-band scatter. Frost-line height of 300–700 mm is used to match the resin’s stress-relaxation behavior; a frost line positioned too low traps excessive transverse direction shrinkage, and a frost line positioned too high can create fluttering on rotating-die towers. Converters test sacks under ASTM D1709-15a Method B for dart drop impact, ASTM D1922-15 for Elmendorf tear, and ASTM D1693-15 Condition B for environmental stress-crack resistance in 10% Igepal CO-630 at 50°C. For food-contact liner structures without carbon black or regrind, 7109LT may meet olefin polymer requirements under 21 CFR 177.1520 and EU Regulation 10/2011 when the finished film passes overall migration limits. Regrind addition up to 15 wt% is common in non-food industrial sacks; beyond this level, dart impact variability increases because the heat history degrades hexene branch regularity.

    Table 1: Qualification and compliance tests for heavy-duty industrial liner film containing 7109LT.

    TestStandardConditionReported metric
    Film thicknessISO 4593:201923°C, 50% RHμm
    Dart drop impactASTM D1709-15aMethod Bg/F50
    Elmendorf tearASTM D1922-1523°C, 50% RHgf or mN
    ESCRASTM D1693-1550°C, 10% Igepal CO-630h/F50
    Melt flow rateISO 1133-1:2022190°C, 2.16 kgg/10 min
    DensityASTM D1505-1823°Cg/cm³

    Tensile hysteresis and puncture propagation in agricultural silage cover film

    The 150–250 μm silage cover structure is less demanding in optics than in slow-rate puncture resistance and cyclic tensile retention after UV exposure. 7109LT is processed in three-layer coex lines with a UV masterbatch at 2.0–4.0 wt%, typically containing hindered amine light stabilizers (HALS) and a benzophenone-class absorber dispersed in a 0.918–0.922 g/cm³ carrier; the carrier density is selected to avoid shifting overall film density above 0.925 g/cm³, which would reduce tear propagation resistance. Blow-up ratios are held between 2.5:1 and 3.5:1, and die gaps between 2.0 mm and 2.5 mm because agricultural film requires balanced machine-direction and transverse-direction impact and puncture propagation. The film is evaluated before and after accelerated weathering under ISO 4892-2 cycle 1 or ASTM G155 Cycle 1; tensile elongation at break is measured by ISO 527-3, and slow-speed puncture resistance by EN 14477 or ASTM D5748. A practical failure mode in bunker covers is not uniform degradation but localized crack propagation from stone abrasion or clamp punctures; therefore the ratio of transverse-direction Elmendorf tear to dart impact after 2,000 hours of UV exposure is often used as a process release criterion. Line speeds are constrained by bubble cooling; air-ring temperature and internal bubble cooling settings are adjusted to keep the frost-line height within 600–1,000 mm. If the film enters the nip with surface temperature above 40°C, blocking is observed after winding, and subsequent slit widths become variable. The outer layers are formulated with 7109LT at 75–85 wt%, while the core may carry higher UV masterbatch loadings because migration from the core to the surface is slower than from the skins.

    What changes when 7109LT replaces butene-grade LLDPE in low-temperature frozen-food pouch structures?

    At converting lines producing stand-up pouches and pillow pouches for frozen vegetables, seafood, or ice cream, the replacement of butene-copolymer LLDPE with 7109LT shifts the failure mode from brittle cracking at -20°C to ductile yield under flex-crack testing. The resin is diluted in the sealant skin or core at 60–85 wt% with LDPE at 10–25 wt% to reduce melt pressure and improve bubble stability, plus 2–5 wt% of an antiblock masterbatch carrying 10–20% synthetic silica and 1–2 wt% slip masterbatch containing erucamide at 5–10% letdown. Film thickness is typically 40–90 μm, and the die gap is narrowed to 1.2–1.8 mm with a blow-up ratio of 2.0:1 to 2.6:1 to control sealant-layer gauge. Low-temperature performance is characterized by ASTM D1709-15a Method A at -18°C after conditioning, ASTM D746-14 for brittleness temperature, and ASTM F392/F392M-21 for flex-crack pinhole formation on three-layer laminates. Seal initiation temperature is measured by heat-seal profile per ASTM F88/F88M-15; the presence of hexene branches in 7109LT lowers the seal initiation temperature and broadens the hot-tack plateau relative to a butene copolymer of identical density and melt index, extending the seal window by 15–20°C in some coextrusions. This is measurable on packaging line dwell times below 0.5 s. The food-contact surface must comply with 21 CFR 177.1520 and EU Regulation 10/2011, including overall migration below 10 mg/dm² for aqueous, acidic, and fatty food simulants. Tunnel freezer converting records show that the limiting parameter is not seal strength but film stiffness after freezing; 7109LT reduces stress-whitening compared with butene-copolymer film at the same thickness.

    Pallet unitization hoods blown at 60–120 μm gauge use 7109LT as the major component in the middle layer, while the two outer layers are modified with cling or slip additives to control film-to-film friction and pallet-wrapping tack. The process window is narrower than in heavy-duty sacks because high pre-stretch ratios expose any melt-fracture streaks or gauge defects. Typical coextrusion conditions are die gap 1.5–2.0 mm, blow-up ratio 2.0:1 to 3.0:1, melt temperature 210–230°C, and output limited by the air ring to maintain bubble diameter variability below ±3%. Mechanical properties are tested per ASTM D882-18 for tensile strength and elongation, ASTM D1922-15 for tear resistance, and ASTM D1894-14 for coefficient of friction after 300% pre-stretch; a cling masterbatch based on low-molecular-weight polyisobutylene is added at 0.5–2.0 wt% in the outer layers, but the center layer avoids cling additives because they migrate into the bubble interior and alter bubble cooling. Lower melt index hexene copolymer grades exhibit optical bulk haze; production release for transparent hoods demands haze below 15% per ASTM D1003-13, which is achievable when the resin is processed at 220–230°C and the die gap is not reduced below 1.5 mm. Published data for this specific formulation is limited; however, converting records show that when die-lip temperature variation exceeds ±3°C, tensile retention after 250% stretch deteriorates before dart impact does. The failure symptom is transverse tearing at the pallet corner rather than film puncture, which indicates orientation imbalance from non-uniform die temperature.

    Setting the sealant layer in coextruded barrier lamination

    In coextruded barrier laminates for vacuum or gas-flushed packaging, 7109LT is used in the sealant skin or sub-skin at 70–100 wt% with a metallocene LLDPE or LDPE blend at 0–20 wt% to control seal initiation. The barrier core is usually EVOH at 3–9 μm with tie layers; the sealant web is coextruded at a thickness of 20–50 μm. Because the sealant layer must not distort the EVOH layer during stretching, die gap is set to 1.5–2.0 mm and blow-up ratio to 1.8:1 to 2.5:1, lower than typical heavy-duty film. The key processing conflict is that higher melt temperatures improve adhesion to the tie layer but raise oxidation risk in the hexene branches; therefore barrel profile is limited to 200–230°C and the resin is kept under nitrogen purge in the hopper when ambient relative humidity exceeds 60%. Heat-seal strength is measured per ASTM F88/F88M-15, hot tack per ASTM F1921-18, and seal initiation temperature by incremental seal testing; the presence of long-chain hexene branches in 7109LT lowers the minimum seal temperature by 5–10°C compared with butene-copolymer linear low density at equivalent density. Vacuum packaging requires the complete laminate to survive hot-fill conditions up to 95°C or refrigerated distribution at 4°C; the sealant layer must be tested per ISO 11607-1 for seal integrity after exposure to vacuum pressure differentials. Compliance includes 21 CFR 177.1520 for the polyethylene sealant, EU Regulation 10/2011 for overall migration, and REACH Annex XVII and SVHC screening applied to imported film.

    If the melt temperature is held below 204°C on a high-output grooved-feed line

    High-output liner lines with 30:1 L/D grooved-feed extruders sometimes run 7109LT at reduced barrel settings to reduce energy costs, but a melt temperature below 204°C at the die creates melt fracture and pressure instability. The melt is more shear-sensitive than butene LLDPE at equivalent melt index; at screw speeds above 80 rpm, die pressure can fluctuate by more than 10% and shark-skin marks become visible in the web. Barrel zone settings are raised sequentially from 180°C at the feed throat to 210–230°C in the metering zone, and the die is held at 215–230°C. A polyfluoroelastomer-based processing aid is added at 200–400 ppm when film thinner than 40 μm is produced; without this additive, die-lip buildup forms after 4–6 hours and creates longitudinal scoring. The bubble is usually run at 2.2:1 to 2.8:1 blow-up ratio with a 1.8–2.2 mm die gap; reducing the gap below 1.5 mm while running cold increases gel-like optical defects that are actually unmelted micro-domains. Motor load is monitored; a 25% increase over the clean-screw baseline indicates insufficient screw recovery or feedbridge plugging. Film is tested under ASTM D1709-15a Method A for dart impact and ASTM D1922-15 for tear; the cold-processing failure signature is a drop in machine-direction Elmendorf tear without a corresponding drop in tensile yield, because the melt-centre strain histories are altered. Published data for this specific configuration is limited, but the corrective sequence is standard on high-output lines: first raise the die temperature, then increase the feedthroat water temperature, and only after that adjust screw speed.

    E-commerce mailer films manufactured at 80–120 μm gauge use 7109LT in two-layer or three-layer structures with recycled LLDPE and HDPE to balance puncture resistance and bending stiffness. The recycled fraction is limited to 20–40 wt% because higher post-consumer recycle content reduces hexene-copolymer tear resistance and narrows the heat-seal window. Extrusion is typically run on a 50–70 mm blown-film line at 200–225°C, die gap 1.8–2.3 mm, blow-up ratio 2.0:1 to 3.0:1; the bubble is internally cooled to maintain gauge uniformity across 1,200–1,600 mm layflat widths. Sealing is performed on rotary or reciprocating sealers at 180–200°C jaw temperature and 0.3–0.8 s dwell; heat-seal strength is checked by ASTM F88/F88M-15 and drop-fill performance by ISTA 3A or ASTM D5276-19 drop testing. The finished mailer must comply with RoHS 2011/65/EU Annex II for heavy metals, REACH Regulation (EC) No 1907/2006 Articles 33 and 67, and no direct food-contact declaration is required for non-food mailers. Tensile properties are reported per ASTM D882-18, and puncture resistance per ASTM D5748-19; converters monitor the difference between dart impact at 23°C and -10°C to detect excessive recycled content or insufficient compatibilization. The most common field failure is bottom-seal peel after drop loading, which is traced to cool seal bars rather than resin deficiency.

    Free Quote

    Competitive Chevron Phillips 7109LT LLDPE Blown Film Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 7109LT is a linear low density polyethylene blown film resin produced as a hexene-1 copolymer. The grade is supplied in pellet form and is specified for monolayer blown film, heavy-gauge tubular film, and skin or sealant layers in coextruded structures. The nominal density of 0.918 g/cm³ per ASTM D1505 and nominal melt index of 0.9 g/10 min per ASTM D1238 at 190°C and 2.16 kg identify a resin with moderate melt elasticity, adequate bubble retention on conventional blown film lines, and the capacity to draw film in gauges from approximately 20 µm to greater than 100 µm depending on die gap, frost-line height, and air-ring configuration.

    Table 1 — Nominal resin parameters for Chevron Phillips 7109LT
    Parameter Nominal value Reference method
    Density 0.918 g/cm³ ASTM D1505 / ISO 1183-1
    Melt index 0.9 g/10 min ASTM D1238 / ISO 1133-1:2022, 190°C, 2.16 kg
    Comonomer Hexene-1 —
    Form Pellets —
    Stabilization Process antioxidant package; lot-specific additive loading appears on the certificate of analysis —

    The values in Table 1 are nominal and are not release limits. The supplier certificate of analysis controls lot-specific values for density, melt index, and additive package.

    How does hexene incorporation influence crystal structure and film optical behavior?

    The hexene-1 comonomer inserts short-chain branches with a four-carbon pendant length along the polyethylene backbone. At the specified density of 0.918 g/cm³, the branches reduce crystallite size and lamellar thickness relative to an ethylene homopolymer of equivalent molecular weight. The modified crystal morphology increases the population of interlamellar tie chains and alters the yield stress, elongation, and dart impact response measured under ASTM D1709 and ASTM D882.

    Optical behavior is coupled to crystal size and surface roughness. In blown film, external haze and internal haze arise from surface irregularities and spherulitic scattering. Hexene copolymers having density near 0.918 g/cm³ generally produce lower haze than butene copolymers at matched density and melt index because the longer hexene branch is more effective at disrupting lamellae without requiring the same molar comonomer addition. Film clarity is nevertheless influenced by die lip finish, frost-line temperature, and cooling air velocity; a resin with lower intrinsic haze does not compensate for unstable bubble geometry or melt fracture at the die exit.

    The molecular weight distribution imparts a balance between shear thinning and melt strength. In practical blown film operation, this balance affects bubble diameter retention at high blow-up ratios and the maximum take-off speed before draw resonance appears. The measured melt index of 0.9 g/10 min is a single-point viscosity indicator and does not define the full shear-rate response; extrusion trials on the target line remain necessary when the downstream conversion speed exceeds the supplier’s recommended drawdown range.

    On a 65 mm single-screw extruder with L/D 24:1 and a barrier feed section, 7109LT is normally processed with barrel temperatures from 177°C to 216°C and an adapter and die zone maintained at 204–216°C. A die gap of 1.5–2.0 mm and blow-up ratio of 2.0:1 to 2.5:1 provide a stable bubble for film thicknesses between 25 µm and 100 µm. Higher blow-up ratios may reduce machine-direction tear and increase transverse-direction tensile strength, measured respectively under ASTM D1922 and ASTM D882. Operation above 3.0:1 can amplify bubble instability on certain single-lip air-ring configurations and should be validated with high-speed bubble photography on the production line.

    No predrying is required for dry pellet handling. If pellets are stored in unprotected outdoor silos at relative humidity above 60%, surface moisture can introduce bubble defects and melt pressure fluctuations. In such cases, a desiccant hopper dryer set at 60°C for 2 h is applied when visual defects persist. Melt temperatures above 232°C should be avoided because oxidative degradation increases gel formation and carbonaceous deposits at the die lip. The use of chilled-air or dual-lip air rings improves gauge uniformity at high output rates; however, the exact frost-line height must be adjusted to maintain film toughness, because excessively high frost lines can increase haze and reduce transverse-direction tear resistance.

    Puncture, tear, and seal response in hexene copolymer film structures

    Hexene-copolymer LLDPE is characterized by a balance between tensile modulus, elongation at break, and impact toughness. In film testing, dart impact resistance is measured under ASTM D1709 using a free-falling dart; Elmendorf tear resistance is measured under ASTM D1922 with a pendulum tear tester. For a hexene copolymer with density 0.918 g/cm³, dart impact response is governed by gauge, frost-line height, blow-up ratio, and orientation balance rather than by resin selection alone. No fixed values are assigned here because the supplier lot certificate and the processor’s orientation balance control the final film property envelope. Published data for this specific configuration is limited; film test values should be generated on the actual line using finished film samples.

    Compared with butene-copolymer LLDPE at analogous density and melt index, hexene grades generally display higher dart impact and machine-direction tear resistance under ASTM D1709 and ASTM D1922. The C6 branch is sterically less likely to be rejected from the crystal lattice as an isolated defect while being more efficient in forming tie chains, which changes the failure mechanism during slow puncture and rapid impact. The effect is more pronounced at temperatures below -20°C, where low-temperature ductility of butene copolymers can decline more rapidly. This distinction supports the use of hexene-copolymer LLDPE in frozen food packaging, ice bags, and cold-chain transport films.

    Seal performance is evaluated on a rotary heat-seal unit under ASTM F1921 for hot tack and on a tensile tester under ASTM F88 for seal strength. Hexene copolymers tend to produce broader hot-tack windows than butene copolymers at similar density because the tie-chain population and crystallization behavior maintain seal integrity over a wider sealing temperature interval before burn-through. Seal initiation is also affected by seal bar pressure, dwell time, and film gauge; therefore, the sealing window should be validated on the converter’s vertical form-fill-seal equipment rather than inferred solely from resin type.

    Metallocene-catalyzed LLDPE may offer lower seal initiation and improved optics due to narrower composition distribution; however, 7109LT often shows higher bubble stability and lower extrusion backpressure on conventional extruders. Cast film and extrusion coating lines do not benefit from the same bubble-stability advantages because orientation and quench rates differ. The grade is primarily intended for blown film processes; suitability for cast film should be confirmed with processing trials and rheological comparison on the target equipment.

    When butene-copolymer LLDPE is the comparison point

    The choice between a butene-copolymer and 7109LT typically occurs when a converter is deciding whether to compensate for lower tear resistance by increasing film gauge. If a butene film is downgauged to match resin cost, the loss in dart impact and seal performance becomes measurable under ASTM D1709, ASTM D1922, and ASTM F88. In those cases, replacement with a hexene-copolymer resin can allow gauge reduction without sacrificing the package integrity parameter that is critical for the distribution cycle. The conversion is not universal; machine-direction tear balance, bubble stability, and seal temperature settings require re-optimization.

    A high-density polyethylene grade may offer stiffness but has lower dart impact and limited low-temperature toughness. Butene-copolymer LLDPE may offer optical properties and lower resin cost in certain markets, but it can require a thicker film to match the tear and impact performance of a hexene copolymer. 7109LT occupies a density point where tear, seal, and low-temperature toughness are balanced for high-integrity packaging, heavy-duty sacks, and demanding monolayer films. The selection should be confirmed by running package-performance tests such as drop tests, compression tests, and distribution simulation rather than by comparing single-point resin properties alone.

    Typical converted forms include frozen food pouches, ice bags, heavy-duty sacks, industrial liners, agricultural silage film, and lamination film. In freezer packaging, low-temperature ductility after sharp flexing is evaluated by performing ASTM D1709 on conditioned film or by puncture propagation testing on production film samples. For heavy-duty sacks, the critical parameters are normally Elmendorf tear and film tensile strength; fill-line trials on vertical form-fill-seal equipment document seal integrity under ASTM F88. For agricultural service, UV stabilization must be added because the neat resin is not formulated for multi-season outdoor exposure. The processing stabilizer package in the neat resin is intended for extrusion protection, not for long-term ultraviolet resistance in the finished article.

    In coextruded structures, 7109LT can be placed as the sealant skin layer in polyolefin-based barrier films. The sealant layer is typically coextruded at 0.8–1.5 mil (20–38 µm). Tie layer selection is determined by the barrier polymer: maleic anhydride grafted polyolefin is used with EVOH or nylon; the 7109LT skin is processed at 204–216°C to maintain adhesion without degrading the barrier layer. Layer ratio adjustments are necessary because the melt index of 0.9 g/10 min may produce higher viscosity than barrier-resin layer streams; die design and feedblock temperature profiling control layer distribution and prevent interfacial flow instability.

    Food-contact status and regulatory documentation under olefin polymer clearances

    Compliance representations should be confirmed with the supplier for the commercial grade and the specific lot. Polyethylene materials of this composition may be covered under 21 CFR 177.1520(c) for direct food contact, subject to density, extractables, and end-use limitations specified in the regulation. For European Union applications, compliance is assessed under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for the final article. Specific migration limits and residual monomer restrictions apply to the finished food-contact article and depend on the other layers, adhesives, inks, and coatings used in the structure.

    Industrial hygiene documentation includes a safety data sheet and REACH registration status. The converter remains responsible for verifying that the final film meets the applicable national and retailer-specific requirements. Any statement of compliance should be obtained from Chevron Phillips Chemical for the actual lot and packaging configuration. When 7109LT is used in food packaging at thicknesses above the migration-testing threshold or in contact with fatty food simulants, migration testing on the final film or article is generally required unless the multilayer structure has been demonstrated to comply as an integrated system.

    Top