Chevron Phillips 7109djt Lldpe Blown Film Resin Hexene Copolymer

Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer

    • Product Name: Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 874661
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Process Blown Film
    Density 0.918 g/cm³
    Melt Index 0.9 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Melt Flow Ratio 30
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 31.0 MPa
    Elongation At Break 600%
    Dart Impact Strength 120 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 10%
    Gloss 45 55%
    Coefficient Of Friction 0.2
    Blocking 50 g

    As an accredited Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 7109DJT LLDPE Blown Film Resin is supplied in 25 kg polyethylene bags, palletized, with 1,000 kg supersacks available.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer in 25 kg bags, palletized, shrink-wrapped, securely stowed.
    Shipping Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer ships as non-hazardous plastic pellets in 25 kg bags, 50 bags per pallet (1,250 kg), or bulk containers. Store dry and cool; avoid direct sunlight, moisture, and excessive heat. Not DOT/IMDG regulated.
    Storage Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original packaging closed and palletized off the floor to prevent moisture pickup and contamination. Avoid prolonged UV exposure and temperature extremes. Maintain clean, dry handling areas and follow local storage regulations.
    Shelf Life Typically 24 months from manufacture when stored unopened in a cool, dry area, protected from direct sunlight, heat, and moisture.
    Application of Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer

    On high-output blown film lines producing 100–160 µm industrial liners, melt fracture and bubble instability become limiting when a hexene-copolymer LLDPE is processed without adequate die-gap clearance or blend melt strength. Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer, is introduced at 70–85 wt% in heavy-duty sack and FIBC liner formulations, with the balance composed of a high-pressure LDPE homopolymer having a melt index of 0.25–0.4 g/10 min under ISO 1133-1:2022; the LDPE component contributes melt strength and stabilizes the bubble at the higher blow-up ratios used to balance machine-direction and transverse-direction tear. Neat resin at 100 wt% is used only on lines equipped with internal bubble cooling and segmented die-lip heaters because gauge uniformity across a 1,800–2,200 mm layflat must remain within ±5% for reliable conversion into gusseted sacks. The downstream process consists of monolayer or coextruded blown film extrusion at a melt temperature of 200–230°C, a die gap of 2.0–2.5 mm, a blow-up ratio of 2.2:1–2.8:1, and a frost line height of 6–8 die diameters; after collapsing and surface treatment to 38–42 mN/m, the web is flexographically printed, gusseted, and sealed into bottom-seal or side-gusset sacks. Terminal product types include UN-certified FIBC inner liners, mineral and chemical bulk sacks, drum liners, and construction debris bags. Compliance for direct food contact liners is governed by FDA 21 CFR 177.1520(c) for olefin polymers and, for EU destinations, by Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; mechanical acceptance is established through tensile testing under ASTM D882-18, Elmendorf tear under ASTM D1922-15a, dart impact under ASTM D1709-16A, and puncture resistance under ASTM D5748-19.

    Compliance checklist for heavy-duty sack and FIBC liner films produced with 7109DJT
    Regulation/StandardTest Method or ClauseApplication Boundary
    FDA 21 CFR 177.1520(c)Olefin polymer extractable limits under 21 CFR 176.170(c)Direct food-contact liners in dry, aqueous, or fatty food classes depending on end-use condition
    Regulation (EU) No 10/2011Overall migration 10 mg/dm²EU food-contact plastic films
    Directive 94/62/ECSum of heavy metals 100 mg/kgPackaging and packaging waste
    ASTM D882-18Tensile strength and elongation100–160 µm film mechanical acceptance
    ASTM D1709-16ADart impactPuncture and shock resistance of sack liner

    When High-Pressure LDPE Is Partially Replaced to Reduce Gauge in Greenhouse Covering

    When high-pressure LDPE is partially replaced by 7109DJT in greenhouse and tunnel film, the primary technical constraint is not bubble stability but the diffusion and retention of hindered amine light stabilizers in a lower-density matrix exposed to UV radiation for 12–36 months. Formulation ratios for three-layer agricultural structures typically place 7109DJT at 60–80 wt%, with 10–20 wt% LDPE for melt strength and 8–12 wt% of a HALS/UV absorber masterbatch; anti-fog surfactant concentrate is incorporated at 1–3 wt%, and an infrared absorber masterbatch at 2–5 wt% when night heat retention is specified. The processing line is a three-layer coextrusion blown film system with a die gap of 1.8–2.4 mm, a blow-up ratio of 2.0:1–2.8:1, and a melt temperature of 210–230°C; the frost line is elevated to 8–10 die diameters to reduce internal haze and permit bubble cooling before the crystalline polymer collapses. Terminal product types include greenhouse covers, low-tunnel films, and temporary crop covers. Compliance for the finished agricultural film is assessed under EN 13206:2017, which requires weathering resistance and tensile retention after artificial ageing according to ISO 4892-2; film tensile properties are measured by ISO 527-3:2018. Published data for the specific UV retention of 7109DJT is limited, so the UV masterbatch dosage is confirmed by outdoor or accelerated weathering on the final coextruded structure rather than extrapolated from neat resin data.

    Stretch Hood Film Melt Strength and Puncture Resistance at 40 µm to 120 µm

    Stretch hood lines processing 40–120 µm film require a hexene-copolymer LLDPE that resists puncture during high-speed pallet application while retaining enough melt strength to survive high-stalk bubble geometries. 7109DJT is formulated at 75–90 wt%, with 10–25 wt% of a single-site-catalyzed polyolefin plastomer or high-pressure LDPE to shift the tear balance toward the transverse direction under ASTM D1922-15a; PIB-free cling additive is dosed at 0.5–2.0 wt%, and antiblock masterbatch at 0.5–2.0 wt% to prevent blocking on high-slip inner surfaces. The downstream line uses a high-stalk bubble with internal bubble cooling, a die gap of 1.5–2.0 mm, a blow-up ratio of 3.5:1–4.5:1, and a melt temperature of 190–220°C; the wide blow-up ratio is necessary because stretch hood application exerts stress along the machine direction while film is stretched over pallet corners. At 7109DJT contents above 90 wt%, film blown at BUR below 3:1 shows a sharp decline in transverse-direction Elmendorf tear and increased splitting during hood application; at BUR above 4.5:1, bubble flutter on rotating die lines reduces gauge uniformity below acceptable limits. Terminal product types are pallet hood films for beverage bottles, white goods, building materials, and chemical pallets. Mechanical acceptance uses tensile properties under ISO 527-3:2018, puncture resistance under ASTM D5748-19, and dart impact under ASTM D1709-16A; where food pallets are wrapped in direct contact, the chemistry must meet Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520(c), although most industrial palletization remains outside direct food-contact enforcement.

    Sealant webs for five-layer coextruded frozen vegetable packaging require seal initiation below 100°C and hot-tack strength sufficient to prevent leaker formation on vertical form-fill-seal machines running at 60–120 packs/min. 7109DJT is placed in the sealant layer at 70–90 wt%, blended with 10–30 wt% high-pressure LDPE or a lower-melting plastomer to depress seal initiation; the sealant layer thickness is typically 10–20 µm inside a 60–90 µm five-layer barrier structure containing an EVOH or polyamide core. The downstream process is blown film coextrusion at a die gap of 1.4–1.8 mm, a blow-up ratio of 2.0:1–2.5:1, and a melt temperature of 210–230°C; post-treatment to 38–42 mN/m is applied to the outer skin layer before lamination or surface printing. Terminal product types include frozen vegetable bags, frozen seafood pouches, and ready-meal film lids. Food-contact compliance is established under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 with overall migration tested below 10 mg/dm² in food simulants; seal strength is measured according to ASTM F88/F88M-21 and hot tack according to ASTM F1921-12. Interlayer adhesion and oxygen transmission are validated on the complete coextruded structure under ASTM D3985-17, because the sealant resin alone cannot predict barrier performance. Published data for this specific five-layer configuration with 7109DJT is limited; seal temperature and dwell must be confirmed on the target form-fill-seal equipment.

    What Determines Load Retention in High-Density Waste Can Liners Blended with LLDPE?

    When the 7109DJT fraction in high-density waste can liners exceeds 40 wt%, load retention under creep declines because the lower modulus of the LLDPE phase allows deformation at perforation points. Typical formulations therefore blend 20–40 wt% 7109DJT with 60–80 wt% of a high-density polyethylene resin having a density of 0.950–0.955 g/cm³; carbon black or color masterbatch is incorporated at 1–3 wt% for opacity and light-shielding. The production line uses a high-density film extruder with a grooved-feed screw, a die gap of 0.9–1.4 mm, a high-stalk bubble with a blow-up ratio of 4:1–5:1, and a melt temperature of 200–230°C; the high-stalk geometry is required to orient the HDPE chains and prevent bubble flutter when the frost line is held at 8–12 die diameters. Terminal product types include commercial can liners, institutional waste bags, and healthcare facility refuse sacks. Compliance for household and commercial refuse sacks in Europe is tested under EN 13592:2017, which defines classification, impact resistance, and tear requirements; for US market acceptance, dart impact under ASTM D1709-16A and Elmendorf tear under ASTM D1922-15a usually define the performance envelope. At 7109DJT additions above 40 wt%, the blend ratio is not increased without re-qualifying the finished liner under the end-user load protocol.

    In bale wrap and bunker silo covers, 7109DJT is run at 25–50 µm on blown film lines with a die gap of 1.8–2.5 mm, a blow-up ratio of 2.5:1–3.5:1, and a melt temperature of 190–220°C. The formulation ratio is 80–100 wt% 7109DJT with 4–8 wt% HALS/UV-stabilizer masterbatch and 0.5–2.0 wt% antioxidant/stabilizer masterbatch; in black/white or black/transparent coextruded films used for silage protection, the white or reflective outer layer includes titanium dioxide masterbatch at 2–6 wt% to reduce surface heating on exposed silage pits. The downstream process is coextrusion or monolayer blown film, with corona treatment to 36–40 mN/m on the side to be printed and lower treatment on the cling side to maintain unwinding and bundling behavior on bale-wrapping machines. Terminal product types include round bale stretch films, silage bags, and bunker silo covers. Compliance for agricultural silage films is based on EN 13207:2018, which covers thermoplastic silage films and specifies mechanical, weathering, and surface properties; mechanical properties are tested under ISO 527-3:2018 and tear propagation under ASTM D1922-15a. Because silage wrap operates under direct UV exposure and mechanical stress during bale wrapping, the film is not used below 25 µm on round bales exceeding 1.2 m diameter unless the wrapping machine applies more than 6 film layers.

    Free Quote

    Competitive Chevron Phillips 7109DJT LLDPE Blown Film Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 7109DJT is an ethylene–1-hexene copolymer linear low-density polyethylene blown film resin. The grade is supplied as pelletised reactor product with a nominal density of 0.918 g/cm³ measured under ASTM D1505 and a nominal melt index of 0.9 g/10 min determined at 190°C with a 2.16 kg load according to ASTM D1238. These two specifications place 7109DJT in the general-purpose LLDPE film range, but the choice of hexene as the comonomer distinguishes it from butene-modified materials. The resin contains stabilisation and processing-aid packages in the base pellet; slip and antiblock are usually converter-added unless a compounded finish is ordered.

    Primary applications include heavy-duty industrial liners, shipping sacks, agricultural silage covers, greenhouse film, and high-strength carrier film. The product is processed as a monolayer or as a toughness layer in coextruded structures. In coextrusion, outer layers may be low-density polyethylene for bubble stability or metallocene LLDPE for lower seal initiation. Layer distribution is application-specific and must be confirmed on the production line because the hexene layer does not always respond to the same frost line and blow-up ratio as a butene layer.

    What Structural Parameters Separate Hexene Copolymer 7109DJT from Butene LLDPE Film Resins?

    At equal density and melt index, an ethylene–hexene copolymer produces butyl branches along the polyethylene backbone, while an ethylene–butene copolymer produces ethyl branches. The butyl branch is less readily incorporated into the orthorhombic polyethylene crystal lattice, so the hexene polymer contains a more interconnected amorphous phase and a higher tie-molecule population. This difference is not captured by density or melt index alone; it appears in fracture-dominated tests. Dart impact is measured by ASTM D1709 Method A, Elmendorf tear by ASTM D1922, and environmental stress-crack resistance by ASTM D1693. Comparative trials on the same blown film line generally show that a hexene LLDPE of this density provides higher dart impact and more balanced machine-direction/transverse-direction tear than a butene LLDPE of identical density.

    The improvement is not universal. Where short-term tensile modulus or die pressure is the limiting factor, a butene or high-density resin may be selected. High frost line heights and high draw can also reduce the machine-direction stiffness of a hexene grade. 7109DJT is therefore used where dart impact, puncture resistance, tear propagation resistance, or slow crack growth performance controls the end-use specification.

    MeasurementMethodPurpose
    DensityASTM D1505Stiffness and permeation balance
    Melt indexASTM D1238 (190°C/2.16 kg)Extrusion control and grade comparison
    Dart impactASTM D1709 Method AFracture toughness of thin film
    Elmendorf tearASTM D1922Machine-direction/transverse-direction tear resistance
    Puncture resistanceASTM D5748Slow puncture energy absorption
    Environmental stress-crack resistanceASTM D1693Resistance to cracking under chemical stress

    Production-scale processing guidance is based on single-screw blown film lines using 40–75 mm barrier screws with 24:1–30:1 L/D ratios and spiral mandrel dies of 150–250 mm diameter. Melt temperatures between 204°C and 232°C are typical for this density class. The lower limit is influenced by melt fracture onset at high screw speeds, while the upper limit reduces the risk of oxidative gels and colour shifts. Die gaps of 1.6–2.3 mm are common for monolayer constructions, with the exact gap selected on the basis of die pressure, output, and gauge control. Narrow gaps raise shear rate and improve bubble stability at high blow-up ratios but increase melt pressure and the risk of melt fracture.

    Blown Film Extrusion Limits and Bubble Geometry Control

    Bubble stability is a central constraint for 7109DJT. Blow-up ratios of 2:1–3:1 and frost line heights between 1 and 3 die diameters are used for balanced properties. A blow-up ratio below 1.8:1 increases machine-direction tear anisotropy, while a ratio above 3.2:1 can produce bubble sag and thickness bands. Hexene LLDPE of this density may have a narrower stable air-ring window than LDPE-rich blends, especially on older single-venturi air rings. Converters often add 10–20 wt% LDPE for bubble support and gauge uniformity. LDPE addition reduces dart impact and puncture resistance; at 30 wt% addition, the hexene toughness advantage can be lost. Published data for this specific configuration is limited, so production-line evaluation is required when changing LDPE content.

    Extruder barrel profiles for 7109DJT should avoid excessive compression-zone heating. Feed-zone setpoints near 185–195°C, compression-zone setpoints of 200–215°C, and metering-zone setpoints of 210–220°C are common starting points. Screw designs with Maddock mixing sections can increase melt temperature by 5–10°C at high backpressure. Die entry pressure and extruder amperage should be recorded; a gradual increase at constant screw speed may indicate gel accumulation on the screen pack or insufficient barrel heating rather than resin viscosity drift.

    In agricultural silage and greenhouse film, 7109DJT is typically converted at thicknesses from 50 µm to 100 µm. Puncture resistance against stubble, stone, and handling damage is a critical requirement; hexene copolymers provide higher resistance to localised deformation than butene copolymers of equivalent density. UV stabiliser masterbatches are required for extended exposure, and compatibility with the base resin should be confirmed because some stabiliser packages can interact with processing-aid chemistry. In heavy-duty shipping sacks, the resin is used to resist drop impact and bruising; the final film must retain sufficient stiffness for automated opening and filling equipment. Static charge decay and surface slip properties are managed through additive masterbatch rather than relying on the base pellet.

    If the Melt Flow Ratio of 7109DJT Exceeds That of a Butene Analogue

    The melt flow ratio, reported as I21/I2 or MI10/MI2, indicates molecular weight distribution width. For a hexene LLDPE of this nominal melt index, a higher melt flow ratio than a butene analogue suggests greater shear thinning and improved processability on high-output lines. The exact ratio for 7109DJT is lot-specific and should be requested on the certificate of analysis. Flow rate at 190°C with 21.6 kg is measured under ASTM D1238. Capillary rheometry under ASTM D3835 with a 20:1 or 30:1 die can generate shear viscosity curves for comparison with the incumbent resin. Converters considering output levels above 0.15 kg/h per millimetre of die circumference should compare low-shear and high-shear viscosity data because hexene and butene resins do not always respond identically to temperature adjustments.

    The molecular weight distribution of 7109DJT is not bimodal in the sense used for high-density film resins. Bubble stability is therefore more sensitive to frost line height and air-ring air velocity than would be the case with a broad or bimodal high-density polyethylene. Elongational viscosity and strain hardening behaviour are best assessed by film blowing trials because conventional rheological tests have limited capability in predicting bubble failure. Published data for this specific configuration is limited; pilot-line or production-line trials remain the reference method.

    Film property measurements are performed on 25 µm or 50 µm film produced on a laboratory blown film line with a 50 mm barrier screw, 100 mm die, 2.5:1 blow-up ratio, and frost line height of 2 die diameters. Dart impact by ASTM D1709 Method A is reported as a comparative value; it depends on film thickness, conditioning, and bubble orientation. Elmendorf tear by ASTM D1922 is not an intrinsic material property and must be interpreted with processing conditions held constant. Tensile properties by ASTM D882 at 500 mm/min crosshead speed provide secant modulus and elongation at break. For a 0.918 g/cm³ hexene LLDPE, tensile yield strength in film is commonly in the range of 9–11 MPa at 23°C, and elongation at break is typically above 500%. These ranges are not product specifications; the exact values for 7109DJT are given in the supplier’s technical data sheet and certificate of analysis.

    Compared with butene LLDPE of the same nominal density and melt index, 7109DJT generally offers higher dart impact and improved slow crack growth resistance. The hexene comonomer disrupts crystallinity more efficiently, so some constructions can be down-gauged without losing burst strength. However, the butene resin may have lower cost and better bubble stability on non-optimised lines. Comparative studies at 25 µm gauge have reported hexene LLDPE dart impact values exceeding butene LLDPE values by 20–40% at equivalent density and melt index; the magnitude is process-dependent, with lower blow-up ratios and higher frost lines often reducing the differential.

    Compared with metallocene-catalysed hexene or octene LLDPE, 7109DJT can have a broader molecular weight distribution, lower extrusion backpressure at high shear rates, and higher haze. Seal initiation temperature must be evaluated by heat-seal testing such as ASTM F2029 or the converter’s standard method. Compared with octene LLDPE, an octene grade may provide further toughness at equivalent density and melt index, but 7109DJT occupies an intermediate position between C4 and C8 copolymers in cost and performance balance.

    Operational limitations include storage moisture and additive compatibility. Surface moisture on pellets can create feed-throat defects; drying at 60–70°C for 2–4 h may be used if condensation is present. Uncontrolled peroxide masterbatch addition should be avoided because free-radical chain scission can generate gels and viscosity drift. The resin is not recommended for clarity-critical applications requiring haze below 5% on a 25 µm blown film. For food-contact uses, compliance with FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 must be verified for the final film structure, including surface additives and laminating adhesives.

    Top