Chevron Phillips 7109clt Lldpe Blown Film Resin Hexene Copolymer

Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer

    • Product Name: Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 950378
    Productname Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Copolymertype Hexene

    As an accredited Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 7109CLT LLDPE Blown Film Resin is packaged in 25 kg (55 lb) polyethylene-lined bags, 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL: palletized 25 kg bags of Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer, approx. 17.5 MT net.
    Shipping Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer ships as non-hazardous polymer pellets in 25 kg polyethylene bags, stretch-wrapped pallets, or bulk trucks/railcars. Transport at ambient temperatures; keep dry, clean, and protected from moisture, UV, and contamination. Not DOT/IMDG/IATA regulated. Follow manufacturer SDS and local rules.
    Storage Store Chevron Phillips 7109CLT LLDPE Blown Film Resin indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed and palletized to prevent moisture, dust, and contamination. Protect from physical damage, avoid excessive stacking, and follow SDS/local regulations. Use first-in, first-out stock rotation.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in a dry, covered area below 50°C.
    Application of Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer

    In dry-flowable chemical packaging operations running gusseted valve sacks at fill rates above 18 bags/min, Chevron Phillips 7109CLT hexene-copolymer LLDPE is used as the primary web where the film must absorb puncture energy from irregular granules without splitting at the corner seal. The governing mechanical acceptance matrix for 25 kg chemical sacks includes ASTM D1709 Method A dart impact at ≥ 400 g for 125 µm film, ASTM D1922 Elmendorf tear at ≥ 15 N in the machine direction and ≥ 18 N in the transverse direction, ASTM D882 tensile elongation at break ≥ 700% MD and ≥ 750% TD, and ASTM D5276 drop testing at 1.2 m with a 25 kg fill mass over 5 drops without burst or sift failure. At the blender, 7109CLT is let down to 80 wt%, high-pressure LDPE with melt index 0.25 g/10 min and density 0.923 g/cm³ is added at 18 wt%, a slip/antiblock masterbatch containing 5% erucamide and 15% synthetic silica is metered at 1.2 wt%, and a polymer processing aid masterbatch is dosed at 0.08 wt%. On a 75 mm single-screw extruder with 30:1 L/D barrier screw and grooved feed section water-jacketed at 40–55 °C, the 250 mm monolayer die is set to a 1.8 mm die gap, melt temperature is held at 204–216 °C, blow-up ratio is 2.5:1, and frost line height is kept at 450–650 mm. Output ranges from 190 kg/h to 210 kg/h; when backpressure exceeds 420 bar, the processing aid is raised to 0.12 wt% to suppress sharkskin on the inner bubble surface. The resulting film tube is slit or gusseted and converted into pinch-bottom sacks, block-bottom valve sacks, and side-gusset sacks for dry-flowable fill weights between 15 kg and 50 kg.

    Cold-Temperature Seal Integrity in IQF Vegetable Packaging

    The regulatory ledger for IQF packaging under frozen storage includes FDA 21 CFR 177.1520(c) 3.1a for olefin polymers in contact with frozen aqueous and fatty foods, Regulation (EU) No 10/2011 Annex I for authorized 1-hexene-derived polyolefins with overall migration limit ≤ 10 mg/dm² under simulated frozen storage, and GB 4806.7-2016 for food-contact polyethylene in export shipments to the PRC. Seal strength testing follows ASTM F88/F88M with a minimum of 2,500 g/25 mm at -20 °C, while hot-tack strength is measured per ASTM F1921 across a 120–145 °C seal-temperature window at 0.5 s dwell and 0.35 N/mm² sealing pressure. In the extruder feed section, the formulation is metered at 72 wt% 7109CLT, 24 wt% high-clarity LDPE with melt index 0.33 g/10 min, 2.5 wt% glycerol-monostearate antifog masterbatch, and 0.7 wt% erucamide-only slip masterbatch. Synthetic silica antiblock is capped below 0.1 wt% to keep haze below 6% per ASTM D1003. On a 3-layer coextrusion line with 200 mm die diameter, 2.0 mm die gap, and internal bubble cooling, the layer ratio is set at 25/50/25, melt temperatures are held within 199–210 °C, blow-up ratio is 2.8:1, and thickness is maintained at 50–80 µm. Downstream conversion produces pillow pouches and gusseted bags for IQF broccoli, cauliflower, mixed vegetables, seafood, and frozen potato products.

    When Hexene LLDPE Is Positioned as a Sealant Web on 3-Layer Laminators

    For snack and dry powder packaging, the sealant web is covered by FDA 21 CFR 177.1520(c) 3.1a, Regulation (EU) No 10/2011, and REACH Annex XVII where applicable to the finished laminate. The finished laminate is tested per ASTM F904-16 for bond strength and ASTM D3985 for oxygen transmission rate; if the structure is intended for hot-fill conditions above 80 °C, seal strength per ASTM F88/F88M is measured after 1 h at the fill temperature. The sealant-side formulation reduces seal initiation temperature without sacrificing dart impact: 7109CLT is metered at 68 wt%, metallocene-catalyzed hexene LLDPE with density 0.916 g/cm³ and melt index 1.0 g/10 min at 28 wt%, and a synthetic silica/erucamide masterbatch at 1.0 wt%. The mLLDPE fraction above 30 wt% lowers seal initiation to 88–92 °C but reduces 50 µm dart impact below 120 g, creating a formulation ceiling at 30 wt%. Blown film substrate is produced at 25–60 µm on a 300 mm die with 1.5 mm die gap, 2.3:1 blow-up ratio, and melt temperature 193–204 °C; the web is corona treated to ≥ 42 dyn/cm and laminated to BOPP or PET with solventless adhesive at 1.8 g/m² coat weight. Terminal types include pre-made stand-up pouches, three-side-seal sachets, and rollstock for dry soup, pasta mixes, pet food, and individually wrapped confectionery.

    Application scenarioCompliance anchorTest conditionAcceptance target
    Heavy-duty chemical sacksASTM D1709 Method A; ASTM D5276125 µm film; 25 kg fill mass, 1.2 m drop≥ 400 g dart impact; no burst over 5 drops
    IQF frozen food packagingFDA 21 CFR 177.1520(c) 3.1a; EU 10/2011; ASTM F88/F88MFrozen food simulant; seal tested at -20 °C≤ 10 mg/dm² overall migration; ≥ 2,500 g/25 mm
    Lamination sealant webASTM F904-16; ASTM D3985; ASTM F88/F88MSolventless laminate; hot-fill up to 80 °CSeal initiation 88–92 °C; bond and OTR per structure
    Agricultural silage coverEN 13206 type B; ISO 4892-3150–200 µm film; 4,000 h weathering cycle 2Elongation retention ≥ 50%; tear ≥ 20 N
    Blown stretch-hood filmASTM D882; ASTM D1709 Method A; ASTM D5458; ASTM D416960 µm film; distribution-cycle vibrationDart impact ≥ 250 g; MD stretch ≥ 600%
    Bulk container linersFDA 21 CFR 177.1520(c) 3.1a; EU 10/2011; ISO 21898; ASTM D1709100 µm liner film; FIBC compatibilityDart impact ≥ 300 g; overall migration ≤ 10 mg/dm²

    Across silage clamp reconstruction in high-altitude dairy regions, UV-induced film embrittlement occurs preferentially at the clamp shoulders where film is stretched over sharp aggregate. Compliance under EN 13206 type B white/black film with durability class N is based on thickness 150–200 µm, tensile elongation retention ≥ 50% after 4,000 h of ISO 4892-3 cycle 2 weathering, and tear propagation resistance per ASTM D1922 at ≥ 20 N in both directions. The extruder-level formulation uses 7109CLT at 68 wt%, high-pressure LDPE at 20 wt%, carbon-black masterbatch at 6 wt%, HALS/UV masterbatch at 5 wt%, and polymer processing aid masterbatch at 0.08 wt%. Carbon black agglomerates above 15 µm create pinholes that initiate premature slit propagation, so the masterbatch is screened through a 120 mesh screen pack before the extruder. Monolayer blown film is run on a 90 mm extruder with 30:1 L/D, 350 mm die, 2.2 mm die gap, 2.8:1 blow-up ratio, melt temperature 196–210 °C, and output 280–310 kg/h. Gauge uniformity across the layflat is held within ± 8% by automatic air-ring control; excursions beyond this range produce localized UV failure at thin spots. Converted products include black/white silage clamp covers, bunker covers, and clamp sheets for chopped maize, grass silage, and high-moisture by-product storage.

    What Limits Gauge Reduction in Blown Stretch-Hood Film Without Puncture Failure?

    Pallet unitization film for automatic stretch-hood lines is tested under ASTM D882 with MD stretch at break ≥ 600% and TD stretch at break ≥ 750%, ASTM D1709 Method A dart impact at ≥ 250 g for 60 µm, ASTM D5458 for cling stretch-film performance, and ASTM D4169 distribution-cycle vibration when transport validation is required. The formulation is metered at 60 wt% 7109CLT, 25 wt% metallocene-catalyzed hexene LLDPE, 10 wt% high-pressure LDPE, and 0.09 wt% polyethylene-based polymer processing aid. Tackifier is not used; cling is mechanical rather than adhesive. Gauge reduction below 45 µm at this blend ratio leads to corner puncture on sharp-edged bottle caps unless the mLLDPE fraction is raised above 35 wt%, which then lowers film stiffness and makes the hood unstable on automatic pallet wrapping lines. Downstream production uses a 350 mm three-layer die, 1.8 mm die gap, 2.4:1 blow-up ratio, melt temperature 190–205 °C, and automated high-speed winders at 180 m/min line speed. Gauge profile is controlled to ± 5% using segmented die-lip heaters and external gauge sensors. Terminal products are stretch-hood sleeves for beverage bottle pallets, building material pallets, and major appliance pallets.

    Application scenarioExtruder and die configurationDie gapBlow-up ratioMelt temperatureThickness range
    Heavy-duty chemical sacks75 mm, 30:1 L/D, 250 mm monolayer die1.8 mm2.5:1204–216 °C125–150 µm
    IQF frozen food packaging200 mm 3-layer die, internal bubble cooling2.0 mm2.8:1199–210 °C50–80 µm
    Lamination sealant web300 mm die1.5 mm2.3:1193–204 °C25–60 µm
    Agricultural silage cover90 mm, 30:1 L/D, 350 mm die2.2 mm2.8:1196–210 °C150–200 µm
    Blown stretch-hood film350 mm 3-layer die1.8 mm2.4:1190–205 °C45–60 µm
    Bulk container liners150 mm or larger die, internal bubble cooling2.0 mm2.2:1190–204 °C80–120 µm

    Bulk Container Liner Gauge Uniformity and Dart Impact Floor

    For food-contact bulk liners, the compliance ledger consists of FDA 21 CFR 177.1520(c) 3.1a, Regulation (EU) No 10/2011 overall migration at ≤ 10 mg/dm², and ISO 21898 for flexible intermediate bulk container compatibility. Mechanical acceptance is based on ASTM D1709 Method A dart impact at ≥ 300 g for 100 µm liner film, ASTM D1922 tear strength at ≥ 25 N MD and ≥ 28 N TD, and ASTM D882 elongation at break above 750%. Formulation is 100 wt% 7109CLT with 0.05 wt% polymer processing aid where gauge uniformity is the primary requirement, or 85/15 7109CLT/mLLDPE where enhanced puncture propagation resistance is required. At 80 µm gauge, the 15 wt% mLLDPE addition raises the dart impact floor from 280 g to 340 g, but addition above 20 wt% reduces bubble stability on high-stalk lines. The liners are blown on a 150 mm or larger die with internal bubble cooling, 2.0 mm die gap, 2.2:1 blow-up ratio, melt temperature 190–204 °C, thickness 80–120 µm, and layflat widths from 1,200 mm to 1,800 mm. Finished types include form-fit liners, baffle liners, and drum liners for FIBCs used with food powders, pharmaceutical excipients, and non-hazardous chemical powders.

    Free Quote

    Competitive Chevron Phillips 7109CLT LLDPE Blown Film Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Chemical 7109CLT is a linear low-density polyethylene blown film resin produced with a hexene-1 comonomer. The nominal resin density is 0.918 g/cm³ when tested in accordance with ASTM D1505, and the nominal melt index is 1.0 g/10 min at 190 °C/2.16 kg when tested in accordance with ASTM D1238-20. The CLT designation identifies a film-grade product within the manufacturer’s LLDPE portfolio, and the hexene copolymer architecture differentiates the material from butene-based LLDPE grades of the same nominal density and melt index. The resin is supplied in pellet form for use in monolayer blown film structures, including produce bags, frozen food packaging, light-duty trash liners, overwrap films, and converted packaging where downgauging, tear resistance, and consistent bubble geometry are process requirements. The exact additive package and lot-specific values should be obtained from the current manufacturer technical data sheet because commercial polyolefin resins are subject to normal lot-to-lot variation.

    How does hexene incorporation alter the crystalline tie-molecule population relative to butene?

    In blown film lines processing 0.918 g/cm³ LLDPE, the length of the short-chain branch introduced by the comonomer has a measurable effect on solid-state crystal organization. Hexene-1 creates a C6 branch that is less efficiently incorporated into the polyethylene orthorhombic crystallite than the C4 branch produced by butene-1. This architectural difference increases the concentration of interlamellar tie molecules at equivalent density and comonomer frequency. The practical result is that film produced from a hexene copolymer such as 7109CLT typically exhibits higher dart impact and higher Elmendorf tear values than butene-based LLDPE of the same nominal melt index when both films are conditioned at 23 °C and 50% relative humidity and tested under ASTM D1709-16a and ASTM D1922-15. The improvement is not uniform across all deformation modes; tensile yield behavior measured under ASTM D882-18 is controlled more strongly by density than by comonomer type, whereas tear propagation and impact energy dissipation are sensitive to tie-chain connectivity. Published data for the exact short-chain branching distribution of 7109CLT is limited, but the hexene designation establishes its structural origin within the C4-to-C8 comonomer spectrum. Film property comparisons across different suppliers require identical gauge, blow-up ratio, frostline height, and die gap because these variables alter molecular orientation and thus the apparent balance between machine-direction and transverse-direction properties.

    Relative to butene-based LLDPE of identical nominal density and melt index, film produced from 7109CLT typically shows higher machine-direction and transverse-direction Elmendorf tear values when measured according to ASTM D1922. The difference is most evident at film gauges below 38 µm, where the crack path must traverse a higher number of load-bearing tie molecules. Compared with autoclave LDPE of similar melt index, the hexene LLDPE has lower extrudate melt tension and a narrower stable-bubble window at high takeoff ratios, but its tensile elongation at break and puncture resistance measured under ASTM D882 and ASTM D5748-18 are generally higher. Blending 10–20 wt% of a tubular or autoclave LDPE into 7109CLT can restore bubble geometry on high-stalk lines, but the addition also depresses dart impact and Elmendorf tear at a rate that is not strictly linear with LDPE concentration. Compared with octene-based LLDPE, hexene copolymers generally occupy an intermediate toughness position; octene comonomers can provide greater tie-molecule generation at equivalent density, while hexene grades often reduce the viscosity penalty associated with longer-chain comonomers during high-shear extrusion. These distinctions are relevant when a converter is evaluating whether a butene-grade replacement will retain sufficient frozen-food impact resistance or whether an octene grade is necessary for severe downgauging applications.

    Blown film extrusion envelope for stable bubble geometry at 0.918 g/cm³

    Barrier-screw extruders with a length-to-diameter ratio between 24:1 and 30:1 and a compression ratio between 2.5:1 and 3.0:1 are appropriate for the thermal and rheological requirements of this resin. A typical feed-throat temperature is maintained between 38 °C and 52 °C, while barrel zones are progressively increased from 177 °C to 221 °C and adapter and die zones are held between 210 °C and 227 °C. The melt temperature at the die exit is preferably maintained between 199 °C and 232 °C. Operation above 246 °C can initiate oxidative chain scission, increase gel formation, and reduce bubble load-bearing capacity. Die gaps for monolayer blown film are typically set between 1.5 mm and 2.5 mm, with blow-up ratios from 2.0:1 to 3.0:1. For high-clarity high-stalk operation, a blow-up ratio of 2.2:1 to 2.6:1 and a frostline height of 1–2 die diameters are commonly used, but the optimum frostline height depends on air ring cooling capacity and ambient line conditions.

    A process conflict arises when the die gap is narrowed to improve optics or orientation. Reducing the die gap below 1.5 mm raises shear rate in the die land and can produce melt fracture in LLDPE, which has a steeper high-shear viscosity curve than LDPE. Widening the die gap beyond 2.5 mm reduces shear and can delay the onset of melt fracture, but it also lowers molecular orientation and may reduce machine-direction tensile modulus. Internal bubble cooling narrows the frostline and improves output consistency, but the higher cooling rate increases crystalline orientation at the outer bubble surface and may shift the balance between dart impact and optical haze. Polyethylene is not hygroscopic in bulk; however, surface condensation from cold storage should be evaporated before extrusion to avoid splay defects. If visible moisture is present, pre-drying for 1–2 h at 60–70 °C may be applied, although dry pellet transfer is normally sufficient. The resin should not be exposed to strong oxidizing agents, chlorinated solvents at elevated temperatures, or peroxide-bearing purging compounds without confirming compatibility with the manufacturer.

    When downgauging shifts the balance from tensile yield to tear propagation resistance

    A reduction in film gauge magnifies the influence of crystalline orientation and melt stress on tear propagation resistance. When a converter downgauges from 38 µm to 25 µm, the limiting mechanical response often changes from tensile yield under ASTM D882 to Elmendorf tear under ASTM D1922 and dart impact under ASTM D1709, because the thinner film contains fewer lamellae through its thickness to arrest crack growth. On high-speed form-fill-seal lines, seal strength is evaluated according to ASTM F88-21 using a gradient heat sealer, typically at 276 kPa seal pressure and 0.5 s dwell, with a universal tensile tester pulling at 200 mm/min. For a 0.918 g/cm³ hexene LLDPE of this class, seal initiation temperature typically falls between 90 °C and 110 °C for 25 µm monolayer film, though published data for this specific configuration is limited and line-specific confirmation is required. Optical haze is quantified under ASTM D1003 and specular gloss under ASTM D2457; film produced at a tighter frostline and higher blow-up ratio generally shows lower haze, but the associated orientation may reduce transverse-direction tear values. The converter therefore balances seal integrity, optical clarity, and tear resistance through die gap, blow-up ratio, and frostline control rather than through resin density alone.

    For food-contact applications, compliance must be confirmed through a supplier statement referencing 21 CFR 177.1520(c) for olefin polymers and, for the European Union, Regulation (EU) No 10/2011 with migration testing under EN 1186 and EN 13130. End-use suitability depends on film thickness, food simulant, contact temperature, and contact time, and a resin compliance statement does not by itself certify a converted film structure. The operational boundaries for 7109CLT are therefore defined by the filmed gauge range, extrusion temperature limits, blend ratios with LDPE, and food-contact regulatory confirmations attached to the specific lot rather than by the density and melt index values alone.