Chevron Phillips 7109bkt Lldpe Blown Film Resin Hexene Copolymer

Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer

    • Product Name: Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 239667
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene
    Density 0.921 g/cm3
    Melt Index 0.9 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 108 °C
    1 Secant Modulus 276 MPa
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 10.3 MPa
    Tensile Strength At Break Md 31.0 MPa
    Tensile Strength At Break Td 26.0 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Dart Drop Impact 150 g
    Haze 12%
    Gloss 45 60%

    As an accredited Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 50 lb (22.7 kg) polyethylene-lined bags, palletized; bulk quantities available in trucks or railcars.
    Container Loading (20′ FCL) 20′ FCL loaded with Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer in 25 kg bags, palletized and secured.
    Shipping Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer is a non-hazardous thermoplastic shipped in 25 kg bags, palletized and stretch-wrapped, or in bulk trucks/railcars. Store dry, away from heat, sunlight, and moisture. Handle with standard equipment; protect packaging from punctures.
    Storage Store Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and oxidizing agents. Keep bags or containers sealed, palletized, and off the ground to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Follow first-in, first-out stock rotation.
    Shelf Life Shelf life is two years from manufacture when stored unopened in original packaging, in a cool, dry place, away from sunlight.
    Application of Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer

    Chevron Phillips 7109BKT is a hexene-copolymer LLDPE blown-film resin whose downstream processing routes differ principally by die gap, layer distribution, additive concentration, and regulatory end-use gate. The application scenarios below separate those variables across six industrial conversion environments and state the equipment, test standards, and operating limits that govern each structure.

    Heavy-Gauge Industrial Sacks and the Need for Puncture Resistance at Gusset Creases

    A three-layer blown-film line configured for form-fill-seal sacks places this hexene copolymer in the core or inner sealant ply, not in a gloss-critical skin layer. The formulation often starts at 65 wt% to 80 wt% 7109BKT, with 20 wt% to 35 wt% LDPE having a melt index below 0.5 g/10 min to increase melt strength and maintain bubble stability at blow-up ratios above 2.8:1. Die gap settings between 1.8 mm and 2.4 mm and melt temperatures between 204°C and 227°C reduce melt fracture while preserving dart impact measured according to ASTM D1709. On a line with 55 mm/65 mm/55 mm screw diameters and an L/D ratio of 30:1, frost-line height is held between 650 mm and 900 mm to balance transverse direction orientation and tear propagation. The finished 160 µm to 220 µm sack body is converted into 25 kg and 50 kg export sacks for polymer pellets, engineering resin powders, and carbon black masterbatches. Gusset creases are the governing failure site; addition of the hexene copolymer above 80 wt% in the core improves puncture propagation resistance but reduces bubble stability, so converters using internal bubble cooling set air temperature between 8°C and 12°C and automatic die control to maintain thickness variation below ±5%. Elmendorf tear in the machine direction, measured with ASTM D1922, becomes the discriminator when sack mass exceeds 35 kg and the film is exposed to pallet-to-pallet abrasion during truck loading.

    Representative three-layer heavy-duty sack formulations using 7109BKT
    Layer positionComposition by weightGauge shareRelease test
    Inner sealant70–80% 7109BKT + 20–30% LDPE25%ASTM F88 seal initiation 105–115°C
    Core75–85% 7109BKT + 15–25% LDPE50%ASTM D1709 dart impact target set by sack mass
    Outer skin20–40% 7109BKT + 60–80% LDPE + 2–5% slip/antiblock masterbatch25%ASTM D1894 kinetic COF 0.15–0.25

    Among converters supplying individually quick-frozen seafood and vegetable packers, the sealant layer is subjected to surface temperatures that move from 110°C at the sealing jaw to -23°C in cold storage within minutes. The hexene copolymer is commonly placed in the 15 µm to 25 µm sealant ply of a five-layer coextrusion with an EVOH oxygen barrier at 3 µm to 5 µm, tie layers at 4 µm to 6 µm, and a polyamide or stiff LLDPE abuse layer on the outer face. Sealing is controlled under ASTM F88 with fin-seal jaw pressure of 0.35 N/mm² to 0.60 N/mm² and dwell time of 0.3 s to 0.8 s; seal initiation at 95°C to 105°C is typical for blends containing 70 wt% to 85 wt% of this hexene copolymer and 15 wt% to 30 wt% plastomer. The finished 40 µm to 80 µm laminate is converted into pillow packs for IQF shrimp, mixed berries, and diced vegetables. Compliance rests on 21 CFR 177.1520 for the olefin polymer sealant layer and Regulation (EU) No 10/2011 with overall migration below 10 mg/dm² under test conditions for the intended frozen-food use. Cold-temperature impact is assessed with ASTM D1709 dart-drop testing on the finished laminate at -18°C; the failure mode shifts from puncture to brittle fracture when the sealant layer exceeds 80% of the total thickness, which is outside the recommended structure. Anti-fog masterbatch can be incorporated into the sealant ply at 0.5 wt% to 1.0 wt% for visible-pack vegetable applications, but it reduces seal strength at temperatures below 105°C unless dwell time is extended. A converter moving the seal layer below 12 µm observes seal failure at the inner crease after drop tests at -18°C; published data for this specific laminate configuration is limited, and line validation is required.

    Why Does Hexene Comonomer Short-Chain Branching Control Tear Performance in Silage Stretch Film?

    Extrusion of a monolayer silage film from this hexene copolymer without a UV masterbatch produces a structure that fails brittleness tests after a single season, but the short-chain branching from hexene contributes to the tear propagation resistance required when wrapping high-density round bales. A typical silage film contains 1.0 wt% to 2.5 wt% of a HALS/UV absorber masterbatch in a polyethylene carrier, with the concentrate let down at the feed throat of a 45 mm to 65 mm single-screw extruder running at 150 kg/h to 250 kg/h. Melt temperature is held between 215°C and 235°C, die gap between 1.4 mm and 2.0 mm, and blow-up ratio between 2.5:1 and 3.5:1 to generate the transverse direction elongation needed around the bale shoulders. Film thickness from 25 µm to 150 µm is supplied in 750 mm to 1,500 mm lay-flat widths for round bales and clamp silage covers. Accelerated weathering under ISO 4892-2 with UVA 340 lamps at 0.68 W/m² and 60°C black-panel temperature is used as an incoming QC release for stabilizer masterbatch lots. The terminal products are 12-month and 24-month silage covers, bale wrap, and silo bags; films without the stated stabilizer loading show tensile elongation retention below 50% after 3,000 hours in high UV regions when tested under ISO 527-3. At the low end of the gauge range, transverse tear resistance is improved by orienting the film at blow-up ratios above 3.0:1, but the same setting increases width variability on unguided bubbles. Compliance for the agricultural structure is based on EN 13207 for silage film and the general packaging requirements of 94/62/EC only where the film is subsequently used as a secondary wrap for bagged feed. Machine-direction Elmendorf tear, measured with ASTM D1922, is the primary discriminator at the end of the season because the film must not split during re-wrapping or bale storage on rough concrete.

    Liquid bulk liner converting from the same hexene copolymer addresses a different constraint: the seal must survive both 0.15 bar internal pressure cycles and chemical attack from low concentrations of hypochlorite, alcohol, or edible-oil permeation. The resin is used as the 70 µm to 100 µm inner web of a laminated structure carrying reverse-printed polyester or metallized PET on the outside. Web tension is set to 20 N/mm² to 35 N/mm² during lamination; surface treatment is held at 38 dyn/cm to 42 dyn/cm after corona discharge to maintain peel strength above 2.0 N/15 mm measured by ASTM F904. Surface treatment decay below 36 dyn/cm on stored rolls leads to lamination bond loss, so corona treaters are placed in-line immediately before the laminator. For food-contact liners, 21 CFR 177.1520 applies for aqueous, acidic, alcoholic up to 8%, and fatty foods; Regulation (EU) No 10/2011 sets overall migration below 10 mg/dm². Terminal products include 5 L to 20 L bag-in-box liners, wine and edible-oil bladders, and food-service condiment pouches. The critical process limit is seal contamination by fatty products; minimum seal bar temperature of 140°C and dwell of 1.0 s are required after hot-fill at 85°C. Bubble cooling air at 6°C to 10°C and die gap 1.8 mm to 2.2 mm prevent blocked film that would cause missed seals on vertical form-fill-seal lines. The film is not recommended for direct contact with chlorinated solvents above 5% active chlorine at 40°C without a barrier tie layer; prolonged contact with concentrated d-limonene causes sealant swelling that reduces peel strength below the 2.0 N/15 mm threshold.

    Compliance gates across application segments
    Application segmentRegulatory gateCritical metric
    Frozen food sealant web21 CFR 177.1520; Regulation (EU) No 10/2011Overall migration ≤ 10 mg/dm²; seal strength per ASTM F88
    Liquid bag-in-box liner21 CFR 177.1520; Regulation (EU) No 10/2011Laminate bond ≥ 2.0 N/15 mm per ASTM F904
    Agricultural silage filmEN 13207Elongation retention ≥ 50% after 3,000 h ISO 4892-2
    Collation shrink sleeve94/62/ECHeavy metal sum ≤ 100 ppm

    When Collation Shrink Film Moves from LDPE-Only to a Hexene LLDPE-Rich Blend

    Replacing 30 wt% to 50 wt% of a conventional autoclave LDPE with this hexene copolymer in collation shrink alters the heat-seal response, shrink force, and puncture resistance of the final sleeve. The converter typically runs a 55 mm to 75 mm single-screw extruder at 170 kg/h to 300 kg/h with a dual-lip air ring, die gap of 1.2 mm to 1.8 mm, and blow-up ratio of 2.2:1 to 3.0:1. For a 45 µm to 70 µm film, the addition of the hexene copolymer at 35 wt% raises machine-direction shrink tension at 130°C from 0.15 N/mm² to 0.30 N/mm² when measured according to ISO 14616. Too high a LLDPE fraction above 60 wt% produces bubble instability at high frost-line settings and makes shrink force directionality difficult to control on steam tunnels operating at 120°C to 140°C. Excess frost-line height above 750 mm with the LLDPE-rich formulation causes fluctuating layflat width, so automatic bubble cage guides are used on the collation line. Terminal uses are 6-pack and 12-pack beverage can sleeves, cosmetics overwrap, and confectionery multipacks. Converters evaluate free shrink and shrink force with ISO 11501 and ISO 14616 and tensile properties with ISO 527-3. Heavy-metal content in the finished printed film is verified against the sum limit of 100 ppm under EU Packaging Directive 94/62/EC. Puncture resistance of the shrink sleeve is measured with ASTM D5748, and a drop from 1.5 m onto a sharp corner is used as a converter-specific abuse test for beverage multipacks.

    On a pallet-containing line operating at 40 pallets per hour, blown stretch-hood film made with the hexene copolymer is drawn over goods at speeds exceeding 7 m/s and must retain sufficient elasticity to return to the pallet foot. The preferred structure is a three-layer blown film with 50 wt% to 70 wt% of the hexene copolymer in the core and outer plies, the balance being metallocene plastomer or LDPE to reduce elongation at break and raise puncture propagation resistance. Gauge runs from 50 µm to 120 µm; high-stalk configurations with frost-line heights above 800 mm and blow-up ratios between 3.5:1 and 4.5:1 give the needed transverse stretch of 60% to 90% during hood application. Hexene copolymer provides higher dart impact and tear propagation than butene-copolymer LLDPE when compared under ASTM D1709 and ASTM D1922, but the film haze is higher; haze is quantified by ASTM D1003, and clarity is not specified for the listed hood applications. Terminal uses are hoods for white-goods distribution, construction material bundles, and glass container palletizing where optical clarity is not required. Puncture resistance is measured by ASTM D5748, tensile by ASTM D882, and cling is not required because the hood is heat-sealed. Ambient temperature in the stretching hall is held above 15°C; below that, the hood loses elastic recovery and fails to lock under the pallet foot. Converters with older extruders below 30:1 L/D report pressure fluctuations above 25 bar when the hexene copolymer fraction exceeds 70 wt% at 220°C, requiring a reduction in screw speed rather than an increase in melt temperature. The lower melt-temperature limit is set at 190°C for this structure; below that, the hexene copolymer fraction above 70 wt% produces high extrusion pressure and visible die lines on the hood surface.

    Free Quote

    Competitive Chevron Phillips 7109BKT LLDPE Blown Film Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 7109BKT is a linear low-density polyethylene blown film resin produced with 1-hexene as the comonomer. Manufacturer product documentation identifies a nominal melt flow rate of 1.0 g/10 min at 190 °C under a 2.16 kg load following ASTM D1238 and a nominal density of 0.918 g/cm³ following ASTM D1505. The resin is supplied as pellets for film extrusion lines producing industrial liners, heavy-duty sacks, agricultural film, and multilayer sealant webs. The hexene-copolymer designation is structurally significant: the butyl branches produced by 1-hexene alter crystalline morphology and tie-molecule population relative to butene-copolymer LLDPE of the same melt flow rate and density. The BKT designation corresponds to a grade-specific additive package documented in the supplier certificate of analysis; slip and antiblock loadings are not defined by the base resin physical properties.

    The grade is not characterized by a single mechanical datum. Film properties are a function of blow-up ratio, die gap, frost line height, and cooling rate. The nominal melt flow rate and density allow a processing window that supports high-output lines with spiral mandrel or pancake dies, but the final balance of tear, impact, and stiffness is process-dependent. Consequently, the supplier certificate of analysis and the current technical data sheet are the controlling documents for the shipped lot; the values cited in this text are class-typical unless identified as manufacturer-specified limits.

    Why does the hexene branch length alter dart impact and tear in 7109BKT?

    Short-chain branch length influences the ability of polymer chains to participate in adjacent lamellar crystals. In butene-copolymer LLDPE, the comonomer contributes ethyl branches from 1-butene. In 7109BKT, the butyl branches from 1-hexene are sterically less tolerated within the ethylene crystal lattice. During crystallization, the longer branch preferentially remains in the amorphous interlamellar region and increases the number of load-bearing tie molecules that bridge adjacent lamellae. This structural difference is not measured by density or melt flow rate but appears in slow puncture, Elmendorf tear, and dart impact tests.

    For film converters, the practical consequence is that a 0.918 g/cm³, 1.0 g/10 min hexene-copolymer LLDPE can exhibit higher Elmendorf tear and dart impact than a butene-copolymer grade of the same nominal density. The degree of improvement is not a fixed percentage because it is modulated by frost line height, blow-up ratio, and downstream annealing. Machine-direction orientation degrades transverse-direction tear; a deep frost line increases this effect. The hexene branch length does not eliminate the trade-off but moves the starting balance toward tougher film. The branch distribution is also not uniform across the molecular weight distribution. High-molecular-weight chains with higher comonomer incorporation are especially effective at tie-chain formation, while low-molecular-weight chains contribute less and participate more directly in seal initiation. This heterogeneity explains why melt flow rate and density alone cannot predict dart impact.

    Typical class-typical comparisons for 25 µm film at 2.5:1 blow-up ratio place dart drop impact in the 120–160 g range for hexene-copolymer LLDPE versus 80–100 g for butene-copolymer LLDPE under ASTM D1709A; Elmendorf tear in the transverse direction may be 350–500 g versus 250–400 g under ASTM D1922. These ranges are not lot specifications for 7109BKT but published class ranges for LLDPE of identical nominal density and melt flow rate.

    On a conventional high-stalk blown film line with a 45 mm extruder and 24:1 L/D barrier screw, 7109BKT is run with barrel temperatures from 180 °C to 215 °C, adapter and die temperatures from 200 °C to 225 °C, and a die gap of 1.5 mm to 2.0 mm. A die gap below 1.2 mm raises shear stress at the die lip and can produce sharkskin surface defects. The bubble is held at a blow-up ratio of 2.0:1 to 3.0:1, with frost line height from 3 to 5 die diameters. Internal bubble cooling is recommended above 200 kg/h throughput on larger lines to maintain bubble diameter and reduce film blocking tendency. These processing data reflect hexene-copolymer LLDPE blown film practice; actual settings are determined by extruder size, screw design, and die diameter.

    At high output, die pressure and motor load should be monitored. When die pressure exceeds 350 bar on a 60 mm grooved-feed extruder, the cause is often feed zone bridging or insufficient melting rather than resin viscosity alone. Reducing first barrel zone temperature by 5–10 °C or increasing screw speed gradually can stabilize the melt. The resin is not preheated in a hopper dryer under normal ambient conditions; if condensation is present, drying at 60 °C for 2 h is sufficient to remove surface moisture without degrading the additive package. Processing below 170 °C can produce unmelted pellets and bubble pinholes, while processing above 240 °C accelerates oxidative degradation and generates gel particles. The preferred melt temperature is therefore 195–215 °C for balanced film toughness and thermal stability.

    For die land pressure calculations, capillary rheometry is required. Apparent viscosity for this LLDPE class at 190 °C and 100 s⁻¹ shear rate is generally in the 800–1200 Pa·s range, but exact values for 7109BKT must be measured under ISO 11443. The flow activation energy of LLDPE is typically 28–32 kJ/mol; a 10 °C melt-temperature change can therefore alter viscosity by approximately 10–15 % depending on shear rate.

    When 7109BKT replaces a butene-copolymer LLDPE of the same nominal density and melt flow rate in heavy-duty sack film

    Substitution is not automatically a drop-in change. The hexene-copolymer film can allow downgauging in monolayer sacks from 100 µm to 80 µm if field failures are dominated by low-speed puncture or tear rather than tensile strength; the safe downgauge must be confirmed by filled-drop and environmental stress-cracking tests. Seal initiation temperature may shift by 3–5 °C because the crystal thickness distribution changes when hexene is used. Seal bar temperature is typically set between 115 °C and 150 °C for monolayer film, but hot-tack and seal strength should be measured on the actual film using ASTM F1921 or ASTM F2622. Published data for 7109BKT-specific seal shift is limited; pilot-line verification is required before commercial substitution.

    Compared with metallocene-catalyzed hexene LLDPE, the non-metallocene 7109BKT may show broader molecular weight distribution and a different haze/gloss balance. The broader distribution generally improves melt strength and bubble stability but can reduce clarity in thin-gauge converter film. If optical haze below 10 % is required, a metallocene-catalyzed grade or an LDPE blend may be necessary. The differentiation is therefore not an absolute performance ranking but a processing and property-position selection.

    Frost line height above the die face controls the balance between MD and TD orientation

    For 7109BKT, frost line position determines the amount of axial drawing before crystallization freezes the film. High frost lines above 4 die diameters stretch the melt in the machine direction, raising MD tensile strength, lowering MD tear propagation resistance, and reducing TD tear. Low frost lines below 3 die diameters reduce orientation, producing more isotropic film with higher dart impact. On high-stalk lines, lowering frost line too much increases bubble flutter and width variability; on in-pocket lines, the cooling-air pattern should be adjusted rather than using frost line height alone.

    Die gap influences the same balance. A larger die gap of 2.0 mm reduces shear orientation in the machine direction and generally improves Elmendorf tear in both directions, while a gap below 1.2 mm can improve optics through higher shear refinement but increases the risk of melt fracture. The selected gap is a compromise between output stability and physical properties; no single gap setting is optimal for all film gauges. For film below 30 µm, internal bubble cooling and a tighter die gap may be used, but the converter should verify roll blocking and coefficient of friction because slip additive migration is time- and temperature-dependent according to ASTM D1894.

    Mechanical property limits for 25 µm and 50 µm blown film

    Class-typical film property ranges for a 0.918 g/cm³, 1.0 g/10 min hexene-copolymer LLDPE at 2.5:1 blow-up ratio
    PropertyTest method25 µm film50 µm film
    Dart drop impactASTM D1709A120–160 g350–550 g
    Elmendorf tear MDASTM D1922250–400 g600–900 g
    Elmendorf tear TDASTM D1922350–500 g800–1100 g
    Tensile yield MDASTM D8829–11 MPa9–11 MPa
    Tensile yield TDASTM D8829–11 MPa9–11 MPa
    Elongation at break MDASTM D882600–800 %600–800 %
    Secant modulus 1% MDASTM D882170–220 MPa170–220 MPa

    These values are not supplier-guaranteed specifications for 7109BKT but are published ranges for hexene-copolymer LLDPE blown film of identical nominal density and melt flow rate. Actual film directionality depends on die gap and frost line settings. The certificate of analysis remains the controlling document.

    Without a barrier layer, 25 µm film of this density class typically shows water vapour transmission rate near 18–22 g/m²·day at 23 °C and 85 % RH by ASTM F1249. Oxygen transmission rate is high, generally 2500–4000 cm³/m²·day·atm by ASTM D3985; therefore 7109BKT is not selected when oxygen barrier is the primary function. Slip additive migration to the film surface is time- and temperature-dependent, with coefficient of friction measured under ASTM D1894. Dissipation of bloom can take 24–72 h after film winding, depending on winding tension and roll hardness. Converters should condition rolls before printing or laminating to avoid surface treatment loss.

    For food-contact applications, the supplier certificate should be consulted for compliance with FDA 21 CFR 177.1520(c) 3.1a and, where applicable, Regulation (EU) No 10/2011 for overall migration. The base LLDPE class does not contain heavy metals above RoHS Directive 2011/65/EU limits and is not classified as hazardous under REACH Regulation (EC) No 1907/2006. Converters are responsible for verifying final film performance after adding masterbatch, recycled material, or processing aids.

    Pellets should be stored below 50 °C in sealed containers. Moisture absorption is low; pre-drying is not normally required. If surface condensation occurs during winter conveying, a desiccant dryer at 60 °C for 2 h removes surface moisture without driving off the slip additive. Process aids and fluoropolymer additives should not be added above the recommended let-down ratio; high levels can reduce film seal strength and raise extractables beyond food-contact limits.

    Heavy-duty shipping sacks and industrial liners produced from 7109BKT are run in 70–120 µm thickness ranges. Agricultural silage and mulch films may use 25–50 µm film with ultraviolet stabilizer masterbatch added at the converter; UV exposure testing is conducted under ASTM G160 or ISO 4892-1 because the base resin does not provide substantial UV resistance. Blending with LDPE at 10–30 wt% improves bubble stability and heat sealability; increasing LDPE beyond 30 wt% reduces dart impact and tear resistance, narrowing the performance advantage of the hexene-copolymer base. Collation shrink and thin-gauge overwrap structures may require a higher melt flow rate or metallocene-catalyzed resin; 7109BKT is not intended for high-clarity shrink film under 10 % haze if optical requirements dominate.