Chevron Phillips 7109bk Linear Low Density Polyethylene Blown Film Resin

Chevron Phillips 7109BK Linear low density polyethylene blown film resin

    • Product Name: Chevron Phillips 7109BK Linear low density polyethylene blown film resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 118089
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 27.6 MPa
    Elongation At Break 750%
    Tensile Modulus 0.207 GPa
    Flexural Modulus 0.241 GPa
    Vicat Softening Point 97°C
    Melting Point 122°C
    Haze 12%
    Gloss 60%
    Dart Drop Impact 130 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g

    As an accredited Chevron Phillips 7109BK Linear low density polyethylene blown film resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 7109BK Linear low density polyethylene blown film resin is supplied in 25 kg polyethylene bags, palletized for shipping.
    Container Loading (20′ FCL) 20′ FCL container securely loaded with Chevron Phillips 7109BK linear low density polyethylene blown film resin in 25 kg bags.
    Shipping Chevron Phillips 7109BK LLDPE blown film resin is a non-hazardous solid. Ship in sealed 25 kg bags or 1,000 kg supersacks, palletized, in dry, clean containers/vans at ambient temperature. Protect from moisture, contamination, heat, and direct sunlight. No UN number, hazard class, or placards required.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep original containers closed when not in use to prevent moisture, dust, and contamination. Maintain stable stacking, avoid physical damage, and follow the manufacturer’s SDS and local regulations. Ensure good housekeeping and spill containment.
    Shelf Life Shelf life is 24 months from date of manufacture when stored cool, dry, and in unopened original packaging.
    Application of Chevron Phillips 7109BK Linear low density polyethylene blown film resin

    Black silage cover film produced from Chevron Phillips 7109BK is typically evaluated against EN 13207:2018, which sets requirements for tensile properties, tear resistance, UV stabilisation, and oxygen permeability in thermoplastic silage films. On high-output spiral mandrel lines with blow-up ratios of 2.0–2.8 and die gaps of 1.8–2.4 mm, the resin is commonly blended with 5–15 wt% LDPE or a LLDPE-rich LDPE/LLDPE mixture to modify melt extensibility and bubble stability during black film production. The carbon black component in this grade requires dispersion control at incoming inspection; ASTM D5596 microscopy is applied to detect agglomerates that can produce pinholes or tear propagation under silage pile settlement. Film thickness for bunker silage covers commonly falls in the 150–250 µm range, with the lower bound set by puncture resistance during compaction and the upper bound set by handling weight and cling. Melt temperature is held at 195–230 °C, and frost line height is maintained at 4–6 die diameters to balance machine-direction and transverse-direction orientation. If the frost line is raised beyond 6 die diameters, dart impact values measured by ASTM D1709 may decline due to excessive transverse-direction orientation. If the die gap is reduced below 1.5 mm while increasing throughput, shear heating in the black compound narrows the bubble stability window and raises backpressure on the extrusion line. The terminal black film is used as a bunker cover, silage bag, or silo sheet, with oxygen transmission controlled to limit aerobic spoilage at the forage surface.

    When a Landfill Cushion Geomembrane Must Satisfy GRI-GM17 Single-Point Puncture

    For a black LLDPE geomembrane liner based on this resin class, the primary conversion route is thick-gauge blown film on equipment with die gaps of 2.0–3.0 mm and blow-up ratios of 1.5–2.5 to preserve impact strength and welding yield. The carbon black loading is controlled within 2.0–3.0 wt% because GRI-GM17 and landfill specifications require carbon black dispersion sufficient to prevent ultraviolet embrittlement; antioxidant materials are typically present at 0.3–0.8 wt% with phosphite co-stabilisers at 0.15–0.40 wt% to protect the resin during high-temperature processing. Welding on site requires hot-wedge or extrusion fusion temperatures of 350–450 °C at the weld interface, with overlap of 75–100 mm and controlled roller pressure; insufficient heat input produces a peel seam that fails before the parent sheet in ASTM D6392 peel tests. Single-point puncture resistance is measured by ASTM D4833, while wide-width tensile and tear values are generated from ASTM D6693 and ASTM D1004, respectively. Stress cracking in liners is evaluated with the notched constant tensile load method ASTM D5397 under accelerated test conditions. The production challenge is not extrusion temperature alone but the interaction between carbon black, stabiliser consumption, and bubble cooling; a low melt temperature of 180–210 °C is generally used to minimise molecular weight loss, but increasing output without increasing air-ring cooling causes a rise in frost line height and a measurable drop in puncture energy. End uses include landfill bottom liners, pond liners, and secondary containment geomembranes installed in contact with soil and leachate.

    Test propertyMethod designationTypical acceptance basis for black LLDPE geomembrane liners
    Carbon black contentASTM D42182.0–3.0 wt%, lot average within specification
    Carbon black dispersionASTM D5596Pass/fail per GRI-GM17 field count
    ThicknessASTM D5199Minimum average thickness per project design
    Single-point punctureASTM D4833GRI-GM17 minimum pass/fail by sheet thickness
    Wide-width tensileASTM D6693GRI-GM17 minimum break and yield values
    Tear resistanceASTM D1004GRI-GM17 minimum tear strength
    Stress crack resistanceASTM D5397No brittle failure before specified hours

    At a flexible intermediate bulk container liner converter running 24 h continuous shifts on a 450 mm spiral die, the black LLDPE film is processed at blow-up ratios of 1.8–2.2 and die gaps of 1.2–1.8 mm to produce tubular liners that combine high dart impact with controlled film-to-film friction. Compliance for FIBC liners is usually driven by the outer woven polypropylene structure under ISO 21898, but the inner film is separately tested for tensile behaviour with ASTM D882, dart impact with ASTM D1709, and pinhole density under light-table inspection. Addition levels for antiblock and slip masterbatch are kept below 0.10 wt% active amide if the liner must remain in place during filling; otherwise, film slippage on the filling lance causes the liner to bunch and tear. Antistatic additives, when specified for chemical or mineral fillers, are introduced as slow-migration types at 0.05–0.20 wt%, but their effect on seal integrity must be checked because blooming can lower seal strength on impulse sealers set at 120–160 °C. The extrusion line often runs with a melt temperature of 190–220 °C and a frost line height of 3–5 die diameters to keep both machine-direction tear and transverse-direction tear within the end-user specification. Reducing the die gap below 1.2 mm while increasing winding speed typically raises shear heating and produces melt fracture in the carbon black compound; this appears as shark-skin on the inner film surface and prevents consistent sealing. End products include tubular liners for bulk bags, box liners for mineral powders, and heavy-duty sacks for fertilisers.

    Where Does Frost Line Height Alter Dart Impact in 0.12–0.20 mm Mulch Film?

    Conventional black LLDPE mulch film produced from this resin type is run on narrow die gaps of 0.8–1.2 mm and blow-up ratios of 2.0–3.0 to achieve a gauge range of 0.12–0.20 mm without excessive transverse-direction profiling. The opacity and weathering performance of the black film are influenced by carbon black loading and dispersion; film used for one-season vegetable production is commonly specified to retain tensile elongation above a critical value after 150–200 days of solar exposure, although published data for this specific configuration is limited and batch-specific UV retention should be checked against the supplier certificate of analysis. Dart impact is measured with ASTM D1709 and tear resistance with ASTM D1922; both values drop when the frost line is raised beyond 4 die diameters because high orientation in the transverse direction reduces impact ductility in thin gauge. Conversely, a frost line below 2 die diameters produces low bubble stability and gauge bands that alter mulch lay-down on raised beds. Melt temperature is controlled at 190–215 °C to limit carbon black thermal oxidation while maintaining enough melt strength for the thin film. The die gap narrows the processing window more than in heavier film: below 0.8 mm, backpressure increases rapidly and the black melt may exhibit melt fracture at commercial output rates. Terminal mulch films are installed over strawberry, tomato, and vine crops, where light exclusion and soil temperature regulation are the primary functions.

    Construction Vapor Retarder and Concrete Curing Liner Thickness Limits

    Black LLDPE film used as a below-slab vapour retarder is produced in thicknesses from 0.20–0.50 mm depending on moisture transport requirements, with the upper range reserved for underslab installations that require puncture survival during reinforcement placement. Water vapour transmission is measured by ASTM E96 and the completed vapour retarder sheet is evaluated under ASTM E1745 for tensile, puncture, and permeance classes. The converter operates with a die gap of 1.8–2.5 mm and a low blow-up ratio of 1.6–2.0 to reduce pinhole density and improve gauge uniformity across the sheet width. Melt temperature is held at 195–225 °C; higher temperatures lower melt strength and increase longitudinal gauge variation at low blow-up ratio. Carbon black is present at levels typical for UV-stable black film, but the primary function in this application is light blocking and resistance to surface contamination rather than long-term outdoor exposure. The processing limit is thickness-related: when converters reduce thickness below 0.20 mm to cut bill-of-material cost, puncture resistance measured by ASTM D1709 may fall below project specification because the film lacks sufficient gauge to redistribute point loads. End products include underslab vapour retarders, temporary concrete curing covers, and crawlspace moisture barriers placed over aggregate.

    Pallet stretch hood film made from this class of black LLDPE requires a different orientation balance than silage or geomembrane film because the hoist-and-stretch cycle imposes high elongation along the machine direction while the film must still resist snagging on pallet edges. Blown film production uses blow-up ratios of 2.0–2.5 and die gaps of 1.2–2.0 mm, with melt temperature set at 185–210 °C to retain high molecular weight and dart impact. The frost line is kept at 3–5 die diameters; a higher frost line increases transverse-direction orientation and reduces recoverable stretch, while a lower frost line destabilises the bubble during rapid start-stop winder cycles. Stretch hood machines apply controlled film elongation, commonly in the 50–80 % range, measured in the machine direction before the film is released over the pallet. Films in this segment are tested for tensile elongation at break with ISO 527-3 or ASTM D882, dart impact with ASTM D1709, cling or release force with ASTM D5458, and protrusion puncture with ASTM D5748. Slip and antiblock packages, if used, are kept below 0.15 wt% to prevent a loss of film-to-pallet friction after the hood retracts. Published data for this specific black resin in automated stretch hood installations is limited; line trials at the converter level are required to set final gauge and formulation because winder acceleration and pallet corner geometry dominate failure performance. End products include black stretch hoods for building material pallets, bagged mineral products, and heavy unit loads stored outdoors.

    Free Quote

    Competitive Chevron Phillips 7109BK Linear low density polyethylene blown film resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 7109BK is a linear low density polyethylene blown film resin supplied in pellet form for monolayer and coextruded film structures. The grade belongs to the Ziegler-Natta-catalysed LLDPE class with a nominal density of 0.918 g/cm³ measured by ASTM D1505 and a nominal melt index of 0.90 g/10 min measured by ASTM D1238 at 190°C under a 2.16 kg load. These values define a medium-molecular-weight film resin intended for heavy-duty sacks, industrial liners, agricultural film, carrier bags, and protective packaging. The product is formulated specifically for blown film extrusion; its molecular architecture and stabiliser package are not optimised for injection moulding or rotational moulding. The resin produces films with toughness, tear resistance, and drawdown behaviour that differ systematically from high-pressure low density polyethylene and metallocene LLDPE grades. The BK designation should be confirmed against the manufacturer’s technical data sheet because colour and carbon black content affect density, opacity, and weathering performance.

    Nominal Property Profile and Test Designations

    Blown film converters typically qualify a resin using melt index, density, and film mechanical properties. For 7109BK, the starting values are summarised below. Melt index may also be reported as ISO 1133-1:2022 at 190°C/2.16 kg; values are equivalent within normal laboratory reproducibility.

    ParameterNominal value or rangeTest method or equipment
    Melt index0.90 g/10 minASTM D1238 at 190°C/2.16 kg
    Density0.918 g/cm³ASTM D1505
    Typical melt temperature190–220°CExtruder melt probe
    Die gap1.5–2.5 mmSpiral mandrel die
    Blow-up ratio2.0:1–3.0:1Continuous blown film line

    Density controls film stiffness, moisture vapour transmission, and shrink tendency. A density of 0.918 g/cm³ is at the lower end of the LLDPE film range, giving lower secant modulus but greater low-temperature toughness than grades above 0.925 g/cm³. Water vapour transmission rate determined by ASTM E96/E96M is typically more favourable at this density because lower density increases free volume relative to higher-density polyethylene; however, the final value depends on gauge, crystallinity, and additive loading. Melt index controls extruder throughput, head pressure, and draw resonance. At 0.90 g/10 min, the resin requires more extruder torque than film grades with melt indices above 1.5 g/10 min, but provides greater bubble stability for films below 50 µm. Film physical properties such as dart impact, tensile strength, and Elmendorf tear are not intrinsic resin properties; they depend on gauge, blow-up ratio, frost line, and cooling rate. Published data for this specific configuration is limited and should be verified with a line trial.

    On production-scale blown film lines, a 65 mm grooved-barrel extruder with L/D 25:1 to 30:1 and a spiral mandrel die is a common starting point. Melt temperature is normally held between 190°C and 220°C; die pressure at a 1.5–2.5 mm die gap typically ranges from 280 bar to 420 bar at output rates of 80–120 kg/h. Operating above 230°C for extended periods promotes oxidative gel formation and can shift melt index, producing visible gel specks and reduced bubble stability. When the die gap is narrowed below 1.2 mm to improve gauge uniformity, the critical shear stress at the die lip may be exceeded, producing sharkskin surface roughness in the machine direction. The frost line should be maintained at 1.5–2.5 times the die diameter for a blow-up ratio of 2.0:1 to 3.0:1. A dual-lip air ring or internal bubble cooling is recommended when the gauge is below 25 µm because a single-lip air ring can allow bubble oscillation greater than ±2 mm and create thickness variation above ±10%. Because 7109BK lacks long-chain branching, its extensional viscosity is lower than that of high-pressure LDPE at equivalent melt index; when coextrusion or high blow-up ratio operation exceeds 3.5:1, a blend with 10–20 wt% high-pressure LDPE is often used to restore bubble stability.

    What Distinguishes 7109BK from High-Pressure LDPE and Metallocene LLDPE?

    High-pressure LDPE films have long-chain branching and typically lower dart impact at equivalent gauge. Under ASTM D1709, 25 µm films from conventional LLDPE in this density and melt index class commonly show dart impact values from 95 g to 140 g, whereas high-pressure LDPE films of similar gauge may fall below 80 g. The mechanical difference originates in the linear polyethylene backbone, which also raises tensile strength at break under ASTM D882 and Elmendorf tear strength under ASTM D1922. LDPE retains an advantage in bubble stability because long-chain branching increases extensional viscosity and strain hardening; therefore LDPE is frequently added to LLDPE at 10–20 wt% for high blow-up ratio lines.

    Metallocene-catalysed LLDPE grades have narrower molecular weight distribution and more uniform comonomer incorporation. These grades typically show higher dart impact and better clarity than Ziegler-Natta LLDPE at equivalent density, but they can require higher extruder head pressure and torque. The broader molecular weight distribution of 7109BK favours shear thinning and permits greater throughput on grooved-barrel extruders; however, optical properties measured as haze under ASTM D1003 are generally higher than those of metallocene grades. Comparative literature indicates dart impact differences of 10–25% between conventional Ziegler-Natta and metallocene LLDPE at equivalent density and gauge. Ethylene-vinyl acetate copolymer films with vinyl acetate contents of 4–12 wt% provide higher low-temperature sealing performance and toughness but lower stiffness and higher surface tack; 7109BK does not contain vinyl acetate and is selected where lower seal initiation temperature is less critical than film stiffness and non-tack surface character.

    When film gauge is reduced from 50 µm to 25 µm, defect sensitivity increases. Gauge bands narrower than ±5% are required to maintain dart impact above typical packaging specifications. This is assessed with a capacitance gauge scanner on the collapsing frame. Dart impact is measured by ASTM D1709, but data from a 25 µm film blown with a die gap of 1.5 mm and blow-up ratio of 2.5:1 cannot be directly transferred to a 50 µm film because orientation and cooling history differ. For heavy-duty sack applications, specifications often require an Elmendorf tear in the transverse direction above 400 g/25 µm when measured by ASTM D1922; machine-direction tear values lower than this do not necessarily indicate material deficiency because orientation effects dominate. Draw-down ratios above 40:1 can induce machine-direction orientation that raises machine-direction tear values but suppresses transverse-direction tear values. Under ASTM D882, films in this density and melt index envelope commonly show tensile strength at break of 35–45 MPa in the machine direction and 30–40 MPa in the transverse direction, with elongation at break of 600–800% depending on cooling and orientation.

    If Regrind, Colour Concentrate, or Slip Packages Are Introduced

    If regrind, colour concentrate, or slip packages are introduced, the resulting film properties must be revalidated under production conditions. Regrind ratios up to 15–20 wt% are common on polyethylene blown film lines; above this range, gel content, melt index drift, and dart impact loss can become measurable. The base resin is compatible with hydrocarbon-based slip agents and silica antiblock at conventional loadings of 500–1500 ppm slip and 1000–3000 ppm antiblock, but excess antiblock above 5000 ppm can reduce dart impact and increase haze. When a black-pigmented masterbatch is used, carbon black dispersion should be examined by ASTM D5596 or ISO 11420; agglomerates above 10 µm in thin film can form pinholes under stress. The use of amine-based antifog additives should be evaluated for interaction with the resin’s stabiliser package, because certain amine packages can accelerate oxidative degradation at melt temperatures above 220°C.

    For compliance, the polyethylene base resin is generally considered a polyolefin under FDA 21 CFR 177.1520 and may be suitable for food-contact applications when final films meet extractive limitations and conditions of use; converters must confirm compliance for the specific additive package and film structure. Under European food-contact regulation EU No 10/2011, overall migration and specific migration of additives must be measured on the final article. The resin should be pre-dried only when regrind or storage conditions have introduced surface moisture above 0.2%; drying at 70°C for 2 h is sufficient to prevent bubble destabilisation and surface grain. The product should not be used in direct contact with strong oxidising acids at temperatures above 40°C, and it is not recommended for solvent-bearing hot-fill applications unless the final film is specifically tested for permeation and seal integrity.

    Top