| HS Code | 835019 |
| Product Name | Chevron Phillips 7108T LLDPE Sheeting Resin |
| Manufacturer | Chevron Phillips Chemical Company |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.918 g/cm³ |
| Melt Index | 0.8 g/10 min at 190°C/2.16 kg |
| Tensile Strength At Yield | 11 MPa |
| Tensile Strength At Break | 27.6 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 276 MPa |
| Vicat Softening Point | 94°C |
| Brittleness Temperature | < -70°C |
| Hardness Shore D | 50 |
As an accredited Chevron Phillips 7108T LLDPE Sheeting Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chevron Phillips 7108T LLDPE Sheeting Resin is packaged in 55-pound multiwall bags, palletized for bulk shipment. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Chevron Phillips 7108T LLDPE Sheeting Resin in palletized bags, securely stowed for safe ocean transport. |
| Shipping | Chevron Phillips 7108T LLDPE Sheeting Resin is shipped as non-hazardous solid pellets in 25-kg bags or bulk containers, palletized and stretch-wrapped. Transport in covered trucks or containers. Store cool, dry, away from direct sunlight, heat, and moisture. Handle with standard industrial equipment; no special DOT placarding required. |
| Storage | Store Chevron Phillips 7108T LLDPE Sheeting Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers sealed to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and excessive stacking. Maintain good housekeeping; use appropriate PPE and follow the manufacturer’s SDS for safe handling and storage. |
| Shelf Life | Store in a cool, dry, well-ventilated area away from direct sunlight; shelf life is approximately two years in unopened original packaging. |
In landfill basal and cap liner service, Chevron Phillips 7108T LLDPE Sheeting Resin is converted into smooth and textured geomembrane panels where the governing property is resistance to notched constant tensile load rather than short-term tensile yield. The resin, supplied as a linear low-density butene copolymer with a manufacturer-listed density of 0.918 g/cm³ per ASTM D1505 and a nominal melt index of 1.0 g/10 min at 190 °C/2.16 kg per ASTM D1238, is typically formulated with 2.0–3.0 wt% carbon black masterbatch in the finished article to satisfy carbon black dispersion and content provisions of GRI-GM17, and with an antioxidant/thermal stabilizer package at 0.3–0.8 wt% where multi-pass extrusion is required. The downstream production route for landfill liner panels is flat-die cast sheet extrusion followed by calendering: melt temperature is held between 200 °C and 240 °C, die lip opening is set 10%–15% above target final thickness to manage neck-in, and chill roll temperatures are maintained below 60 °C to suppress surface tack. Because butene-copolymer LLDPE exhibits a broader molecular weight distribution than metallocene grades, it tolerates this high-shear extrusion but requires a reduced draw ratio relative to conventional HDPE to prevent edge tear at the calender nip. Terminal finished product types include single-sided textured, double-sided textured, and smooth geomembrane rolls in thicknesses from 1.0 mm to 2.5 mm, used as basal liner, leachate capping, and stormwater pond components under 40 CFR 258.40 landfill design performance standards. A documented operational boundary is that the weldability window narrows when the sheet contains more than 3.0 wt% carbon black because the lower melt flow at the weld root reduces fusion penetration into the beveled edges; published data for this specific formulation boundary is limited, and production trials on wedge-welding equipment with hot-air preheat are required before fixing the masterbatch level.
Gold cyanidation cells and copper heap leach pads impose a demanding combination of acidic sulfate exposure and coarse drainage gravel puncture; here, a liner membrane composed largely of 7108T must retain flexibility while exposed to sulfuric acid at pH < 2 or sodium cyanide at pH 10–11, and the primary failure mode is stress cracking initiated at the apex of a drainage gravel point. Compliance begins with GRI-GM17 LLDPE geomembrane specification, supplemented by puncture index testing under ASTM D4833 and notched constant tensile load testing under ASTM D5397 to establish environmental stress crack resistance. Formulators generally treat 7108T as the major phase at 80–100 wt%, with 2.0–3.0 wt% carbon black masterbatch for UV stabilization and, where higher stiffness is required in double-textured drainage sheets, 10–20 wt% HDPE blended in the melt phase; the exact HDPE concentration is set by a trade-off between ESCR and puncture resistance, because the higher crystalline HDPE fraction raises tear initiation sensitivity under low-temperature bending. The manufacturing route for heap leach panels is calendar-stacked cast extrusion followed by either spray-on or embossed texturing, with final sheet thickness of 1.5 mm or 2.0 mm and roll width from 7 m to 8 m. Finished product types include single-sided textured geomembrane where drainage must be preserved on one face, and double-sided textured geomembrane where slope stability requires friction against both crushed rock and clay subgrade. Field seaming uses hot wedge welding, and air-channel overpressure testing is applied to each completed seam. An operational limitation is that 7108T should not be used alone as a heap leach liner resin when the design life requires sustained exposure to strong oxidative solutions above 50 °C; published data for this specific resin under cyanide leach conditions is limited, and long-term immersion testing per ASTM D5747 is required before specifying 7108T as the sole resin in that configuration.
| Service environment | Primary specification | Supporting test standards | Typical numerical verification condition |
|---|---|---|---|
| Landfill basal/cap | GRI-GM17 | ASTM D1505, ASTM D1238, ASTM D1004, ASTM D5397 | Sheet thickness 1.0–2.5 mm |
| Mining heap leach | GRI-GM17 | ASTM D4833, ASTM D5397, ASTM D5747 | Sheet thickness 1.5–2.0 mm |
| Secondary containment | 40 CFR 264.193 | ASTM D5747, ASTM D638 | Sheet thickness 1.0–2.0 mm |
| Agricultural irrigation | GRI-GM17 | ASTM D5199, ASTM D1505 | Sheet thickness 0.5–1.5 mm |
| Aquaculture/pond | GRI-GM17 | ASTM D1004, FDA 21 CFR 177.1520 | Sheet thickness 0.75–1.5 mm |
Secondary containment around above-ground storage tanks and drum storage areas uses extruded LLDPE sheeting as a chemically resistant and weldable membrane; the governing regulatory language is 40 CFR 264.193, which requires imperviousness and compatibility with the stored chemicals. For 7108T, compatibility is not assumed but is screened by immersion testing under ASTM D5747 with retained tensile properties under ASTM D638 after 7-day and 30-day exposure to representative hydrocarbons, weak acids, and alkalis. Because butene-copolymer LLDPE can swell when exposed to aromatic hydrocarbons, tanks storing benzene, toluene, or xylene-containing mixtures typically require the liner to be evaluated at 40 °C rather than 23 °C; swelling beyond 15% mass gain generally disqualifies the material for that chemical service unless a sacrificial layer is added. Formulations for secondary containment generally use 7108T at 90–100 wt%, with 2.0–3.0 wt% carbon black or alternate UV stabilizer masterbatch, and where higher flexural modulus is required for large flat floor panels, a 10–20 wt% HDPE fraction is added to reduce panel sag at installation temperatures above 35 °C. Production is by flat-die extrusion into rolls of 1.0 mm to 2.0 mm thickness, followed by factory fabrication into large pre-welded panels and installation by fusion wedge welding; welded seams are non-destructively tested by air-channel overpressure and vacuum box techniques. Terminal finished product types include prefabricated tank liner panels, floor sheets, sump liners, pipe penetration boots, and pH-adjusted containment pond liners for fire suppression water. An explicit operational boundary is that amine-based or nitrile-based sealants should not be used in contact with the LLDPE liner without compatibility testing because certain polar additives can migrate into the polyolefin and reduce crystallization at the weld interface.
Adjacent to irrigation district canals and agricultural water storage ponds, 7108T is selected for thin, flexible lining rather than for maximum stiffness. In this application, 7108T is typically blended at 95–97 wt% with 2.0–3.0 wt% carbon black masterbatch and processed by blown-film or cast-film extrusion into narrow-to-wide sheeting, although flat-die extrusion is preferred above 1.0 mm to control gauge variation. The governing specification is GRI-GM17 for LLDPE geomembranes, with thickness tolerances checked by ASTM D5199 and density by ASTM D1505; field seams are qualified by shear and peel testing before line production. Terminal finished product types include canal liner rolls, ditch lining panels, cistern membranes, and modular water storage pond liners. The main processing conflict is the lower zero-shear viscosity of butene LLDPE compared with HDPE; this limits machine direction draw tension and requires chilled nip roll temperatures below 50 °C to avoid blocking in-roll. Published data for 7108T in irrigation canal service is more limited than for HDPE canal liners, but the resin’s flexibility allows design of anchor trenches without excessive thermal expansion stress at 20 °C to 35 °C service temperatures.
The continuity of an installed flexible pond liner made from 7108T is set by notch-free seam root penetration and by the width of the heat-affected zone during hot wedge welding. Pond and aquaculture liners are often thinner than landfill sheets, typically 0.75 mm to 1.5 mm, which makes welding speed and wedge temperature the critical process parameters rather than the forming method. The resin enters the converter as a compound containing 2.0–3.0 wt% carbon black and a stabilizer package; because carbon black increases infrared absorption, welded seam temperatures measured by a thermocouple at the wedge trailing edge should not exceed 230 °C to avoid accelerated thermal oxidation at the root. Standards referenced for this scenario are GRI-GM17 for base material and ASTM D1004 for tear resistance of the finished sheet, while aquaculture liner installers may also apply FDA 21 CFR 177.1520 to ensure the polymer does not introduce contaminants into water used for subsequent food production. The downstream process is either cast extrusion or blown film extrusion followed by panel seaming in the field; the preferred seam method is dual-track hot wedge for sheet above 1.0 mm, while sheets below 0.75 mm are often joined by adhesive tape or hot-air overlap welds, which produce lower peel strength. Finished product types include single-sheet pond liners, aquaculture tank liners, ornamental lake liners, and anaerobic lagoon covers. The operational boundary for processing is the requirement to re-dry regrind at 80 °C for 2 h when reusing edge trim above 10 wt% to prevent steam-induced pinholes during extrusion; this is particularly critical in humid plant conditions above 60% relative humidity.
Because temporary construction sheeting and jobsite containment membranes require rapid deployment over irregular ground and resistance to puncturing from construction debris, 7108T is extruded into relatively thin reinforced or unreinforced sheet at 0.15 mm to 0.50 mm. The compliance framework here differs from geomembrane containment: low-permeability sheeting is tested for water vapor transmission under ASTM E96 and for thickness uniformity under ASTM E154, while flammability may be screened by ASTM D635 if the sheet is used inside occupied structures. In this sector, formulation is kept simple; 2.0–3.0 wt% black or colored masterbatch is used for UV resistance and opacity, with no mineral filler because high filler loadings would reduce dart drop impact and create pinholes at thin gauge. The downstream production process is cast film/sheet extrusion at high line speed with downstream slitting and center-folding, followed by hemming or tape seaming at the jobsite. Terminal finished product types include concrete curing blankets, dust containment curtains, temporary weatherproofing sheeting, and disposable spoil pile covers. The main equipment constraint is that a low-friction surface is required if the material contacts slip-sheeted formwork; therefore, converters add an antiblock masterbatch at 0.5–1.0 wt% to reduce blocking during hot stacking in warehouse storage. Published data for 7108T in this specific thin-gauge construction configuration is limited, so the conversion parameters are usually established by pilot cast-film trials before commercial runs.
Competitive Chevron Phillips 7108T LLDPE Sheeting Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips 7108T LLDPE sheeting resin is a pelletized butene-comonomer linear low density polyethylene supplied for monolayer and coextruded sheet, thin-gauge thermoforming, industrial dunnage, and low-temperature packaging. Supplier technical literature identifies a nominal density of 0.918 g/cm³ when determined by ASTM D4883 or ISO 1183-1:2019 and a nominal melt index of 1.0 g/10 min at 190 °C under 2.16 kg per ASTM D1238 or ISO 1133-1:2022. The butene-derived short-chain branch distribution differentiates the resin from autoclave LDPE sheet grades and from hexene- or octene-copolymer LLDPE grades by shifting the balance among environmental stress crack resistance, low-temperature dart impact, and flexural modulus. Because long-chain branching is absent in the linear backbone, melt elasticity and die swell are lower than those of LDPE at equivalent melt index; therefore die gap, melt temperature, and draw ratio must be controlled to prevent edge weave and sag in downstream forming. The product is classified as a sheeting resin rather than a blown film or rotomolding resin; substitution into other processes should be validated by shear history, melt residence time, and orientation differences.
At the mechanical-property level, the principal differences are tensile yield strength, flexural modulus, and low-temperature toughness. Manufacturer-published typical values for 7108T place tensile yield strength at approximately 11 MPa per ASTM D638, elongation at break above 800% per ASTM D638, flexural modulus at approximately 276 MPa per ASTM D790, and environmental stress crack resistance above 1,000 h per ASTM D1693 condition B in 100% Igepal CO-630. These values are typical lot performance, not specification minima. General-purpose LDPE sheet of similar density and melt index typically shows lower tensile yield strength and flexural modulus but higher melt strength because long-chain branching contributes to extensional strain hardening. HDPE sheet has higher flexural modulus and heat distortion temperature, yet lower ESCR and lower impact at freezer temperatures. The short-chain branch distribution in 7108T therefore positions it between LDPE and HDPE for higher modulus and moderate draw capability, with the caveat that low-temperature drop impact must be confirmed by ASTM D5276 or customer-specific distribution testing.
| Parameter | Test method | 7108T | LDPE sheet | HDPE sheet |
|---|---|---|---|---|
| Density | ASTM D4883 / ISO 1183-1 | 0.918 g/cm³ | 0.920–0.925 g/cm³ | 0.945–0.965 g/cm³ |
| Melt index | ASTM D1238, 190 °C, 2.16 kg | 1.0 g/10 min | 0.5–2.0 g/10 min | 0.2–1.0 g/10 min |
| Tensile yield strength | ASTM D638 | ≈11 MPa | 8–10 MPa | 20–30 MPa |
| Flexural modulus | ASTM D790 | ≈276 MPa | 200–250 MPa | 900–1,500 MPa |
| ESCR | ASTM D1693 condition B | >1,000 h | variable | >600 h |
| Long-chain branching | rheology | absent | present | absent |
Melt temperature, die gap, and back pressure are the primary variables controlled on production-scale sheet lines. A 90 mm single-screw extruder with 24:1 to 30:1 L/D, barrier feed section, and 20/40/60 mesh screen pack uses a flat melt temperature profile of 210 °C to 235 °C for sheet thicknesses from 0.25 mm to 3.0 mm. Die gap is typically set between 0.5 mm and 1.5 mm, with higher gaps used for low-draw sheet to reduce machine-direction orientation. Back pressure upstream of the screen pack is commonly monitored in the 10–20 MPa range at screw speeds of 80–120 rpm; a gradual increase after screen changes indicates gel or additive accumulation, while a sudden increase suggests unmelts or unmelted regrind. Extrusion should not exceed a melt temperature of 260 °C. Sustained operation above 260 °C can cause oxidative chain scission, localized crosslinking, discoloration, and gel deposition, especially when high regrind levels are used. For thin sheet below 0.5 mm, edge tear and draw resonance may appear if die gap is reduced below 0.4 mm or draw-down ratio exceeds 20:1. Grade-specific published extrusion data for 7108T beyond these ranges is limited; line qualification trials should record melt pressure, melt temperature, and gel count per ASTM D3350 or internal standards.
For food-contact sheet, compliance is governed by FDA 21 CFR 177.1520 for olefin polymers. The supplier’s food-contact statement will specify the applicable paragraph, food-contact conditions, and limitations; the converter must verify that the final article made from 7108T complies with the conditions of use, including temperature, food simulant, and fatty-food restrictions. For European Union applications, EU 10/2011 applies, with overall migration limited to 10 mg/dm² and specific migration limits for additives as listed. The resin’s regulatory documentation is separate from mechanical testing; density and melt index do not establish food-contact compliance by themselves. REACH SVHC screening and RoHS Directive 2011/65/EU declarations are provided in the supplier’s lot documentation but apply primarily to the resin as supplied, not to downstream additives or colorants. ASTM D4976-12a is the general specification for polyethylene plastics and should be used to define the material call-out in the converter’s purchase specification.
Before production startup, incoming resin lot testing should record density per ASTM D4883, melt index per ASTM D1238, and pellet geometry. Because molecular weight distribution affects processability beyond the single melt-index value, the melt flow ratio I21/I2 may be measured per ASTM D1238; typical polyolefin sheet extrusion grades show I21/I2 values of 25–35, but lot-specific values should be used. Melt flow ratio drift above the supplier’s control range indicates contamination or degradation and should trigger quarantine. This is an incoming quality control requirement, not a performance claim.
Die lip deposits on LLDPE sheet lines are usually mixtures of low-molecular-weight polyethylene fractions and inorganic antiblock particles. Silica-based antiblock at typical concentrations of 1,000–3,000 ppm can increase surface roughness and reduce blocking but may deposit at the die exit if die temperature is nonuniform. Fluoropolymer or polysiloxane processing aids at 200–800 ppm are added to suppress melt fracture and reduce die lip buildup. These additives alter surface energy and may affect seal, printing, and lamination performance; their effect is measured by contact angle or dyne testing rather than tensile properties. During coextrusion of 7108T with LDPE or HDPE caps, transition purging with high-viscosity purging compounds is recommended to prevent time-dependent back pressure spikes and haze bands. Published data for blends of 7108T with biobased additives or pro-oxidant masterbatches is limited; such blends should be avoided in high-regrind sheet because oxidative chain scission can reduce melt viscosity and mechanical properties. Post-industrial regrind levels up to 30% are commonly used for non-food sheet, but the percentage must be controlled by monitoring melt index, gel count, and sheet color.
On polished roll stacks, post-extrusion cooling determines sheet crystallinity and thickness tolerance. Chill roll temperatures of 60–90 °C are typical for LLDPE sheet; higher roll temperatures may increase clarity but can cause blocking, while lower temperatures can induce orientation and increase shrinkage. Sheet thickness uniformity should be maintained within ±3% of nominal because thermoforming thinning behavior amplifies variation at draw ratios above 2:1. On-line thickness scanners and closed-loop die bolts are standard; die bolt adjustments should be limited to ±0.05 mm increments to avoid localized haze bands.
In vacuum and pressure forming trials, sheet behavior of 7108T is dominated by lower melt strength relative to LDPE. Typical sheet surface temperatures are 140–165 °C, with plug temperatures of 110–130 °C for syntactic foam or nylon plug assists. Draw ratios up to 3:1 are achievable in shallow to moderate shapes; deep-draw parts require plug-assisted pre-stretching and optimized plug speed to prevent thin corners and webbing. The higher flexural modulus of 7108T permits demolding at slightly higher part temperature than LDPE, but nonuniform mold cooling can produce post-mold shrinkage, measurable by ASTM D2732. When sheet surface temperature is too high, sag and fold formation appear; reductions of 5–10 °C and increased plug speed are typical first corrections. Because the grade is orientation-sensitive, extruded sheet should be tested for tensile properties in both machine and transverse directions per ASTM D638, and thermoformed parts should be evaluated for drop impact under ASTM D5276 or ISTA distribution protocols rather than compression-molded plaque data alone.
For sheet converters, density and melt index are the initial classification values, but comonomer length and molecular weight distribution often control end-use toughness. At equal 0.918 g/cm³ density and 1.0 g/10 min melt index, a butene LLDPE such as 7108T may exhibit lower Elmendorf tear strength per ASTM D1922 and lower dart drop impact per ASTM D1709 than hexene- or octene-copolymer LLDPE. The reason is that longer comonomers can generate more tie chains and more effective entanglement at equivalent density. However, the difference in ESCR per ASTM D1693 may be less pronounced than the difference in tear and dart. Therefore 7108T should be benchmarked against hexene LLDPE sheet grades when tear propagation and puncture are controlling; where flexural modulus, ESCR, and wall-thickness consistency are controlling, the butene grade may be sufficient. Selection testing must use the same specimen preparation method, because compression-molded plaques per ASTM D4703 do not reproduce the molecular orientation of extruded sheet. Standard comparisons should include notched Izod impact per ASTM D256 for rigid parts and dart drop per ASTM D1709 for flexible sheet.
| Standard or regulation | Purpose | Typical use |
|---|---|---|
| ASTM D1238 / ISO 1133-1 | Melt flow rate | Incoming inspection and lot drift |
| ASTM D4883 / ISO 1183-1 | Density gradient column | Classification and density verification |
| ASTM D638 | Tensile yield strength and elongation | Sheet and formed part testing |
| ASTM D790 | Flexural modulus | Stiffness comparison |
| ASTM D1693 | Environmental stress crack resistance | Packaging chemical exposure |
| ASTM D1709 | Dart drop impact | Freezer drop performance |
| ASTM D1922 | Elmendorf tear | Film and thin sheet tear resistance |
| ASTM D2732 | Plastic sheet shrinkage | Thermoforming quality control |
| ASTM D3350 | Polyethylene classification system | Material call-out and traceability |
| FDA 21 CFR 177.1520 | US food-contact olefin polymers | Food package compliance |
| EU 10/2011 | European plastics food contact | Overall and specific migration |
| RoHS 2011/65/EU | Heavy metal restrictions | Regulatory documentation |
Under standard indoor storage at 23 °C and 50% relative humidity, drying is generally not required before sheet extrusion. If cold storage or high-humidity exposure produces surface condensation, drying at 80–85 °C for 3–4 h in a desiccant hot-air dryer is a standard corrective measure. The resin should not be blended with unapproved pro-oxidant additives, unsaturated esters, or high-peroxide recycle streams because melt index drift and gel formation may occur. In multilayer structures, direct contact with unprimed metal surfaces under high-alkalinity conditions should be avoided. The product is positioned for sheet extrusion and thermoforming; substitution into blown film, rotomolding, or injection molding requires revalidation of melt residence time, orientation, and additive consumption. Converters should establish incoming inspection of density per ASTM D4883, melt index per ASTM D1238, and visual pellet contamination, and should record these values against the supplier certificate of analysis before startup.