Chevron Phillips 7105glt Lldpe Blown Film Resin Hexene Copolymer

Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer

    • Product Name: Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 891860
    Comonomer Hexene
    Polymer Type LLDPE
    Density 0.918 g/cm³
    Melt Index 0.5 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Break Md 5500 psi
    Tensile Strength At Break Td 5000 psi
    Elongation At Break Md 600 %
    Elongation At Break Td 700 %
    1 Secant Modulus Md 25000 psi
    1 Secant Modulus Td 27000 psi
    Dart Impact 200 g
    Elmendorf Tear Md 250 g
    Elmendorf Tear Td 400 g
    Haze 10 %
    Gloss 70 %
    Coefficient Of Friction 0.2

    As an accredited Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer is packaged in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg net).
    Container Loading (20′ FCL) 20′ FCL container loaded with Chevron Phillips 7105GLT LLDPE blown film resin, hexene copolymer, in 25 kg bags on pallets.
    Shipping Chevron Phillips 7105GLT LLDPE Blown Film Resin is a non-hazardous solid polyethylene pellet. Ship in sealed 25-kg bags, bulk bags, or bulk trucks/railcars. Protect from moisture, heat, direct sunlight, and punctures. Store in a cool, dry, well-ventilated area. Standard freight; no special DOT/IMDG/IATA hazard classification required.
    Storage Store Chevron Phillips 7105GLT LLDPE Blown Film Resin in original, sealed packaging in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources and strong oxidizers. Palletize off the floor, avoid prolonged outdoor storage, and follow first-in, first-out inventory practices. Keep containers closed when not in use, and maintain clean, dry handling conditions.
    Shelf Life Stable under normal storage conditions; store cool, dry, away from sunlight. No specific expiration when kept in original packaging.
    Application of Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer

    Chevron Phillips 7105GLT is a hexene-copolymer linear low-density polyethylene designed for blown film extrusion, with nominal melt index 0.50 g/10 min at 190°C/2.16 kg under ISO 1133-1 and nominal density 0.918 g/cm³ under ISO 1183-1. The following application routes address six downstream converting segments, each stated with compliance framework, formulation loading window, production equipment constraints, and converted article classes.

    Heavy-Duty Shipping Sack Lines and the Hexene Comonomer Toughness Threshold

    In heavy-duty shipping sack conversion, 7105GLT is blended as the primary hexene-LLDPE toughness component in monolayer and coextruded webs where filling operations generate puncture from polymer granules, mineral fillers, or crystalline fertilizer prills. The hexene comonomer creates longer short-chain branches than butene-copolymer LLDPE at equivalent density, increasing tie-molecule formation and raising dart impact energy absorption measured according to ASTM D1709-16A / ISO 7765-1 and Elmendorf tear resistance measured according to ASTM D1922-15 / ISO 6383-2. Sacks intended for exported chemical goods are additionally drop-tested under ASTM D5276-19 or ISTA 1A loaded-container protocols. A starting formulation loading is 70–85 wt% 7105GLT, 10–25 wt% fractional-melt LDPE with nominal melt index 0.25 g/10 min, and 2–4 wt% carbon black/UV masterbatch for outdoor storage; closed-warehouse polymer pellet sacks reduce the pigment masterbatch to 0.5–1.5 wt% clarity-neutral antiblock.

    On a production-scale blown film line using a 90 mm grooved-feed extruder with 30:1 L/D barrier screw and Maddock mixing tip, a 250 mm die with 1.8–2.5 mm die gap is operated at 2.0:1–2.8:1 blow-up ratio. Melt temperature at the adapter is maintained between 200°C and 230°C; screen-pack pressure typically remains below 40 MPa, and excursions above that threshold are treated as screen blinding caused by pigment agglomeration rather than resin viscosity drift. Bubble stability is preserved by holding the frost line low enough to suppress machine-direction splitiness; lines without internal bubble cooling require a 15–25% reduction in haul-off speed when processing at the upper end of the 7105GLT loading window. Converted articles include gusseted heavy-duty shipping sacks in 80–200 µm, FIBC outer liners, valve sacks for polymer granules, cementitious dry-mix bags, and mineral filler packaging.

    Why Is Tear Propagation Resistance Critical in Silage Barrier Film?

    Agricultural silage films manufactured from hexene LLDPE grades are selected when repeated handling on stony ground and conventional bale wrapping machinery produces flex-crack and puncture. 7105GLT contributes low-temperature flexibility and tear resistance, but the film must retain sufficient oxygen barrier to support ensiling fermentation; the balance is controlled by film gauge and comonomer architecture rather than densification of the polymer. Silage cover and bag film is qualified under EN 13207:2018 for thermoplastic silage films and tubes, with tensile properties measured using ISO 527-3 and tear properties using ISO 6383-2. A production formulation for a 120–180 µm monolayer silage sheet is 80–90 wt% 7105GLT, 5–15 wt% LDPE at 0.25 g/10 min, 1–2 wt% HALS UV masterbatch, and 0.5–1.0 wt% carbon black masterbatch for storage beyond 12 months. In white/black coextruded silage film, the outer white layer carries 5–7 wt% titanium dioxide masterbatch.

    Downstream conversion runs on a 70 mm extruder with a 250 mm die, 1.6–2.2 mm die gap, and 2.0:1–2.5:1 blow-up ratio. With a dual-lip air ring and internal bubble cooling, output is constrained primarily by bubble stability at the selected frost-line position; without internal bubble cooling, output is limited by bubble chatter when frost-line height exceeds 4 die diameters. Terminal products include bunker silo cover sheet, silage bag tube, round-bale cover film, and temporary grain storage coverage.

    Frozen food converting operations that run 7105GLT in monolayer or coextruded web are primarily concerned with dart impact brittleness at -20°C and seal integrity through frost-laden product. The hexene comonomer architecture preserves cold-temperature impact because secondary crystallization during frozen storage is less severe than in higher-density or butene-copolymer LLDPE of comparable melt index. Food-contact compliance is anchored to FDA 21 CFR 177.1520 and EC No 10/2011, with overall migration verified under the time and temperature conditions assigned to frozen, non-acidic food simulants and against the 10 mg/dm² limit. A starting formulation for IQF bag-in-box liners is 90 wt% 7105GLT with 10 wt% LDPE, 0.5–1.0 wt% antiblock masterbatch, and 0.5–1.0 wt% slip masterbatch; printed frozen food pouches use 60–80 wt% 7105GLT and 15–30 wt% LDPE to improve seal initiation while retaining cold-impact resistance.

    Blown film lines for this segment typically use a 50–80 mm extruder, 1.2–2.0 mm die gap, and 2.0:1–2.5:1 blow-up ratio with automated gauge control holding thickness variation to ±4%. A low frost-line position prevents haze bands; corona treatment is maintained at 38–40 mN/m for ink adhesion on printed webs. Terminal film structures include frozen vegetable bags, bag-in-box liners for IQF seafood, frozen meat pouches, and peelable lidding base web where the sealant layer is coextruded.

    When Blown Film Replaces Cast Structures in Pallet Unitization

    Pallet load containment requirements expose a processing conflict: blown stretch film must balance machine-direction elongation with transverse-direction tear resistance, while cast stretch film derives cling from low melt-temperature processing. 7105GLT in blown pallet unitization film delivers elevated dart impact and puncture resistance, but the converter must operate at a higher blow-up ratio than conventional packaging film to prevent anisotropy. Cling and mechanical properties are measured under ASTM D5458-95 for peel cling, ASTM D882-18 / ISO 527-3 for tensile elongation, and ASTM D5748-19 for protrusion puncture resistance. A formulation window for blown stretch is 80–95 wt% 7105GLT with 5–15 wt% metallocene LLDPE or LDPE as cling/viscosity modifier and 1–2 wt% tackifier masterbatch where base resin cling is insufficient. Published data for the exact cling retention of 7105GLT in high-speed pre-stretch equipment is limited; converter trials should screen tackifier additions in 5 wt% steps before locking the formula.

    Downstream film is produced on a 70 mm barrier-screw blown film line with 1.5–2.2 mm die gap and 2.8:1–3.2:1 blow-up ratio, with melt temperature held at 190–210°C to limit oxidative viscosity drift. On webs wider than 1,000 mm, film thickness variation above ±6% produces camber at the pre-stretch rollers; production lines therefore use a segmented air ring or automatic die lip control to maintain gauge uniformity. Converted articles include hand stretch film, machine stretch wrap for logistics centers, and stretch hood film for pallet stabilization.

    Adhesive Lamination Web Stock and Heat-Seal Integrity

    Adhesive lamination web stock based on 7105GLT functions as the sealant or print-side substrate in flexible packaging laminates bonded to BOPP, PET, or aluminium foil with solventless adhesive. The primary technical requirements are heat-seal initiation temperature, hot-tack window, and coefficient of friction after lamination. Seal strength is tested under ASTM F88/F88M-21, hot tack under ASTM F1921-20, and coefficient of friction under ASTM D1894-14; food-contact status is established under FDA 21 CFR 177.1520 and EC No 10/2011. A sealant web formulation uses 60–75 wt% 7105GLT with 25–35 wt% LDPE at 0.25 g/10 min to reduce seal initiation temperature by 5–10°C relative to a 100% 7105GLT control, with 0.5–1.5 wt% antiblock concentrate and 0.5–1.0 wt% slip concentrate.

    Production of the blown web runs at 25–50 µm thickness on a 50–80 mm extruder with 1.2–1.6 mm die gap and 2.2:1–2.7:1 blow-up ratio. In-line corona treating is maintained at 38–42 mN/m before winding; lamination is subsequently performed at 150–250 m/min using solventless adhesive, with bond strength measured by ASTM D1876-08 T-peel. Terminal laminates include stand-up pouch sealant web, bakery film laminate, detergent pouch inner web, and coffee bag liner film.

    Form-fill-seal industrial liner lines using 7105GLT monolayers are configured for high hot-tack strength and low gel count because seal failures at production speeds above 40 bags/min generate immediate line stoppage. The hexene-copolymer molecular architecture provides a wider hot-tack window than butene LLDPE of equivalent melt index, which allows seal jaws to operate at lower temperature set points without generating stringing. Hot-tack force is measured under ASTM F1921-20, seal strength under ASTM F88/F88M-21, and chemical-regulatory status for EU shipments is assessed under REACH (EC) No 1907/2006; food-contact liners are evaluated under FDA 21 CFR 177.1520. A typical high-speed FFS liner formulation is 85–95 wt% 7105GLT with 5–15 wt% LDPE and 0.5–1.0 wt% polymer processing aid, while thick 100–150 µm chemical drum liners can be run at 100% 7105GLT.

    On a 60 mm 24:1 L/D extruder with a 150 mm die, 1.8 mm die gap, and 2.0:1 blow-up ratio, melt temperature is held at 195–215°C. Die lip purge is scheduled after 72 hours of continuous operation because LLDPE melt fracture and die lip deposit increase surface roughness that reduces seal transfer efficiency. Seal jaw set points are 115–130°C with 0.5–1.0 s dwell; hot-tack is measured at 0.2 s after seal release. Terminal articles include chemical drum liners, FIBC inner liners, bulk box liners, and heavy-duty refuse sacks.

    Free Quote

    Competitive Chevron Phillips 7105GLT LLDPE Blown Film Resin, Hexene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Designated as a hexene-copolymer linear low-density polyethylene, Chevron Phillips Marlex® 7105GLT is engineered for blown film conversion where toughness and downgauging potential dominate material selection. The grade belongs to the LLDPE blown film resin class produced via gas-phase or solution polymerization, with 1-hexene as the alpha-olefin comonomer. Melt flow rate, determined under ASTM D1238-20 at 190 °C with a 2.16 kg load, and density, determined under ASTM D1505-18, constitute the primary specification axes. The resin is processed on conventional blown film lines with die gaps of 1.0 mm to 2.5 mm and is formulated for monolayer and coextruded structures in heavy-duty shipping sacks, industrial liners, agricultural film, and food-contact packaging. Published 7105GLT-specific nominal values are contained in the current Chevron Phillips Chemical product datasheet; representative hexene LLDPE film grades occupy a melt index band of 0.5 g/10 min to 1.2 g/10 min and a density band of 0.917 g/cm³ to 0.922 g/cm³.

    Hexene Comonomer Functionality and Short-Chain Branch Distribution

    The choice of 1-hexene as comonomer introduces butyl branches of 4 carbon atoms along the polyethylene backbone, whereas butene-based LLDPE relies on ethyl branches of 2 carbon atoms. The longer alpha-olefin side chain reduces crystalline lamella thickness more efficiently per unit comonomer mass, enabling density reduction while retaining tie-molecule connectivity between adjacent crystallites. This molecular architecture translates into measurable film property shifts: Elmendorf tear resistance under ASTM D1922-15 and dart impact resistance under ASTM D1709-16A typically exceed butene-copolymer values at equivalent density and melt index when tested on 25 µm monolayer film. Differential scanning calorimetry per ASTM D3418-21 records a primary melting endotherm between 122 °C and 126 °C for commercial hexene LLDPE blown film grades, with crystallinity in the 40% to 50% range. The short-chain branching distribution also governs the onset of melt fracture; hexene grades processed at high shear rates may require die gaps above 1.0 mm on lines generating shear rates above 500 s⁻¹. The presence of butyl branches shifts the critical shear rate for sharkskin onset relative to butene grades, a difference observable on laboratory capillary rheometers but often submerged by processing-aid technology on production lines.

    Extrusion of 7105GLT on monolayer blown film lines requires coordination of screw geometry, barrel profile, and bubble cooling. Smooth-bore or grooved-feed extruders with length-to-diameter ratios of 24:1 to 30:1 are specified for LLDPE conversion, with barrier flights or Maddock mixers contributing to melt homogeneity without excessive shear heating. Barrel temperature profiles are typically ramped from 150 °C in the feed zone to 210 °C to 230 °C at the adapter and die, while melt temperature measured at the die exit is maintained between 200 °C and 230 °C by immersion thermocouple. Die gap settings of 1.0 mm to 2.0 mm and blow-up ratios of 2.0:1 to 3.0:1 control bubble geometry; frost line height maintained at 2 to 6 die diameters establishes the balance between machine-direction and transverse-direction orientation. On lines equipped with internal bubble cooling and dual-lip air rings, output rates exceed single-lip configurations by 20% to 30% while maintaining gauge uniformity within ±5% at 50 µm using non-contacting beta gauges. Pressure in the extruder head assembly, monitored with melt-pressure transducers, normally remains below 35 MPa under clean screen-pack conditions; sustained readings above this threshold on 75 mm extruders indicate filter blinding or screw wear.

    What limits the downgauging window when 7105GLT replaces butene-copolymer LLDPE?

    Downgauging trials conducted on production-scale lines replace butene LLDPE with hexene LLDPE at layer ratios from 20% to 80% in coextruded structures. The primary limiting parameter is retained dart impact at target gauge, tested under ASTM D1709-16A on films between 25 µm and 65 µm. In published comparative trials, hexene-copolymer grades demonstrate dart impact retention advantages over butene grades at equal gauge when measured under ASTM D1709-16A, with gauge reduction potential reported in converter trials typically bounded by 10% to 15% before acceptance thresholds are breached. Machine-direction tear strength under ASTM D1922-15 often emerges as the failure criterion in heavy-duty sack applications, where puncture during filling is simulated under ASTM F1306-19 at 45 N to 70 N on 50 µm film. Modulus loss associated with higher comonomer content can reduce 1% secant modulus under ASTM D882-18 to 180 MPa to 230 MPa, which may require blend modification with LDPE or HDPE to restore stiffness. Published data for 7105GLT-specific downgauging limits is limited; converter trials on specific packaging machinery remain determinative.

    Representative comparative blown film data at 25 µm; values are typical commercial ranges, not 7105GLT-specific.
    MetricMethodButene LLDPEHexene LLDPE80/20 Hexene LLDPE/LDPE
    DensityASTM D1505-180.918–0.922 g/cm³0.917–0.921 g/cm³0.919–0.923 g/cm³
    Melt indexASTM D1238-200.5–1.0 g/10 min0.5–1.2 g/10 min0.3–0.8 g/10 min
    Dart impactASTM D1709-16A80–120 g110–160 g90–130 g
    Elmendorf tear MDASTM D1922-15150–250 gf200–350 gf120–220 gf
    Elmendorf tear TDASTM D1922-15300–450 gf350–550 gf250–400 gf
    Tensile at break MDASTM D882-1835–50 MPa35–55 MPa25–35 MPa
    1% secant modulusASTM D882-18190–240 MPa180–230 MPa160–210 MPa
    Puncture forceASTM F1306-1940–60 N45–70 N35–55 N

    In heavy-duty shipping sack lines, 7105GLT is coextruded with LDPE or HDPE skins to balance toughness, stiffness, and heat-seal integrity. Form-fill-seal equipment operating at 40 to 80 bags/min exposes the film to rapid draw acceleration and high-rate seal bar contact; the hexene-copolymer core contributes impact absorption under ASTM D1709-16A at film gauges from 75 µm to 125 µm, while the outer layers protect against melt fracture and seal jaw sticking. Hot-tack performance evaluated under ASTM F1921-12 at seal temperatures from 115 °C to 150 °C requires stable heat-seal initiation; hexene LLDPE grades exhibit seal initiation temperatures in the range of 105 °C to 115 °C, which is approximately 5 °C to 10 °C higher than LDPE-rich structures and may necessitate seal jaw dwell adjustments. On commercial lines with 50 mm to 75 mm extruders, stable bubble geometry is maintained at blow-up ratios of 2.2:1 to 2.8:1, but transitions from butene LLDPE may require a 10% to 15% increase in frost line height to offset the lower melt strength of hexene copolymers. Production logs from multi-layer lines have recorded periodic bubble instability when hexene-copolymer layers exceed 70% of total structure weight, requiring either external bubble stabilizing cages or higher internal bubble pressure.

    When 7105GLT is incorporated into food-contact coextruded film structures

    When 7105GLT is incorporated into food-contact coextruded film structures, compliance documentation becomes part of the specification. The resin is evaluated for use in contact with food under FDA 21 CFR 177.1520 for olefin polymers, subject to extractables limits and end-use conditions specified in subparagraph (c). For the European Union, compliance with Commission Regulation (EU) No 10/2011 requires overall migration testing under EN 1186-1:2002 and specific migration of additives under EN 13130-1:2004, with the resin vendor providing a Declaration of Compliance for the supplied grade. Recycled content claims, if applicable, must be verified against ISO 14021:2016 with documented chain-of-custody. Products exported to jurisdictions requiring halal or kosher certification are subject to third-party certifications listed on the manufacturer’s documentation. Published data on the full additive package for 7105GLT is not exhaustively disclosed in this document; the safety data sheet and food-contact statement from Chevron Phillips Chemical remain the controlling references.

    Compliance verification matrix for 7105GLT blown film structures; certification status must be confirmed with the resin supplier.
    Regulatory frameworkDesignationVerification requirement
    U.S. food contactFDA 21 CFR 177.1520Olefin polymer compliance; extractables and end-use limitations
    EU food contactRegulation (EU) No 10/2011Overall migration EN 1186-1:2002; specific migration EN 13130-1:2004
    REACH registrationRegulation (EC) No 1907/2006Substance registration and safety data sheet conformance
    Heavy metalsDirective 2011/65/EU RoHSRestricted substance screening
    Recycled content claimISO 14021:2016Chain-of-custody documentation
    Kosher/Halal optionalThird-party certificationCertification letter from resin vendor

    Controlling die-lip buildup and melt fracture during high-output blown film runs

    Controlling die-lip buildup and melt fracture during high-output blown film runs involves management of shear stress at the die land and additive migration. Hexene LLDPE grades processed at shear rates above 500 s⁻¹ may exhibit sharkskin melt fracture when die gaps fall below 1.0 mm; the inclusion of a fluoroelastomer processing aid at 200 ppm to 1000 ppm reduces apparent melt viscosity at the die wall and suppresses surface defects within 20 to 60 minutes of purge. Die-lip buildup, often caused by low-molecular-weight waxes and antiblock migration, is minimized by selecting silica-based antiblock at 2000 ppm to 5000 ppm and by maintaining die temperature 5 °C to 10 °C above the adapter temperature to prevent condensation and additive deposition. On lines with oscillating or rotating die heads, lip cleaning intervals extend from 8 hours to 24 hours depending on film grade, output, and ambient humidity. Production logs on 75 mm extruders with 300 mm dies indicate that head pressure fluctuations above 5 MPa signal filter screen blinding or additive plate-out and require corrective action. The use of metallocene-catalyzed hexene LLDPE variants on the same line can alter the molecular weight distribution sufficiently to shift the onset of sharkskin to lower shear rates; this effect is controlled through die gap increase rather than melt temperature reduction.

    Under high-humidity storage conditions exceeding 60% relative humidity, moisture condensation on cold pellet surfaces can introduce surface splay and gauge defects during film extrusion. The resin should be stored in sealed silos or original packaging and allowed to equilibrate to ambient temperature before use; if condensation is observed, pre-drying in a desiccant-air hopper dryer at 60 °C to 80 °C for 2 to 4 hours removes surface moisture without altering the antioxidant package. Thermal processing above 250 °C or residence times exceeding 30 minutes in the extruder barrel initiate oxidative degradation and crosslinking, producing gel particles visible under light transmission. Reintroduction of edge trim and scrap into the film line is limited to 10% to 30% by weight, depending on gel count requirements and gauge tolerance; higher recycle fractions require filtration through 100 µm to 150 µm screen packs to control specks. Blending with butene LLDPE is permitted, but comonomer mismatch can create melt-pool stratification in thick gauges above 125 µm, requiring mixer-section modification. The resin is not intended for applications requiring autoclave steam sterilization above 121 °C or prolonged ultraviolet exposure without carbon black or hindered amine light stabilizer additions.