Chevron Phillips 6335 Lldpe Cast Blown Film Resin Butene Copolymer

Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 753973
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Melt Index I2 0.70 g/10 min
    Density 0.918 g/cm³
    Melting Point 122 °C
    Vicat Softening Point 101 °C
    Tensile Strength At Yield Md 10.3 MPa
    Tensile Strength At Yield Td 9.65 MPa
    Tensile Strength At Break Md 22.8 MPa
    Tensile Strength At Break Td 17.9 MPa
    Elongation At Break Md 500 %
    Elongation At Break Td 700 %
    1 Secant Modulus Md 172 MPa
    1 Secant Modulus Td 193 MPa
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Dart Drop Impact 200 g
    Haze 12 %
    Gloss 60 %
    Coefficient Of Friction 0.20
    Blocking 100 g
    Brittleness Temperature < -70 °C

    As an accredited Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer is supplied in 50 lb multiwall bags, 40 bags per pallet (2,000 lb total).
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer, shrink-wrapped.
    Shipping Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer is shipped as non-hazardous, free-flowing pellets. Typical packaging: 25-kg bags, 1,000-kg supersacks, octabins, or bulk trucks/railcars. Store cool, dry, and ventilated, away from heat, sunlight, and moisture. Keep containers sealed. Handle using standard equipment. Ensure dry conditions. Not DOT-regulated for transport.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep bags or containers closed, labeled, and off the floor on pallets. Protect from moisture, dust, and contamination. Avoid excessive stacking, physical damage, and prolonged UV exposure. Use first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Store in cool, dry, well-ventilated area away from direct sunlight; typical shelf life is 12 months in unopened original packaging.
    Application of Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer

    On high-output cast film lines producing machine-grade pallet wrap, Chevron Phillips 6335 LLDPE butene copolymer serves as the principal web-forming component where the published sheet density of 0.918 g/cm³ (ASTM D1505) and nominal melt-flow rate of 3.5 g/10 min (ASTM D1238) permit continuous drawdown to thicknesses of 12–30 μm at chill-roll speeds above 300 m/min. A three-layer A/B/A structure typically blends 6335 at 75–85 wt% in the skin layers and 60–70 wt% in the core, with the balance split between metallocene-catalyzed linear low-density polyethylene at 10–25 wt% and low-density polyethylene at 0–10 wt%; cling masterbatch containing polyisobutylene or similar tackifying resin is added to one skin layer at 1–3 wt%. Industrial pallet wrap is not governed by food-contact migration limits, but procurement specifications commonly reference ASTM D4649-20 and mechanical acceptance is measured by ASTM D882 for ultimate tensile, ASTM D1922 for Elmendorf tear, and ASTM D1894 for static and kinetic coefficient of friction. Melt temperatures are maintained at 245–260°C, the flat die gap is set to 0.8–1.2 mm, and edge pinning is achieved with a combination of air-knife and vacuum-box equipment; the primary chill roll is held at 18–28°C to balance web cooling with cling-agent migration. The terminal formats are pre-stretched machine film, hand pallet wrap, and lighter-gauge bundling stretch film used for unitizing pallet loads in warehousing and logistics operations. A critical processing boundary exists at the melt-temperature set point: excursions beyond ±5°C can destabilize the cling additive, causing transfer to the chill roll and increasing web-break frequency at velocities above 500 m/min.

    Blown-Film Sealant Webs in Three-Layer Lamination Structures

    Where the 6335 resin is converted into blown sealant webs for lamination to oriented polyester or biaxially oriented polypropylene, the butene comonomer lowers the seal initiation temperature relative to high-density polyethylene while retaining sufficient hot-tack strength for vertical form-fill-seal packaging at speeds between 40 and 80 cycles/min. The sealant layer formulation commonly uses 6335 at 70–85 wt%, low-density polyethylene at 10–20 wt%, and metallocene-catalyzed linear low-density polyethylene at 5–10 wt%; a silica-based antiblock masterbatch is introduced at 0.5–1.5 wt% and erucamide slip masterbatch at 0.2–0.5 wt% to control blocking and coefficient of friction after lamination. Food-contact compliance is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers used in contact with food, and under EU Regulation No 10/2011, which specifies an overall migration limit of 10 mg/dm² for plastic materials and articles intended to come into contact with foodstuffs. The blown-film process uses coextrusion dies with diameters between 250 and 400 mm, die gaps in the 1.4–2.0 mm range, and blow-up ratios from 2.0:1 to 2.8:1; melt temperature is controlled at 190–220°C, with output from 180 to 260 kg/h depending on extruder size. The terminal forms are sealant layers in three-layer laminate structures for dry snack packaging, frozen-food pouches, and bag-in-box liners where the sealant web must remain flexible at temperatures below -20°C.

    Which Barrier and Tear Properties Make Butene LLDPE Suitable for Silage Bale Wrap?

    Silage bale wrap imposes simultaneous demands for high-cling, oxygen exclusion, and resistance to film puncturing from stemmy forage. In this application, 6335 is formulated at 75–90 wt% with metallocene-catalyzed polyethylene at 10–25 wt%; ultraviolet stabilizer masterbatch is added at 1–3 wt% and a carbon black or titanium dioxide masterbatch at 1–2 wt% when multi-season weathering is required. The governing product standard is EN 13207:2018, which addresses thermoplastic silage films and tubes; mechanical verification is typically done with ISO 527-3 for tensile properties of film and ASTM D1922 for tear resistance. Blown-film conversion is carried out at a blow-up ratio between 2.8:1 and 3.5:1 to impart higher TD toughness, with a die gap of 1.6–2.2 mm and melt temperature of 190–210°C; the bubble is operated in a high-stalk configuration to increase orientation before the frost line. A process conflict occurs when the frost-line height is raised more than 10 die diameters because TD elongation increases but MD tear resistance declines sufficiently to cause split propagation during bale wrapping. Finished products include round- and square-bale stretch film, silage cover sheeting, and oxygen-barrier coextruded structures used for high-moisture ensiling.

    For specification alignment across the downstream application classes, the following matrix consolidates the primary regulatory frameworks and mechanical qualification methods.

    Application segmentPrimary reference frameworkTest method designationParameter monitored
    Machine cast stretch filmASTM D4649-20ASTM D882, ASTM D1922, ASTM D1894tensile, tear, coefficient of friction
    Food-contact sealant webFDA 21 CFR 177.1520(c), EU Regulation No 10/2011ASTM F2029, ASTM F1921heat seal strength, hot-tack
    Silage bale wrapEN 13207:2018ISO 527-3, ASTM D1922tensile, tear
    Stretch-hood pallet filmREACH 1907/2006, EU Directive 94/62/ECASTM D882, ASTM D1922, ASTM D5748tensile, tear, cling
    Freezer-grade food filmFDA 21 CFR 177.1520(c), EU Regulation No 10/2011ASTM D1709, ASTM D882, ISO 7765-1dart impact, tensile
    Heavy-gauge industrial linerREACH 1907/2006ASTM D1709, ASTM D1922, ASTM D5747dart impact, tear, puncture

    At gauge ranges from 50 to 120 μm, stretch-hood pallet film produced from 6335 is formulated as a three-layer heavy-gauge blown structure in which the core layer contains 6335 at 65–80 wt% and the skin layers contain 6335 at 70–85 wt%, with the remaining fraction divided between metallocene-catalyzed polyethylene at 20–30 wt% and low-density polyethylene at 5–10 wt%; antiblock masterbatch is dosed at 0.2–0.8 wt% and slip masterbatch at 0.05–0.2 wt% in the outer skins. For industrial transport packaging, conformity is assessed under REACH 1907/2006 and packaging minimisation requirements of EU Directive 94/62/EC; mechanical lot acceptance uses ASTM D882 for ultimate tensile, ASTM D1922 for tear, and ASTM D5748 for cling between adjacent film surfaces. The blown-film line operates with a die diameter of 250–450 mm, die gap of 1.6–2.4 mm, and blow-up ratio of 2.0–2.8:1; melt temperature is held at 190–215°C, and gauge is maintained by an automatic air ring with die-bolt control to avoid thickness variation exceeding ±5%. Converters wind the output into stretch hoods for palletized cement sacks, beverage crates, and chemical bag loads, where the hood is stretched down over the load at ambient temperature. Published laboratory data for this exact stretch-hood structure is limited, but the cited processing limits are derived from commercial butene-copolymer blown-film conversion. An operational boundary appears at 6335 fractions exceeding 85 wt%, where pinhole formation at sharp package corners increases during vertical down stretching; below 60 wt%, cling force may fall below the level required for secure load retention in transit.

    When Freezer-Grade Film Requires Low-Temperature Ductility Without Plasticizer Migration

    Blown film used for frozen-food inner liners and ice-cream pouches is formulated without monomeric plasticizers because low-temperature flexibility is supplied by the butene comonomer in 6335 rather than by migratory additives. A monolayer or three-layer construction typically uses 6335 at 80–95 wt%, low-density polyethylene at 5–15 wt%, and a combination slip/antiblock masterbatch at 1–3 wt%; the slip agent is an erucamide or oleamide chemistry selected for controlled bloom after conversion. The structure is intended for food contact and is evaluated under FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011 with an overall migration limit of 10 mg/dm²; converters may additionally reference EC 1935/2004 for general food-contact safety requirements. Processing takes place on a three-layer blown-film line with a 250–350 mm die, die gap 1.4–1.8 mm, blow-up ratio 2.0–2.5:1, and melt temperature 185–205°C; output is typically 150–250 kg/h, and the bubble is collapsed through a low-tension collapsing frame to reduce centerfold crease orientation. Finished formats include frozen vegetable pouches, ice-cream bags, and frozen meat inner liners that must survive bag-drop and rough handling at storage temperatures near -25°C. The relevant low-temperature acceptance protocol commonly includes ASTM D1709 dart-impact testing at room temperature and ISO 7765-1 free-falling dart testing on cold-conditioned specimens, because a film that passes dart impact at 23°C may still fail at freezer temperature if the blend contains excess LDPE or off-spec regrind.

    At 200 μm Gauge, Fold-Crease Puncture Resistance Determines Liner Service Life

    Heavy-gauge liners for flexible intermediate bulk containers and construction containment are manufactured from 6335-based blown film at thicknesses from 100 to 250 μm, where the primary failure mode is fold-crease puncture rather than tensile overload. The formulation commonly comprises 6335 at 70–90 wt%, low-density polyethylene at 5–15 wt%, recycled linear low-density polyethylene at 0–10 wt%, and calcium carbonate masterbatch at 0–8 wt% where stiffness is required; carbon black masterbatch is added at 1–2 wt% for ultraviolet resistance in outdoor exposure. Regulatory conformity for non-food industrial film is handled under REACH 1907/2006, and mechanical qualification references ASTM D1709 for dart impact, ASTM D1922 for Elmendorf tear, ASTM D5747 for puncture resistance, and ASTM D882 for tensile. The blown-film line is set with a die gap of 1.8–2.4 mm, a blow-up ratio between 2.0:1 and 3.0:1, and melt temperature 195–215°C; heavy-gauge production uses an internal bubble cooling system to manage heat removal because air-side cooling alone becomes limiting beyond 150 μm. The finished web is converted into FIBC liners, construction moisture barriers, temporary containment film, and equipment protection shrouds. A processing threshold is observed when calcium carbonate content exceeds 8 wt%, because dart-impact retention drops rapidly and fold-crease puncture resistance measured by ASTM D5747 falls below the values required for bag-drop compliance in logistics cycles.

    Free Quote

    Competitive Chevron Phillips 6335 LLDPE Cast/Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6335 is an ethylene/1-butene copolymer linear low-density polyethylene pellet resin designed for cast and blown film extrusion. The grade is sold as part of the Marlex polyethylene portfolio and is specified by a nominal density of 0.918 g/cm³ and a nominal melt index of 2.0 g/10 min when measured under ASTM D1238 at 190 °C and 2.16 kg. The butene-1 comonomer inserts ethyl short-chain branches along the polyethylene backbone, disrupting crystallinity and producing a different mechanical profile from hexene-1 and octene-1 LLDPE resins. In cast and blown film conversion, the product is directed toward monolayer and coextruded structures such as refuse sacks, industrial liners, garment bags, over-wrap films, and selected sealant layers. Because the resin is a conventional butene LLDPE rather than a metallocene or higher-alpha-olefin grade, its performance envelope is defined by moderate toughness, controlled seal initiation, and stable draw under medium line speeds.

    The structural distinction between 6335 and higher-alpha-olefin grades is not limited to raw material cost. Butene-1 produces ethyl branches, hexene-1 produces butyl branches, and octene-1 produces hexyl branches. Longer branches increase the probability of interlamellar tie-molecule formation during quiescent crystallization, which raises dart impact and Elmendorf tear resistance at equivalent density and melt index. The practical consequence is that 6335 is often specified in layers where yield stress, stiffness, and thickness control matter more than extreme puncture or low-temperature abuse. In coextruded films, butene LLDPE can be placed in core or upper-middle layers while hexene or octene skins carry abuse resistance.

    Nominal resin specifications are characterized through standardized rheological and density measurements

    The nominal property set for 6335 is defined by melt flow and density because these two parameters influence extruder throughput, shear heating, film tensile balance, and seal temperature. The following values are taken from standard resin specification practice for the grade and should be confirmed against the supplier certificate of analysis.

    PropertyNominal valueTest method
    Density0.918 g/cm³ASTM D1505 / ISO 1183-1
    Melt index2.0 g/10 minASTM D1238 / ISO 1133-1:2022 at 190 °C, 2.16 kg
    Comonomer typeButene-113C NMR or FTIR copolymer analysis
    DSC peak melting temperature122–126 °CASTM D3418
    Vicat softening point95–107 °CASTM D1525

    Density and melt-index targets are not static manufacturing guarantees; a certificate of analysis should state lot-specific values and the test standard used. A melt-index shift of ±0.2 g/10 min can alter extruder motor load on a fixed screw profile by roughly 3–8% depending on machine size and transfer-line pressure. Similarly, density variation of ±0.001 g/cm³ can modify film tensile modulus by 5–12% under ASTM D882. These are conversion risks that should be managed through incoming inspection and silo segregation.

    At receiving, density should be measured by ASTM D1505 or ISO 1183-1 and melt flow rate by ASTM D1238 or ISO 1133-1:2022. Oxidation induction time by ASTM D3895 at 200 °C provides a check on antioxidant retention; conventional stabilized butene LLDPE usually shows OIT above 15 min, but the exact lower control limit must come from the supplier stability study. Bulk density measured under ASTM D1895 Method A is relevant for hopper inventory and conveying. Pellets should be free of fines; fines above 0.2 wt% can generate feeding variation and localized gel formation. Moisture is normally not a critical variable for polyethylene, but condensation after cold storage can introduce surface moisture. If pellet surface moisture exceeds 0.05 wt%, drying with dehumidified air at 60–80 °C for 1–2 h is sufficient to restore surface quality.

    Cast film conversion of 6335 is performed on extruders with length-to-diameter ratios of 24:1 to 30:1 using barrier screws or Maddock mixing sections. Production-scale lines typically start with barrel zone temperatures of 176–204 °C at the rear, rising to 204–221 °C in the metering zone, with head and die set at 232–246 °C. Melt temperature at the die lip should be maintained between 232 °C and 274 °C; the lower bound prevents excessive screw torque and the upper bound avoids oxidative gel formation. Die gaps of 0.25–0.50 mm are used for light-gauge cast film, while heavier gauges may require gaps up to 0.76 mm. Chill-roll temperature is typically 15–30 °C for high-gloss film, with higher temperatures used only when blocking control and downstream converting permit. On such lines, film haze at 25 µm is commonly measured under ASTM D1003 in the 3–6% range when chill-roll finish and temperature are optimized. Fluoropolymer processing aid at 200–800 ppm can be added as masterbatch to reduce die-lip deposit and delay sharkskin. Screen packs of 60/80/100 mesh are a common starting point; an increase in pressure drop above 10–15% of the clean-screen baseline indicates that the screen pack should be inspected.

    Published tensile behavior for butene LLDPE cast film at 25 µm tested under ASTM D882 generally falls in the range of 20–35 MPa machine-direction tensile strength at break and 15–25 MPa transverse-direction tensile strength at break. Elongation at break is typically 400–700% machine direction and 500–800% transverse direction. These values are strongly draw-ratio dependent; parallel and perpendicular orientation induced by the cast roll and line speed should be measured on the target line because published data for the exact 6335 configuration on a given line is limited.

    How does butene-1 comonomer content influence solid-state mechanical performance relative to hexene and octene grades?

    At constant density and melt index, butene-1 comonomer produces less impact resistance than hexene-1 or octene-1 because C2 branch lengths are less able to connect lamellae. In 0.025 mm monolayer blown film tested under ASTM D1709 Method A, butene-copolymer grades in the 0.918 g/cm³, 2.0 g/10 min class may exhibit dart impact in the 60–110 g range, while hexene and octene grades often span 90–180 g and 120–250 g, respectively. Machine-direction Elmendorf tear under ASTM D1922 for butene-copolymer LLDPE commonly falls between 1.5 N and 2.5 N; octene-copolymer film may exceed 4.0 N at the same gauge. The stiffness, measured as 1% secant modulus under ASTM D882, remains similar across comonomer types at constant density but can be 5–15% higher for butene grades because of subtle yield stress and crystal perfection differences. These differences justify placing 6335 in core or non-critical layers rather than in layers that must withstand crease flexing or cold-temperature drop.

    Performance attributeButene LLDPEHexene LLDPEOctene LLDPETest method
    Comonomer branch lengthC2C4C6N/A
    Dart impact, 25 µm60–110 g90–180 g120–250 gASTM D1709
    MD Elmendorf tear, 25 µm1.5–2.5 N2.0–3.5 N3.0–5.0 NASTM D1922
    TD Elmendorf tear, 25 µm2.5–5.0 N3.5–6.0 N5.5–9.0 NASTM D1922

    The data above are class-level ranges and are not lot-specific guarantees. They demonstrate that 6335, as a butene-copolymer resin, is positioned for applications that require adequate, rather than maximum, film toughness. In abusive packaging applications where puncture or cold-temperature impact is limiting, converters often switch to hexene or octene LLDPE, metallocene LLDPE, or coextrusions with a tougher skin layer. The stiffness of butene LLDPE at equivalent density is not a performance penalty; in fact the difference in secant modulus measured under ASTM D882 is usually less than 10% relative to hexene grades, while lower comonomer cost and stable cast-line processability can favor butene products in high-output structures.

    Compared with high-pressure LDPE, 6335 has higher tensile strength and elongation at break measured under ASTM D882 but lower melt strength and extrusion extension hardening. This is the main reason blown-film converters blend LLDPE with LDPE at 10–30 wt% to stabilize bubble geometry and reduce melt fracture. The tradeoff is an increase in film haze under ASTM D1003, often from 4–8% to 9–15% at 25 µm, and a measurable decrease in dart impact under ASTM D1709 in the range of 10–20% depending on LDPE molecular weight.

    When bubble instability emerges during thin-gauge blown film production

    Thin-gauge blown film below 25 µm produced from 6335 can exhibit bubble flutter, draw resonance, sharkskin, or film blocking. These defects are related to the relatively narrow molecular weight distribution of linear low-density polyethylene and the absence of long-chain branching. Production-scale observation on 100 mm grooved-feed blown lines with 30:1 L/D barrier screws indicates that a stable operating point often begins with a melt temperature of 193–221 °C, die gap of 0.8–1.5 mm, blow-up ratio of 2.0:1–2.8:1, and frost-line height of 8–14 times die diameter. If sharkskin persists, a fluoropolymer processing aid masterbatch at 200–800 ppm is introduced at the feed throat. The processing aid conditions the die wall within 20–90 min, depending on concentration and die shear stress; completion of conditioning is identified when die pressure stabilizes and surface roughness under a 30× microscope is eliminated. Excessive processing aid above 1000 ppm can depress adhesion of printing inks and laminating adhesives; corona treatment after blending should then be verified by ASTM D2578 wetting tension tests to keep film surface energy in the 38–42 dyn/cm range for lamination or printing.

    Oxidative degradation in blown film is managed by controlling melt temperature below 249 °C and by limiting residence time in the die and adapter to less than 8 min. When gel formation appears as clear or black flecks, the processor should examine screen pack pressure, dead spots in the adaptor, and percent recycled edge trim. Post-industrial recycled monolayer LLDPE may be introduced, but contamination with polypropylene or polyamide is not acceptable; these materials remain solid at LLDPE processing temperatures and create stress concentrations that reduce Elmendorf tear and dart impact. On lines with internal bubble cooling, the cooling air temperature should be maintained between 10 °C and 18 °C to avoid condensation and bubble chatter. Output rates for thin-gauge film are best determined empirically from die diameter and take-off speed; a 200 mm die running 6335 at 25 µm may be started at 90–120 kg/h and increased only after thickness uniformity measured by a scanning capacitance gauge remains within ±5%.

    In cast film and sealant-layer structures, 6335 is often evaluated for heat-seal performance. Seal initiation temperature under ASTM F1921 at 0.4 MPa and 1.0 s dwell for a 25 µm film typically falls between 85 °C and 105 °C; hot-tack strength under the same standard is commonly 0.5–2.5 N/25 mm across the sealing range. Seal strength under ASTM F88 generally increases from 5 N/25 mm at the initiation point to 12–20 N/25 mm when sealed above 130 °C. These values are strongly affected by slip and antiblock additives, film aging, and coextrusion layer thickness, and must be reproduced on the target film. If 6335 is used as a sealant skin, the skin thickness should be maintained above 5 µm to avoid localized low-seal areas; below this thickness, gauge variation can create intermittent seal channels under high-speed form-fill-seal operations.

    Regulatory status of 6335 should be confirmed with the supplier product-specific compliance letter. The base resin is typically represented as an olefin polymer within the scope of 21 CFR 177.1520; the final food-contact article must meet the extraction and end-use limitations of that section. In the European Union, the converter must evaluate the final film or package under Commission Regulation (EU) No 10/2011; overall migration and specific migration of butene-derived oligomers depend on film thickness, sealant composition, and use conditions. REACH Regulation (EC) No 1907/2006 and CLP Regulation (EC) No 1272/2008 apply to the pellet product, and the safety data sheet lists stabilizer decomposition species. The resin is not intended for medical implants, sustained hot-water piping, or continuous exposure to strong oxidizers. Long-term service above 80 °C is outside typical stabilizer design for a film-grade butene LLDPE because oxidative depletion accelerates above this point.

    Published data for the exact performance of 6335 on a given converter’s cast or blown line is limited. The ranges above should be used as feasibility inputs rather than as lot release specifications. Final suitability for packaging requires analysis of additive migration, seal strength, tear resistance, and gauge uniformity against the specific article’s performance standard.

    Top