| HS Code | 350866 |
| Density | 0.920 g/cm3 |
| Melt Index | 1.0 g/10 min |
| Comonomer | Butene |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 26.2 MPa |
| Elongation At Break | 1000% |
| Flexural Modulus | 207 MPa |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g/mil |
| Elmendorf Tear Strength Td | 400 g/mil |
| Haze | 12% |
| Gloss | 60% |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Brittleness Temperature | -70 °C |
As an accredited Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Standard packaging: 25 kg polyethylene-lined multiwall paper bags, palletized and stretch-wrapped; 1,000 kg bulk bags may also be available. |
| Container Loading (20′ FCL) | 20′ FCL: Chevron Phillips 6120 LLDPE cast/blown film resin, butene copolymer; 25 kg bags, palletized, stretch-wrapped, approx. 22 MT net. |
| Shipping | Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer ships as non-hazardous, combustible solid pellets, typically in 25-kg bags, 1,000-kg bulk bags, or bulk trucks/railcars. It is generally not DOT/IMDG/IATA regulated. Store dry, away from heat/ignition, prevent pellet loss, and follow local environmental rules. |
| Storage | Store indoors in a cool, dry, well-ventilated warehouse. Keep original containers or bags sealed, off the floor, and away from direct sunlight, heat, ignition sources, and incompatible oxidizers. Protect resin from moisture, dust, dirt, oils, and other contaminants. Avoid extreme temperatures and excessive stacking. Practice first-in, first-out rotation and follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in original unopened packaging under cool, dry, well-ventilated conditions. |
High-speed cast pallet stretch film operations running Chevron Phillips 6120 butene-copolymer LLDPE in the core layer operate with a nominal resin density of 0.918 g/cm³ under ASTM D1505 and a nominal melt index of 1.0 g/10 min under ASTM D1238 at 190°C/2.16 kg. The formulation addition ratio for 6120 is held between 60 wt% and 80 wt% in the core layer, with metallocene octene LLDPE at 10–30 wt% and low-density polyethylene at 5–15 wt% in adjacent layers to manage dart impact and edge-trim uniformity. A tackifier-bearing polyisobutylene cling masterbatch is added at 1.0–2.5 wt% in the cling layer, while a silica anti-block masterbatch at 0.5–1.5 wt% is used on the opposite outer layer. Above 3.0 wt% anti-block, cling force measured under ASTM D5458 drops below 0.40 N, which is the lower bound observed on automated pallet wrapping lines operating at 2.5–3.0 m/s film feed rate. The compliance framework for industrial stretch film is not food-contact-specific; it falls under EU Packaging and Packaging Waste Directive 94/62/EC Article 11 with a combined lead, cadmium, mercury, and hexavalent chromium limit of 100 mg/kg. Physical property verification uses ASTM D5748 for trapezoidal tear propagation and puncture resistance, ASTM D882 for machine-direction and transverse-direction tensile yield, ASTM D1922 for Elmendorf tear, and ASTM D1894 for kinetic coefficient of friction.
On production lines, the resin is processed through a single-screw extruder with L/D 30:1, a barrier screw with Maddock mixing tip, and screen pack of 60/80/100 mesh. The cast die gap is set at 0.5–0.8 mm, melt temperature at 235–250°C, and the air gap between die lip and chill roll at 20–40 mm. The chill roll temperature is maintained at 15–25°C. When chill roll temperature falls below 12°C at line speeds above 400 m/min, condensation on the chill roll can create pinholes at frost bands, and the edge trim tends to fracture under oscillation from the air knife. Melt temperatures above 255°C increase gel count and produce die-lip deposit from degraded polyisobutylene cling additive. The terminal product types include machine stretch film slit to 500 mm at 20–23 µm, hand-held stretch film slit to 450 mm at 12–17 µm, and heavy-duty pallet wrap slit to 750 mm at 25–35 µm.
| Cast film gauge | Chill roll temperature | Line speed | Slit width and film type |
|---|---|---|---|
| 12–17 µm | 15–20°C | 350–500 m/min | 450 mm hand stretch film |
| 18–23 µm | 18–25°C | 300–450 m/min | 500 mm machine stretch film |
| 25–35 µm | 20–25°C | 250–350 m/min | 750 mm heavy-duty pallet wrap |
Seal initiation in blown food-contact webs based on 6120 is governed less by nominal melting point than by the distribution of short-chain branches introduced by the butene comonomer. The food-contact layer is typically compounded at 70–85 wt% 6120 with 10–20 wt% LDPE and 5–15 wt% linear medium-density polyethylene for stiffness. Slip and anti-block masterbatches are added at 1.0–2.0 wt%, and fluoropolymer-free polymer processing aid is used at 200–800 ppm. Elevated processing aid above 1,000 ppm can interfere with heat seal strength in the finished laminate; seal strength is measured under ASTM F88/F88M-21 at 0.5-second dwell and 2.8 bar jaw pressure. The butene-copolymer structure widens the seal initiation range, and the measured seal initiation temperature is typically between 85°C and 95°C on crimp sealers with 0.5-second dwell. At heat-seal jaw temperatures above 130°C, high-crystallinity fractions in the butene LLDPE cause zoned seal deformation and inconsistent seal width.
Extrusion is carried out on three-layer blown film lines with die gap 1.8–2.5 mm, blow-up ratio 2.2–2.8, melt temperature 190–210°C, and output 2–4 kg/h/mm die circumference. Frost line height is set between 6 and 9 die diameters to balance bubble stability and tear resistance. Air ring and internal bubble cooling are operated with moderately low cooling rates to prevent the butene-copolymer film from excessive crystalline orientation that raises haze above 12% measured by ASTM D1003. The downstream production process includes corona treatment to 38–42 mN/m before lamination or printing. Terminal product types include frozen vegetable bag film at 60–80 µm, fresh-cut produce lidding substrate at 20–40 µm, and vertical form-fill-seal webs for dry food powder sachets at 40–60 µm.
| Standard or regulation | Clause or test method | Measured boundary |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymers for direct food contact | Conditions of use B through H; extractables limited by paragraph (d) |
| Regulation (EU) No 10/2011 | Annex I, Annex III, Annex IV | Overall migration limit 10 mg/dm²; simulant selection per Annex III food categories |
| EC 1935/2004 | Articles 3, 11, 15 | No transfer of constituents in quantities endangering human health |
| Commission Regulation (EC) No 2023/2006 | Annex | Good manufacturing practice for food-contact material production |
| REACH EC 1907/2006 | Annex XVII | Restricted heavy metal and PAH limits for packaging components |
In heavy-duty form-fill-seal packaging of granular fertilizers, chemical intermediates, and polymer pellets, 6120 is compounded at 60–75 wt% with high-density polyethylene at 15–25 wt% and metallocene LLDPE at 10–20 wt%. The HDPE fraction increases secant modulus, but above 25 wt% the Elmendorf tear measured by ASTM D1922 drops below 5 N at 140 µm thickness, creating a formulation ceiling that is not present at 180 µm. Carbon black UV masterbatch is added at 1–2 wt%, and an antioxidant/acid-scavenger masterbatch at 0.1–0.3 wt% if the sack is destined for products containing residual metal ions. The compliance framework for non-food heavy-duty sacks relies on ISO 527-3:2018 for tensile strain at break, ASTM D3786/D3786M-20 for burst strength, ASTM D1922 for propagation tear, and ASTM F392/F392M-23 for flex-crack resistance in multilayered constructions. When an end user requires transport packaging for dangerous goods, the full sack-and-filling construction must be qualified separately under the relevant UN transport packaging performance test; film resin data alone is not sufficient for that classification.
Extrusion is performed on a three-layer blown film line with die diameter 400–600 mm, die gap 2.0–2.8 mm, blow-up ratio 2.0–2.5, and melt temperatures 180–205°C. Internal bubble cooling is required above 160 µm thickness. Output drops from 3.0 kg/h/mm die circumference to 1.8–2.2 kg/h/mm when the bubble is undercooled because the butene LLDPE crystalline network builds too slowly, causing web bagging at the collapsing frame. Frost line height is set at 7–10 die diameters. Corona treatment is applied after the collapsing frame at 38–42 mN/m for printability. Terminal articles include 120–180 µm polymer pellet sacks, 150–220 µm mineral filler bags, and 140–200 µm pet food sacks with gusseted side seams.
Agricultural silage wrap produced from 6120 at film thickness below 25 µm requires a blend of 60–80 wt% 6120 with 10–20 wt% metallocene LLDPE and 5–15 wt% EVA or polar copolymer. The butene comonomer distribution in 6120 yields a broader melting range that can absorb stress during bale wrapping at −10°C, but dart impact measured by ASTM D1709 drops sharply when the film is oriented at blow-up ratios above 3.5. UV stabilization is introduced through a HALS-based masterbatch at 5–10 wt%; white pigment masterbatch is added at 8–12 wt% for light reflection and thermal load reduction. Compliance for agricultural silage films is governed by EN 13207:2018 for mechanical specifications, ISO 527-3:2018 for tensile elongation, ASTM D1922 for tear resistance, and ASTM D1709 for puncture impact. Under REACH EC 1907/2006 Annex XVII, the formulation must avoid cadmium-, lead-, and chromium-based pigments above restricted thresholds.
Process conditions on a three-layer blown film line include die gap 1.8–2.5 mm, blow-up ratio 2.5–3.5, melt temperature 185–205°C, and internal bubble cooling to stabilize the high blow-up ratio. At thicknesses from 25 µm to 50 µm, the film is wound as wide-web bale wrap. Thicker products include pit covers at 150–200 µm and greenhouse films at 150–200 µm. A process incompatibility occurs when recycled silage film contains soil residue: quartz particles of 10–30 µm create tear propagation sites in films below 20 µm, so filtration through a 100–150 mesh screen pack is required when post-industrial regrind exceeds 10 wt%. Terminal product types include bale wrap at 25–30 µm, silage pit cover at 150–200 µm, greenhouse cover film at 150–200 µm, and agricultural mulch film at 15–25 µm.
In breathable cast backsheet lines for absorbent hygiene articles, 6120 is evaluated only as the polymer fraction in a calcium carbonate-filled microporous web and is not run neat. The formulation addition ratio begins with 45–55 wt% surface-treated calcium carbonate masterbatch, with 6120 occupying 30–45 wt% of the total compound, metallocene octene LLDPE at 10–15 wt%, and LDPE at 5–10 wt%. The calcium carbonate is specified at 1.2–2.0 µm median particle size with stearic acid surface coating. Moisture content of the filled compound is maintained below 200 ppm before extrusion; above this limit, hydrolytic degradation produces pinholes and reduces machine-direction orientation uniformity. Titanium dioxide is added at 1–3 wt% for opacity and ultraviolet scattering. Compliance for non-medical absorbent hygiene backsheet falls under General Product Safety Directive 2001/95/EC, REACH EC 1907/2006 Annex XVII, and ISO 10993-5:2009 when the finished article is a component of a medical device. The downstream production process is cast extrusion followed by embossing and machine-direction orientation at a stretch ratio of 2.5:1–3.5:1; die gap is set at 0.6–0.8 mm, melt temperature at 220–245°C, and line speed at 150–300 m/min. If the production environment exceeds 60% RH, the calcium carbonate masterbatch is pre-dried at 80°C for 4–6 h. Terminal product types include diaper backsheet at 12–20 µm, adult incontinence backsheet at 20–35 µm, and feminine hygiene strip film at 12–18 µm. Published data specific to 6120 in high-filler breathable cast configurations is limited; pre-production trials across the orientation gap and embosser pressure are required before commercial output.
For protective masking films applied to stainless steel sheet, anodized aluminum, and pre-painted coil, 6120 is formulated at 70–90 wt% with LDPE at 10–30 wt% and an adhesion-modifying polyolefin masterbatch at 1–3 wt%. The low-molecular-weight fraction of 6120 affects both corona holding time and the peel force after application to flat metal. Slip and anti-block are limited to 0.5–1.5 wt% because higher slip loadings cause surface energy decay from 42 mN/m to below 36 mN/m within 30 days, compromising adhesion under shear. The compliance framework for electronics-protecting films includes RoHS 2011/65/EU Annex II restricted substance limits and REACH EC 1907/2006 Annex XVII; metal-facing protective films used in prolonged outdoor storage are additionally tested under ISO 4892-3:2016 UV exposure protocols. Processing is conducted on a cast film line at melt temperature 220–250°C, die gap 0.5–0.8 mm, chill roll temperature 15–25°C, and line speed 200–400 m/min. Corona treatment is applied at 38–42 mN/m. Terminal product types include 30–50 µm stainless steel sheet protection, 50–70 µm pre-painted coil masking, and 30–40 µm acrylic sheet protective film.
Competitive Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chevron Phillips 6120 LLDPE Cast/Blown Film Resin, Butene Copolymer is a pelletized linear low-density polyethylene manufactured with butene as the short-chain branching comonomer. It is specified by a nominal melt index of 1.0 g/10 min (ASTM D1238, 190 °C/2.16 kg) and a nominal density of 0.918 g/cm³ (ASTM D1505). These values establish the product within the cast and blown film envelope: density controls stiffness, moisture vapor transmission rate, and crystallization kinetics, while melt index governs extruder backpressure, drawdown, and maximum line speed. The product is supplied without a primary slip or antiblock package; converters add masterbatch concentrates to meet coefficient of friction targets measured by ASTM D1894 and blocking limits measured by ASTM D3354. The material is intended for monolayer film and coextruded structures where the skin layer must combine drawdown with a heat-seal range verified by ASTM F88. Unlike high-pressure low-density polyethylene, the linear backbone changes sheet drawdown behavior and bubble stability; these effects must be evaluated on the target line.
Nominal resin properties reported by the manufacturer are reproduced below for incoming inspection guidance. These are not lot release limits; certificate of analysis values may vary within the sales specification.
| Property | Nominal value | Method |
|---|---|---|
| Melt index | 1.0 g/10 min | ASTM D1238 (190 °C/2.16 kg) |
| Density | 0.918 g/cm³ | ASTM D1505 |
| Comonomer | Butene | Manufacturer designation |
| Processing target | Cast or blown film, 25–75 µm | Supplier processing guide |
The butene comonomer places ethyl branches along the linear backbone. These branches interrupt crystallite thickening and reduce density to 0.918 g/cm³, but the branch length is shorter than the butyl and hexyl branches present in hexene and octene copolymers. As a result, the probability of forming tie molecules between adjacent lamellae is lower. In 25 µm blown film prepared under standard conditions, tensile properties measured per ASTM D882 are characterized by machine-direction tensile strength at break values typically above 25 MPa and elongation at break above 500%. Dart impact measured by ASTM D1709 Method A commonly falls below equivalent hexene grades. Comparative technical literature indicates a dart impact penalty of 15% to 40% for butene LLDPE relative to hexene LLDPE at the same density and melt index. Elmendorf tear per ASTM D1922 shows a similar reduction, with machine-direction tear values commonly 20% to 35% lower. The penalty is not a processing artifact; it is reproduced across cast and blown film samples and is related to the low molecular weight tail and short-chain branch distribution.
Heat seal response is governed by the broad melting range. Differential scanning calorimetry per ASTM D3418 records a peak melting endotherm between 121 °C and 124 °C for this density band. Laboratory heat seal tests at 0.5 MPa seal bar pressure and 0.5 s dwell produce seal initiation from 95 °C to 110 °C, with hot tack measured per ASTM F1921 peaking near the final melting shoulder. The exact initiation threshold shifts with quench rate: fast chill roll cooling depresses the onset temperature by 2–5 °C, while slow air cooling in thick-gauge blown film raises the onset temperature by a similar margin. Converters should not transfer a single seal curve between cast and blown film lines without re-verification on the target equipment.
On a 45 mm grooved-feed extruder with an L/D of 30:1, the butene resin exhibits a feed zone set-point of 35–50 °C to prevent pellet bridging at the grooved liner. Compression zones are set from 180 °C to 210 °C, and the metering zone from 210 °C to 230 °C. The observed die pressure at 25 kg/h output through a 150 mm blown film die with a 1.5 mm die gap is approximately 18–25 MPa, which is 15% to 30% higher than an equivalent melt index LDPE at the same throughput. The rheological response follows a shear-thinning curve with a melt flow ratio I21/I2 in the range 22–30, but the extrapolated zero-shear viscosity is not indicative of process behavior because film extrusion occurs at apparent shear rates above 100 s⁻¹. The onset of gross melt fracture in a 0.8 mm cast film die is typically observed at shear rates above 300–500 s⁻¹, depending on die temperature; lowering die temperature from 240 °C to 220 °C can reduce the critical shear rate by 20% and produce regular sharkskin on the film surface.
Cast film conversion requires adapter and die zones at 220 °C to 250 °C. At 250 °C, the resin has sufficient molecular mobility to permit drawdown ratios up to 25:1 without edge instability, but exceeding 260 °C for more than 15 min of residence time promotes gel formation, visible as specks in 25 µm film. The die gap is set at 0.4–0.8 mm. A narrower gap raises draw resonance and increases machine-direction tear imbalance; a wider gap reduces melt fracture but forces greater drawdown to reach final gauge. The chill roll surface temperature is maintained at 15–30 °C. When the chill roll is set below 10 °C, surface condensation creates optical defects; above 35 °C, film clarity deteriorates because crystal growth proceeds too slowly and the film remains tacky at the winder. Corona treatment is typically applied to achieve a surface energy of 38–42 mN/m, measured by ASTM D2578. Untreated film of this resin may retain a surface energy below 32 mN/m, which is inadequate for solventless lamination or water-based ink adhesion.
Edge trim recovery on cast lines can be added back in-line at 10–20% by weight. Trim that has been exposed to multiple heat cycles or contaminated with paper dust can raise gel counts; a 20/40/80 mesh screen pack is used to trap agglomerated gel before the die. When trim content exceeds 20%, some cast film lines report a measurable increase in film haze as determined by ASTM D1003 and a reduction in Elmendorf tear as determined by ASTM D1922. The performance loss is not caused by molecular weight degradation alone; it also reflects the re-crystallization history of the reground edge material.
For cast stretch film structures, typical layer distribution places the butene resin in the core at 70–85% of the total gauge, with cling layers of ethylene-vinyl acetate or metallocene LLDPE at 7.5–15% each side. The core layer extruder is run with a melt temperature of 220–245 °C; the cling layers are kept below 220 °C to limit additive migration. Interlayer adhesion is maintained by viscoelastic interdiffusion rather than adhesive tie layers. A 3-layer feedblock with adjustable vanes allows the core layer to occupy 75% of the die exit without excessive layer encapsulation. Film gauge control is measured downstream by beta transmission at 25 µm with a tolerance of ±5%. When the butene core is replaced by an octene LLDPE, dart impact of the finished cast film improves by up to 30%, but the machine may require a 5–10 °C reduction in core melt temperature to avoid edge draw instability.
In air-cooled blown film operation, a die gap of 1.5–2.5 mm is used because the shear viscosity of this butene resin at processing temperatures is higher than that of high-pressure LDPE. The blow-up ratio is maintained at 2.0:1 to 3.0:1; outside this range, gauge uniformity suffers. The frost line height is set at 1.5–2.5 die diameters for 25–50 µm gauge. At a blow-up ratio above 3.0:1, bubble flutter can develop, particularly on towers without internal bubble cooling. A double-lip air ring is specified for line speeds above 30 m/min. If the frost line is raised too high, haze measured by ASTM D1003 increases because slow cooling permits larger spherulites; if the frost line is too low, the film freezes in a state of high molecular orientation and may show elevated machine-direction shrinkage measured by ASTM D2732. The resin does not require drying in ambient warehouse conditions below 60% RH; surface moisture on pellets from cold storage can be removed by a 70–80 °C dehumidified air dryer for 2–4 h before extrusion.
In a direct substitution trial on a monolayer blown film line producing 25 µm film, a hexene LLDPE of the same 0.918 g/cm³ density and 1.0 g/10 min melt index will generally show higher dart impact by 15% to 40% per ASTM D1709 Method A and higher machine-direction tear by 20% to 35% per ASTM D1922. The improvement is due to longer short-chain branches that increase tie-molecule concentration. The butene grade retains a processing advantage in some cast film lines: its broader molecular weight distribution and higher melt strength reduce draw resonance, and its lower catalyst cost may allow downgauging without loss of tensile strength. Metallocene LLDPE grades, by contrast, have a narrower molecular weight distribution and a lower seal initiation temperature. Hot tack measured per ASTM F1921 on a metallocene film can remain above 1 N/25 mm across a wider temperature interval than the butene grade, but the metallocene bubble can be less stable in air-cooled blown film because of lower melt strength. Converters should run a structure-specific comparison using ASTM D1709, ASTM D1922, ASTM F88, and ASTM F1921 before selecting the resin.
Storage should be in unopened containers below 50 °C, away from direct sunlight and standing water. The resin is stabilized with an antioxidant package, but outdoor weathering resistance is not inherent; films intended for outdoor exposure must be compounded with UV stabilizers and tested per ASTM D4329 or ASTM G154. Avoid blending with amine-based slip or antistat concentrates that can react with the phenolic antioxidant system at prolonged melt temperatures above 240 °C; such combinations can produce color shifts and reduce oxidative induction time measured by ASTM D3895. Extruder shutdowns should be purged with a lower-viscosity LDPE or purge compound because the resin can carbonize if left in idle barrels above 200 °C for more than 15 min. This material is not designed for medical implant or pharmaceutical contact applications; no USP Class VI or ISO 10993 biocompatibility statement is assigned by the standard sales specification.
The supplier identifies the resin for food-contact use under FDA 21 CFR 177.1520(c) 3.2a. That designation covers olefin polymers with density below 0.926 g/cm³ and is conditional on the finished article meeting extraction tests and end-use limitations. The matrix below summarizes the relevant frameworks.
| Framework | Designation | Boundary or condition |
|---|---|---|
| U.S. food contact | FDA 21 CFR 177.1520(c) 3.2a | Olefin polymers; final article subject to extraction limits |
| EU food contact | Regulation (EU) No 10/2011, Annex I | Overall migration limit 10 mg/dm² for final article |
| EU chemicals | REACH | Monomer and additive registration required for EU supply |
| Heavy metals | RoHS Directive 2011/65/EU | Not intentionally added; article-level compliance must be verified |
No statement in this document replaces the lot-specific certificate of analysis. Published data for some specialized multi-layer structures containing this resin are limited, and the converter must verify oxygen permeability, moisture vapor transmission rate, and seal performance on the final film using ASTM D3985, ASTM F1249, and ASTM F88.