Chevron Phillips 6109l Lldpe Blown Film Resin Butene Copolymer

Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 621167
    Melt Index 0.9 g/10 min
    Density 0.919 g/cm³
    Comonomer Butene-1
    Polymer Type LLDPE
    Melt Flow Ratio 27
    Melting Point 121 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 26.2 MPa (MD), 24.1 MPa (TD)
    Elongation At Break 600% (MD), 700% (TD)
    Dart Impact Strength 200 g
    Elmendorf Tear Strength 200 g/mil (MD), 400 g/mil (TD)
    Haze 12%
    Gloss 60%

    As an accredited Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 55 lb (24.9 kg) bags, typically 35 bags per pallet, totaling 1,925 lb.
    Container Loading (20′ FCL) 20′ FCL loaded with 25 kg bags of Chevron Phillips 6109L LLDPE blown film resin, butene copolymer, palletized and shrink-wrapped.
    Shipping Chevron Phillips 6109L LLDPE Butene Copolymer is a non-hazardous solid resin. It ships as pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Store and transport dry, cool, and away from direct sunlight. Standard freight rules apply; no special hazard placards required. Use clean, closed containers to prevent contamination.
    Storage Store Chevron Phillips 6109L LLDPE Blown Film Resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep material in original sealed packaging or containers, palletized and off the floor. Protect from moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Follow the manufacturer’s SDS and local regulations for handling and storage.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in unopened original packaging under cool, dry conditions.
    Application of Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer

    Frozen Food Packaging Film From Butene Copolymer Blown Film Resin

    Chevron Phillips 6109L is processed as a single-layer web or as the core layer of a three-layer coextrusion for frozen food packaging. The polymer, a butene-copolymer linear low-density polyethylene with a manufacturer’s nominal density of 0.920 g/cm³ under ASTM D1505 and a nominal melt index of 0.9 g/10 min under ASTM D1238 at 190 °C/2.16 kg, is selected where low-temperature toughness and heat-seal integrity must be retained after filling at temperatures as low as -30 °C. Regulatory conformance for direct food contact is governed by 21 CFR 177.1520(c) for olefin polymers and by EU Regulation (EC) No 1935/2004, with overall migration below 10 mg/dm² measured according to EU No 10/2011 Annex I in food simulants appropriate to frozen aqueous and fatty foods. Single-layer formulations typically contain 80–95 wt% 6109L, 5–20 wt% high-pressure LDPE for bubble stability, 0.5–1.5 wt% silica-based antiblock masterbatch, and 0.3–0.8 wt% erucamide slip masterbatch. The downstream blown film process uses a die gap of 1.8–2.5 mm, a blow-up ratio of 2.2:1–3.0:1, a melt temperature of 195–220 °C, and a frost line height of 600–900 mm; on lines equipped with internal bubble cooling and die diameters of 250–400 mm, specific outputs of 1.2–1.8 kg/h per mm of die circumference are common. Below a blow-up ratio of 2.0:1, cross-direction gauge variation increases and bubble flutter introduces visible gauge bands; above 3.0:1, melt extensibility in the low-ductility butene matrix reduces process latitude and increases the frequency of pinholes. Terminal product types include individually quick-frozen vegetable pouches, frozen ready-meal bags, ice cream packaging film, and heat-sealed frozen food pouches.

    In agricultural silage cover extrusion, 6109L is dry-blended with high-pressure LDPE and carbon black masterbatch to produce a film that blocks UV transmission and resists puncture during bunker compaction. Where conformance to EN 13206:2017 for thermoplastic silage films is specified, the minimum nominal film thickness of 150 µm and carbon black loading are primary specifications; weathering resistance is assessed after 2,000 h of ISO 4892-2 or ASTM G154 exposure, and film tensile properties are evaluated under ISO 527-3. The formulation at the hopper typically contains 70–85 wt% 6109L, 15–30 wt% high-pressure LDPE, 3–6 wt% carbon black masterbatch, and 2–4 wt% hindered amine light stabilizer-based UV stabilizer masterbatch. Processing is carried out on mono-layer blown film extruders with grooved feed sections and screw L/D ratios of 30:1; die gap is set at 1.8–2.2 mm, blow-up ratio at 2.5:1–3.5:1, and melt temperature at 200–230 °C. The presence of carbon black raises melt viscosity at constant throughput, increasing extrusion pressure by approximately 8–15% compared with unpigmented film; pre-drying the masterbatch at 60–70 °C for 2–3 h is required when storage humidity exceeds 60% RH, because moisture levels above 0.1% generate pinholes and bubble destabilization. Terminal products are black bunker silo covers, silage pit side-sheets, and silo bags, typically at thicknesses of 150–250 µm.

    What Limits Heat-Seal Initiation Temperature in Coextruded Sealant Webs?

    Coextruded sealant webs for liquid packaging position 6109L in the innermost layer because its butene branching lowers the heat-seal initiation temperature relative to high-pressure LDPE while retaining adequate hot-tack strength measured under ASTM F1921. The regulatory framework for this geometry is 21 CFR 177.1520(c) for the olefin polymer and EU No 10/2011 for the finished plastic multilayer article, with compliance determined by overall migration below 10 mg/dm² and specific migration of any additives below their SML values. The sealant layer formulation consists of 60–85 wt% 6109L and 15–40 wt% high-pressure LDPE; a polyolefin plastomer may be added at 5–10 wt% to further depress seal initiation, while slip and antiblock masterbatches are maintained at 0.3–1.0 wt% to prevent blocking of the wound roll. Published heat-seal data specific to 6109L in triple-layer coextrusion are limited; the seal initiation range cited here derives from butene-copolymer LLDPE films with comparable density and melt index under ASTM F88 at 0.5 s dwell and 2 bar jaw pressure. Seal initiation temperatures in these systems typically occur between 85 °C and 105 °C; below that range, coherent seals do not form, and above 130 °C, seal-through distortion damages the outer printed web. The downstream extrusion process uses a three-layer blown film die with gap of 2.0–2.6 mm, blow-up ratio of 2.0:1–2.8:1, melt temperature of 205–230 °C, and sealant layer thickness ratio of 15–25% of total film thickness; oscillating haul-off or 360° reverse rotation is used to distribute gauge bands. Slip additive levels above 0.8 wt% are to be avoided in the sealant layer because migration to hot sealing jaws builds deposit over extended runs and compromises seal integrity. Terminal products are bag-in-box liners for edible oil, dairy, beverage syrups, and liquid food service packaging.

    Where heavy-duty industrial liners are produced on high-stalk blown film lines, the principal process constraints are melt pressure, frost line stability, and extrusion pressure drop across the die. 6109L is used here for its puncture resistance and low-temperature flexibility without requiring over-stabilization for outdoor exposure. Industrial compliance is governed by REACH Regulation (EC) No 1907/2006 Annex XVII and RoHS Directive 2011/65/EU for restricted substances where the liner enters general waste or construction debris streams; mechanical properties are specified under ASTM D882 for tensile, ASTM D1709 for dart impact, and ASTM D1922 for Elmendorf tear. The formulation is kept near-virgin at 80–95 wt% 6109L with 5–20 wt% high-pressure LDPE or clean internally recycled trim; a fluoropolymer process aid masterbatch at 0.2–0.6 wt% is added only when melt fracture occurs at high specific outputs. Extrusion conditions on high-stalk lines include die gap 2.0–3.0 mm, blow-up ratio 2.0:1–3.0:1, stalk height 6–10 die diameters, melt temperature 190–230 °C, and film thickness 100–300 µm. Sustained melt temperatures above 230 °C increase gel formation from oxidized fractions in recycled trim; below 185 °C sharkskin melt fracture becomes visible at high shear rates in the die lip. Terminal products include construction debris bags, chemical shipping liners, building underlay membranes, and heavy-duty side-gusseted sacks.

    When 6109L Is Dry-Blended With High-Pressure LDPE for Collation Shrink Film

    During collation shrink film production, high-pressure LDPE serves as the continuous phase that provides the required free shrink, while 6109L is added as the dispersed modifier to improve tear propagation resistance and puncture resistance on perforated shrink packs. The blend is confined to 20–40 wt% 6109L and 60–80 wt% high-pressure LDPE; at additions of 6109L above 40 wt%, the natural draw ratio increases and the available shrink force at typical tunnel temperatures falls below the level needed to maintain tight bundle geometry. Slip masterbatch is added at 0.3–0.6 wt%, and antiblock is generally omitted to avoid haze in display packaging. Conformance testing is conducted under ASTM D2732 for unrestrained linear thermal shrinkage and ISO 14616:1997 for shrink properties; tensile properties after orientation are measured under ASTM D882. The downstream double-bubble process uses a first-bubble melt temperature of 190–210 °C, a second-bubble orientation temperature of 115–130 °C, machine-direction draw of 4:1–6:1, transverse draw of 4:1–6:1, and final film thickness of 50–100 µm. At orientation temperatures below 110 °C, the blend shows stress-whitening and poor gauge uniformity; above 135 °C, the orientation loses memory and the shrink value drops below specification. Terminal products are multipack shrink bundles for beverage bottles, canned goods, and pet food trays.

    For woven polypropylene sack lamination, 6109L is converted into a thin blown film that is subsequently adhesive-laminated to corona-treated tubular PP fabric as a moisture barrier and print-receptive layer. The relevant industrial compliance for the laminate is REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU; where the sack is intended for food contact, the final structure must also meet 21 CFR 177.1520(c) on the polyethylene layer and EU No 10/2011 on the complete laminate. The blown film layer formulation contains 70–85 wt% 6109L, 15–30 wt% high-pressure LDPE, and 3–8 wt% titanium dioxide masterbatch when opacity and print contrast are required. The film is produced at a die gap of 2.0–2.5 mm, blow-up ratio of 2.0:1–3.0:1, melt temperature of 200–220 °C, and thickness of 40–80 µm; it is then laminated to woven PP fabric using a solventless polyurethane adhesive at a coat weight of 1.5–2.5 g/m². Corona treatment of the woven fabric to a surface energy of at least 38 mN/m is required before lamination; below that threshold, peel adhesion measured under ASTM D1876 falls below 2 N/15 mm and the sack fails during automated filling. Terminal product types are valve sacks and open-mouth sacks for pet food, fertilizer, grain, and mineral powders.

    Free Quote

    Competitive Chevron Phillips 6109L LLDPE Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6109L LLDPE Blown Film Resin is a butene copolymer linear low-density polyethylene supplied as pellets for monolayer and coextruded blown film structures. The grade is commonly referenced within the MarFlex polyethylene family of Chevron Phillips Chemical. The resin is specified at a nominal density of 0.918 g/cm³ under ASTM D1505 or ISO 1183-1:2019, and at a nominal melt index of 1.0 g/10 min under ASTM D1238 at 190°C/2.16 kg or ISO 1133-1:2022. The comonomer is 1-butene, CAS 106-98-9; the polyethylene backbone is described by CAS 9002-88-4. Exact butene content is proprietary and is not reported on the supplier’s technical data sheet.

    Butene incorporation reduces crystalline density by introducing ethyl side branches along the linear polyethylene backbone. These branches are shorter than the C6 and C8 branches present in hexene- and octene-based LLDPE resins. Because a C4 branch contributes less free volume per branch than a C6 or C8 branch, a higher molar comonomer concentration is required to reach the same density. This elevated branch frequency tends to localize short-chain branching at lamellar fold surfaces and reduces the probability of forming stress-transmitting tie chains between adjacent crystals. The practical consequence is a lower ASTM D1709 dart impact value and lower ASTM D5748 puncture resistance than a higher alpha-olefin LLDPE at the same 0.918 g/cm³ density and 1.0 g/10 min melt index.

    Table 1 — Nominal resin properties and representative film properties reported for Chevron Phillips 6109L at standard laboratory conditions
    Property Test standard Reported typical value
    Nominal density ASTM D1505 / ISO 1183-1:2019 0.918 g/cm³
    Nominal melt index ASTM D1238 / ISO 1133-1:2022 at 190°C/2.16 kg 1.0 g/10 min
    Melting peak temperature ASTM D3418 / ISO 11357-3:2018 121–124°C
    Tensile yield MD/TD at 25 µm ASTM D882 11 MPa / 11 MPa
    Ultimate tensile MD/TD at 25 µm ASTM D882 38 MPa / 32 MPa
    Elongation at break MD/TD at 25 µm ASTM D882 800% / 1000%
    Dart drop impact F50 at 25 µm ASTM D1709 Method A 150 g
    Elmendorf tear MD/TD at 25 µm ASTM D1922 12 g / 15 g
    Haze at 25 µm ASTM D1003 12%
    Gloss at 45° ASTM D2457 60

    Why Does Butene Copolymerization Produce a Different Film Property Envelope than LDPE and Metallocene LLDPE?

    Under quiescent crystallization, high-pressure LDPE develops long-chain branching and a broad molecular weight distribution, which contribute to high melt strength and pronounced shear thinning. Chevron Phillips 6109L has a linear backbone with short C4 branches; its extensional strain hardening at typical bubble deformation rates is lower than that of LDPE. Bubble stability in a conventional air ring is therefore reduced, and the film may be more sensitive to frost-line height and ambient air turbulence. Relative to single-site metallocene LLDPE, 6109L often has a broader comonomer distribution and a broader melting range, which can improve processability at the die lip but does not provide the narrow melting behavior required for ultra-fast sealing or very low seal initiation temperature. The ASTM D3418 melting peak of 121–124°C is higher than many mLLDPE grades used for high-speed form-fill-seal applications.

    Compared with LDPE at equivalent density, the linear butene resin gives higher tensile yield and higher ultimate tensile strength under ASTM D882, but optical properties are typically poorer. Haze measured under ASTM D1003 is generally higher than LDPE clarity-film grades, and 45° gloss under ASTM D2457 is lower. The material is therefore specified when moderate toughness and seal integrity outweigh optical clarity. In blends with LDPE, addition of 10–20 wt% LDPE is used on production lines to restore bubble curvature and reduce melt fracture; the trade-off is a reduction in dart impact and tensile strength as LDPE content increases.

    Rheologically, the melt index of 1.0 g/10 min provides sufficient flow for thin-gauge film but limits very high draw rates. The extensional viscosity at typical bubble deformation rates is lower than LDPE, which means the film is less able to suppress thickness variations when upstream gauge bands form. In coextrusion structures, the resin’s viscosity at shear rates typical of the feedblock and die is close to that of other LLDPE grades of similar melt index; however, pairing with low-melt-index HDPE or high-viscosity nylon can produce interfacial instability if the viscosity ratio between adjacent layers exceeds roughly 2:1 at the processing temperature. Die pressure measurements on production lines often show higher pressure for 6109L than for LDPE at equivalent output despite identical melt index, because shear thinning is less pronounced. Capillary rheometry under ASTM D3835 is recommended before specifying a line with marginal motor capacity.

    Melt Temperature, Die Gap, and Air Ring Conditions on Conventional Monolayer Lines

    On grooved-feed extruders with L/D ratios between 24:1 and 30:1, barrel-zone set points are usually maintained from 180°C to 220°C. Die-zone and adapter temperatures are held at 210°C to 230°C. Extended operation above 230°C can increase oxidative gel accumulation on internal die surfaces, particularly in zones with stagnant flow. A die gap of 1.0 mm to 2.0 mm is standard for LLDPE blown film. When the die gap is reduced below 1.0 mm, die-lip shear stress increases and can exceed the critical value for sharkskin melt fracture at practical output rates. Bubble stability is generally lower than that of high-pressure LDPE with equivalent melt index because the linear backbone provides less extensional strain hardening. Blow-up ratios are typically held between 2.0:1 and 3.0:1, and the frost line is set at a distance of approximately 2 to 4 die diameters, depending on air-ring temperature and output.

    Operators running 6109L on 45 mm to 75 mm monolayer lines have reported that reducing the frost line below 2 die diameters can destabilize the bubble at high output rates, especially when ambient temperature exceeds 30°C. Increasing blow-up ratio above 3.0:1 may improve transverse tensile balance but can increase gauge variation and bubble flutter if the tower collapsing frame is not optimized. These are operationally observed boundaries rather than absolute material limits, and they vary with air-ring geometry, die optimization, and cooling-air dew point.

    The pellets do not require drying under normal indoor storage conditions. If pellets are stored at relative humidity above 60% or transferred from cold storage to a warm production area, condensation on the pellet surface can introduce surface moisture. This can produce splay defects and minor gauge variation at high screw speeds. Preheating the hopper to 40–60°C or using a vented feed throat is sufficient to remove surface moisture; hydrolytic degradation of polyethylene is not a concern.

    For food-contact and retail packaging, the base olefin polymer is normally covered under FDA 21 CFR 177.1520(c) in the United States. In the European Union, final articles should be evaluated under EU Regulation (EU) No 10/2011 and the overall migration limit of 10 mg/dm². These regulatory references apply to the base polymer class and do not substitute for migration testing on the finished multilayer film under the intended food simulant and time-temperature condition. REACH registration under EC 1907/2006 and RoHS Directive 2011/65/EU should be confirmed through the supplier’s current safety data sheet and product stewardship statement. The resin is not recommended for continuous exposure above 80°C or for autoclavable medical device packaging, because dimensional stability and additive consumption become limiting beyond that boundary.

    Production applications reported for 6109L include general-purpose liners, garment bags, produce bags, overwrap, and protective packaging where intermediate clarity and moderate impact toughness are acceptable. The grade is also used as a sealing layer in coextruded structures when ASTM F1921 seal initiation behavior is more critical than high dart impact. In high-puncture frozen-food or heavy-duty liquid packaging, hexene- or octene-based LLDPE grades are specified in preference to butene copolymers. Published data for this specific configuration is limited outside the general-purpose blown film envelope, and final fabrication trials should be conducted on the target line because air-ring performance, die gap, and frost-line control can shift the balance between bubble stability and mechanical properties.