Chevron Phillips 6109k Lldpe Blown Film Resin Butene Copolymer

Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 149525
    Product Name Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer
    Manufacturer Chevron Phillips Chemical Company
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Copolymer Type Butene Copolymer
    Density 0.918 g/cm³
    Melt Index 1.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Break Md 29 MPa
    Tensile Strength At Break Td 26 MPa
    Elongation At Break Md 700%
    Elongation At Break Td 800%
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 300 g/mil
    Elmendorf Tear Strength Td 500 g/mil
    Haze 12%
    Gloss 45 60%
    Coefficient Of Friction 0.2

    As an accredited Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer supplied in 25 kg polyethylene-lined bags, 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL loading of palletized 25 kg bags of Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer, securely stowed.
    Shipping Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer is typically shipped as non-hazardous resin pellets in 25 kg polyethylene bags, stacked on pallets and stretch-wrapped, or in bulk trucks/railcars. Store in a cool, dry area away from direct sunlight, heat, and moisture. Follow manufacturer’s SDS and local transport regulations.
    Storage Store Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original containers or bags closed, palletized, and off the floor to prevent moisture pickup and contamination. Avoid excessive stacking, dust generation, and static discharge. Follow manufacturer SDS and local regulations.
    Shelf Life Shelf life: generally indefinite when stored unopened in a cool, dry area away from direct sunlight, heat, and moisture.
    Application of Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer

    On blown-film lines configured for heavy-duty industrial shipping sacks, Chevron Phillips 6109K—a butene-copolymer linear low-density polyethylene with nominal density 0.922 g/cm³ and melt index 0.9 g/10 min at 190 °C/2.16 kg—is processed into monolayer and coextruded sack film at die gaps between 1.8 mm and 2.2 mm. In converter trials, a 70–85 wt% loading of 6109K blended with 15–30 wt% low-density polyethylene is used to raise bubble stability because the low melt strength of the butene copolymer at blow-up ratios above 2.8 can cause fluctuation in frost line height and gauge variation. At film thickness from 120 µm to 200 µm, the addition of 1.0–2.5 phr slip/antiblock masterbatch is applied for controlled coefficient of friction, while 0.3–0.8 phr fluoropolymer processing aid is used to postpone melt fracture on 50 mm grooved-feed extruders with L/D ratios of 30:1.

    Compliance for non-food industrial sacks is anchored to ASTM D1709-16a for dart impact, ASTM D1922-15 for Elmendorf tear propagation, and ISO 527-3:2018 for tensile properties, with incoming resin tested per ASTM D1238-20 for melt flow rate and ASTM D1505-18 for density. Where sacks are used for dangerous goods packaging, drop and stack stability are evaluated under the UN Manual of Tests and Criteria rather than resin-level food-contact standards. Extrusion of 6109K on a 65–90 mm barrier screw at 190–220 °C, with die diameter 250–400 mm and blow-up ratio 2.2–2.8, yields film output of 150–220 kg/h; frost line height is maintained at 6–8 die diameters to balance machine-direction/transverse-direction orientation. The bubble is collapsed through a slatted collapsing frame and gusseted to produce flat or gusseted tubing. After surface treatment to 38–42 mN/m dyne level, the film is converted on side-seal or bottom-seal sack machines.

    Compliance matrix for heavy-duty non-food industrial sack film:

    RequirementMethod / StandardRelevant Output
    Resin melt flow rateASTM D1238-20Mass flow rate at 190 °C/2.16 kg
    Resin densityASTM D1505-18Density at 23 °C
    Dart impact resistanceASTM D1709-16aImpact failure weight
    Elmendorf tear resistanceASTM D1922-15Propagation tear force
    Tensile strength and elongationISO 527-3:2018Machine-direction/transverse-direction stress-strain behavior

    Finished formats include FIBC liners, heavy-duty valve sacks, asphalt and chemical shipping sacks, and pallet hoods. 6109K alone without LDPE has insufficient bubble stability at blow-up ratio above 3.0, and at film gauges below 30 µm the butene branch architecture produces lower tear resistance than hexene- or octene-copolymer LLDPE grades; thin-gauge applications below that boundary are excluded from this scenario.

    What Limits the Frost Line Height Range in Frozen Food Lamination-Grade Monolayers?

    Frozen food lamination-grade films produced with 6109K must satisfy EU Regulation No 10/2011 for overall migration below 10 mg/dm² and specific migration limits for butene-derived oligomers, while FDA 21 CFR §177.1520 applies for olefin polymers in contact with aqueous and fatty foods at low temperatures. The resin is formulated at 60–80 wt% with 20–40 wt% of a 0.918 g/cm³ LDPE or metallocene LLDPE in the core layer of a three-layer A/B/A coextrusion, with 1.0–2.0 phr antiblock masterbatch and 0.5–1.0 phr slip masterbatch in the skin layers. The processing window on a 3-layer blown-film line with a 350 mm die, 1.5 mm die gap, and blow-up ratio 2.0–2.5 requires melt temperature 200–225 °C; if frost line height is set below 4 die diameters, bubble instability and blocking occur. Published converter data for the specific 6109K grade at this exact multilayer structure is limited; the seal range cited is the observed window on a 3-layer line processing a 0.922 g/cm³ butene copolymer. Side-seal jaw temperatures between 95 °C and 110 °C at 0.5 s dwell produce acceptable seal strength, but heat seal initiation is slower than for hexene or octene copolymers at the same density.

    On a production 3-layer line, a repeated failure mode is film blocking on the collapsing frame when internal bubble cooling air temperature drops below 15 °C and ambient humidity exceeds 60% RH due to condensation on the film surface. The extruder configuration uses 50–70 mm grooved-feed screws with L/D 30:1 and a 400 mm die; output is held at 180–250 kg/h to prevent frost line movement. Terminal products include bags for frozen vegetables, seafood pouches, pre-formed pouch stock, and ice cream packaging. This structure is not used for boil-in-bag or retort applications because the butene copolymer seal layer lacks sustained hot-tack above 110 °C.

    Where silage pile covers must withstand UV exposure for 18–24 months, 6109K is blended with 5–15 wt% of a 0.924 g/cm³ low-density polyethylene or a C6 linear low-density polyethylene to improve melt strength during bubble formation at blow-up ratios of 2.0–2.6. The formulation includes 2–5 phr HALS-based UV stabilizer masterbatch and, for black or white films, 3–6 phr carbon black or titanium dioxide masterbatch. Compliance for agricultural cover films is governed by EN 13206:2017; oxygen barrier claims are not made for monolayer polyethylene because oxygen transmission measured per ASTM D3985-17 remains above the threshold required for silage fermentation control, so coextrusion with EVOH or polyamide is required where oxygen barrier is specified. REACH Annex XVII restricts cadmium-based pigments and certain phthalate plasticizers in these formulations.

    Extrusion of silage cover film uses a 2.0–2.4 mm die gap, melt temperature 190–220 °C, and blow-up ratio 2.0–2.6; film thickness ranges from 25 µm for low-tunnel covers to 150 µm for silage pit covers. On a 90 mm barrier-screw extruder with L/D 30:1 and a 400 mm die, output rates of 300–400 kg/h are achievable, but the addition of UV stabilizer masterbatches reduces melt strength and requires frost line height to be lowered by 1–2 die diameters relative to unstabilized film. Terminal product types include clamp silage covers, ensilage pit liners, low-tunnel greenhouse films, and mulch film substrates. Without adequate UV stabilization, the film embrittles after a single season; 6109K should not be specified for long-term exterior geomembrane or pond-liner service.

    Stretch Hooder Film and the Thickness Uniformity Threshold on Rotating-Die Blown Lines

    On stretch hooder pallet-load containment equipment, 6109K is extruded as 80–120 µm monolayer blown film where thickness uniformity across the bubble must remain within ±4% to prevent uneven stretching around pallet corners. The formulation is 85–95 wt% 6109K with 5–15 wt% LDPE to raise melt strength, plus 0.5–1.0 phr slip/antiblock masterbatch and 0.5–1.5 phr UV stabilizer masterbatch for outdoor pallet storage. Compliance for mechanical properties follows ASTM D882-18 for tensile, ASTM D1709-16a for dart impact, and ASTM D1922-15 for tear propagation, with density and melt flow rate checked per ASTM D1505-18 and ASTM D1238-20.

    Blown-film processing uses a rotating die with diameter 400–600 mm, die gap 2.0–2.2 mm, blow-up ratio 2.0–2.5, and melt temperature 200–230 °C. The die rotates at 0.5–1.0 rpm to randomize gauge bands; output on a 90 mm extruder with L/D 30:1 is held at 180–250 kg/h. Terminal products include industrial pallet hooder film, protective film for tall palletized loads, and outdoor storage covers. Operational boundary: at film thickness below 60 µm, the film has insufficient tear resistance at pallet corners during high-speed hooder application.

    Because dry food and detergent pouches require a sealant web that seals at 105–120 °C at 0.5 s without distorting printed PET outer layers, 6109K is extruded as a 15–30 µm sealant web on tandem extrusion lamination lines; the resin component is used at 100 parts per hundred resin, with 1.0–2.0 phr antiblock masterbatch and 0.5–1.0 phr slip masterbatch because a laminating adhesive bonds to the corona-treated surface at 38–42 mN/m. Lamination-grade film compliance follows EU Regulation No 10/2011 for overall migration and FDA 21 CFR §177.1520 for olefin polymers; the adhesive system must independently comply with 21 CFR §175.105. Blown-film processing on a 1.5–2.0 mm die gap, blow-up ratio 2.0–2.5, and melt temperature 190–225 °C is used before adhesive lamination to BOPP, PET, or metallized PET. The low seal initiation of butene LLDPE minimizes deformation of the printed substrate during sealing.

    The production limitation is that 6109K exhibits limited hot tack above 110 °C compared with octene-based grades, causing seal creep during vertical form-fill-seal at speeds above 60 packs/min; converters often blend 20–30 wt% metallocene LLDPE for hot tack. Terminal product types include stand-up pouches, detergent sachets, dry mix pouches, and snack packaging. Excessive slip additive above 1500 ppm erucamide is avoided because migration to the adhesive interface reduces laminate bond strength.

    When Temporary Construction Vapor Barriers Must Outperform Standard LDPE in Dart Drop Resistance

    Temporary construction vapor retarder films made from 6109K are used where ASTM E1745-17 Class A requires water vapor permeance below 0.1 US perms. The film is extruded as a monolayer at 150–250 µm thickness with 2.0–2.5 phr carbon black masterbatch and 1.0–2.0 phr processing antioxidant masterbatch. Formulation is 95–100 wt% 6109K; up to 5 wt% LDPE is added to raise melt strength at thick gauge. Processing uses blown-film extrusion with a 2.4 mm die gap, blow-up ratio 1.8–2.2, melt temperature 200–230 °C, and high-capacity air ring cooling. Water vapor permeance is measured per ASTM E96/E96M-16 desiccant method, and dart impact per ASTM D1709-16a.

    Production-scale observations on 90 mm extruders with L/D 30:1 show that output is reduced by 30–40% relative to 50 µm film at the same melt temperature because thick-gauge bubble cooling becomes the limiting factor. The bubble collapse and flattening section must use rollers set below 40 °C to avoid blocking. Terminal products include crawl space vapor barriers, temporary floor protection films, concrete curing covers, and below-slab moisture barriers. 6109K is not suitable for permanent below-grade waterproofing membranes where hot-welded seams and long-term hydrostatic resistance are specified; those applications require HDPE or composite membranes.

    Free Quote

    Competitive Chevron Phillips 6109K LLDPE Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6109K is a linear low density polyethylene blown film resin produced with butene as the alpha-olefin comonomer. The commercial designation places it in the butene-copolymerized LLDPE class, which differs from hexene and octene LLDPE grades because the shorter butene branch produces a different balance of melt rheology, dart impact, tear resistance, and seal initiation. The nominal melt flow rate is 0.9 g/10 min measured by ASTM D1238-20 at 190°C with a 2.16 kg load. The nominal density is 0.918 g/cm³ measured by ASTM D1505-18. Lot-to-lot density variation of ±0.001 g/cm³ is common for this resin class. Melt flow rate may also be reported under ISO 1133-1:2022 procedure A at the same temperature and loading. The resin is supplied in pellet form. Additive loading, such as slip or antiblock, is lot-specific and must be confirmed on the certificate of analysis. The comonomer content is not typically disclosed as a numerical specification; the butene-derived short-chain branching is inferred from the density, melting profile, and mechanical response. Published data for this specific commercial grade is limited in some high-output multilayer configurations, and the processing boundaries below are therefore derived from typical behavior of 0.918 g/cm³ butene-copolymerized LLDPE blown film resin.

    Film extruders converting this resin on conventional monolayer blown film lines generally use a grooved-feed extruder with a barrier screw. On a 40 mm or 50 mm single-screw extruder with an L/D ratio of 24:1 to 30:1, the barrel temperature profile is typically set from 160°C in the feed zone to 190°C in the metering zone. The adapter is maintained at 205°C to 210°C, and the die zones are set at 210°C to 220°C. Melt temperatures below 190°C can result in insufficient homogenization and sharkskin at the die lip. Melt temperatures above 225°C are unnecessary for this resin and can reduce bubble stability by lowering melt strength. Pre-drying is not required for LLDPE under normal indoor storage. If surface moisture has condensed from storage at high relative humidity above 60%, a hopper dryer at 60°C for 2 h is sufficient to remove surface water.

    What Limits Stable Bubble Geometry in Thin-Gauge Blown Film?

    The controlling processing conflict for 6109K at gauges below 25 µm is the interaction between die lip shear rate, melt temperature, frost line height, and cooling air velocity. Butene-copolymerized LLDPE has lower melt strength than LDPE and less strain hardening than high-pressure LDPE, so the bubble tends to oscillate when the frost line is raised above 450 mm at a 2.5:1 blow-up ratio. Field observations on monolayer production lines indicate that reducing the frost line to 250–350 mm and increasing die lip temperature by 5°C can restore gauge uniformity when dart impact begins to fall. The die gap should be held between 1.5 mm and 2.0 mm. A 1.0 mm die gap increases wall shear rate and may initiate sharkskin. A 2.5 mm die gap reduces transverse orientation and lowers transverse-direction Elmendorf tear.

    At 12 µm film thickness, the process window narrows to approximately ±5°C around a 210°C die target. Outside this band, thickness variability measured by an on-line capacitance gauge can exceed ±7%. Under those conditions, dart impact measured by ASTM D1709-16a Method A can decrease to 50–60 g. When a converter without internal bubble cooling attempts to maintain a stalk height above 400 mm, bubble flutter becomes more probable. With internal bubble cooling, the frost line can be extended to 400 mm while retaining stable bubble geometry. Without internal bubble cooling, the recommended upper frost line is 350 mm.

    Blending with 10–20 wt% low-density polyethylene improves bubble stability and increases melt strength. The trade-off is a reduction in dart impact and Elmendorf tear in proportion to the LDPE addition. Head pressure at constant screw speed may change by 5–15% during the blend transition because of viscosity differences between the two materials. Edge trim regrind addition should be limited to 20% or less to control gel formation and optical loss. If coefficient of friction must remain between 0.15 and 0.25 under ASTM D1894-14, the slip additive concentration should be verified on the certificate of analysis, because pellet-to-pellet additive variation and storage time can shift the coefficient of friction by 0.05 units or more.

    Tensile, Tear, Optical, and Seal Property Benchmarks

    The representative film property envelope for 6109K is shown in the table below for 25 µm monolayer film produced at a 2.5:1 blow-up ratio, 2.0 mm die gap, and 210°C melt temperature. These values are typical lot data, not contractual sales specifications.

    Representative film property envelope for Chevron Phillips 6109K at 25 µm thickness
    Property Test Method Nominal Value or Range
    Density ASTM D1505-18 0.918 g/cm³
    Melt flow rate ASTM D1238-20 0.9 g/10 min
    Dart impact F50 ASTM D1709-16a Method A 90–110 g
    Elmendorf tear MD ASTM D1922-15a 200–250 g
    Elmendorf tear TD ASTM D1922-15a 450–550 g
    Tensile strength at break MD ASTM D882-18 40–50 MPa
    Tensile strength at break TD ASTM D882-18 30–40 MPa
    Elongation at break MD ASTM D882-18 700–900%
    Elongation at break TD ASTM D882-18 850–1000%
    Haze ASTM D1003-13 12–16%
    Gloss at 45° ASTM D2457-13 50–65
    Vicat softening temperature ASTM D1525-17e1 90–95°C

    Differences in laboratory film preparation equipment can shift these values by 10–15%. In particular, dart impact values obtained on a cast-film lab unit may not reproduce the orientation state of blown film produced on an in-line 40 mm extruder. Certification limits must be obtained from the supplier technical data sheet for the specific lot.

    In heat sealing, the resin shows the characteristic low seal initiation of butene LLDPE relative to hexene LLDPE. On a 25 µm monolayer film, a seal strength of 4–6 N/15 mm is generally reached at 95–105°C when tested according to ASTM F88/F88M-21 with 0.5 s dwell and 0.275 MPa jaw pressure. Plateau seal strength is commonly 7–9 N/15 mm from 115°C to 130°C. At jaw temperatures above 135°C, seal failure becomes governed by film deformation rather than interfacial fusion. This is a practical upper boundary for form-fill-seal equipment running thin-gauge films.

    When a Butene Copolymer Replaces Hexene LLDPE in Flexible Packaging

    Selection of 6109K over a hexene-copolymerized LLDPE at equivalent melt index and density is driven by the shorter branch length of butene. Butene-derived short-chain branches create more frequent but less efficient tie-chain interactions, which lower dart impact and Elmendorf tear relative to hexene grades. At 25 µm, a typical hexene LLDPE of 0.918 g/cm³ and 0.9 g/10 min may provide dart impact values 30–50% higher and transverse-direction Elmendorf tear 20–40% higher than the butene resin at the same gauge. The butene copolymer is substituted in applications where the lower toughness remains within specification and where raw-material cost per kilogram is the primary selection variable.

    Compared with LDPE, 6109K provides higher tensile strength at break and higher dart impact at equivalent gauge, but lower melt strength and lower optical gloss. Blown film converters therefore use it in structures where tensile properties are more important than clarity. Compared with metallocene LLDPE, the resin processes with lower shear heating and may be more tolerant of older die designs, but it does not match the toughness and optical performance of metallocene grades at equivalent density. In coextruded film, 6109K can be placed in a core or skin layer. If used as a skin layer, the additive package must be checked for surface bloom; haze may increase by 2–4% after 48 h at 40°C because of additive migration within the polymer matrix.

    Film structures made from 6109K are found in industrial liners, consumer packaging, produce bags, ice bags, and light-duty carrier bags. In a 50 µm industrial liner processed at a 2.5:1 blow-up ratio, dart impact typically falls in the 200–250 g range and transverse-direction Elmendorf tear exceeds 900 g. These values are suitable for dry-goods packing where the service environment does not exceed 60°C. Continuous service above 60°C is outside the normal use envelope for this resin without an additional thermal stabilization review.

    For food-contact use, the supplier typically provides a compliance letter referencing 21 CFR 177.1520(c) for olefin polymers, subject to extractives limits in that section. For European Union applications, the finished article must meet the overall migration limit of 10 mg/dm² specified in Regulation (EU) No 10/2011, Annex I. Specific migration of slip and antiblock additives must be verified on the final packaging structure because migration kinetics depend on film thickness, time, and temperature. REACH obligations under Regulation (EC) No 1907/2006 apply to the monomers and additives; the polymer itself is exempt from registration as a polymer, but the supplier must provide substance information for the monomer residues when required. The raw polyolefin is not inherently within the scope of RoHS Directive 2011/65/EU heavy-metal restrictions, but homogeneous material testing is required after additive incorporation if the final article is placed on the European market.

    Top