Chevron Phillips 6109fk Linear Low Density Polyethylene Blown Film Resin

Chevron Phillips 6109FK Linear low density polyethylene blown film resin

    • Product Name: Chevron Phillips 6109FK Linear low density polyethylene blown film resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 486145
    Density 0.918 g/cm³
    Meltindex 0.9 g/10 min
    Comonomer Butene-1
    Meltingpoint 122 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatbreakmd 3800 psi
    Tensilestrengthatbreaktd 3300 psi
    Elongationatbreakmd 600 %
    Elongationatbreaktd 700 %
    Onepercentsecantmodulusmd 28000 psi
    Onepercentsecantmodulustd 32000 psi
    Dartimpact 120 g
    Elmendorftearmd 250 g
    Elmendorfteartd 450 g
    Haze 12 %
    Gloss45degree 55 %
    Coefficientoffriction 0.2
    Blocking 80 g

    As an accredited Chevron Phillips 6109FK Linear low density polyethylene blown film resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing For Chevron Phillips 6109FK: packaged in 25 kg (55 lb) polyethylene bags, 35 bags per pallet (875 kg), stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL loaded with Chevron Phillips 6109FK LLDPE blown film resin in 25 kg bags, palletized, shrink-wrapped, and securely stowed.
    Shipping Chevron Phillips 6109FK LLDPE blown film resin is typically shipped as non-hazardous polyethylene pellets in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars. Keep packages dry, clean, and sealed; transport in covered vehicles, avoiding excessive heat, moisture, and contamination. Follow the SDS and local regulations.
    Storage Store Chevron Phillips 6109FK Linear low density polyethylene blown film resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed to prevent moisture, dust, and contamination. Stack pallets securely to avoid package damage. Protect from prolonged UV exposure and follow first-in, first-out rotation and local storage regulations.
    Shelf Life Chevron Phillips 6109FK LLDPE blown film resin shelf life: indefinite if stored sealed, cool, dry, away from sunlight and heat.
    Application of Chevron Phillips 6109FK Linear low density polyethylene blown film resin

    Conversion of 6109FK into heavy-duty industrial liners is typically carried out on monolayer blown film lines equipped with a 55 mm to 75 mm single-screw extruder at an L/D ratio between 24:1 and 30:1. The screw is commonly a barrier design with a Maddock mixing element to restrict melt-temperature overshoot above 225 °C, which would otherwise initiate oxidative gel formation and reduce dart impact. Melt discharge measured at the die adapter is held at 190 °C to 220 °C, with a die head set to 1.8 mm to 2.2 mm die gap and a 250 mm to 400 mm die diameter. A blow-up ratio of 2.4:1 to 2.8:1 and a frost-line height of 6 to 8 die diameters are used to balance machine-direction tear against transverse-direction tear while retaining bubble stability on older air-ring systems. Processors append 5 wt% to 15 wt% of a higher-melt-index LDPE or 10 wt% to 20 wt% of clean edge-trim regrind to improve bubble symmetry, provided the regrind fraction is free of high-gel contamination from degraded polyolefins. The terminal articles are 40 µm to 125 µm embossed or smooth film converted into drum liners for 208 L steel and fibre drums, FIBC liners, and box liners for bulk solid chemicals. Mechanical acceptance is confirmed by dart impact according to ASTM D1709-16a Method A, Elmendorf tear according to ASTM D1922-15, and puncture resistance according to ASTM D5748-19. Industrial liners filled with non-hazardous solids do not invoke direct food-contact obligations; however, when the liner is placed into transport packaging for hazardous materials, the assembled package must meet the UN Model Regulations performance tests appropriate to the packing group. In multi-layer constructions, a 6109FK-rich core can be coextruded with a thin HDPE or LDPE skin to modify slip without sacrificing dart impact, but the skin layer fraction is normally kept below 30% so that the LLDPE core controls tear propagation and drop resistance.

    What Stabilises a 25 µm Silage Cover Against Oxygen Ingress and UV Embrittlement?

    For agricultural silage covers and low-tunnel greenhouse cladding, 6109FK is blown into wide sheeting at 25 µm to 150 µm thickness on lines equipped with internal bubble cooling and a dual-lip air ring. The formulation requires a hindered amine light stabiliser package, typically at 0.20 wt% to 0.60 wt% of a compounded HALS masterbatch plus 0.05 wt% to 0.20 wt% of an antioxidant synergist, although the exact let-down ratio is determined by the target service life under ISO 4892-2:2013 accelerated weathering against a reference unstabilised film. White or chalk masterbatches are partially incorporated at 8 wt% to 12 wt% to reduce solar heat gain and increase opacity for silage clamp layering. Extrusion conditions are held at 210 °C to 230 °C melt temperature with a 70 mm extruder, 30:1 L/D, and a 350 mm die, using a blow-up ratio of 2.8:1 to 3.0:1. The terminal product is a 6 m to 8 m layflat silage cover, frequently specified for one full field season in northern European and North American conditions. Oxygen transmission is measured on the barrier film according to ASTM D3985-17 at 23 °C and 0% RH, while water vapour transmission is measured according to ASTM F1249-20 at 38 °C and 90% RH; the latter is used to confirm that the cover limits moisture ingress into silage clamps. Under EU legislation, agricultural covering films fall within the scope of EN 13206 for thermoplastic films used in agriculture and horticulture, while REACH Registration under Regulation (EC) No 1907/2006 applies to the resin itself. Processors report that bubble instability at high HALS let-downs is controlled by reducing frost-line height to 5 die diameters and adding 2 wt% to 4 wt% LDPE; failure to do so generates visible chatter marks in the layflat and increases local thickness variation beyond ±8%. Additives based on pro-oxidant transition-metal complexes should be avoided in this application because they compromise the intended multi-season UV performance.

    Under direct-contact frozen food packaging conditions, 6109FK is converted into 40 µm to 80 µm blown film bags for individually quick-frozen vegetables, seafood, and baked goods. The film is processed at the lower end of the LLDPE melt-temperature window, 175 °C to 195 °C, to limit oxidative degradation products that can raise hexanal and total volatile off-flavour concentrations. Extruder diameters between 45 mm and 60 mm with a barrier screw and L/D of 25:1 to 28:1 are common, and a blow-up ratio of 2.0:1 to 2.4:1 with a die gap of 1.5 mm to 1.8 mm provides the required balance between dart impact and machine-direction tear on fast bag-winding lines. A 10 wt% to 20 wt% addition of a higher-MI LLDPE or LDPE lowers bubble pressure and improves gauge uniformity down to ±5%, while slip and antiblock are introduced as 5 wt% to 8 wt% masterbatch to reduce the coefficient of friction to 0.2 to 0.4 as measured by ISO 8295:1995. The terminal articles are pillow pouches and side-seal bags used for frozen retail packaging. For the US, the resin must comply with 21 CFR 177.1520 as an olefin polymer under conditions of use A through H; for the EU, the finished article must comply with Regulation (EU) No 10/2011 and the overall migration limit of 10 mg/dm² using food simulant E for frozen conditions. Sealing parameters on VFFS lines are typically 140 °C to 165 °C jaw temperature and 0.3 s to 0.5 s dwell, with hot tack measured by ASTM F1921-12 to confirm package integrity before the frozen product drops through the forming tube. Processors note that melt temperatures above 195 °C in this gauge range can reduce seal initiation window and increase trim regrind odour, while melt temperatures below 175 °C can produce visible unmelts and high back-pressure on small extruders.

    If a Sealant Web Is Coextruded with PA or EVOH for Woven-PP Lamination

    In extrusion lamination to woven polypropylene or polyester woven sacks, 6109FK is used as the blown sealant web rather than the coating resin. A three-layer coextruded blown film may consist of a 15 µm to 25 µm 6109FK sealant layer, a 4 µm to 6 µm tie resin layer, and a 10 µm to 15 µm PA or EVOH layer; the overall layflat is then thermally laminated to a woven PP substrate using a dedicated laminating nip. The sealant-layer thickness fraction should remain between 25% and 40% of the total film so that seal initiation temperature is dominated by the LLDPE phase and not by the higher-melting barrier layer. Processing on a three-layer blown film die with 1.8 mm die gap and 250 mm die diameter requires separate extruder temperature profiles: 180 °C to 200 °C for the 6109FK layer, 220 °C to 240 °C for the polyamide or EVOH layer, and 200 °C to 220 °C for the tie resin. The frost line is held high, at 8 to 10 die diameters, to prevent interlayer instability between the semi-crystalline barrier and the sealant. The terminal article is a pet food, fertiliser, or cement sack with an inner PE/EVOH liner that provides moisture and oxygen resistance after repeated drop cycles. For food-contact applications, the sealant resin must satisfy 21 CFR 177.1520 and Regulation (EU) No 10/2011 Annex I, while the complete structure must meet the applicable overall migration limit of 10 mg/dm² according to EN 1186-1:2002. Seal strength before and after lamination is tested according to ASTM F88/F88M-21, with a minimum target set by the brand owner; published data for 6109FK in this exact coextrusion configuration is limited, so line qualification is required. The most common failure mode observed on production-scale equipment is sealant-layer delamination at the tie-resin interface, which is addressed by raising the tie-resin melt temperature within the supplier-specified window and increasing the lamination nip pressure until peel interface separation disappears.

    Downstream conditionNormative anchorTest property
    Heavy-duty industrial linerASTM D1709-16a Method ADrop dart impact
    Agricultural silage coverISO 4892-2:2013Accelerated weathering
    US direct food contact21 CFR 177.1520Olefin polymer compliance
    EU direct food contactRegulation (EU) No 10/2011Overall migration
    Lamination sealant webASTM F88/F88M-21Seal strength
    Collation shrink filmASTM D2732-14Free shrink

    Collation Shrink Force and Machine Direction Orientation Limits

    Collation shrink film is converter-blown at 35 µm to 60 µm thickness from a 70:30 to 80:20 dry blend of 6109FK and a high-shrink LDPE; the LDPE fraction increases machine-direction shrink and lowers seal-jaw temperature, while the LLDPE fraction contributes puncture resistance during bottle transport. Extruder size is typically 55 mm to 65 mm, L/D 24:1 to 30:1, with a die gap of 1.8 mm and a blow-up ratio of 3.0:1 to 3.5:1. Melt temperature is held between 190 °C and 205 °C with a control band of approximately ±5 °C to prevent oxidation that would increase haze and reduce shrink force. Free shrink is measured according to ASTM D2732-14 in both machine and transverse directions; blown structures based on this resin class typically develop 20% to 30% shrink at 120 °C, with the majority in the transverse direction unless a high-stalk bubble is employed. The terminal article is a clear printed film for bundling 6-pack and 12-pack beverage bottles, where shrink must occur without crushing lightweight aluminium cans or distorting PET bottle sidewalls. Because the film is secondary packaging and not intended for direct food contact, it is subject to general packaging requirements rather than food-contact migration; in the EU, Regulation (EC) No 2023/2006 on good manufacturing practice for food contact materials applies only where the film could contact food during unit loading. Processors observe that shrink-film slitting on high-speed winders above 150 m/min can create edge-trim static that induces blocking when slip levels are below 0.05%; antistatic masterbatch is therefore added at 1 wt% to 2 wt% on operations running continuous slitting without a static bar.

    When vertical form-fill-seal conversion of 50 µm to 90 µm pouches for dry beverage mixes, sugar, and powdered soups is required, 6109FK is processed as a monolayer web with an addition of 5 wt% to 10 wt% of a slip/antiblock masterbatch and, when necessary, 8 wt% to 12 wt% of a titanium dioxide white masterbatch for opacity and shelf impact. The extrusion line uses a 50 mm single-screw extruder with L/D 25:1, a 300 mm die, and a die gap of 1.8 mm; melt temperature is held at 190 °C to 215 °C to avoid viscosity loss that would cause surge in the downstream bubble cage. A blow-up ratio of 2.2:1 to 2.6:1 is selected so that the film yields balanced tear after puncture by sharp sugar crystals. The formed pouches are run on vertical form-fill-seal machines at speeds of 60 to 90 packages per minute, with seal jaw temperature 140 °C to 170 °C and dwell 0.25 s to 0.45 s. Heat seal strength is checked according to ASTM F88/F88M-21, and hot tack is evaluated according to ASTM F1921-12 at 100 °C sealing temperature. Compliance for US food contact relies on 21 CFR 177.1520; for the EU, the finished pouch must comply with Regulation (EU) No 10/2011 overall migration limit of 10 mg/dm² and the specific migration limits for any additives used in the slip and pigment masterbatches. The terminal article is the filled pouch sold as a dry-goods pack. Published data for the specific film gauge on high-speed vertical form-fill-seal machines is limited; converters commonly qualify the web on the target machine to confirm hot-tack and seal-through-contamination performance when fine powder deposits form on the seal area.

    Free Quote

    Competitive Chevron Phillips 6109FK Linear low density polyethylene blown film resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6109FK Linear low density polyethylene blown film resin is a 1-hexene copolymer supplied in pellet form for monolayer and coextruded blown film structures. The nominal density is 0.918 g/cm³ when measured by ASTM D1505. The nominal melt index is 0.90 g/10 min at 190 °C under 2.16 kg load using ASTM D1238. The additive package typically contains slip and antiblock agents. The grade is intended for heavy-duty shipping sacks, industrial liners, freezer films, agricultural silage film, carrier film, and lamination webs. It is not formulated for injection molding, rotational molding, or cast extrusion processes where capillary instability and draw resonance differ from blown film operation.

    Density and melt index are lot-release parameters; other film properties are not product specifications and vary with blow-up ratio, die gap, frost-line height, and downstream converting conditions. The current lot certificate and product data sheet should be obtained from the manufacturer before qualification.

    Why Is 1-Hexene Comonomer Selected Over 1-Butene for Heavy-Duty Film?

    In LLDPE solid-state deformation, branch length controls the probability of forming tie chains between adjacent lamellae. A 1-butene branch is shorter and more easily included in the crystal lattice, whereas a 1-hexene branch is more efficiently rejected during crystallization, increasing the tie-chain concentration at equivalent density. At the same 0.918 g/cm³ density and 0.90 g/10 min melt index, 6109FK generally offers higher dart impact strength and improved Elmendorf tear retention than butene-based LLDPE film of comparable gauge. Converter evaluations typically assess dart impact at 25 µm by ASTM D1709 and tear by ASTM D1922. Published film property data for this exact grade under all converting conditions is limited; therefore, the comparison must be verified on the intended production line. The lower melting peak of hexene-based LLDPE also permits a reduced heat-seal initiation temperature relative to some butene grades, but final sealing temperature must be determined on the packaging line using ASTM F88 seal strength testing and a calibrated dwell-time profile.

    Relative to metallocene LLDPE of similar density and melt index, 6109FK exhibits a broader molecular weight distribution typical of Ziegler-Natta slurry-loop polymerization. This broader distribution reduces shear viscosity at film extrusion rates and improves bubble stability on conventional low-backpressure dies; it also generally increases haze and raises seal initiation temperature compared with narrow-distribution metallocene resins. The product is therefore selected for processability on standard blown film lines rather than for maximum optical clarity or ultra-low heat-seal thresholds. Capillary rheometry data at 190 °C are available from manufacturer technical literature; when such data are unavailable, a melt index ratio measured at 10.0 kg load versus 2.16 kg load can serve as a processability proxy. A higher melt-flow ratio indicates broader molecular weight distribution and greater shear sensitivity. The selection of 6109FK over a metallocene LLDPE of equal density is often influenced by lower extruder amperage and head pressure at the same screw speed; however, the same feature lowers pinning strength and may require a higher frost line or higher air-ring velocity.

    On a production-scale blown film line using a 90 mm grooved-feed extruder with a 24:1 L/D barrier screw and a 250 mm annular die, 6109FK is typically extruded at melt temperatures from 190 °C to 230 °C. Die gap settings from 1.5 mm to 2.5 mm and blow-up ratios from 2.0 to 3.0 are common starting conditions. The die lip set point may be maintained 5 °C to 10 °C above the adapter temperature to offset pressure drop across the die. Air-ring air temperature is typically held between 10 °C and 20 °C, with frost-line height adjusted to 2 to 5 die diameters above the die face. The resin does not require pre-drying under normal handling; however, if surface condensation occurs on cold pellets at relative humidity above 60% with pellet temperature below the dew point, the pellets should be conditioned to ambient temperature before hopper loading. Residence time above 250 °C should be avoided to minimize gel formation and additive degradation. Purging with low-density polyethylene of similar melt index or a commercial purging compound is recommended before shutdown and after processing high-viscosity resins. During start-up, melt fracture can be controlled by widening the die gap or adding a fluoropolymer processing aid; changes to the additive package should be verified for film surface coefficient of friction.

    Screw designs with excessive shear heating should be avoided because wall shear rate in a 90 mm extruder at 80 rpm typically falls in the range of 100 s−1 to 1000 s−1, depending on channel depth. At these shear rates, viscous dissipation can raise melt temperature above the set zone by 5 °C to 15 °C. Melt temperature should be monitored with an immersion probe rather than relying on zone set points alone. A screen pack with 40/60/80 mesh is common for film-grade LLDPE to trap contaminants without excessive pressure drop. If head pressure exceeds 40 MPa, the screen pack should be inspected because high pressure may indicate gel accumulation or a partially blocked breaker plate.

    When Internal Bubble Cooling Is Applied to High-Stalk Film Production

    In high-stalk film production, internal bubble cooling increases the stabilizing effect of the stalk and permits higher throughput, but it also reduces cooling time before the frost line. Typical IBC settings for 6109FK include a bubble internal pressure of 20 Pa to 40 Pa above ambient and an air exchange rate above 1.5 m³/min per 100 mm of die diameter. The stalk height is usually held between 4 and 7 die diameters. Higher stalk orientation increases machine-direction tensile yield and machine-direction Elmendorf tear while reducing transverse direction tear. If blow-up ratio falls below 2.0, the resulting anisotropy can produce cross-direction tear failure in heavy-duty sacks and uneven slip distribution. Roll blocking may occur because the slip additive requires post-extrusion migration of 24 h to 72 h before the coefficient of friction stabilizes. Gauge uniformity should be measured with a non-contact capacitance gauge across the layflat; localized thickness variation greater than ±5% from the target requires adjustment of the air-ring damper or IBC exhaust. Published data for this specific configuration is limited, but the polymer architecture indicates that the hexene branch length inhibits the quench-induced cracking observed in some butene-rich LLDPE formulations.

    Compared with low density polyethylene, 6109FK has lower melt strength and higher draw-down capacity, which is favorable for thin-gauge film but requires internal bubble cooling to counter bubble instability. Compared with high-density polyethylene, the 0.918 g/cm³ density reduces modulus, tensile yield, and moisture barrier, but increases dart impact and puncture resistance. These differences are quantified by ASTM D882 and ASTM D1709, respectively. Converting 6109FK on an HDPE line without adjusting die gap or screw profile may result in melt fracture and low melt strength due to the higher shear sensitivity of linear low density polyethylene.

    Critical Film Property Thresholds and Compliance Endpoints

    Film property measurements for 6109FK must be treated as fabrication-dependent. Density and melt index are lot-release parameters; film optical and mechanical properties are affected by stalk height, frost line, blow-up ratio, die gap, and additive migration. Acceptable mechanical levels should be established by the converter using capability studies on the specific film line. Standard test methods applicable to 6109FK film include ASTM D882 for tensile properties, ASTM D1922 for Elmendorf tear, ASTM D1709 for dart impact, ASTM D1003 for haze, and ASTM D2457 for gloss at 60°. Coefficient of friction is measured by ASTM D1894 after a defined conditioning period because slip migration is time-dependent.

    Regulatory areaReferenceCondition and boundary
    United States food-contact base polymer21 CFR 177.1520Finished article is subject to end-use migration testing and food-type simulation.
    European Union food-contact overall migrationEU 10/2011Overall migration limit 10 mg/dm² for the finished article.
    European packaging metals restrictionEU 94/62/ECAggregate Pb, Cd, Hg, Cr(VI) not to exceed 100 mg/kg.
    European REACH registrationEU 1907/2006Registration status and use tables are product-specific; verify the current safety data sheet.
    United States resin release testsASTM D1505, ASTM D1238Nominal density 0.918 g/cm³; nominal melt index 0.90 g/10 min at 190 °C/2.16 kg.

    For flexible intermediate bulk container liners and heavy-duty shipping sacks, 6109FK is processed into film gauges from 50 µm to 150 µm. The resin’s hexene-based branch structure and slip/antiblock package provide coefficient-of-friction control during filling and palletization. In freezer film, low-temperature dart impact resistance is combined with heat-sealing performance; converters often blend 6109FK with LDPE to improve optical properties and melt strength, accepting a reduction in tear resistance. In agricultural silage film, blends with metallocene LLDPE are used to balance puncture resistance measured by ASTM D5748 with retained stretch and tear propagation. Published data for this specific blend configuration is limited; qualification must be performed on the target silage wrapper because film tension, pre-stretch ratio, and seal quality determine field performance. The product is not recommended for applications requiring high clarity because the slip/antiblock package and broad molecular weight distribution produce haze levels above those of high-clarity metallocene or LDPE film grades.

    For workplace handling, the product is supplied as pellets with negligible residual monomer. The safety data sheet identifies mechanical slip, dust explosion, and thermal decomposition products as primary process risks. Ventilation should control airborne waxes and decomposition products below occupational exposure limits. When the resin is purged from a die, the purge should be cooled before handling to prevent skin contact with hot polymer. 6109FK should not be directly mixed with HDPE in high proportions without recalibrating die gap and blow-up ratio; high-density polyethylene can lower dart impact and increase modulus, producing stretch failure in lamination. Storage in direct sunlight or at temperatures above 40 °C for extended periods should be avoided because additive bloom and oxidation may alter coefficient of friction and color. Pellets should be kept free of fines and angel hair from high-velocity conveying; these can appear as gels or fisheyes in film. The lot-to-lot additive level should be verified by requesting the certificate of analysis, particularly for slip and antiblock concentrations, if the film is used on high-speed form-fill-seal equipment.