Chevron Phillips 6109dk Lldpe Blown Film Resin Butene Copolymer

Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 208667
    Manufacturer Chevron Phillips Chemical
    Product Name Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Resin Form Pellets
    Density 0.919 g/cm3
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1400 psi
    Tensile Strength At Break Md 4000 psi
    Tensile Strength At Break Td 3500 psi
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    1 Secant Modulus Md 27000 psi
    1 Secant Modulus Td 31000 psi
    Dart Drop Impact 100 g
    Elmendorf Tear Strength Md 250 g/mil
    Elmendorf Tear Strength Td 350 g/mil
    Haze 12%
    Gloss 45 55
    Coefficient Of Friction 0.2
    Vicat Softening Point 100°C
    Brittleness Temperature -70°C

    As an accredited Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for transport.
    Container Loading (20′ FCL) 20′ FCL: 25 kg bags on pallets, approx. 24–25 MT net Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer.
    Shipping Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer is shipped as solid pellets in 25 kg bags or 1,000 kg bulk bags, palletized and stretch-wrapped. It is typically non-hazardous for transport and should be kept dry, clean, and in a cool, ventilated area.
    Storage Store Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Use appropriate grounding during handling. Follow manufacturer’s SDS and local regulations for safe storage and housekeeping.
    Shelf Life Stable under normal conditions; manufacturer typically recommends use within 24 months when stored cool, dry, and sealed in original packaging.
    Application of Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer

    Chevron Phillips 6109DK is a butene-copolymer linear low-density polyethylene blown-film resin with supplier-published nominal density 0.918 g/cm³ and nominal melt index 0.90 g/10 min at 190 °C/2.16 kg per ISO 1183-1:2019 and ISO 1133-1:2022. The butene comonomer distribution produces a controlled balance between dart impact, tear, and optical properties; this balance is exploited only when the resin is formulated with LDPE, HDPE, or metallocene plastomers in the downstream applications below. Pellets are non-hygroscopic, but surface condensation on cold pellets transferred into humid extrusion halls above 60% RH is controlled by hopper drying at 60–70 °C for 1–2 h to prevent bubble defects.

    What Changes When 6109DK Replaces Standard LDPE in Deep-Freeze Film Blends?

    In deep-freeze packaging, film must retain ductility after severe folding at freezer temperatures while resisting puncture by frozen product edges. The butene copolymer is compounded at a nominal ratio of 70 wt% 6109DK, 25 wt% high-clarity LDPE with a density of 0.923 g/cm³ and melt index of 0.3 g/10 min, and 5 wt% slip/antiblock masterbatch; this ratio holds haze below 9% per ASTM D1003-21 while maintaining dart impact above 140 g for 50 µm film per ASTM D1709-16a, Method A. Frost line height is set at 5–7 die diameters to balance quench rate and bubble stability; die gap is 1.9–2.3 mm, blow-up ratio is 2.2–2.8, and melt temperature is held between 193 °C and 210 °C on a linear low-density film screw with 24:1–30:1 L/D. Food-contact extrudate is specified under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 with overall migration not exceeding 10 mg dm-2; seal strength is checked by ASTM F88/F88M-15 with seal initiation over a 90–120 °C jaw temperature range. Converted products include IQF vegetable and seafood bags, ice cube bags, and frozen fruit pouches.

    Container liner and refuse sack extrusion introduces 6109DK at 40–60 wt% with film-grade HDPE at 30–50 wt% and reclaimed edge trim up to 10 wt%. The blend is processed on a grooved-feed extruder with 30:1 L/D, a 200–300 mm die, internal bubble cooling, die gap 1.4–2.0 mm, blow-up ratio 3.0–4.2, and melt temperature 193–221 °C; increasing HDPE fraction raises tensile stiffness but narrows the melt fracture window, so adapter pressure is maintained below 40 MPa. Compliance for non-food industrial sack and can liner production is demonstrated under Regulation (EC) No 1907/2006 and Directive 94/62/EC, with combined lead, cadmium, mercury, and hexavalent chromium below 100 mg kg-1 in packaging components. The film is drawn to 25–80 µm for refuse sacks and 80–120 µm for 200-L drum liners; dart impact is assessed by ISO 7765-1:2004 or ASTM D1709-16a, while puncture resistance is assessed by ASTM D5748-12 where liner integrity is critical. Finished applications include can liners for solvent and aqueous waste, hospital infectious-waste bags, and retail refuse sacks.

    Garment Bag Films Where Haze Below 8% Must Be Held Across 25–50 µm Gauges

    For transparent apparel packaging, the film compound is based on 60 wt% 6109DK, 35 wt% high-clarity LDPE, and 5 wt% silica-based antiblock masterbatch; erucamide slip is maintained at 500–800 ppm to keep static coefficient of friction between 0.25 and 0.45 per ISO 8295:2004. The extrusion line uses a single-flighted barrier screw with 25:1–30:1 L/D, a 150–250 mm die, die gap 1.8–2.2 mm, blow-up ratio 2.0–2.5, and melt temperature no higher than 200 °C to suppress gel formation from recycle. Corona discharge is applied to one surface at 38–42 dyn cm-1 for flexographic or rotogravure printing; the opposite seal surface is kept below 36 dyn cm-1 to prevent premature seal failure. Compliance is limited to Directive 94/62/EC heavy-metal restrictions and Regulation (EC) No 1907/2006 because garment film is not a primary food-contact structure; brand-specific restricted substance lists may add limits for phthalates under REACH Annex XVII or Commission Regulation (EU) 2018/2005. Terminal products include continuous perforated rollstock for automatic baggers, shirt bags, dress covers, and retail mailer envelopes.

    Perforated fresh-produce flow-wrap films are formed from 70 wt% 6109DK, 15 wt% metallocene ethylene-octene plastomer with density 0.902 g/cm³, and 15 wt% LDPE; anti-fog masterbatch is added at 1–2 phr rather than as part of the polymer matrix. The plastomer depresses seal initiation to approximately 85–95 °C but lowers bubble stability, requiring a dual-lip air ring and internal bubble cooling at blow-up ratio 2.0–2.4. A 65 mm extruder with 30:1 L/D barrier screw feeds a 300 mm die with 1.8 mm gap; melt temperature is capped at 193 °C to avoid degradation of anti-fog or antimicrobial additives. Downstream perforation by needle or laser brings oxygen transmission into the 2,500–6,000 cm³ m-2 day-1 atm-1 range at 23 °C and 50% RH per ASTM D3985-17. Food-contact compliance is specified under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, with anti-fog additive authorization and migration limits from Annex I. Converted products include open bags for leafy greens, broccoli florets, fresh herbs, and bakery items requiring condensation control.

    Can 6109DK Function as the Sealant Web in Adhesive-Laminated Dry Food Packaging?

    As a sealant web in adhesive-laminated structures, 6109DK is extruded into 25–40 µm monolayer film with 85 wt% 6109DK, 12 wt% LDPE, and 3 wt% slip/antiblock masterbatch; higher slip loadings are avoided because erucamide migration to the lamination surface reduces solventless polyurethane bond strength per ASTM F904-16. Primary substrates include 12 µm BOPP, 12 µm PET, or 9 µm aluminum foil, laminated with solventless adhesive at 2.0–2.5 g m-2 coat weight and cured at 40–60 °C for 24–48 h. Heat seal strength is evaluated per ASTM F88/F88M-15, with a required minimum of 12 N/15 mm for dry snack pouches and 18 N/15 mm for pet food pouches under 0.2–0.4 MPa jaw pressure and 0.5–1.0 s dwell time. The sealant layer must satisfy FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 where direct dry food contact is intended; specific migration limits for masterbatch additives are confirmed against Annex I. Converted structures are used for powdered beverage sachets, dry soup pouches, cereal liner bags, and laminated pet food packaging.

    When Blending 6109DK with Bimodal HDPE for Heavy-Duty Industrial Sacks

    Heavy-duty shipping sacks for mineral fillers, fertilizer, and polymer pellets use 50 wt% 6109DK, 45 wt% bimodal HDPE with density 0.949 g/cm³ and melt index 0.1 g/10 min, and 5 wt% recycled plant scrap. The HDPE phase increases stiffness and top-load resistance, but Elmendorf tear per ASTM D1922-15 drops sharply when the 6109DK fraction falls below 35 wt%, establishing the lower bound as a hard processing limit. Extrusion runs on a high-stalk blown-film line with a 350 mm die, die gap 2.2–2.8 mm, blow-up ratio 2.0–2.8, melt temperature 204–218 °C, and stalk height 8–10 die diameters to limit thickness variation to ±8%. For dangerous goods transport, the finished sack must meet UN Model Regulations Chapter 6.1 for non-bulk packagings, using plastic film sack code 5H4 where applicable; material compliance is additionally verified under Regulation (EC) No 1907/2006 and Directive 94/62/EC heavy-metal limits. Finished sack bodies range from 100–180 µm, with gusseted widths up to 600 mm, and are supplied as flat or gusseted tubes for conversion into cement, fertilizer, salt, and chemical additive sacks.

    Free Quote

    Competitive Chevron Phillips 6109DK LLDPE Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6109DK LLDPE Blown Film Resin is a linear low-density polyethylene produced with 1-butene as the copolymer comonomer. The nominal density is 0.918 g/cm³ when measured under ASTM D1505, and the nominal melt index is 0.9 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg load. These parameters place the material in the blown film LLDPE class rather than in high-pressure low-density polyethylene or higher-density film resin categories. The 1-butene comonomer introduces ethyl side branches along the ethylene backbone; this short-chain branching depresses crystallite thickness and density while maintaining sufficient melt extensibility for conventional single-layer blown film operations. The resin is supplied in pellet form for conversion on single-screw blown film extrusion lines. Film property values such as dart impact, Elmendorf tear, haze, and coefficient of friction are dependent on die gap, blow-up ratio, frost line height, screw design, and thermal exposure history. They should therefore be obtained from the supplier’s certificate of analysis for a specific lot rather than transferred from a different converter’s processing conditions.

    Selected producer-published nominal resin characteristics for Chevron Phillips 6109DK
    PropertyTest methodNominal value or status
    DensityASTM D15050.918 g/cm³
    Melt indexASTM D1238, 190 °C/2.16 kg0.9 g/10 min
    Comonomer—1-butene
    Dart impact validationASTM D1709Consult supplier certificate of analysis
    Elmendorf tear validationASTM D1922Consult supplier certificate of analysis

    What Processing Conditions Are Required for Stable Bubble Formation?

    Stable bubble formation in butene copolymer LLDPE is governed by the relationship between melt extension stress and the cooling rate at the frost line. A melt with a nominal value of 0.9 g/10 min may exhibit lower tension than high-pressure LDPE of similar density, which requires a smaller die gap or a higher blow-up ratio correction to maintain neck stability. Blown film dies with a lip gap between 1.0 mm and 1.5 mm are typically specified for film thicknesses below 75 μm. Wider die gaps above 2.0 mm can reduce shear heating and melt fracture tendency, but they may lower machine-direction orientation and tensile stiffness in thin films. The die gap must be matched to gauge and target output; an excessively narrow gap at high throughput can generate sharkskin melt fracture, while an excessively wide gap can reduce molecular orientation and lower final film toughness.

    Melt temperatures in the range of 190 °C to 220 °C are used for similar 0.918 g/cm³ butene LLDPE resins. Processing above 230 °C with extended residence time can initiate oxidative degradation and create gel particles. Barrel zones should be profiled from feed throat to die to maintain a positive temperature ramp without overheating the compression section. A dual-lip air ring or internal bubble cooling system is used on high-output lines because the additional heat-transfer surface reduces frost line variability. Frost line height should be maintained between two and four die diameters above the air-ring discharge for a balance of haze, blocking, and transverse-direction toughness. Lower frost lines may improve clarity but increase film blocking if the formulation lacks adequate antiblocking additives; higher frost lines can increase toughness but reduce bubble symmetry in high-air-flow production environments.

    Production-scale experience with similar butene copolymer grades indicates that extruders of 25:1 to 30:1 L/D and barrier-flight screws provide adequate homogenization for additive distribution. Grooved-feed sections can increase output but may raise melt-pressure variability and should be matched with suitable screen-pack filtration. When melt fracture appears at economic output rates, a fluoropolymer polymer processing aid can be introduced at supplier-recommended loadings to reduce sharkskin and die-lip buildup. Purging before shutdown should use a lower-MI purge compound or high-density polyethylene to displace the LLDPE from the die, because stagnant melt in die corners can crosslink and generate black specks in subsequent production runs. Published data for this specific configuration is limited; start-up and shutdown procedures should be qualified on the intended production line.

    In light-duty can liner and consumer trash bag production, 6109DK is processed at film thicknesses of 25 μm to 50 μm on single-layer blown film lines. Gauge uniformity becomes the primary failure predictor because localized thinning below the nominal gauge reduces dart impact capacity; ASTM D1709A reports energy per unit area and does not isolate the minimum-thickness resistance path. Lines equipped with automatic gauge-control systems and segmented die lips are used to maintain total thickness variation within ±5%. At a 2.5:1 blow-up ratio, the orientation ratio between machine direction and transverse direction changes; this affects Elmendorf tear anisotropy and must be measured per ASTM D1922 for each film construction rather than inferred from resin density alone. In multilayer structures, the resin can be placed in sealant or cost-reduction layers if the adjacent layer viscosity is matched at the die lip to prevent interfacial flow instabilities.

    Frozen food overwrap is another application in which low-temperature ductility is required. Butene copolymer polyethylene retains ductility in the amorphous phase below 0 °C, but the exact brittleness temperature depends on molecular weight, film orientation, and additive loading. Published data for this specific configuration is limited; low-temperature impact testing per ASTM D1790 or dart impact after conditioning at -20 °C should be conducted before specifying the resin in cold-chain packaging. The same applies to liquid packaging and garment bags, where high-speed sealing, hot tack, and coefficient of friction interact with film stiffness and blocking behavior on automatic bag-filling equipment.

    Mechanical and Optical Property Benchmarks

    Mechanical property reporting for blown film produced from 6109DK requires standardized laboratory conditioning at 23 °C and 50% relative humidity per ASTM D618. Tensile properties are measured under ASTM D882 with 25.4 mm wide specimens and a crosshead speed of 500 mm/min; secant modulus is determined at 1% or 2% strain. The density of 0.918 g/cm³ yields a lower secant modulus than higher-density LLDPE grades such as 0.926 g/cm³ film resins, which reduces stiffness but increases ductility and impact absorption. Puncture resistance measured by slow puncture per ASTM D5748 or dynamic puncture per ASTM D5497 is relevant for liners, overwrap, and heavy-gauge packaging films. Machine-direction tensile yield increases with draw-down ratio because chain segments align in the machine direction; transverse-direction tear increases with blow-up ratio due to transverse orientation. These orientation effects are not fixed resin properties and must be measured after the line reaches steady-state conditions.

    Haze and gloss are not inherent resin constants; they are processing-dependent responses. Haze per ASTM D1003 measures forward scattering through the film and is influenced by surface roughness and internal scattering from crystallites. Gloss per ASTM D2457 at a 60° angle is higher when the film surface is smooth and frost line height is optimized. Butene LLDPE usually produces lower haze than HDPE but may not match the optical clarity of a metallocene-catalyzed LLDPE with the same density and melt index when run on the same die. Coefficient of friction per ASTM D1894 and blocking force per ASTM D3354 should be monitored if the DK suffix denotes an additive package; the exact slip and antiblock contents must be verified from the supplier’s lot-specific certificate of analysis. Heat seal strength per ASTM F88 and hot tack per ASTM F1921 are required for converter qualification of bag and pouch formats, because seal initiation temperature depends on seal bar temperature calibration, dwell time, pressure, and film thickness.

    When a Butene Copolymer Replaces Hexene or Octene LLDPE

    The mechanical distinction between a butene copolymer and a hexene or octene copolymer at equal density and melt index arises from the length of the short-chain branch. A 1-butene comonomer contributes an ethyl branch length of two carbons after incorporation; 1-hexene contributes a butyl branch length of four carbons, and 1-octene contributes a hexyl branch length of six carbons. Longer branches are more effective at connecting crystalline lamellae through the amorphous phase, increasing the population of load-bearing tie chains. This is why hexene and octene LLDPE grades typically exhibit higher dart impact and lower brittle failure in heavy-gauge films than butene grades of the same density. The difference is less visible in thin-gauge films below 30 μm because geometry and gauge variation often dominate the failure mechanics. The lower comonomer cost and easier incorporation of butene make this type of material suitable for high-volume, thin-gauge applications where extreme dart impact is not the controlling specification.

    When substituting 6109DK for a hexene or octene LLDPE on an existing blown film line, the bubble stability window may narrow. Lower melt tension relative to higher-alpha-olefin grades can require a reduction in die gap, an increase in frost line height, or a reduction in blow-up ratio to maintain stable neck geometry. The lower cost per kilogram of butene comonomer may allow thicker gauges to compensate for lower impact resistance, but this trade-off must be evaluated per ASTM D4272 impact testing and not inferred from nominal density alone. Conversely, heavy-duty stretch film, agricultural silage wrap, and high-performance packaging that specify high puncture resistance are better served by higher-alpha-olefin grades unless downgauging has been accepted after full ASTM D1709 and ASTM D5748 validation. Published data for this specific configuration is limited; direct substitution should be qualified on the intended conversion line using the same die, air ring, and take-up configuration.

    Regulatory declarations for 6109DK must be confirmed against the specific lot. Polyethylene homopolymers and copolymers may be used in food-contact articles when they meet the specifications of FDA 21 CFR 177.1520. European direct food-contact assessment follows Regulation (EU) No 10/2011 and its overall migration limit of 10 mg/dm². Industrial packaging converters should verify REACH registration for the monomer and additives under Regulation (EC) No 1907/2006, and electrical/electronic packaging may require RoHS Directive 2011/65/EU conformity for cadmium, lead, mercury, hexavalent chromium, PBB, and PBDE.

    Regulatory and standards checklist for blown film grade qualification
    Standard or regulationTypical assessment
    FDA 21 CFR 177.1520Polyethylene articles for food contact; conditions of use must be verified with supplier declaration
    Regulation (EU) No 10/2011Overall migration limit 10 mg/dm²; specific migration limits per Annex II
    Regulation (EC) No 1907/2006REACH polymer exemption under Article 2(9); monomer registration required
    RoHS Directive 2011/65/EUCadmium 100 ppm, lead 1000 ppm, mercury 1000 ppm, hexavalent chromium 1000 ppm, PBB/PBDE 1000 ppm where applicable

    Pellets should be stored in a cool, dry area at or below 40 °C. Polyethylene is not hygroscopic, but condensation on cold pellets introduced into the feed throat can produce steam and surface porosity in the film. If moisture-related defects appear, use a desiccant hopper dryer at 60 °C to 70 °C with a dew point below -20 °C; published data for this specific configuration is limited. The resin should not be blended with incompatible acid- or amine-containing additive masterbatches without examining thermal-oxidative stabilizer interactions and film gel counts.