Chevron Phillips 6109cl Lldpe Blown Film Resin Butene Copolymer

Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 641803
    Productname Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Copolymertype Butene Copolymer
    Density 0.918 g/cm³
    Meltindex 0.9 g/10 min (190°C/2.16 kg)
    Meltingpoint 122 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyieldmd 11.0 MPa
    Tensilestrengthatyieldtd 10.3 MPa
    Tensilestrengthatbreakmd 34.5 MPa
    Tensilestrengthatbreaktd 31.0 MPa
    Elongationatbreakmd 600%
    Elongationatbreaktd 700%
    Elmendorftearstrengthmd 250 g/mil
    Elmendorftearstrengthtd 400 g/mil
    Dartdropimpact 200 g
    Haze 10%
    Gloss 55%

    As an accredited Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 6109CL LLDPE butene copolymer resin is packaged in 50-lb (22.7-kg) multiwall paper bags and 1,000-kg bulk bags, palletized.
    Container Loading (20′ FCL) 20′ FCL loading: palletized 25 kg bags of Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer, shrink-wrapped, fully secured.
    Shipping Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer is typically shipped as nonhazardous resin pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Keep dry, cool, and clean; avoid moisture, heat, contamination, and direct sunlight. No DOT/IMDG/IATA hazard classification. Follow the SDS and local transport regulations.
    Storage Store Chevron Phillips 6109CL LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original packaging closed and palletized off the floor to prevent moisture pickup and contamination. Avoid contact with strong oxidizers. Maintain good housekeeping to control dust and static. Use first-in, first-out stock rotation; inspect containers regularly for damage.
    Shelf Life Shelf life is generally 12 months from manufacturing date when stored sealed in a cool, dry, ventilated area away from sunlight.
    Application of Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer

    Heavy-duty industrial liner production with Chevron Phillips 6109CL butene-copolymer LLDPE typically begins with a 70–80 wt% resin phase blended with a 20–30 wt% LDPE homopolymer phase selected at 0.25–0.5 g/10 min melt index to improve bubble stability. Bulk container liners for FIBCs carrying mineral powders, resin pellets, or dry construction additives are extruded on a 55 mm 24:1 L/D grooved-feed blown-film line fitted with a 250 mm spiral mandrel die and 1.8 mm die gap. The barrel temperature profile is set from 180 °C in the feed zone to 215 °C at the adapter, with melt temperature held at 210–220 °C. A blow-up ratio of 2.4:1 and frost line height of 250 mm produce a 50–80 µm film with balanced machine-direction and transverse-direction tear. Additive delivery uses a 4 wt% masterbatch let-down containing 10 µm median particle-size synthetic silica antiblock and 0.8 wt% erucamide slip; the final kinetic coefficient of friction is checked according to ASTM D1894 and held at 0.25–0.45. Dart impact is measured per ASTM D1709 method A, with production specifications commonly requiring not less than 150 g at 50 µm, while Elmendorf tear is tested per ASTM D1922. Food-contact and industrial lot acceptance relies on FDA 21 CFR 177.1520(c) olefin polymer provisions, EU Regulation 10/2011 overall migration of 10 mg/dm², and 94/62/EC heavy-metal limits of 100 ppm cumulative lead, cadmium, mercury, and hexavalent chromium. Moisture on pellet surfaces above 0.1 wt% must be removed with heated air at 65–75 °C before extrusion because surface water disturbs melt film uniformity, although the resin itself is not hygroscopic. End articles are flat or gusseted liners from 250 kg to 1000 kg capacity with impulse-welded seams.

    Seal Integrity in Frozen Food Packaging Is Governed by Dwell Time More Than Jaw Temperature

    Seal strength in frozen food VFFS operations is dominated by dwell time because the butene-copolymer sealing layer solidifies rapidly after jaw release. The film structure for 1 kg IQF vegetable or frozen seafood bags uses 85 wt% 6109CL, 15 wt% LDPE homopolymer, 1.5 wt% glycerol monostearate anti-fog masterbatch, 1200 ppm synthetic silica antiblock, and 600 ppm erucamide slip. Blown-film conversion is performed on a 45 mm 24:1 L/D extruder with 1.6 mm die gap, 2.5:1 blow-up ratio, melt temperature of 208 °C, and 50 µm final thickness. On the VFFS line, jaw temperature is set between 130 °C and 150 °C, dwell time is held at 0.2–0.4 s, and jaw pressure is maintained at 0.48 MPa. Seal strength is tested according to ASTM F88 with a common minimum target of 12 N/15 mm after 24 h conditioning; hot-tack testing follows ASTM F1921. Low-temperature abuse resistance is measured by dart impact per ASTM D1709 after conditioning at −20 °C, with converters often specifying not less than 120 g at 50 µm. Compliance for direct food contact is assessed under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with overall migration limited to 10 mg/dm² for frozen aqueous and fatty food simulants. The operational boundary is that jaw temperature below 140 °C combined with dwell time under 150 ms produces channel leakers at the seal corners; published data for this exact film gauge on high-speed VFFS equipment is limited, so pilot trials are required when line speed exceeds 80 pouches/min.

    In three-layer agricultural blown film producing 25 µm silage wrap, this butene-copolymer LLDPE is confined to the non-cling skin and core layers at 20–35 wt% while a metallocene octene LLDPE carries the load-bearing portion. The 6109CL-containing layers require a stabilizer package of 0.5 wt% HALS, 0.2 wt% triazine UV absorber, and 0.1 wt% phosphite process antioxidant to survive 12-month outdoor bale storage. Extrusion is performed on a three-layer blown-film die of 300 mm diameter with 2.0 mm die gap, 2.6:1 blow-up ratio, and melt temperature of 215 °C; output on a 75 mm core extruder with 25:1 L/D commonly reaches 320 kg/h. Tensile properties are tested per ISO 527-3, tear resistance per ISO 6383-2, and weathering by ASTM D4329 QUV-A screening; retained tensile strength after 1000 h exposure is held above 70% of the unaged value. The end article is a 750 mm × 1500 m round bale wrap applied at 60–70% pre-stretch on a bale wrapper. This resin is not recommended as the sole polymer below 25 µm because butene-copolymer short-chain branching produces lower puncture propagation resistance than an octene copolymer at equivalent density, which increases film failure risk on rough stubble and frozen silage bales. Compliance for non-food agricultural film is not covered by EU Regulation 10/2011; producers instead apply EN 13207 silage film requirements and REACH SVHC screening for imported and exported rolls.

    Produce Bag Film Antiblock Loading and Haze Development

    On a 40 mm 24:1 L/D blown-film line running 15–20 µm produce-bag film, the formulation combines 70 wt% 6109CL with 30 wt% LDPE homopolymer, 3 wt% glycerol monostearate anti-fog masterbatch, and 800 ppm synthetic silica antiblock with 5 µm median particle size. Die gap is set at 1.4 mm, blow-up ratio at 2.8:1, melt temperature at 202 °C, and frost line height at 180 mm. Optical testing uses ASTM D1003 haze procedures with a target below 8%, while 45° gloss is measured per ASTM D2457 and held above 60 GU. Blocking resistance is evaluated per ASTM D3354, with blocking force kept below 50 g/cm; kinetic coefficient of friction is measured according to ASTM D1894 and maintained at 0.25–0.45. If the silica median particle size exceeds 7 µm, 45° gloss falls below 55 GU and the film becomes visibly grainy on the produce display; if antiblock loading falls below 500 ppm, blocking on the wicket may exceed 50 g/cm after 48 h storage at 35 °C. Compliance for food-contact thin films relies on FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, subject to overall migration testing at 10 mg/dm². The end articles are perforated or wicket-mounted produce bags for leafy greens, root vegetables, and citrus with open-mouth sealing or twist-tie closure.

    For surface-protection film applied to PVC window profiles and aluminum extrusions, 50–80 µm blown film from 6109CL is used as an adhesive-free masking layer that is corona-treated offline before pressure-sensitive adhesive coating. Slip additives are held below 500 ppm because erucamide migration above 800 ppm interferes with peel adhesion of the subsequently applied low-tack adhesive. Extrusion uses a 60 mm 24:1 L/D line with 2.0 mm die gap, 2.2:1 blow-up ratio, and melt temperature of 205 °C. Tensile properties are tested per ISO 527-3, with elongation at break above 500%; corona-treated surface energy is checked with dyne solutions at 40 dyn/cm minimum. Heavy-metal and restricted-substance compliance is documented under 94/62/EC packaging limits of 100 ppm cumulative lead, cadmium, mercury, and hexavalent chromium, RoHS 2011/65/EU, and REACH SVHC screening. The operational boundary is that reclaimed material containing stearate concentrations above 1500 ppm must be excluded from the blend because die-lip plate-out disturbs gauge uniformity and creates adhesive wetting streaks. The end article is a 1200 mm × 1000 m roll slit to profile width for automated application on extrusion lines.

    When Lamination Speed Exceeds 150 m/min, Sealant Web Gauge Uniformity Governs Pouch Integrity

    Extrusion lamination sealant webs of 15–20 µm produced from 6109CL are used in three-layer flexible pouches for dry-mix food and beverage powders. The blown film is made from 90 wt% 6109CL, 10 wt% LDPE homopolymer, and 1 wt% antiblock masterbatch on a 50 mm 24:1 L/D line with 1.5 mm die gap, 2.0:1 blow-up ratio, and melt temperature of 207 °C. Gauge variation is controlled to ±5% across the web because at lamination line speeds of 150–180 m/min, variation greater than ±6% creates channel leakers after pouch sealing. The sealant web is corona-treated to 42 dyn/cm immediately before lamination to orient PP or PET reverse-printed films with 2–3 g/m² solventless adhesive. Lamination bond strength is tested per ASTM D1876, and seal strength is measured per ASTM F88 with a common target above 10 N/15 mm at 145 °C jaw temperature and 0.3 s dwell. Food-contact compliance is evaluated under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011, with migration testing appropriate to dry beverage powders in 10 mg/dm² overall migration. Published data for this exact combination of 6109CL sealant web and high-speed lamination is limited; pilot trials are required before specifying line speed above 180 m/min. The end article is a 200 g dry beverage mix pouch with top gusset and notch tear feature.

    When pallet hood film of 60 µm thickness is extruded on a high-stalk line, the butene-copolymer resin is blended with 25 wt% LDPE to stabilize the stalk and prevent bubble flutter. The structure is produced on a 250 mm three-layer die with 1.8 mm die gap, 3.0:1 blow-up ratio, and melt temperature of 215 °C; the tubular film is collapsed through a collapsing frame with 1.5 m side gusset. Dart impact is measured per ASTM D1709 with a production minimum of 300 g, and Elmendorf tear per ASTM D1922 is checked in both directions. The end article is a pallet hood for white goods, insulation batts, or lumber packages, applied at 3–5% pre-stretch. Below 40 µm, pinhole formation during pre-stretch increases because butene-copolymer LLDPE has lower melt strength retention than hexene or octene copolymers at equivalent density; published data for 6109CL in high-stalk pallet hood film at thicknesses below 40 µm is limited, and converters should not extrapolate octene-grade performance. Compliance for industrial non-food packaging is governed by REACH SVHC screening and 94/62/EC heavy-metal limits of 100 ppm cumulative lead, cadmium, mercury, and hexavalent chromium, without a food-contact migration requirement.

    Free Quote

    Competitive Chevron Phillips 6109CL LLDPE Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6109CL LLDPE blown film resin is a butene-copolymer linear low-density polyethylene supplied in pellet form for tubular blown film extrusion. The product code 6109CL identifies the grade within the supplier’s LLDPE film portfolio; the exact additive package, including slip, antiblock, and processing-aid content, is controlled at the manufacturing site and must be confirmed for the specific lot. Nominal density is 0.918 g/cm³ when measured according to ISO 1183-1:2019. Nominal melt mass-flow rate is 1.0 g/10 min when measured at 190 °C under a 2.16 kg load according to ISO 1133-1:2022. The combination places 6109CL in the general-purpose LLDPE blown film range, where gauge reduction, mechanical strength, and bubble stability are balanced for unsupported film applications.

    The primary intended conversion process is blown film. Typical end uses include industrial liners, can liners, garment bags, overwrap, medium-duty agricultural film, and construction film. The base resin is not a long-term UV-stabilized grade; outdoor exposure requires converter-added UV stabilizer masterbatch. The resin is not positioned as a cast-film or extrusion-coating grade unless the specific equipment is evaluated against the supplier’s processing guidance. Food-contact and medical-packaging applications require lot-specific compliance documentation before use.

    When 6109CL Runs on a High-Stalk Blown Film Line

    On conventional single-screw blown film lines with 24:1 to 30:1 L/D and barrier or mixing screw configurations, 6109CL is typically run with a die gap of 1.5 mm to 2.5 mm. Melt temperatures between 190 °C and 230 °C are common; temperatures above 240 °C should be avoided because the combined effect of residence time and oxidative degradation can generate gel particles and raise yellowness index. Blow-up ratios of 2.0:1 to 3.0:1 and frost-line heights of 2 to 4 die diameters are used as starting conditions. The high-stalk geometry is frequently selected because the longer melt strand increases cooling time and improves bubble stability, but an excessively high stalk can produce periodic diameter oscillation, visible as gauge bands. Operators should change stalk height in increments no greater than 10% of die diameter because the bubble responds nonlinearly to internal air-volume changes.

    Because 6109CL has a linear backbone and a narrow molecular weight distribution relative to high-pressure LDPE, shear viscosity is less sensitive to screw speed. On grooved-feed extruders from 55 mm to 75 mm screw diameter, head pressure can exceed that of an LDPE with equivalent nominal melt index, but the pressure rise is not a direct indicator of melt temperature and should be monitored against the supplier’s maximum. The practical output ceiling is frequently set by bubble flutter or melt fracture rather than by extruder torque. When sharkskin develops at the die lip, the preferred interventions are die-temperature adjustment, die-gap widening within the recommended range, output reduction, or a fluoropolymer processing aid if permitted by the formulation. Raising melt temperature above 230 °C is the least desirable response because it narrows the thermal safety margin against oxidation.

    Startup and shutdown require purging with a fractional-melt LDPE or a purging compound specified by the equipment supplier. Direct barrel shutdown with 6109CL can leave material in the die that degrades during the next heat-up, leading to black specks and poor film appearance. The purge should be continued until the melt pressure and film clarity stabilize. Published product-specific purging data is limited, but the procedure is consistent with standard LLDPE blown film practice.

    Pre-drying is generally unnecessary because polyethylene is hydrophobic. Ambient relative humidity above 60% does not require drying unless water condensation has formed on the pellet surface after outdoor storage or rapid temperature change. If surface moisture is present, drying at 70 °C to 80 °C for 2 h with desiccant air is a conventional corrective step. Published moisture-uptake data for this specific grade is limited, so the dry time should be extended only if the pellet surface remains wet. The pellets should be protected from direct sunlight and prolonged UV exposure because photoinitiated oxidation can raise surface carbonyl concentration, measurable by ASTM D5576, and generate off-odor or extrusion gels.

    The stabilization and additive package is proprietary. A converter that requires a defined coefficient of friction, a particular antiblock level, or a custom hot-tack response must confirm that the specific 6109CL lot contains the required additives. A base resin and an additivated variant with the same density and melt index are not interchangeable without requalifying the final film.

    What Distinguishes Butene Copolymer Branching from Hexene and Octene Copolymer Architectures?

    1-Butene insertion creates ethyl side branches on the polyethylene backbone. 1-Hexene creates butyl side branches, and 1-octene creates hexyl side branches. The longer side chains in hexene and octene copolymers are more effective at forming tie molecules between crystalline lamellae during orientation and strain. As a result, at equivalent density and melt index, butene-copolymer film generally exhibits lower dart impact and Elmendorf tear resistance than hexene or octene film of the same thickness. The difference is more visible in films below 25 µm, where impact strength is governed by tie-molecule concentration and orientation rather than gross thickness. Measurements are made with ASTM D1709-16a for dart impact and ASTM D1922-15 for Elmendorf tear. Direct comparative data for 6109CL against hexene grades should be taken from the supplier technical bulletin; published data for this specific configuration is limited.

    Compared with high-pressure LDPE, 6109CL lacks long-chain branching. The lower melt strength reduces bubble stability and requires more precise air-ring and frost-line control. However, the linear structure also increases tensile strength, puncture resistance, and dart impact at a given density and gauge, because strain-induced orientation is not terminated by long-chain branch points to the same degree. Film tensile properties are measured under ISO 527-3:2018 and puncture resistance under ASTM D5748-19. LDPE remains preferred when high melt strength is required for heavy-gauge shrink or extrusion coating; 6109CL is used when the application prioritizes downgauging and mechanical toughness.

    Compared with metallocene LLDPE, 6109CL generally has a broader molecular weight distribution and a less homogeneous comonomer distribution. The broader distribution reduces melt pressure and improves throughput on older extrusion lines, but it can raise haze and reduce low-temperature impact. If a producer requires haze below 5% on a 25 µm film measured under ISO 14782:2021, a metallocene or hexene-rich formulation may be necessary. For 6109CL, actual haze must be measured on the production line; laboratory film values do not transfer directly to commercial equipment.

    In can-liner and industrial-liner applications, 6109CL is generally evaluated for dart impact, tear propagation, and seal integrity. Medium-duty liners are often produced in the 38 µm to 100 µm range, but the lower tie-molecule population of butene LLDPE means that puncture-critical waste streams require verification of dart impact on the actual converted film. Heat-seal initiation for butene LLDPE in this density and melt-index class is commonly reported between 95 °C and 115 °C, and hot tack is measured by ASTM F1921-12. The exact 6109CL seal initiation temperature must be obtained from the supplier technical data sheet rather than inferred from other butene grades because the additive package shifts the seal curve.

    Frozen-food packaging is a boundary use. At service temperatures below -20 °C, impact strength drops and butene-copolymer LLDPE can fail in a brittle mode more readily than hexene or octene grades. If frozen-food packaging is targeted, converters typically select a hexene, octene, or metallocene LLDPE, or coextrude 6109CL with a tougher skin layer. Low-temperature impact may be evaluated with ASTM D1790-21 or by end-user pack tests under actual distribution conditions.

    Rheological Curves, Die-Lip Deposition, and Film Gauge Repeatability

    If the supplier data sheet does not report a melt flow ratio or rheological curve, a capillary rheometer scan under ISO 11443:2021 at 190 °C from 10 s⁻¹ to 1000 s⁻¹ is used to establish shear-thinning behavior. The viscosity at 100 s⁻¹ is a practical comparison point for blown film extrusion, but the exact value depends on temperature control. Because 6109CL is a linear butene copolymer, its viscosity curve is less steep than that of LDPE and may be steeper than some metallocene grades; this material response affects screw torque and die pressure.

    Die-lip deposition can occur with butene LLDPE when low-molecular-weight species migrate to the die lip. This deposit changes the local film gauge and can create thin bands. Periodic die lip cleaning is required on some high-output lines. The use of a fluoropolymer processing aid reduces the frequency of die-lip buildup, but if the grade already contains an additive package, converters should not add an unapproved processing aid without supplier confirmation.

    Film gauge repeatability is monitored with a noncontact capacitance or beta gauge. A production line should hold thickness variation within ±5% of target for consistent conversion performance. If thickness variation exceeds this limit, the air ring, die centering, frost-line height, and melt-temperature profile should be checked before adjusting the resin formulation. Published studies of blown film gauge variability show that air-ring geometry and die temperature uniformity dominate over pellet-to-pellet viscosity differences in stable conditions.

    Moisture Uptake, Purging, and the Food-Contact Boundary

    For food-contact use, polyethylene resins fall within the scope of FDA 21 CFR 177.1520 as olefin polymers. Compliance of the specific 6109CL formulation must be confirmed by the supplier for the intended end use; the same condition applies to Commission Regulation (EU) No 10/2011 and its amendments, including overall migration and specific migration limits. A generic statement that the polymer is polyethylene is not sufficient for audit. The converter must obtain a compliance letter that lists the exact additive package and any conditions of use, such as temperature, fat content, and contact duration.

    Operational limitations include avoiding melt temperatures above 240 °C for extended periods, avoiding direct contact with strong oxidizing agents or halogenated solvents during cleaning, and controlling regrind addition. Regrind levels above 20% can raise gel count and reduce dart impact because the reprocessing history consumes part of the antioxidant package. The exact regrind tolerance for 6109CL should be established on the target blown film line; published data for this specific formulation is limited. The resin should not be blended with high-density or polypropylene scrap without verifying compatibility, because viscosity mismatch and crystallization-rate differences can generate unmelted domains and die-lip buildup.

    If Clarity Specifications Approach Metallocene Haze Levels

    Optical specifications are often the first point of failure when 6109CL is substituted for a metallocene or high-clarity LDPE. Haze in blown film is influenced by surface roughness, melt temperature, die gap, and frost-line height, not just by the resin. A high frost line increases crystal size and can raise haze; a low frost line may improve clarity but reduce bubble stability. The target haze for a given film must be measured under ISO 14782:2021 or ASTM D1003-21. If the 6109CL film fails clarity after all processing adjustments, a metallocene or an LDPE-rich blend should be evaluated. Claiming a clarity value without specifying film gauge, die gap, and cooling conditions is not technically valid.

    Top