Chevron Phillips 6109bk Lldpe Blown Film Resin Butene Copolymer

Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 689872
    Resin Type Linear Low Density Polyethylene (LLDPE)
    Copolymer Type Butene Copolymer
    Density 0.919 g/cm3
    Melt Index 0.9 g/10 min
    Melting Point 124 °C
    Vicat Softening Point 100 °C
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g/mil
    Elmendorf Tear Strength Td 350 g/mil
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1500 psi
    Tensile Strength At Break Md 5000 psi
    Tensile Strength At Break Td 4500 psi
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Haze 12%
    Gloss 60

    As an accredited Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer is supplied in 25 kg polyethylene bags, palletized for shipment.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer in 25 kg bags, palletized and securely loaded.
    Shipping Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer is shipped as a non-hazardous solid in 25 kg polyethylene bags, palletized and stretch-wrapped. Transport in clean, dry trucks, railcars, or containers. Keep cool, dry, and away from direct sunlight, moisture, heat, and contamination. Handle pallets carefully to prevent bag damage.
    Storage Store Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer in a cool, dry, well-ventilated area in original, sealed packaging. Protect from direct sunlight, moisture, excessive heat, sparks, flames, and oxidizing agents. Keep away from contaminants and odors. Stack pallets securely without crushing. Use first-in, first-out inventory. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is typically 24 months when stored unopened in a cool, dry, well-ventilated area away from direct sunlight.
    Application of Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer

    Heavy-gauge industrial refuse and construction debris liners made from Chevron Phillips 6109BK butene LLDPE are usually extruded as monolayer blown film in the 80 μm to 150 μm thickness band. Production on a 30:1 L/D single-screw extruder with a barrier screw and 1.8 mm die gap is standard. Melt temperature is held between 196°C and 215°C. Blow-up ratio is set at 2.2:1 to 2.8:1. Operation above 2.8:1 becomes unstable because the low melt strength of butene LLDPE produces periodic bubble diameter oscillation; thickness variation on 100 μm film increases beyond ± 8%. When the converter requires higher bubble expansion, 10–15 wt% low-melt-index LDPE is added. The LDPE component should have melt index 0.25 g/10 min to 0.40 g/10 min at 190°C/2.16 kg. Dart impact is tested under ASTM D1709 Type A. Industrial liner specifications for 125 μm construction debris film frequently demand 350 g to 500 g dart drop. Elmendorf tear is run under ASTM D1922; transverse direction tear at 100 μm is commonly controlled at 15 N/mm or higher. Puncture propagation resistance is checked under ASTM D2582. Converted articles include bottom-seal rubble bags, demolition waste liners, gusseted drum liners, and autoclave liners for biohazardous waste streams. Export documentation typically covers REACH SVHC declarations and RoHS heavy metal restrictions because waste-handling infrastructure accepts packaging as a temporary containment article, not as food-contact material.

    What Changes in Sealant Layer Performance When 6109BK Is Coextruded With LDPE for Frozen Food Laminations?

    In frozen food lamination construction, a blown sealant web made from 70–80 wt% 6109BK and 20–30 wt% high-pressure LDPE is coextruded at 30 μm to 50 μm. The LDPE phase is included to stabilize the primary bubble and to lower the heat-seal initiation temperature. Seal initiation on a 35 μm monolayer web shifts from 118°C to 112°C when LDPE content increases from 10 wt% to 25 wt%. Hot tack is measured under ASTM F1921, with peak hot tack recorded near 115°C on laboratory sealers calibrated to 0.5 N/cm² seal bar pressure. Heat-seal strength is evaluated under ASTM F88; a 40 μm sealant web laminated to a 12 μm polyester outer ply commonly specifies 8 N/15 mm minimum sealed seam strength after 0.5 s dwell. The butene copolymer chain architecture contributes to acceptable cold impact down to −20°C; below −25°C, the sealant film should include a metallocene octene LLDPE fraction because spherulitic cracking can initiate in the seal region under corner folding. The film is used for IQF vegetable packs, frozen seafood pouches, and frozen meat carton overwrap. Food-contact status is covered by FDA 21 CFR 177.1520 and EU 10/2011, provided overall migration does not exceed 60 mg/kg under the intended simulant and temperature condition.

    Regulation / MethodCodeCondition
    US olefin polymer food-contactFDA 21 CFR 177.1520Density <0.94 g/cm³; use above −20°C
    EU overall migrationEU 10/201160 mg/kg overall migration limit
    Hot tackASTM F19210.5 s dwell, 0.5 N/cm² seal bar pressure
    Heat seal strengthASTM F88Minimum 8 N/15 mm on 40 μm laminate

    Agricultural silage cover and bale wrap films made with 6109BK are built as three-layer coextrusions in which the butene LLDPE occupies the outer and mid plies. A common formulation is 55–65 wt% 6109BK, 20–30 wt% octene LLDPE, and 12–15 wt% carbon black/UV masterbatch. The carbon black masterbatch is pre-compounded on a twin-screw extruder; direct addition of carbon black powder onto the blown film screw is avoided because dispersion deficits produce micrometer-scale agglomerates that lower transverse tear. Extrusion uses a 2.0 mm die gap, blow-up ratio 2.0:1 to 2.5:1, and frost line height 1.0 m to 1.3 m. Melt temperature is capped at 220°C to preserve hindered amine light stabilizers. The film is tested under ISO 527-3 for tensile strength and elongation; agricultural specifications often require minimum machine and transverse elongation above 600% after 2,000 h xenon-arc weathering under ISO 4892-2. Tear strength by ASTM D1922 in the transverse direction is more sensitive to carbon black addition than machine direction; a loss of more than 15% relative to natural film indicates poor masterbatch distribution. End products include silage bale wrap, silage pit cover, silo bag structures, and blackout greenhouse film. Where the film is used in the EU, silage film durability claims are checked against EN 13206, including covered storage periods of 12 months or more.

    When Post-Consumer Recyclate Content Reaches 20 wt% in Retail Can Liners

    Retail can liners and janitorial sacks are produced by blending 80 wt% 6109BK with 20 wt% post-consumer LDPE/LLDPE film recyclate. The recyclate stream is first melt-filtered through a 120 μm screen pack; production extended beyond 8 h without screen change can raise screen pack pressure above 350 bar and initiate die lip plate-out. The base polymer melt index is typically 0.9 g/10 min; if the PCR fraction shifts above 1.2 g/10 min, the melt viscosity difference exaggerates bubble instability and can reduce dart impact. A gear melt pump and internal bubble cooling are recommended on 60 mm lines. Film thickness is 18 μm to 30 μm; at thickness below 20 μm, gel count per square meter is inspected by ASTM D3351 and controlled to a defined action limit derived from the recyclate wash history. The bubble is maintained at 2.0:1 to 2.6:1 blow-up ratio to reduce edge flutter associated with variable PCR melt elasticity.

    Process ParameterUnitControl Range
    Extruder barrel zone 1°C175–190
    Die temperature°C195–210
    Screen pack finenessμm80–120
    Melt pressure before screenbar<350
    Blow-up ratio—2.0:1–2.6:1
    Film thicknessμm18–30

    End products include retail can liners, janitorial waste sacks, and controlled-waste disposal bags. Recycled content claims are documented under EN 15343 or regional recycled plastics certification; these products do not carry food-contact status because the PCR fraction cannot be traced under FDA 21 CFR 177.1520 without a closed-loop manufacturing protocol. The main operational failure modes are screen pack pressure excursions, gel streaking at the die lip, and screw feed bridging when lightweight PCR flake is not compacted before the hopper throat.

    Stretch hood pallet unitization film positions 6109BK as the core ply rather than the skin ply. A three-layer line running 2.2 mm die gap and 3.0:1 blow-up ratio produces a low-gauge hood with skin plies of metallocene octene LLDPE and a core containing 50–70 wt% 6109BK blended with 30–50 wt% octene mLLDPE. Elastic recovery is tested under ASTM D5459 permanent set method; hood film intended for 100% stretch cycles typically requires less than 15% set after 10 min relaxation at 23°C. The butene copolymer in the core contributes stiffness and puncture resistance but reduces snap-back recovery if used above 70 wt%. High-stalk production with frost line height at 1.5 m is necessary to control orientation; internal bubble cooling is used on 65 mm coextrusion lines at output of 120–180 kg/h. Published data specific to 6109BK in high-stalk stretch hood production is limited; plant trials on three-layer lines are required before commercial homogenization. End products are pallet hoods for insulation board stacks, cement bag pallets, and shrink-hood alternative applications where heat systems are not permitted in the warehouse. The main rejection criterion in use is uneven film thickness measured by ASTM D374, with transverse gauge variation above ± 5% causing poor load-holding geometry.

    Under-Slab Vapor Retarder Film and Its Puncture Trade-Offs

    Monolayer blown film intended for under-slab vapor retardation is run at 0.15 mm to 0.25 mm using a 2.5 mm die gap and blow-up ratio of 2.0:1. Melt temperature is controlled between 210°C and 230°C. The butene copolymer supplies low-temperature impact toughness during construction foot traffic. Water vapor permeance is evaluated under ASTM E96 desiccant method; a 0.15 mm 6109BK monolayer typically falls into Class C of ASTM E1745, meaning permeance below 0.1 perm may require a coextruded metallized layer or a polyethylene film with an integral aluminum foil core depending on the slab design. Puncture resistance is tested under ASTM D4833; under-slab specifications frequently require a minimum puncture force of 300 N at 0.15 mm. Thickness tolerance shall remain within ± 5% across the web; if the bubble is operated above 2.2:1, width and thickness chatter reduces puncture consistency at the roll edges. Converted products include below-slab vapor barriers, crawlspace encapsulation liners, temporary construction enclosures, and concrete curing films. The film meets ASTM E1745 minimum tensile strength and puncture criteria for temporary and permanent below-grade use when converted at the specified thickness. For projects requiring Class A vapor retarder levels, a laminate or metallized barrier is required because a pure butene LLDPE monolayer has a permeance limit above 0.01 perm. The principal field failure mechanism is puncture propagation at sharp aggregate points, which is why ASTM D4833 puncture resistance and ASTM D1709 drop impact are both specified when the film is installed under rough subgrade conditions.

    Free Quote

    Competitive Chevron Phillips 6109BK LLDPE Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips 6109BK is a linear low-density polyethylene blown film resin based on a butene comonomer and is specified for converters that require black, weather-resistant film. The grade is marketed under the Chevron Phillips Chemical product family, and the BK suffix denotes a black pigmentation system; the certificate of analysis should be reviewed to confirm whether the black component is pre-compounded at full letdown or supplied as a masterbatch-ready natural base. The butene copolymer backbone produces a broader molecular weight distribution and different melt draw behavior than octene-based metallocene LLDPE grades, typically with lower dart impact and transverse-direction tear resistance at equivalent density and melt index.

    Typical physical-property data for 6109BK are presented only as representative values because published lot-specific data for this black film configuration is limited. For purchase specifications, the current certificate of analysis must be obtained from the supplier. The resin is generally characterized by a nominal density of 0.918 g/cm³ and a nominal melt flow index of 1.0 g/10 min under 190 °C/2.16 kg according to ASTM D1238-20 or ISO 1133-1:2022. The butene comonomer places the material in the lower stiffness range of LLDPE blown film resins while retaining sufficient melt strength for conventional high-stalk extrusion.

    Property Test method Typical value
    Melt flow index ASTM D1238-20 / ISO 1133-1:2022 190 °C, 2.16 kg; 1.0 g/10 min
    Density ASTM D1505-18 / ISO 1183-1:2019 0.918 g/cm³
    Vicat softening temperature ASTM D1525-17 100 °C
    Melting point, DSC peak ASTM D3418-15 / ISO 11357-3:2018 122 °C
    Carbon black content ASTM D1603-14 Not specified in public literature; verify by certificate of analysis

    What Limits the Processing Envelope in Blown Film Lines?

    On a standard 45 mm single-screw extruder with an L/D ratio between 24:1 and 30:1, the resin is processed as a conventional LLDPE blown film. The melt temperature at the die is usually held between 200 °C and 230 °C, with a die gap of 1.8 mm to 2.5 mm; die gaps below 1.5 mm may intensify melt fracture because carbon black raises apparent shear viscosity relative to natural LLDPE. The blow-up ratio should be maintained between 2.0:1 and 3.0:1, and frost line height may require adjustment to 5 to 8 die diameters for bubble stability. When throughput is increased beyond the air-ring cooling capacity, bubble instability and gauge variation usually appear first at the frost line; this is a known bottleneck on high-stalk film lines.

    Barrel zone settings are normally set in a rising profile from 170 °C to 210 °C from hopper to die, but carbon black can produce temperature overshoot in the compression zone during extended runs at maximum screw speed. Screen-pack configurations of 20/40/80 mesh are typical for general-purpose film. A pressure drop above 280 bar at the breaker plate indicates screen blinding and requires a screen change. The resin is not highly hygroscopic, but surface condensation during seasonal relative humidity excursions above 60% can cause splay and pinholes; pre-drying at 70 °C for 2 h is sufficient for wet pellets.

    Air ring cooling should be set with lower air velocity than natural LLDPE because black film absorbs radiative heat and can become tacky at the collapsing point. Blower speed reductions of 10–20% relative to natural LLDPE are common starting adjustments. The collapsing frame should use low-friction slat surfaces to reduce visible scratching on black film. Gauge control is managed by an automatic profile air ring or by maintaining frost line height within ±5 mm of setpoint. A bubble cage is recommended for die diameters above 300 mm when output exceeds 120 kg/h.

    Comparative Performance Boundaries Against Hexene Copolymers and LDPE

    For converters selecting between materials, the butene comonomer separates 6109BK from hexene and octene LLDPE grades in several performance categories. At equivalent density and melt index, hexene copolymer films generally show higher dart drop impact strength and higher Elmendorf tear resistance in the transverse direction, while octene grades provide better puncture resistance and improved film toughness. The butene-based resin tends to be favored when lower melt temperatures, lower back pressure, and economical blown film output are the primary constraints. Direct comparison to unpigmented resins is incomplete because carbon black can reduce dart impact by concentrating stress at particle-polymer interfaces and can also lower surface gloss.

    Property Test method 6109BK butene LLDPE film General-purpose hexene LLDPE film General-purpose LDPE film
    Dart drop impact, F50, Method A, 25 µm ASTM D1709-16A 90–130 g 150–200 g 60–100 g
    Elmendorf tear, MD/TD ASTM D1922-15 150/350 g 180/450 g 130/120 g
    Tensile strength at break, MD/TD ASTM D882-18 38/32 MPa 45/40 MPa 25/22 MPa
    Gloss, 60° ASTM D2457-13 50–60 for black film 65–75 70–80

    When Carbon Black Masterbatch Is Compounded into the Resin Matrix

    When carbon black masterbatch is added at the hopper rather than supplied as a pre-compounded pellet, the concentrate letdown ratio and mixing quality become the primary sources of film defect. Uneven dispersion of carbon black produces visible streaks and can increase dart impact variation by creating local stress concentrations. A pressure transducer at the breaker plate records combined viscosity effects; a rising trend of more than 10% across an 8 h run without a throughput change typically indicates screen plugging from carbon agglomerates or gel. Use of a gear pump after the extruder can stabilize melt delivery to the die, but only if carbon black dispersion is already acceptable; a gear pump does not correct inadequately mixed pigment. For blown film lines without continuous melt filtration, a 100 mesh or finer screen pack is commonly used to remove carbon agglomerates above 50 µm.

    The black pigmentation system in 6109BK is intended to provide ultraviolet screening and reduce the rate of outdoor embrittlement in applications such as silage covers, temporary geomembrane liners, agricultural mulch film, and construction film. Weathering performance depends on film thickness, carbon black dispersion quality, and surface carbon black retention, not only on the resin base. Converters should validate field service life by accelerated exposure under ASTM G154-23 or ISO 4892-2:2021, followed by tensile retention testing according to ASTM D882-18. For critical geomembrane applications, published data for this specific configuration is limited; the buyer must request long-term oxidative-induction-time data using ASTM D3895-19 or ISO 11357-6:2018 and evaluate against project-specific requirements.

    Because 6109BK is a butene copolymer, the short-chain branching distribution is broader and shorter than that of hexene or octene copolymers, producing a lower entanglement density in the crystalline regions. This is observed in a lower melting point and lower density for a given melt index. In blown film, the butene branch length yields a lower melt relaxation time, so bubble stability is often easier to maintain at high stalk heights than with metallocene octene grades. However, the gain in process stability is offset by lower Elmendorf tear in the transverse direction and lower dart impact resistance. The molecular weight distribution and long-chain branching content are not detailed in the public literature for this specific grade; converters should request rheology data such as extensional behavior if heavy-duty sack applications demand high melt strength.

    On production-scale blown film lines, two failure modes are frequently observed with black butene LLDPE grades. First, die lip fouling from carbon black can produce edge tear and gel films; cleaning schedules may need to be shortened to 8–12 h intervals on lines running high-carbon-black masterbatch. Second, motor load variability increases when the hopper blend of natural LLDPE and black masterbatch segregates; gravimetric dosing of the masterbatch at 0.5 wt% accuracy reduces lot-to-lot color variation. Converters that buy pre-compounded 6109BK avoid these blend segregation problems but lose flexibility in adjusting black concentration.

    Compared with metallocene-catalyzed hexene LLDPE grades of similar density and melt index, 6109BK exhibits lower dart impact and lower puncture resistance but can be processed at lower die lip pressures and lower motor amps on the same extruder. The broader molecular weight distribution also yields lower sensitivity to melt fracture, which permits a thinner die gap and higher drawdown in some film structures. However, when coextrusion structures require a high-clarity outer layer, the carbon black in 6109BK restricts its use to black or hidden-layer positions; it is not suitable where optical transparency is required.

    Heat seal and weld performance also differ from high-pressure LDPE. The butene LLDPE has a higher melting point and longer seal initiation temperature, typically 100 °C to 120 °C for 25 µm film on a hot-bar sealer. In downstream converting, this narrows the sealing window when 6109BK is run against LDPE sealant layers. The black film may also absorb more infrared energy during radiation heating in shrink or converting processes; line speed setpoints require adjustment relative to unpigmented LLDPE.

    Compliance status should be confirmed against the current safety data sheet and grade-specific documentation. Users must verify conformity to REACH, RoHS Directive 2011/65/EU, and FDA 21 CFR 177.1520 for the specific end-use and grade; compliance statements are furnished by the supplier and are not inferred from raw material description. Handling of carbon black-containing pellets should follow occupational exposure limits for nuisance dust under OSHA 29 CFR 1910.1000, especially during pellet conveying and masterbatch addition.

    Top