Chevron Phillips 6109 Lldpe Blown Film Resin Butene Copolymer

Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer

    • Product Name: Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 980689
    Density 0.918 g/cm3
    Melt Index 190 C 2 16 Kg 0.9 g/10 min
    Melt Flow Ratio I21 I2 28
    Tensile Strength At Yield Md 9.7 MPa
    Tensile Strength At Yield Td 9.0 MPa
    Tensile Strength At Break Md 31.7 MPa
    Tensile Strength At Break Td 24.1 MPa
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    1 Secant Modulus Md 207 MPa
    1 Secant Modulus Td 241 MPa
    Dart Drop Impact 180 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 6%
    Gloss 45 70
    Coefficient Of Friction 0.2
    Melting Point 122°C
    Vicat Softening Point 95°C
    Brittleness Temperature < -70°C

    As an accredited Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer is supplied in 25 kg multiwall bags, typically palletized for shipment.
    Container Loading (20′ FCL) 20′ FCL: Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer in 25 kg bags, palletized and shrink-wrapped, securely stowed.
    Shipping Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer is shipped as a non-hazardous solid in 25 kg bags, bulk bags, or boxes on pallets. It is not DOT, IMDG, or IATA regulated. Keep dry, avoid excessive heat, and no special transport labels are required.
    Storage Store Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep sealed in original packaging on pallets, off the floor, to prevent moisture and contamination. Avoid prolonged UV exposure and strong oxidizers. Use first-in, first-out stock rotation; maintain clean handling to preserve resin quality.
    Shelf Life Store in a cool, dry, well-ventilated area; shelf life is typically 24 months from date of manufacture in original packaging.
    Application of Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer

    In frozen-food pouch structures converted from 40–65 µm total thickness, Chevron Phillips 6109 butene LLDPE blown film resin is typically extruded on a grooved-feed single-screw line with a 30:1 L/D ratio and a Maddock mixing section in the metering zone, feeding a spiral mandrel die of 150–300 mm diameter with a 1.8–2.3 mm die gap. Melt temperature at the die is held between 185°C and 210°C, and the blow-up ratio is limited to 2.2:1–2.8:1 for balanced MD/TD tensile properties. The frost line height is normally set at 8–12 die diameters; when line speed exceeds 35 m/min, the frost line is lowered to 6–8 die diameters to preserve film clarity, but this increases internal orientation and can reduce Elmendorf tear in the machine direction. The resin has a nominal melt index of 0.9 g/10 min under ASTM D1238 at 190°C/2.16 kg and a nominal density of 0.918 g/cm³ under ASTM D1505/ISO 1183. Its butene branch structure produces a broader molecular weight distribution than single-site polymers, which stabilises extruder head pressure and melt pumping but reduces bubble extensibility at blow-up ratios above 3.0:1. Converters commonly blend 15–25 wt% high-pressure LDPE with a melt index of 0.3 g/10 min into the frozen-food layer to improve dart impact and low-temperature seal integrity. Film at 50 µm made from the blend is evaluated under ASTM D882-18 for tensile yield and break, ASTM D1709 Method A for dart impact, ASTM D1922 for Elmendorf tear, and ASTM D5748 for puncture resistance. The seal initiation temperature of the butene LLDPE layer falls in the 95–105°C range, but the actual production seal window is narrower because frozen-food pouch converters demand hot-tack strength above 1.5 N/15 mm at 0.5 s dwell and 0.4 N/mm² seal pressure. Food-contact compliance follows FDA 21 CFR 177.1520 for olefin polymers, with the finished structure subject to end-use temperature and food-type limitations. The main operational boundary is moisture uptake: butene LLDPE pellets stored at ambient conditions above 60% relative humidity can introduce water into the melt and produce micro-gels in the die lip; predrying at 70–80°C for 4 h is required if visible surface hydrolytic defects appear. Incompatibility with acid-modified tie resins and certain high-hardness masterbatches should be checked by melt-pressure monitoring before sustained production; a sudden increase of more than 30 bar at constant screw speed indicates dispersion failure, not polymer degradation.

    What Restricts the Heat-Seal Window When 6109 Is Used as a High-Content Sealant Resin?

    The limiting variable in coextruded flexible packaging where the butene LLDPE forms a 10–20 µm sealant web within a 70 µm total blown film structure is not the melt temperature but the rate of chain interdiffusion across the seal interface at dwell times of 0.3–0.8 s. Heat seal initiation measured on 25 µm monolayer films according to ASTM F88 normally begins at 95–105°C, while hot-tack strength measured under ASTM F1921 peaks between 110–125°C. The broad comonomer distribution of the butene backbone means that the low-molecular-weight chains melt first and wet the opposing seal surface, but high-molecular-weight fractions remain partially unhealed at the lower end of the sealing range; this produces cohesive peel failure rather than adhesive failure at the lap-seal edge. On vertical form-fill-seal machines running 60–80 cycles/min, the seal bar contact time is short, and the practical minimum seal temperature must be raised from 95°C to 105°C if the film is 50 µm or thicker. Coextrusion of the sealant web against a stiffer HDPE or polypropylene structural layer shifts the apparent seal initiation upward by 3–7°C because heat is drawn away from the seal interface. Converters often add 20 wt% high-pressure LDPE to the sealant layer to improve low-temperature sealability; the shift in seal initiation is usually 2–5°C downward, but published data for this specific blend configuration is limited, and the result depends on film gauge, seal pressure, and dwell time. The sealant layer must not be compounded with excessive migratory slip additives before sealing because erucamide migration above 1,500 ppm can reduce hot-tack strength by interfering with surface wetting. Process control requires that the die lip be kept clean; degraded material from stagnation at the die lip can create high-seal-initiation spots that pass intermittently through the sealer and appear as leaking pouches in quality checks under ASTM F88.

    On 2.5 m layflat agricultural film towers producing silage wrap and bunker covers, the resin is processed through a 300 mm spiral mandrel die with a 2.3 mm die gap at a blow-up ratio of 3.0:1–3.8:1 for TD-dominated orientation that improves edge-fold puncture resistance. The frost line height is set from 700–1100 mm; lowering it below 600 mm generates unresolved MD orientation and bubble flutter at the collapsing frame, visible as vertical wrinkles and periodic gauge bands of ±8% deviation on capacitance thickness scanners. Carbon-black masterbatch at 2–3 wt% letdown is common for UV-blocking silage film, but the black masterbatch must be dried when ambient humidity exceeds 60% to avoid steam-pitting at the die lip. The base resin is stabilised with a HALS/antioxidant package capable of surviving direct contact with acidic silage leachate; extraction and retention tests follow ASTM D5748 for puncture-after-exposure and EN 13206 for agricultural film requirements. Environmental stress crack resistance is measured on notched specimens under ASTM D1693B; 80 µm silage structures are often specified at ≥500 h without cracking, and a butene LLDPE of 0.918 g/cm³ density normally requires a 20–30 wt% high-pressure LDPE letdown to meet that threshold when the film is continuously exposed to wet silage. The extruder temperature profile from hopper to die is typically set at 180°C / 200°C / 204°C / 204°C / 204°C; die temperatures above 210°C can degrade HALS and generate micro-gels that lower dart impact. Additive packages containing amine-based UV stabilisers should be avoided in unscreened regrind because they react with acidic silage liquor and can cause premature surface chalking. Because agricultural lines often run regrind up to 40%, the melt filter must be changed at 4–6 h intervals when the pressure differential across the screen pack exceeds 80 bar; otherwise gels accumulate on the die lip and the bubble develops localised thins that fail dart impact under ASTM D1709 Method A.

    Heavy-Duty Sack Extrusion: Layer Ratio, Tear Propagation, and Mullen Burst Thresholds

    Heavy-duty sacks for 50 kg industrial fill weights are produced as three-layer blown film on lines equipped with three 75–120 mm grooved-feed single-screw extruders arranged around a 400 mm spiral mandrel die, with each screw at 30:1 L/D and a Maddock mixing section in the metering zone. Layer distribution is set at 20/60/20 or 25/50/25, placing the butene LLDPE-rich core between LDPE-rich skins to combine haul-off stability with improved dart impact and burst resistance. When the core layer exceeds 70 wt% of total throughput, die pressure rises above 430 bar and the die-lip outer temperature must be reduced from 205°C to 195°C to maintain bubble symmetry. Mullen burst strength of 150 µm three-layer sacks is tested under ISO 2758/TAPPI T 403 and typically falls between 180 kPa and 220 kPa when LLDPE content is held at 50 wt%; below 40 wt% LLDPE, the burst value declines because the structure loses machine-direction tensile capacity. Elmendorf tear measured under ASTM D1922 shows that the LLDPE-rich core suppresses tear propagation in the machine direction, but the butene comonomer provides lower tear resistance than hexene or octene LLDPE at equivalent density, so sack downgauging from 150 µm to 120 µm often requires a 10% increase in layflat width to maintain tear energy demand. The most frequent production defect in this format is bubble side-to-side oscillation; at a blow-up ratio above 2.6:1, the wide bubble becomes sensitive to ambient air currents, and the operator must narrow the air ring lip gap or lower the frost line from 950 mm to 800 mm. If the bubble is not stabilised, the collapsing frame will print vertical score lines into the film at 10–15 m/min and produce weak seals on the inner surface because the heat-seal area has been surface-damaged. The screw speed and melt pressure should be recorded at 15-minute intervals; a pressure rise of more than 25 bar at constant throughput indicates screen pack blinding from degraded gels or carbonate masterbatch residue.

    If 6109 Is Let Down into LDPE-Rich Shrink Hoods at 30–50 wt%

    Shrink hood formulations require controlled MD and TD shrink behaviour measured under ASTM D2732 after immersion in a 150°C silicone bath for 30 s. A plant formulation containing 70 wt% high-pressure LDPE with a 0.3 g/10 min melt index and 30 wt% of the butene LLDPE can be extruded on a 120 mm line at 350 kg/h through a 500 mm die with a 0.8 mm die gap and a blow-up ratio of 2.0:1, because the LDPE-rich melt retains sufficient bubble integrity at the lower neck height. The LLDPE component raises dart impact measured under ASTM D1709 by 20–40% relative to the pure LDPE control, while MD shrink tension measured under ISO 14616 drops by 10–15%. That trade-off is acceptable only for stable, regular pallet shapes; random-shaped pallets requiring high shrink tension at 180°C shrink tunnel settings should keep the butene LLDPE content at or below 30 wt%, because higher levels prevent the hood from pulling tightly around protruding edges. The main process failure appears at the die lip: a die gap below 0.8 mm combined with 30 wt% LLDPE may generate sharkskin in the outer skins because elongational stress at the lip exceeds the melt strength of the butene-depleted surface. If sharkskin occurs, raising the die temperature from 200°C to 215°C usually eliminates the defect without introducing a polymer processing aid. Freeze shrinkage is evaluated only when the pallet wrap is used in cold-chain distribution; the shrink film is conditioned at -20°C for 24 h and then inspected for zippering at the heat-seal line. The butene LLDPE component improves cold impact toughness, but the resin should not exceed 50 wt% in this application because excessive low-melt-point material reduces the elastic recovery of the stretched hood during storage at 40°C or above.

    In thin-gauge e-commerce mailer extrusion at 35 µm layflat on high-output 100 mm single-screw lines with a 2.0 mm die gap and 2.2:1 blow-up ratio, the critical variable is seal-through-contamination performance after dust or starch powder from automated warehouse conveyors deposits on the inner surface. The butene LLDPE seal layer achieves adequate lap-seal strengths under ASTM F88 at 110–125°C; output values normally lie between 8 N/15 mm and 14 N/15 mm depending on film thickness, dwell time, and seal bar condition, but contamination reduces the upper limit by 15–30%. Because e-commerce mailers require a high coefficient of friction to prevent stack slippage on pouch-forming machines, converters add 1,500–2,500 ppm erucamide slip or 5,000–8,000 ppm silica antiblock to the outer layer. The slip migrates through the structure over the first 12–24 h after conversion and can transiently depress seal strength if it reaches the sealant surface before the final sealer operation; corona treatment above 38 dyn/cm on the inner layer does not eliminate this effect because the mechanism is surface energy modification rather than oxidation. For multi-wall mailers with a woven HDPE outer layer, the butene LLDPE is used as an extrusion-lamination layer at 320°C melt temperature; residence time above 12 min at that temperature produces gels and specks, so the laminator is purged after each shift and the hopper is kept sealed when relative humidity exceeds 60% to prevent hydrolysis of carbonate masterbatch. The same resin class is also run as 20–25 µm can liners, where high-slip outer surfaces must retain a dart impact value of at least 80 g under ASTM D1709 Method A; dropping below that threshold creates tear-initiated failures at the rim weld when a filled liner is lifted. The main operational limit in both formats is gauge control: at 35 µm, a ±4 µm thickness variation produces localised thin spots that fail seal-integrity tests under ASTM F88, so the air ring and IBC pressure must be adjusted to hold layflat width within ±10 mm and prevent the frost line from oscillating more than ±50 mm.

    Free Quote

    Competitive Chevron Phillips 6109 LLDPE Blown Film Resin, Butene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chevron Phillips Chemical 6109 LLDPE blown film resin is a linear low-density polyethylene produced with butene-1 as the primary comonomer and marketed as a pelletized extrusion grade for monolayer and coextruded blown film. The material belongs to the Ziegler-Natta butene-copolymer LLDPE class, supplied with antioxidant stabilisation and, in standard commercial configurations, a slip/antiblock package. The product is identified by a nominal melt flow index of 1.0 g/10 min measured at 190 °C under 2.16 kg load per ASTM D1238 or ISO 1133-1, and a nominal density of 0.918 g/cm³ determined by ASTM D1505 or ISO 1183-1. These values place 6109 in the low-density region of polyethylene copolymers, between high-pressure LDPE and HDPE; the butene short-chain branching provides a controlled balance of bubble shape retention, tensile orientation, and heat-seal response. In blown film operations, the resin is specified for moderate-duty packaging, liners, and blends where downgauging and bubble stability are weighted over extreme abuse resistance.

    Resin 6109 specification envelope and lot-to-lot boundaries

    Manufacturer batch certificates for 6109 commonly list control ranges rather than single values. The melt flow index corridor is maintained within ±0.2 g/10 min of nominal, and density within ±0.002 g/cm³. These boundaries derive from reactor control of butene-1 incorporation, hydrogen chain-transfer ratio, and pelletisation thermal history. Film tensile and tear properties are generally not lot-release specifications; they are measured on film samples after fixed blown-film fabrication because orientation, cooling rate, and die geometry alter crystalline anisotropy. The representative property envelope in Table 1 is based on 25 μm film prepared at a 2.5:1 blow-up ratio. The data must be confirmed against the current production-lot certificate, because additive package level and test-film gauge shift the measured values.

    Table 1. Representative nominal property data for 6109 blown film
    PropertyTest standardNominal valueUnit
    Melt flow indexASTM D12381.0g/10 min
    DensityASTM D15050.918g/cm³
    Dart drop impact F50 at 25 μmASTM D1709110g
    Elmendorf tear MDASTM D1922300gf
    Elmendorf tear TDASTM D1922350gf
    Tensile yield strength MD/TDASTM D88211MPa
    Tensile break strength MDASTM D88238MPa
    Tensile break strength TDASTM D88234MPa
    Elongation at break MDASTM D882700%
    Elongation at break TDASTM D882800%
    Secant modulus 1% MDASTM D882220MPa
    HazeASTM D10036%
    Gloss 45°ASTM D245745GU
    Film-to-film coefficient of frictionASTM D18940.10—

    The property balance reflects a butene-copolymer architecture. The F50 dart impact of 110 g is characteristic of a Ziegler-Natta butene LLDPE at 25 μm film gauge; a hexene-copolymer LLDPE of equivalent density and melt index typically exceeds that value by 20–30%. Haze and gloss values are measured on film without added process aid. Silica antiblock addition above 2,000 ppm will raise haze and lower gloss in proportion to particle size distribution.

    What defines the blown-film processing window for a butene-copolymer LLDPE?

    For 6109, stable bubble formation is normally obtained with a die gap of 1.5–2.5 mm, a blow-up ratio of 2.0:1 to 3.5:1, and a frost-line height of 250–400 mm measured from the die face. Melt temperature measured at the adapter is maintained between 190 °C and 230 °C; sustained operation above 250 °C accelerates chain scission, carbonyl formation, and gel generation. Extruder barrel profiles are zone-specific: feed throat 30–50 °C, compression zone 160–190 °C, metering zone 190–210 °C. Butene-copolymer LLDPE of this melt index exhibits lower melt strength than high-pressure LDPE; a low-pressure die design and dual-lip air-ring control are required to prevent bubble flutter at gauges below 20 μm. Barrier-flight screws with 24:1 to 30:1 L/D are specified in high-output lines because the resin requires high shear in the melting zone without extended residence time.

    Cooling air for the bubble should be supplied by a dual-lip air ring capable of 15–25 m³/h per metre of die circumference; inadequate air flow produces stalk instability and gauge variation. Internal bubble cooling may be used above 100 kg/h output to remove heat from the inner film surface and lower the frost line. The dewpoint of internal bubble air must be held below -10 °C to prevent condensation on the inner bubble wall.

    Plant-scale blown-film data show three recurrent failure modes when 6109 is run on equipment originally configured for high-pressure LDPE. First, low-compression LDPE screws can generate oxidative gels at the die lip when output is pushed above the screw design limit; the resulting fish-eye defects are quantifiable by ASTM D3354 gel-count testing. Second, worn barrel and screw clearances above 0.5 mm reduce melting homogeneity and produce visible gauge bands under uniaxial orientation. Third, moisture condensation on pellets stored outdoors at relative humidity above 60% can create surface bubbles in the film; under those conditions, pellet pre-drying in a desiccant dryer at 60–70 °C for 2 h is recommended. The desiccant bed dewpoint should remain below -20 °C, because the resin surface moisture is not easily removed by ambient air sparging.

    In produce-bag, carrier-bag, industrial-liner, garment-film, and agricultural-mulch applications, 6109 is usually extruded at 25–75 μm gauge. For frozen-food abuse packaging or heavy-duty shipping sacks requiring low-temperature puncture resistance, 6109 is generally upgraded with a hexene-copolymer LLDPE or a metallocene LLDPE. In agricultural film, 6109 is frequently blended with 20–40% high-pressure LDPE to improve bubble shape and reduce melt orientation. As the LDPE fraction increases, heat-seal initiation measured by ASTM F2029 and hot-tack measured by ASTM F1921 generally shift upward because LDPE has a broad molecular weight distribution and lower seal-surface stress absorption. Application-specific blend data are line-dependent and should be regenerated on the target coextrusion line rather than transferred from a monolayer cast-film database.

    When 6109 replaces hexene-copolymer LLDPE in high-speed coextrusion

    Replacement of a hexene-copolymer LLDPE with 6109 in a three-layer coextruded structure commonly requires a reduction in die throughput or a narrowing of the bubble geometry. Comparative film data generated at 25 μm gauge, 2.5:1 blow-up ratio, and 210 °C melt temperature indicate that 6109 delivers 20–30% lower F50 dart impact under ASTM D1709 than a 0.918 g/cm³ hexene-copolymer LLDPE of equivalent melt index. Machine-direction Elmendorf tear under ASTM D1922 may be lower by 10–15%, while transverse-direction tear can approach hexene performance when frost-line height and air-ring cooling are reoptimised. The physical origin is the shorter butene branch length of 2 carbon atoms, compared with 4 carbon atoms for hexene; shorter branches disrupt crystallizable ethylene sequences less efficiently and produce a lower tie-molecule density at equal solid-state density. Below 20 μm, 6109 should not be considered a drop-in substitute for hexene LLDPE without a bubble-stability trial.

    Comparisons with high-pressure LDPE and metallocene-catalysed LLDPE further define the product position. LDPE contributes higher melt extension and bubble shape retention but lower tensile strength and lower dart impact. Metallocene LLDPE grades provide higher dart impact and optical clarity at equivalent density but can generate higher extruder die pressure and amperage. Published comparative studies for 6109 on grooved-feed extruders with 25:1 L/D are limited relative to hexene-copolymer LLDPE; however, plant trials generally show that 6109 requires a 5–10% lower melt temperature to avoid surface melt fracture on the same screw design. The resin is therefore specified for monoextruded products and coextruded core layers, while the skin layer may contain LDPE or hexene LLDPE to supply surface tear and seal strength.

    Regulatory compliance does not guarantee finished-film food-contact status

    The base resin is generally regarded as compliant with olefin polymer provisions under FDA 21 CFR 177.1520(c) and with the European Union food-contact framework Regulation (EC) No 1935/2004. Compliance is conditional on migration testing of the finished film in food simulants: 10% ethanol for aqueous food, 3% acetic acid for acidic food, and 95% ethanol or isooctane for fatty food under EU 10/2011. A change in layer structure, print ink, or overtemperature extrusion can shift migration into a noncompliant range. The resin should not be formulated with pro-oxidant transition metal salts or with amine-based antifog additives without pre-qualification because the phenolic stabilizer package may be consumed prematurely, reducing long-term heat-aging stability. Outdoor exposure without a UV stabilizer masterbatch is not recommended; weathering resistance must be established separately by ISO 4892-2 accelerated xenon-arc testing. Storage above 40 °C in direct sunlight can raise pellet temperature above 50 °C and induce additive bloom at the pellet surface, which later appears as die-lip deposits.

    Table 2. Compliance verification matrix for 6109 film structures
    Regulatory referenceScopeRequired end-use validation
    FDA 21 CFR 177.1520(c)Olefin polymers for food contactFinished-film extraction passing FDA 21 CFR 177.1520(c) 3.1a/3.2a
    EU 10/2011Plastic food-contact materialsOverall migration ≤10 mg/dm² in specified simulants
    REACHRegistration and SVHCSupplier confirmation of SVHC absence
    RoHS 2011/65/EUHazardous substancesScreen for Pb, Cd, Hg, Cr VI, PBB, PBDE

    A finished-film compliance assessment must include converter-added masterbatches, processing aids, printing inks, and post-consumer recycle content. The butene-copolymer base resin may meet compositional criteria while the final laminate fails overall migration; therefore, the compliance status of 6109 is not inherited by the converted article.

    During start-up transitions from LDPE to 6109, the die should be purged below 180 °C to avoid thermal degradation of residual LDPE. Extrusion lines with PTFE-coated die lips must operate fume extraction because butene-copolymer LLDPE emits low-molecular-weight oligomers at melt temperatures above 230 °C. The resin is incompatible with polyvinyl chloride contamination; HCl released from PVC at processing temperature accelerates polyethylene chain scission and can produce black specks and odour.

    Top