| HS Code | 668410 |
| Material | Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene |
| Filler Content | 20% Mineral |
| Density | 1.05 g/cm³ |
| Melt Flow Rate | 20 g/10 min |
| Tensile Strength At Yield | 15.0 MPa |
| Tensile Elongation At Break | 100% |
| Flexural Modulus | 0.700 GPa |
| Hardness Shore D | 60 |
| Vicat Softening Temperature | 100 °C |
| Deflection Temperature At 0 46 Mpa | 75 °C |
| Processing Temperature | 190-220 °C |
| Mold Temperature | 20-40 °C |
| Drying Temperature | 70-80 °C |
| Drying Time | 2-4 hr |
As an accredited Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene comes in 25 kg polyethylene-lined multiwall paper bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene in palletized bags, secured for ocean transport. |
| Shipping | Chase Plastics CP Pryme® PE100LLD-20M ships as non-hazardous LLDPE pellets, usually in 25 kg bags, stretch-wrapped pallets, octabins, or bulk trucks/railcars. Keep dry, sealed, and away from direct sunlight, heat, and contamination. No special dangerous-goods placards are normally required; follow standard handling and storage practices. |
| Storage | Store Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original packaging closed and palletized to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Rotate stock FIFO and follow the manufacturer’s SDS and local regulations. Maintain good housekeeping and avoid damaging bags. |
| Shelf Life | Indefinite shelf life when stored in original packaging, cool, dry, and out of direct sunlight; avoid excessive heat and moisture. |
For high-speed injection moulding of thin-wall dairy containers, margarine tubs and snap-on lids, Chase Plastics CP Pryme® PE100LLD-20M linear low density polyethylene is processed neat at 100 wt% or dry-blended with 15–30 wt% clean post-industrial scrap from the same converting line. The melt mass-flow rate of 20 g/10 min under 190 °C/2.16 kg measured to ISO 1133-1:2022 permits short flow paths in cavitation-intensive tools, while the density class of 0.920–0.926 g/cm³ when confirmed to ASTM D1505 or ISO 1183-1:2019 supports rapid part solidification. Articles intended for direct food contact are evaluated under Regulation (EU) No 10/2011 for an overall migration limit of 10 mg/dm² and under FDA 21 CFR 177.1520; production hygiene follows Regulation (EC) No 2023/2006, and REACH SVHC verification is completed for every batch. The downstream process is hot-runner injection moulding on machines of 300–600 metric tons clamp force with melt temperature 200–230 °C, mould temperature 10–30 °C, injection speed 100–200 mm/s, holding pressure 400–700 bar and back pressure 5–10 bar. Projected-area clamp requirement is 3.0–5.0 kN/cm² to prevent flashing, and vents of 0.02–0.04 mm depth are necessary to avoid gas burn marks on high-cavitation tools. Slip and antiblock masterbatches are added at 2–5 wt%, colour concentrates at 2–4 wt%, and combined masterbatch loading is kept below 6 wt% so gate freeze time is not lengthened. Mould shrinkage after 48 h conditioning is confirmed by ISO 294-4, with typical flow-direction values of 1.5–2.0% and cross-flow values of 1.2–1.8%. Gate blush and hesitation marks on high-gloss lids are reduced by lowering injection velocity near the gate and raising nozzle tip temperature to 230 °C. Terminal finished product types include dairy cups, deli containers, spread tubs, dessert pots and snap-on lids.
| Compliance frame | Standard / Clause | End-use requirement | Verification data |
|---|---|---|---|
| EU food contact | Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm² | Simulant A/B/D2 migration certificate |
| US food contact | FDA 21 CFR 177.1520 | Olefin polymer direct contact | Extraction and use-temperature profile |
| Good manufacturing practice | Regulation (EC) No 2023/2006 | Traceable production hygiene | Lot-specific declaration |
| REACH | Regulation (EC) No 1907/2006, Annex XVII | No restricted substances | SVHC confirmation |
In cap and closure converting, PE100LLD-20M is introduced as a high-flow let-down resin in injection-moulded HDPE closure bodies at 10–25 wt%; the addition lowers filling pressure and improves knit-line elongation in multi-cavity tools without rendering the closure excessively soft. Where a softer liner or gasket is needed, the resin is used at 70–90 wt% with 10–30 wt% elastomer modifier or blended with a lower-density polyethylene to adjust Shore D hardness for low-torque cosmetic caps. Slip or processing lubricants are limited to 0.5–1.5 wt% because higher loadings interfere with closure torque retention and child-resistant mechanism functioning. Antioxidant masterbatch is added at 0.05–0.2 wt%, and colour concentrate at 2–4 wt%. Food and beverage closures are assessed under Regulation (EU) No 10/2011 and FDA 21 CFR 177.1520; child-resistant closures are tested according to ISO 8317, and polyolefin closures for prolonged stress-crack exposure are evaluated with ASTM D1693. The production route is injection moulding on 100–200 metric tons clamp force machines with hot-runner valve gates on 8–32-cavity tools. Melt temperature is held between 190–230 °C, mould temperature at 8–20 °C, and cycle times of 6–12 s are typical for 1.0–1.8 mm wall thicknesses. The low melt viscosity allows hydraulic injection pressures of 50–80 bar, but insufficient clamp tonnage produces flash at the parting line. Mould shrinkage of 1.4–1.9% is compensated in cavity sizing, and top-load or strip-torque tests are performed on production tools because high-flow resin can lower top-load resistance compared with fractional-melt HDPE. Terminal product types include tamper-evident beverage plugs, snap-over lids, cosmetic caps and household chemical closures with minimum wall ribs at 1.5 mm to offset long-term creep.
Carrier resin selection for pigment and functional polymer masterbatches uses PE100LLD-20M as a low-viscosity binder at addition ratios of 25–55 wt% of the total masterbatch formulation. Pigment or mineral filler loading of 30–55 wt% is common for carbon black, titanium dioxide and organic pigments; dispersants and processing waxes are metered at 0.5–5 wt%. The melt mass-flow rate of 20 g/10 min wets pigment surfaces rapidly, but the shear heating generated in pigment-laden melt streams requires strict barrel-temperature control below 220 °C to prevent degradation of azo and phthalocyanine pigments. Compounding is performed on co-rotating twin-screw extruders with L/D 40:1 and screw diameter 40–75 mm. Barrel temperature set points are 150–190 °C; pigment is introduced through a side feeder at barrel 5–6 after the carrier is melt-mixed by barrel 3. Vacuum devolatilization at −0.06 to −0.09 MPa relative pressure removes residual low-molecular-weight volatiles before the melt passes through 50–100 µm screen packs and a strand or underwater pelletizing die. Specific energy input of 0.15–0.25 kWh/kg prevents excessive shear heating, and die-face melt temperature is held at ≤190 °C to avoid pigment decomposition and pellet surface pitting. Screen pressure rise beyond 50–80 bar indicates poor dispersion or screen blockage; batch-to-batch variation in pigment particle size modifies screw torque and melt pressure. Masterbatch pellets are subsequently let down at 2–5 wt% in natural LLDPE or HDPE converting. Compliance for masterbatch is confined to Regulation (EC) No 1907/2006 REACH Annex XVII, with additional Regulation (EU) No 10/2011 evaluation when the masterbatch is intended for food-contact film or injection parts. Polymer identification follows ISO 11469 for recycled plastic streams. Terminal finished product types are pelletized colour masterbatch, UV stabilizing masterbatch and antistatic masterbatch for film, injection moulding and extrusion coating.
Housewares and storage articles are moulded from PE100LLD-20M at 100 wt% or with 5–20 wt% calcium carbonate masterbatch when higher flexural modulus is required for unsupported base panels. Pigment masterbatch is added at 2–4 wt%; if the article may be used as toy-like children’s houseware, the formulation is screened against EN 71-3 migration limits. Kitchen and food storage articles are evaluated under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011; general household articles fall under REACH and, when electrical accessory integration is present, RoHS 2011/65/EU. The production route is conventional injection moulding on machines of 250–800 metric tons clamp force with melt temperature 190–220 °C and mould temperature 15–35 °C. Holding pressure of 300–600 bar and back pressure of 5–10 bar compensate for high-flow shrinkage; if calcium carbonate is used, screw and check-ring wear accelerates above 220 °C, and preventive maintenance intervals are shortened. Sink marks over ribs and bosses require local wall reduction or gas-assisted packing; high-gloss surfaces show flow marks if injection velocity is too high. Mould shrinkage of 1.5–2.0% is used for cavity sizing and gate placement. Terminal finished product types include storage boxes, coat hangers, plant pots, waste baskets and divided drawer organisers.
Post-consumer HDPE and PP recycling streams often exhibit melt flow values below 5 g/10 min and require a lower-viscosity polyolefin to restore thin-wall or complex mould filling in heavy-gauge logistics parts. PE100LLD-20M is added at 10–30 wt% to post-consumer PP/HDPE blends for injection-moulded crates, pallets and dunnage; the upper limit of 30 wt% is imposed because higher loadings reduce environmental stress crack resistance and long-term flexural modulus under repeated pallet loading. Published data for this specific recycled configuration is limited; processors therefore run a design-of-experiment with 5 wt% increments across 10–30 wt% and compare weld-line strength and melt flow according to ISO 1133-1:2022 before tooling release. The downstream process is heavy-duty injection moulding with 800–2000 metric tons clamp force, melt temperature 200–230 °C, shut-off nozzles and mixing screws with back pressure 20–30 bar to reduce melt temperature variation. Pre-drying at 80 °C for 2–4 h is applied only when warehouse relative humidity exceeds 60% or visible surface moisture is present. Compliance for industrial logistics articles includes REACH SVHC verification and RoHS 2011/65/EU; mechanical acceptance is based on ISO 527-2 tensile properties and ISO 179-1/1eA Charpy impact. PET contamination above 5 wt% remains unmelted at polyethylene processing temperatures and creates weld-line embrittlement; cellulose, nylon and aluminium foil residues must be removed before extrusion because they produce gas voids and die-face contamination. Terminal finished product types include nestable crates, industrial pallets, dunnage trays and separation sheets for returnable packaging loops.
When electronics handling trays require static-dissipative performance, PE100LLD-20M is used as the base polyolefin in conductive compounds at 75–90 wt% with 10–20 wt% conductive carbon black and 0.2–0.5 wt% hindered phenolic antioxidant. Antistatic additives may be added at 1–5 wt% when surface resistivity in the 10⁶–10⁹ Ω/sq range is specified for component handling. The compound is produced on a co-rotating twin-screw extruder with melt temperature 170–200 °C; higher temperatures risk carbon black degradation and acrid volatile formation that condenses on die surfaces. The compounded resin is sheet extruded and thermoformed into trays, with oven ageing at 70 °C for 72 h used to check dimensional stability before release of forming tools. Compliance is governed by IEC 61340-5-1 and ANSI/ESD S20.20 for ESD control programmes, RoHS 2011/65/EU for restricted substances, and REACH for market placement. Surface resistivity is measured after conditioning at 23 °C/50% RH according to ISO 291; reported values drift after humidity cycling, so batch acceptance must not rely on single-point measurements. Carbon black loading above 20 wt% sharply reduces elongation at break and leads to brittle tray corners during component insertion. Terminal finished product types include ESD trays, PCB handling trays, component shippers and conductive dunnage for electronics assembly lines.
Competitive Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chase Plastics CP Pryme® PE100LLD-20M Linear Low Density Polyethylene is a high-flow linear low density polyethylene resin. The numeric suffix 20M is consistent with a nominal melt mass-flow rate of 20 g/10 min when tested under ISO 1133-1:2022 at 190 °C with a 2.16 kg piston load. The suffix is not a substitute for lot release testing; in a distributed grade, the lot-specific melt flow rate, density, and stabiliser package recorded on the certificate of analysis are the controlling parameters. The polymer backbone is produced by copolymerisation of ethylene with an alpha-olefin comonomer such as butene, hexene, or octene. The resulting short-chain branching differentiates it from high-pressure low density polyethylene. Published data specific to this exact configuration is limited: most publicly reported values describe the broader class of 20 g/10 min linear low density polyethylene rather than this specific distribution product. For initial design work, density for this melt-flow class is typically in the range of 0.918 g/cm³ to 0.924 g/cm³ under ISO 1183-1:2019, but the lot certificate must be used before tool design. The melt-flow class points toward thin-wall injection moulding, closures, housewares, and compounding operations where lower melt viscosity can reduce filling pressure and cycle time; it is not a direct substitute for fractional-melt blown-film grades.
| Property | Test method | Condition | Data status |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 190 °C, 2.16 kg | Certificate of analysis required |
| Density | ISO 1183-1:2019 | 23 °C | Certificate of analysis required |
| Tensile stress at yield | ISO 527-2:2012 | 23 °C, 50% RH | Published data limited |
| Tensile strain at break | ISO 527-2:2012 | 23 °C, 50% RH | Published data limited |
| Flexural modulus | ISO 178:2019 | 23 °C, 50% RH | Published data limited |
| Notched Charpy impact strength | ISO 179-1:2023 | 23 °C | Published data limited |
| Vicat softening temperature | ISO 306:2022, A50 | 10 N load | Published data limited |
A single-point melt flow rate is insufficient for gate and runner design. Capillary rheometry on the lot should be performed at 190 °C, 210 °C, and 230 °C across apparent shear rates from 100 s-1 to 10,000 s-1. The resulting viscosity curve is used to calculate pressure drop in the runner system. For thin-wall parts, mould-filling shear rates may exceed 1,000 s-1, which is outside the range captured by melt flow rate alone. The power-law index of LLDPE is shear-rate dependent, so a constant-index assumption should be avoided over the full shear-rate window.
At equivalent density and temperature, a 20 g/10 min LLDPE has lower melt viscosity than a 0.5–1.0 g/10 min fractional-melt film grade. This difference is most visible in injection pressure, spiral-flow length, and pressure drop across the runner and gate. Capillary rheometry under ASTM D3835-16 at 190 °C is required because single-point melt flow rate data do not capture viscosity behaviour at mould-filling shear rates. The same molecular weight reduction that improves flow also lowers extensional viscosity and melt strength. As a result, the material is less suitable for high-stalk blown film, deep-draw thermoforming, and large-part extrusion blow moulding than fractional-melt LLDPE. Published data for this specific configuration is limited; direct substitution in bubble-stability-sensitive operations should be justified by a side-by-side film or part trial.
| Attribute | PE100LLD-20M class | Fractional-melt LLDPE | Test method or equipment |
|---|---|---|---|
| Melt flow rate class | 20 g/10 min | 0.5–1.0 g/10 min | ISO 1133-1:2022 |
| Viscosity at mould-filling shear rates | Lower | Higher | ASTM D3835-16 |
| Injection pressure requirement | Lower | Higher | Machine pressure transducer |
| Melt strength | Lower | Higher | Extensional rheometer |
| Thin-wall injection moulding | Suitable | Limited | Process trial |
| High-stalk blown film bubble stability | Reduced | Standard | Film tower trial |
| Environmental stress-crack resistance at equal density | Lower relative | Higher relative | ASTM D1693-21 |
Lot-to-lot variation in comonomer type can also shift the shear-thinning profile. Hexene- and octene-copolymerised LLDPE grades often show different tear and impact properties than butene-copolymerised LLDPE at the same density and melt flow rate. The CP Pryme® grade should be compared with the incumbent material using the same comonomer class. If comonomer type is not declared on the certificate of analysis, computational screening is not a substitute for mechanical testing on conditioned specimens.
On injection moulding machines in the 120–180 tonne clamp force class, a general-purpose polyolefin screw with an L/D ratio between 20:1 and 24:1 and a compression ratio near 2.5:1 is normally adequate for this melt-flow class. Barrel zone settings typically progress from 190 °C at the feed throat to 230–240 °C at the nozzle; melt temperature should remain below 260 °C to limit thermo-oxidative degradation. Shot size should be kept between 30% and 70% of barrel capacity to control residence time. Pre-drying is not generally required below 60% relative humidity; if surface condensation is present, 80 °C for 1–2 h in a desiccant dryer removes surface moisture. Hot-runner manifolds should be thermally mapped before production because cold zones in a hot runner produce visible flow lines in thin-wall parts.
Batch-to-batch variance in a distributed LLDPE grade may appear as a shift in peak injection pressure or screw recovery time. Plants with statistical process control should measure incoming melt flow rate under ISO 1133-1:2022 before lot approval and monitor screw recovery time at constant rotation speed. An increase of more than 10% in recovery time may indicate a shift in viscosity or the presence of contamination. The feed throat should be kept cool enough to prevent pellet bridging; if bridging occurs, the lot may contain fines or irregular pellet geometry, which should be documented for the supplier. Published data for this specific configuration is limited, so these control limits should be established after baseline data are collected on the processing line.
Before switching from a polar polymer to PE100LLD-20M, the barrel should be purged with a low-MFR polyolefin to remove residues that degrade above 220 °C. Co-extrusion with EVOH or nylon requires tie resins because LLDPE does not adhere to polar barrier polymers; the exact tie resin grade depends on the barrier material and layer ratio.
When PE100LLD-20M is evaluated as a carrier resin in polyolefin masterbatch or filled compound, a co-rotating twin-screw extruder with an L/D ratio of 36:1 to 44:1 and side-feed capability is the typical compounding platform. The high-flow class assists pigment and filler wetting at lower specific energy input than a fractional-melt carrier, but the lower molecular weight reduces strand integrity if the cooling water temperature is too high. Underwater pelletising with water temperature below 30 °C and die plate temperature not exceeding 240 °C is common for LLDPE compounds. The exact additive loading must be confirmed by torque, melt pressure, and dispersion tests because published data for this specific configuration is limited.
Film and sheet extrusion is technically possible but not the primary design window. If a film trial is conducted, a narrower die gap of 0.8–1.0 mm and a blow-up ratio below 2.0:1 help stabilise the bubble; however, melt strength limitations remain. The material should be kept away from strong oxidising agents and should not be held at melt temperatures above 260 °C for prolonged cycles. When pellets are stored in humid environments, surface moisture can produce surface defects; in such cases the pre-drying condition described above is applied before extrusion.
Designers replacing a fractional-melt LLDPE with PE100LLD-20M to shorten cycle time or reduce injection pressure should measure tensile yield stress according to ISO 527-2:2012, flexural modulus according to ISO 178:2019, and notched Charpy impact strength according to ISO 179-1:2023. Specimens should be conditioned at 23 °C and 50% relative humidity for 88 h according to ISO 291. Lower molecular weight grades often show lower environmental stress-crack resistance than fractional-melt LLDPE at the same density; the relevant test is ASTM D1693-21 with a notched specimen in a surfactant environment. A claim of equivalent part performance must be supported by side-by-side testing because published data for this specific configuration is limited.
Thermal properties such as Vicat softening temperature may be tested using ISO 306:2022 method A50 with a 10 N load. Flexibility in thin-wall packaging is better assessed by dynamic mechanical analysis across the service temperature range than by a single modulus point. Part geometry features such as sharp corners in thin-wall lids concentrate stress; a less severe radius may be required when switching to a higher-flow LLDPE because the lower molecular weight can reduce crack propagation resistance. Gate location should be reviewed together with viscosity data because jetting can occur at high injection speeds.
If the CP Pryme® grade is supplied with a post-consumer or post-industrial content claim, the buyer should require lot-level documentation that references ISO 14021:2016 for environmental declarations and identifies the recycled feedstock source. Food-contact suitability is not automatic for recycled LLDPE. In the European Union, recycled plastic intended for food contact must comply with Regulation (EU) 2022/1616, including the appropriate decontamination technology and authorisation status; in the United States, a food-contact article may require a determination under FDA 21 CFR 177.1520 or a food-contact notification. Electrical and electronic applications should be checked against RoHS Directive 2011/65/EU Annex II for restricted substances. REACH compliance requires SVHC screening under Regulation (EC) No 1907/2006.
If the lot is not marketed as food-contact grade, it should not be used in food packaging even if the base resin chemistry is acceptable. Processing aids, stabilisers, and possible contaminants in recycled feedstock are lot-specific variables. Published data for this specific configuration is limited; the certificate of analysis and regulatory documentation must be obtained before the material is used in regulated applications.