| HS Code | 156258 |
| Polymerbase | Polybutylene terephthalate (PBT) |
| Reinforcement | Glass fiber |
| Glassfibercontent | 20 wt% |
| Hydrolyticresistance | Hydrolytically stabilized |
| Density | 1.45 g/cm3 |
| Tensilestrength | 110 MPa |
| Elongationatbreak | 2.5% |
| Flexuralmodulus | 6500 MPa |
| Notchedimpactstrength | 6 kJ/m2 |
| Hdtat1 82mpa | 205 °C |
| Meltingpoint | 225 °C |
| Waterabsorption | 0.08% |
| Moldingshrinkage | 0.4% |
| Flamerating | UL 94 HB |
| Dielectricstrength | 20 kV/mm |
| Volumeresistivity | 1E15 Ω·cm |
| Moldingtemperature | 240-260 °C |
| Dryingcondition | 120 °C for 3-4 h |
As an accredited Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB is packed in 25 kg moisture-barrier bags, 40 bags per pallet (1,000 kg net). |
| Container Loading (20′ FCL) | 20′ FCL dry container loaded with palletized 25 kg bags of Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB, securely strapped. |
| Shipping | Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB is shipped as non-hazardous, glass-fiber-reinforced PBT pellets in sealed moisture-barrier bags or octabins. Store and transport in a cool, dry, ventilated area away from direct sunlight and moisture; no UN number or transport hazard class applies. Keep packaging closed and avoid heat/moisture exposure. |
| Storage | Store Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and incompatible materials. Keep containers tightly sealed and palletized off the floor. Do not expose to open flames or excessive heat. Protect bags from punctures and contamination, and follow first-in, first-out stock rotation to preserve material properties. |
| Shelf Life | Shelf life is 2 years under recommended storage conditions: dry, cool, sealed original packaging, away from direct sunlight and moisture. |
In multicavity tooling for automotive underhood connector bodies, LONGLITE® PBT+GF-Hydrolytic 4820 NCB is pre-dried at 120 °C for 4–6 h in a dual-bed desiccant dryer with −30 °C dew-point air until residual moisture remains below 0.02 wt%. The melt is introduced through a general-purpose 3-zone screw with compression ratio 2.5:1 and non-return valve maintained to prevent drool; barrel temperatures are set from 240 °C in the rear zone to 260 °C at the nozzle, with measured melt temperature held at 255–265 °C. Mould temperature is controlled at 80–90 °C through a pressurised water thermolator to reduce anisotropic glass-fibre orientation around gate lands and maintain long connector-channel flatness within ±0.05 mm. Production-scale failure modes observed on multicavity tools include splay and gate blush when granulate reabsorbs moisture at ambient relative humidity above 60 %, burn marks at unvented end-of-fill locations when injection velocity exceeds 300 mm/s, and short shots in 0.5 mm snap-latch sections when holding pressure drops below 80 MPa. Cold-runner regrind is limited to 15 wt% for engine-compartment programmes, and only dried regrind is returned to the hopper. The black NCB colour package provides ultraviolet opacity for storage and handling, but does not replace a dedicated heat-stabiliser system where continuous underhood wall temperatures exceed 150 °C. Qualification is normally performed against USCAR-2 for terminal retention, ISO 16750-4 for damp heat cyclic exposure, and SAE J1455 for chemical exposure to engine oil and washer fluid; published data for this specific grade should be checked on the supplier certificate of analysis because variations in glass-fibre sizing can shift hot-water tensile-strength retention by more than 10 % after 1000 h of ageing.
Electric coolant pump impellers moulded from this grade operate in 50:50 ethylene glycol/water mixtures at return-line temperatures reaching 115–125 °C during thermal throttling; the dominant degradation pathway is acid-catalysed chain scission of the PBT ester linkage, which the hydrolytic stabiliser package in 4820 NCB is formulated to suppress by capping reactive chain ends and reducing the equilibrium concentration of free acid groups. Moulding is carried out with a low-shear screw design and melt temperature at 260–270 °C, while the tool is maintained at 100–120 °C to promote crystallinity in the hub and blade root sections and to reduce internal stress that can accelerate microcracking under thermal cycling. The impeller gate should be placed at the hub centre, not at the blade tip, because glass-fibre orientation crossing blade leading edges creates stress concentrations where cavitation-induced pitting initiates at pump speeds above 12 000 min⁻¹. Post-mould annealing for 1 h at 130 °C may be used to stabilise dimensions of the shaft bore, but longer annealing consumes the hydrolysis stabiliser and reduces hot-water property retention. If regrind is used in impeller production, the ratio is held at ≤ 10 wt% because repeated shear causes fibre attrition that shifts the part balance by 5–10 mg·mm and increases water-uptake heterogeneity. Relevant validation includes water absorption per ISO 62, tensile-strength retention per ISO 527-2 after immersion at 95 °C, and UL 746C evaluation for use in water-contact service. Operational boundaries include avoidance of strongly alkaline cooling-system cleaners with pH above 9 at temperatures above 80 °C, because these accelerate ester hydrolysis even in stabilised PBT; published data for this specific configuration under long-term glycol immersion is limited, so final impeller testing must include pressure-cycle and cavitation exposure.
Relay bobbins and terminal carriers in appliance control modules demand a different balance of thin-wall filling and low post-mould distortion. LONGLITE® PBT+GF-Hydrolytic 4820 NCB is dried at 120 °C for 5 h and processed at a melt temperature of 245–260 °C with mould temperature 60–80 °C to avoid core-pin dragging on bobbin axes. Thin-wall sections of 0.4–1.2 mm are filled using a valve-gate hot runner with high speed injection, but screw rotation must be reduced to prevent fibre breakage that lowers tracking resistance across coil-flange surfaces. Regrind from cold sprue breakages is acceptable up to 20 wt% in bobbin cores but is excluded from terminal carriers with walls below 0.5 mm, where flow-length variation from inconsistent regrind particle size produces short shots and weld-line voids. The carbon-black NCB pigmentation contributes to uniform colour stability but does not guarantee flame retardance; if the assembly must satisfy IEC 60335-1 clause 30.2.3.1 at 750 °C glow-wire without ignition, the final part must be tested as a complete appliance component rather than relying on bulk resin performance. Comparative tracking index is evaluated per IEC 60112, with a typical screening threshold of ≥ 250 V for control-module relay bobbins used in humid household environments. End products include coil bobbins, relay bases, and terminal-position assurance housings where dimensional stability after 1000 h at 85 °C/85 % RH is the primary selection criterion.
Water-inlet manifolds and dispenser housings in washing machines are moulded from this hydrolysis-resistant PBT/GF grade by hot-runner systems with sequential valve gating to prevent air traps at sealing faces. Granulate is pre-dried at 120 °C for 4 h to below 0.02 wt% moisture, and melt temperature is kept at 250–265 °C; the tool is maintained at 80–100 °C to produce flat gasket grooves with lateral dimensions stable within ±0.08 mm after 24 h water immersion at 23 °C. A cold sprue is generally not generated because the manifold system is direct-gated; where cold sprues occur, regrind is limited to 12 wt% and only after re-drying. Seal-compression flanges require holding pressure above 100 MPa and packing time of at least 1.5 s/mm wall thickness, otherwise differential shrinkage between the glass-rich core and unfilled sealing surface creates sink marks and flange leakage. Compliance testing follows IEC 60335-1 clause 30.2 for resistance to heat and fire, along with UL 746C water-contact exposure; the material is not automatically suitable for potable-water approvals such as NSF/ANSI 61, and such use requires separate certification. Continuous exposure to undiluted alkaline descaler, especially at pH above 10 and temperature above 80 °C, is outside the operational boundary because hydrolysis stabilisers cannot compensate indefinitely for aggressive alkaline ester cleavage. End products include washing-machine water manifolds, dispenser bodies, and pump-retaining flanges where the replacement of brass reduces weight and provides resistance to detergent corrosion, but stress-cracking resistance must be confirmed on the assembled part under full spray-water cycling.
In automotive actuator motors, brush holder assemblies are insert-moulded or assembled over copper carriers; the hydrolysis-stabilised PBT/GF material is processed at 260–270 °C melt temperature and 90–100 °C mould temperature to minimise fibre-rich weld lines around inserted brush tubes. Insert cores are preheated to 120 °C before moulding to reduce differential thermal contraction at the polymer-copper interface; without preheating, cracking may appear at the insert edge after 500 thermal cycles from −40 °C to 150 °C. The black NCB pigmentation provides sufficient opacity for laser marking of date codes and batch identifiers without additional colour masterbatch, which would dilute the hydrolytic stabiliser if added at the press. Regrind is excluded from insert-moulded brush-card production because carbon-black dispersion and fibre-length distribution in recycled material change the coefficient of linear thermal expansion and increase brush-tube misalignment. Electrical insulation system eligibility is assessed under UL 1446, while motor-end thermal ageing follows IEC 60034-1 guidance; the grade is not a substitute for a dedicated high-temperature thermoplastic where brush-card hot-spot temperatures exceed 180 °C for extended periods. End products include brush-card frames, commutator carrier plates, and actuator sensor brackets where dimensional stability, low water uptake in gearbox enclosures, and resistance to dilute glycol mist from adjacent cooling circuits are required simultaneously.
Outdoor enclosure lids and base flanges moulded from LONGLITE® PBT+GF-Hydrolytic 4820 NCB are dried at 120 °C for 4–6 h and then processed with melt temperature 250–265 °C and mould temperature 80–100 °C to stabilise sealing-groove flatness. Large rectangular flanges are gated near the central mould insert rather than at corner locations to prevent differential glass-fibre orientation from producing saddle-shaped warp, which can exceed 0.2 mm across a 300 mm seal land on improperly gated tools. Holding pressure is set between 100 MPa and 140 MPa, with packing time adjusted to 1.5 s/mm wall thickness at the sealing rib; insufficient holding pressure produces visible sink at rib intersections and increases the risk of water ingress under IEC 60529 IP65 spray conditions. The carbon-black NCB formulation provides significant ultraviolet radiation absorption, and UL 746C f1 recognition is the appropriate certification when the final part is specified for outdoor water and UV exposure; however, f1 recognition is thickness- and colour-dependent, so the enclosure wall must be tested in the final moulded configuration rather than assumed from raw-material data alone. Regrind is permitted up to 20 wt% in non-sealing enclosure walls, but sealing flanges are moulded from virgin material to avoid carbon-black agglomeration leading to microporosity at the seal surface. Exposure testing under ISO 4892-3 QUV-A may be used to screen crack formation after 1000 h, but final qualification for telephone-network outdoor equipment usually requires testing under both UV and condensation cycles because repeated wetting can leach surface stabiliser and alter gloss without reducing bulk mechanical strength. End products include NEMA-style outdoor telecommunication boxes, IoT node enclosures, and IP65-rated cable junction housings where long-term dimensional stability and hydrolytic resistance in rain-washed environments are the governing design constraints.
| Assembly segment | Standard / method | Key clause or testing condition | Typical acceptance target |
|---|---|---|---|
| Automotive underhood connector bodies | USCAR-2 | Terminal retention after 150 °C ageing | No terminal push-out below 75 N |
| Electric coolant pump impeller | UL 746C | Immersion in 50:50 ethylene glycol/water at 95 °C | Tensile-strength retention ≥ 50 % after 1000 h |
| Relay bobbin | IEC 60112 | Comparative tracking index | ≥ 250 V |
| Appliance water manifold | IEC 60335-1 | Clause 30.2.3.1 glow-wire | No ignition at 750 °C / 2 s on final part |
| Motor brush holder | UL 1446 | Insulation system evaluation | System class ≤ 155 °C |
| Outdoor telecom enclosure | UL 746C f1 | UV and water exposure suitability | No crack after 1000 h QUV-A |
Competitive Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 NCB is a 20 wt-% glass fibre reinforced polybutylene terephthalate compound containing a hydrolytic stabilisation additive system. The grade fragment 4820 identifies the glass fibre loading, and the suffix NCB identifies the colour package of the supplied pellets. The material is melt-processed on reciprocating-screw injection moulding machines, and it is also available in pellet form for further compounding or conversion. The hydrolytic stabiliser slows chain scission in wet heat, but it does not eliminate the need for drying or make the polymer suitable for unlimited exposure to saturated steam. Before melting, residual pellet moisture is reduced below 0.02 wt-% as determined by ISO 15512. Dry pellets exposed to ambient air at 60% RH or higher can exceed 0.04 wt-% residual moisture within 4 h; production feeding therefore uses closed-loop dehumidifying dryers with a supply-air dew point of −30°C or lower. Typical injection-moulding parameters are melt temperature 250–270°C, barrel temperature 240–270°C, mould surface temperature 80–100°C, and back pressure 0.3–0.7 MPa. The material is supplied as cylindrical pellets with bulk density generally between 0.70 g/cm³ and 0.90 g/cm³. The grade is used in under-hood connector housings, sensor bodies, automotive pump housings, and electrical switch carriers where mechanical load and condensing moisture occur simultaneously. Published data for the specific 4820 NCB configuration is limited in the open literature; the following technical sections therefore give representative property ranges for comparably stabilised 20 wt-% glass-filled PBT compounds and the processing boundaries observed on production-scale equipment. These ranges are qualification starting points and must be confirmed against the current Chang Chun technical data sheet for 4820 NCB before any final part acceptance.
Drying is performed at 120°C for 3–4 h in a desiccant-wheel dryer. Hopper air flow should be sized at 0.6–1.0 m³/h per kg/h of polymer consumption; lower air flow produces uneven drying in the bottom of the hopper and increases lot-to-lot property scatter. Direct gas-fired dryers without a desiccant bed are not suitable because the inlet-air dew point cannot be held below −20°C, especially in hot-humid plants. Outlet moisture is measured with a calibrated loss-in-weight moisture analyser under nitrogen purge; capacitive sensors can under-report residual moisture in glass-filled pellets. If the drying hopper is opened for refilling, the feeder throat should be purged with dry nitrogen at 0.2–0.4 MPa to reduce moisture ingress during operation. Melt temperature measured by air-shot pyrometer must not exceed 270°C; at 260°C, residence time should not exceed 8 min, and at 270°C the limit is 5 min. Beyond these limits, hydrolytic stabiliser decomposition and random polyester chain cleavage produce an increase in carboxylic acid end groups, which is detectable as a melt-viscosity drop and a reduction in tensile strength after moulding. Screw geometry with compression ratio 2.5:1–3.0:1 and a low-shear metering section is preferred; high-compression screws increase viscous dissipation and drive the melt temperature above the set barrel temperature. On twin-screw compounding lines, co-rotating extruders with 32:1 to 40:1 L/D ratio are operated with side-stuffed glass fibre to preserve fibre length. Aggressive distributive mixing downstream of the fibre feed reduces fibre length, lowers notched impact, and increases mould-shrinkage anisotropy. In injection moulding, a melt cushion of 2–4 mm and a decompression stroke of 2–5 mm are typical; excessive decompression draws air and moisture into the barrel and produces splay. Clamp force requirement is approximately 0.6–0.8 kN per cm² of projected area for sections 1.0–2.0 mm thick. For flow lengths greater than 150 mm, gate location should be re-evaluated because glass-filled PBT shows anisotropic shrinkage and weld-line weakness. Lot-to-lot melt viscosity is controlled by MVR per ISO 1133-1:2022 at 250°C and 2.16 kg. A shift greater than ±15% from the qualified baseline requires re-validation of cushion, injection velocity, holding time, and hot-runner balance; fill imbalance in multi-cavity tools is the common first failure mode on production lines. Hot-runner systems should use independent tip-temperature control, with manifold temperature 250–270°C and tip temperature 240–260°C, because dead spots at the tip allow local residence time to exceed 8 min and generate dark-coloured hydrolysis products.
Mechanical design values for 20 wt-% glass-filled hydrolytically stabilised PBT are orientation-dependent. Tensile bars moulded to ISO 527-2 type 1A and tested in the end-gated flow direction give higher modulus than cross-flow specimens cut from a plaque. The following representative ranges are for conditioned specimens at 23°C and 50% RH per ISO 291; they are not simultaneous lot minima or maxima.
| Property | Test method and condition | Representative range | Unit |
|---|---|---|---|
| Density | ISO 1183-1 | 1.43–1.47 | g/cm³ |
| Tensile stress at break | ISO 527-1/-2, 5 mm/min | 95–120 | MPa |
| Tensile modulus | ISO 527-1/-2, 1 mm/min | 6.0–7.5 | GPa |
| Flexural modulus | ISO 178, 2 mm/min | 5.0–6.5 | GPa |
| Notched Charpy impact, 23°C | ISO 179-1/1eA | 7–10 | kJ/m² |
| Heat deflection temperature, 1.8 MPa | ISO 75-1/-2 | 190–210 | °C |
| Mould shrinkage, flow | ISO 294-4 | 0.3–0.6 | % |
| Water absorption, 24 h | ISO 62 | 0.15–0.25 | % |
Electrical breakdown and tracking performance must be verified on the specific colour lot. Glass-filled PBT compounds of this class typically exhibit dielectric strength of 18–22 kV/mm at 2.0 mm thickness under IEC 60243-1; comparative tracking index is commonly 250–300 V per IEC 60112. The UL 94 classification for non-flame-retardant glass-filled PBT is generally HB at 1.6 mm, but the specific yellow card for 4820 NCB controls. Because NCB is not a brominated flame-retardant system, applications requiring V-0 at the same wall thickness require selection of a flame-retardant grade. ASTM and ISO tensile data are not interchangeable; ASTM D638-14 type I specimens and ISO 527-2 type 1A specimens differ in gauge dimensions and strain rate, and design data generated under one method cannot be transferred directly to the other.
Hydrolytic stabilisation becomes the controlling material variable when PBT components are exposed to condensing humidity, hot water, or glycol-water mixtures in engine compartments and pump housings. In unstabilised PBT, absorbed water attacks the ester linkage, generating carboxylic acid and hydroxyl end groups. The carboxylic acid groups then catalyse further random chain scission, producing an autocatalytic loss of average molar mass and a rapid drop in tensile strength. A hydrolytic stabilisation package functions by capping carboxylic acid end groups or by consuming dissolved water before chain cleavage propagates. The effect is not complete protection but a slower rate of property loss under identical exposure. For qualification, specimens are immersed in distilled water at 80°C per ISO 175 and tensile-tested according to ISO 527-2. Accelerated humidity ageing is run at 85°C and 85% RH in a temperature-humidity chamber conforming to IEC 60068-2-78; tensile properties are measured after 500 h and 1000 h. Retention values for the specific 4820 NCB configuration must be obtained from Chang Chun’s current comparative data. Published data for this specific configuration is limited, but hydrolytically stabilised PBT grades generally show less carboxylic acid end-group build-up than standard PBT-GF20 after hot-wet aging. Acid value titration, expressed in meq/kg, is a more direct measure of stabiliser exhaustion than tensile strength alone because molecular weight loss precedes the final brittle failure.
Continuous service above 80°C in pressurised steam or hot engine coolant can deplete the stabiliser pool and should be validated on the actual part. Weld-line regions are particularly susceptible because fibre orientation creates a resin-rich channel that absorbs moisture and carries it along the knit line. If a connector snap feature contains a knit line, the drop in notched Charpy after hot-wet aging is usually larger in that region than in straight-flow sections; component testing on moulded parts is required, not only on ISO flex bars. Alkaline media are incompatible because hot dilute sodium hydroxide or alkaline glycol coolants saponify the ester backbone independently of the hydrolytic stabiliser. Exposure to pH above 9.0 at temperatures above 60°C is considered an operational boundary. Amine-based additives or blowing agents can deplete stabiliser activity and should not be compounded without compatibility data.
The primary difference between 4820 NCB and a general-purpose PBT-GF20 is the stabilisation package. This difference is not observed as a large dry-state tensile modulus shift; it is observed primarily as retained molar mass and retained tensile strength after moist-heat aging. Compared with unfilled PBT, 4820 NCB has higher tensile modulus and heat deflection temperature but lower notched impact and greater mould-shrinkage anisotropy. Compared with a 30 wt-% glass-filled PBT, 4820 NCB has lower melt viscosity, lower density, and lower flexural modulus; the 20 wt-% glass loading is often used where thin-wall fill and reduced mass are more important than maximum stiffness.
| Attribute | Unfilled PBT | PBT+GF-Hydrolytic 4820 NCB | PBT-GF30 | |
|---|---|---|---|---|
| Density, ISO 1183-1 | 1.30–1.32 | 1.43–1.47 | 1.52–1.56 | g/cm³ |
| Tensile modulus, ISO 527-1/-2 | 2.4–3.0 | 6.0–7.5 | 8.0–10.0 | GPa |
| HDT, 1.8 MPa, ISO 75-1/-2 | 55–65 | 190–210 | 200–215 | °C |
| Mould shrinkage, ISO 294-4 | 1.2–1.8 | 0.3–0.6 | 0.2–0.5 | % |
For applications involving long-term saturated steam above 100°C or continuous exposure to hot glycol-water above 80°C, a polyester-elastomer or polyphenylene sulphide grade may be selected unless part-level testing demonstrates sufficient retained tensile properties. 4820 NCB is not recommended for use with hot alkaline solutions above pH 9, for direct contact with amine-cured epoxy potting compounds under heat, or for repeated steam sterilization cycles above 121°C. Regrind addition above 20% should be validated because granulation reduces glass fibre length and can shift tensile modulus, impact, and mould shrinkage. If metal inserts are used, the insert boundary should be treated as a notch in finite element analysis because moulded-in stress at the metal-polymer interface accelerates moist-heat fracture. The current product technical data sheet, lot-specific MVR, and UL 94 yellow card remain the controlling documents for final validation.