Chang Chun Longlite Pbt Gf Hydrolytic 4820 Bk

Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK

    • Product Name: Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 225885
    Filler Content 20% glass fiber
    Hydrolysis Resistance Yes
    Color Black
    Density 1.45 g/cm³
    Water Absorption 24 H 0.04%
    Tensile Strength 115 MPa
    Elongation At Break 3.0%
    Flexural Strength 175 MPa
    Flexural Modulus 6500 MPa
    Notched Izod Impact Strength 7 kJ/m²
    Heat Deflection Temperature At 1 82 Mpa 205 °C
    Melting Point 225 °C
    Mold Shrinkage 0.3–0.7%
    Volume Resistivity 1E16 Ω·cm
    Dielectric Strength 20 kV/mm
    Flammability Rating UL 94 HB

    As an accredited Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant bags, palletized and stretch-wrapped for safe industrial storage and transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with palletized 25 kg bags of Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK, shrink-wrapped and secured for export.
    Shipping Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK ships as moisture-sensitive, glass-fiber-reinforced PBT pellets in sealed original bags or drums. Keep dry, cool, ventilated, and protected from heat, sunlight, and contamination. Handle as non-hazardous industrial resin; verify current SDS, packaging, labeling, and local transport regulations before shipment.
    Storage Store Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK in original sealed packaging in a cool, dry, well-ventilated area, away from direct sunlight, heat, moisture, and strong oxidizers. Keep containers closed to prevent contamination and moisture pickup. Use first-in, first-out stock rotation and avoid prolonged storage in humid conditions. Follow local regulations and the supplier’s safety data sheet.
    Shelf Life Store in a cool, dry, well-ventilated area in unopened original packaging; typical shelf life is 12 months from manufacture.
    Application of Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK

    In production of multi-pin automotive underhood connector housings, the hydrolysis-resistant PBT compound is dried in desiccant-bed dryers at 120 °C for 4–6 h or at 130 °C for 2–3 h until the residual moisture is below 0.02 % by Karl Fischer titration of the granulate. The melt temperature window is 250–270 °C; barrel residence time is kept below 8 min, and the melt is not allowed to exceed 280 °C because the hydrolytic stabiliser package can decompose into volatile species that produce splay on the connector face. Screw back pressure is restricted to 1–2 MPa and screw speed to 60–120 rpm to limit glass-fibre attrition; fibre length reduction is measured by ash-burning and sieving only when a batch exhibits abnormally low notched Charpy impact at weld lines according to ISO 179-1/1eA:2020. Mould temperature is maintained at 70–90 °C for wall thicknesses from 0.8 mm to 2.0 mm, while hold pressure of 60–80 MPa and gate-seal time verification are used to avoid sink marks around metal terminal retainers. Multi-cavity hot-runner valve-gate tools are balanced until cavity-to-cavity shot-weight deviation is below 3 %; unbalanced filling causes differential glass orientation and changes terminal withdrawal force. Terminal products include engine-harness connector bodies, transmission solenoid connector bodies, and lambda-sensor connector boots. Electrical tracking is assessed to IEC 60112, mechanical data to ISO 527-2:2012 and ISO 178:2019, and end-use connector performance to SAE/USCAR-2; flammability classification is verified on moulded plaques under IEC 60695-11-10 or UL 94. The black concentrate is added only by the compounder; in-mould dry colour is not used because raw carbon black can increase moisture uptake and alter melt rheology. Regrind beyond 20 wt% is not recommended for snap-fit latch features because repeated heat history shortens fibre length and reduces elongation at break. The black pigmentation does not by itself confer a defined surface resistivity; if electrostatic dissipation is required, a dedicated conductive grade or secondary coating must be validated on production parts.

    What Limits Tensile Strength Retention in Coolant Temperature Sensor Housings After 1,000 h Water–Glycol Ageing?

    The key limiting variable for coolant temperature sensor housings is not the as-moulded tensile strength but the retention of tensile strength at break after immersion in a 50/50 vol% ethylene glycol/deionised water mixture at 120–125 °C for 1,000 h. Test specimens moulded to ISO 527-2:2012 Type 1A are sealed in PTFE-lined stainless steel pressure vessels; the relevant supplemental measurement is notched Charpy impact according to ISO 179-1/1eA:2020 before and after ageing. Hydrolysis proceeds preferentially at the fibre–matrix interphase because absorbed water and glycol accumulate in microvoids around glass-fibre ends created during injection moulding. Ester bond cleavage in the PBT backbone increases carboxylic-acid end-group concentration and reduces molecular weight, which lowers the stress transfer efficiency between matrix and fibre; the hydrolytic stabilisation in 4820 BK retards this end-group increase but does not eliminate measurable degradation above 120 °C. Because published comparative data for this exact grade outside the manufacturer’s technical datasheet is limited, production-component validation depends on actual moulded trial batches rather than tabulated nominal values. Dilution with unfilled PBT is not recommended for sensor housings because it reduces heat deflection temperature and increases the coefficient of linear thermal expansion mismatch with the brass insert. Insert-moulded brass or stainless sensor pins are preheated to 90–120 °C to prevent a quenched amorphous skin around the pin; that skin is more permeable to water and becomes the initiating site for premature hydrolysis. Melt temperature is held at 255±5 °C, and the injection speed is profiled so that the melt front advances around the metallic insert without jetting. If cavity pressure does not reach 50 MPa within the first 0.5 s of the packing phase, the threaded sensor housing develops microporosity that lowers hydrostatic burst resistance. Terminal products include coolant temperature sensor bodies, thermostat sensor bosses, and differential pressure sensor housings for exhaust-gas recirculation loops. Validation commonly includes ISO 16750-4:2010 climate loads with hot storage at 125 °C and thermal shock into ice water; acceptance limits are controlled by the end user’s drawing rather than by a generic material standard.

    Electric coolant pump impellers and diversion valve rotors produced from this hydrolysis-resistant PBT are gated at the hub rather than at the blade tip to prevent glass-fibre concentration at the blade root and to place the weld line away from the highest bending stress. Melt temperature is set at 250–265 °C, mould surface temperature at 90–110 °C, and screw speed is limited to 80–120 rpm; the screw cushion is maintained at 3–5 mm because a smaller cushion produces erratic packing and weak knit lines, while a larger cushion increases barrel residence time and promotes tetrahydrofuran formation from PBT degradation. Additional venting is required at the last-filled blade edges because the hydrolytic stabiliser and black pigment package release low-molecular-weight volatiles at the upper end of the processing window; blocked vents produce burn marks and embrittlement on the blade pressure side. Regrind is limited to 15 wt% for impellers because lower fibre length reduces creep resistance. The application is not judged by short-term tensile strength alone; continuous exposure to hot coolant at 105–120 °C under pressure cycling creates creep-fracture mechanisms at fibre ends. Design calculation uses creep modulus measured to ISO 899-2:2003 rather than instantaneous tensile modulus, and the part is inspected for void content by micro-computed tomography when burst testing fails at blade roots. Terminal products include electric coolant pump impellers, coolant diverter valve rotors, and water-valve spacers in battery thermal management loops. The material is not suitable for continuous dry-heat exposure above 180 °C or for pressurised steam above 121 °C without end-user validation because the hydrolytic stabiliser package is outside its intended thermal boundary.

    When Dishwasher Drain Pump Housings Require Resistance to Alkaline Detergent Media at 80–95 °C

    In dishwasher drain pump bases and impeller covers, the pumped water contains alkaline builder chemicals at pH 9–11 and temperatures from 80 °C to 95 °C during the discharge phase. General-purpose glass-filled PBT can develop exposed fibre bundles and a measurable reduction in burst strength after repeated exposure, whereas the hydrolytically stabilised 4820 BK formulation delays fibre–matrix debonding under the same alkaline conditions. Pump housings with wall thicknesses of 2.0–4.0 mm are moulded at a melt temperature of 250–265 °C and a mould temperature of 70–90 °C; the thick section requires extended holding pressure, but total barrel residence time is kept below 6 min to avoid molecular weight reduction. Impact modifiers are not added at the press because they reduce the hydrolytic stabiliser efficiency; the pump housing relies on the compound’s as-supplied ductility. The sealing face is designed as a U-shaped retaining groove rather than a flat gasket face to reduce creep under clamp load. Acceptance testing includes a pressurised water leakage test after 1,000 h of cyclic operation at 85 °C; dimensional verification is performed according to ISO 294-4:2018. Electrical creepage distances and ball-pressure behaviour are checked under IEC 60335-1. Terminal products include drain pump bases, impeller covers, and filter retaining shells in household appliances. The material is not automatically approved for potable-water contact; NSF/ANSI or local regulatory certification is required if the part is used upstream of the final backflow preventer.

    When engine bay condensation cycling subjects electronic control unit housings to repeated 85 °C/85 % RH damp heat followed by -40 °C cold starts, the 4820 BK compound is selected where PA66 alternatives show excessive moisture absorption and dimensional shift. The granulate is dried at 120 °C for 4 h, and the melt is processed at 250–270 °C with an injection speed of 30–80 mm/s; the relatively low speed reduces shear heating around mounting bosses and supports uniform glass-fibre orientation in the part. Mould temperature is set at 80–100 °C. No additional impact modifier is introduced at the press because it would reduce hydrolytic stability and degrade the stabiliser’s acid-scavenging efficiency. When low locked-in stress is specified on the drawing, post-moulding annealing is carried out at 120–130 °C for 1 h; unannealed parts may show dimensional drift during the first thermal cycles because moulded-in stress relaxes in the engine bay. After 85 °C/85 % RH exposure to IEC 60068-2-78:2012, the compound retains a higher fraction of its mechanical properties than general-purpose PBT, but the end user must verify insulation resistance on the moulded part because hygroscopic uptake at the glass interface can reduce surface resistivity from the conditioned value. Terminal products include engine control unit brackets, sensor support frames, and high-humidity module covers. If the enclosure is exposed to alkaline battery electrolyte or strong base cleaning agents, compatibility testing is mandatory because PBT is attacked by strong bases regardless of hydrolytic stabilisation.

    High-Humidity Enclosure Inserts for AC and DC Charging Infrastructure

    Charging-station socket inserts and internal insulation partitions made from 4820 BK are evaluated for damp-heat resistance and electrical tracking rather than for long-term hot-water immersion. The key processing requirement is control of glass-fibre distribution around the contact apertures; a central gate with sequential hot-runner valve opening is preferred because multi-gate pin-point systems create a weld line running through the contact retention shoulder. Melt temperature is set at 255±5 °C and mould temperature at 80–100 °C to reduce fibre prominence on the contact guide face. The grade is processed as supplied; adding non-conductive PBT would alter tracking performance and reduce dimensional robustness. Because the hydrolysis-stabilised melt has a relatively low viscosity at the upper processing temperature, flash penetration into ejector clearances below 0.03 mm must be prevented by maintaining precise tool alignment and using vacuum venting. Terminal products include socket inserts, connector retainers, and phase partition walls in AC and DC charging inlets. Electrical clearance and creepage performance are evaluated to IEC 62196-1 and IEC 60664-1; flammability classification is confirmed on production-representative samples to IEC 60695-11-10 or UL 94. Continuous outdoor exposure is outside the scope of this application unless the insert is shielded from direct UV, because PBT grades without UV-stabilised cap layers can exhibit surface chalking and gloss loss over extended weathering.

    Free Quote

    Competitive Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK is a black-pigmented, 20 wt% glass-fiber-reinforced polybutylene terephthalate compound stabilized against hydrolytic degradation in hot-humid service. The 4820 designation aligns with a 20% glass-fiber loading in the LONGLITE PBT family; the BK suffix denotes black coloration. The product is intended for components requiring mechanical strength retention, dimensional stability, and low moisture uptake after exposure to water-glycol mixtures, condensing humidity, or cyclic thermal loads. Representative end-use categories include automotive underhood connectors, sensor housings, water pump impellers, electrical enclosures, circuit-breaker housings, and appliance power modules. Grade-specific physical, thermal, and mechanical values should be referenced from the manufacturer’s certificate of analysis and processing guide.

    What Distinguishes Hydrolytically Stabilized PBT From Standard 20% Glass-Filled PBT?

    The primary differentiation lies in the additive package and molecular weight retention strategy. Standard PBT GF20 grades undergo random chain scission of ester groups when exposed to hot water, steam, or glycol-water solutions. Tensile strength loss occurs because hydrolysis reduces number-average molecular weight and creates carboxylic acid end groups that autocatalyze further hydrolysis. Hydrolytically stabilized PBT grades incorporate chain-extension, acid-scavenging, or end-group-capping additives that slow this autocatalytic cycle. Published comparative data for hydrolysis-resistant PBT indicate that after 1,000 h at 85°C and 85% RH, tensile strength retention is typically 80–90%, while unstabilized glass-filled PBT may retain 40–60% depending on glass loading and saturation level. Elongation at break is a more sensitive marker: stabilized grades often retain 50% or more of initial elongation, whereas unstabilized controls can fall below 20%. These ranges are drawn from generic PBT hydrolysis literature, not from a specific supplier guarantee, and should be verified against the manufacturer’s datasheet and lot certification.

    Compared with nylon 66 grades containing 30 wt% glass, the PBT+GF-Hydrolytic grade processes at lower melt temperatures, typically 250–270°C versus 280–300°C, and absorbs less equilibrium moisture: 0.2% versus 2.5% at 23°C/50% RH when tested to ISO 62. This lower moisture uptake reduces post-molding dimensional movement and electrical property drift. However, PA66-GF30 generally offers higher continuous-use temperature capability and better fatigue resistance above 150°C. Against standard PBT GF30, the 20% glass loading provides lower density, lower melt viscosity, and reduced fiber-orientation warpage, but lower flexural modulus and tensile strength. Flexural modulus for 20% glass-reinforced PBT is commonly 6,000–7,000 MPa measured to ISO 178, while 30% glass-reinforced PBT is usually 8,000–9,500 MPa. Against unfilled hydrolysis-resistant PBT, the glass-reinforced version has higher strength and heat deflection temperature but reduced elongation at break and increased anisotropy in molded parts.

    In multi-cavity injection molding of connector bodies, the hydrolytic stabilizer does not eliminate the need for rigorous feedstock drying. Water absorbed by PBT reacts during melt processing and causes viscosity loss, surface splay, and reduced weld-line strength. A dehumidifying dryer with a dew point below −30°C should dry virgin pellets at 120–130°C for 4 h. Regrind or material exposed to storage at relative humidity above 60% should be dried for 6–8 h and verified by Karl Fischer titration to a residual moisture content below 0.02%. On twin-screw compounding lines with L/D ratios of 40:1, the same moisture discipline is required because hydrolytic degradation during compounding is irreversible and cannot be corrected later by the hydrolysis-stabilizing additive. Batch-to-batch variations in glass fiber length distribution can shift spiral flow length by 10–15%; therefore incoming fiber length and compounding screw profile should be controlled rather than relying solely on melt flow rate measurements.

    When Pre-Drying Deviates from the Vendor’s Drying Curve

    When pre-drying deviates from the vendor’s drying curve, the failure mode is frequently observed as silver streaks, foaming at the gate, or reduced screw recovery. In hydrolytically stabilized PBT, the apparent stability during normal processing can mask partial degradation until a lot is subjected to hydrothermal aging. Residual moisture above 0.02% before plastication intensifies chain scission and consumes end-group capping additives; the resulting carboxylic acid end groups then accelerate further hydrolysis under service conditions. Production-scale dryers should therefore be audited for actual dew point and air flow rather than setpoint alone. A desiccant bed that is not regenerated correctly may show a setpoint of 120°C while delivering air with a dew point of only −10°C, which is insufficient. The same applies to hopper capacity: if material consumption is high and the drying hopper residence time falls below 4 h, pellets may reach the feed throat with core moisture still elevated. Recommended drying hardware includes closed-loop desiccant systems with regeneration at 150–180°C, aftercooling, and dew point monitoring. Dryer outlet air flow should be 3.0–3.5 m³/h per kg/h of polymer throughput.

    Melt Rheology and Screw Design for 20% Glass-Fiber PBT

    Melt processing of this grade is controlled by a narrow thermal window. Barrel temperatures are typically set from 240°C at the rear zone to 260°C in the front zone, with nozzle temperature 250–265°C. Melt temperatures above 270°C for more than 8 min cumulative residence time should be avoided, because thermal and hydrolytic decomposition accelerate simultaneously. In reciprocating screw injection molding machines, a screw with L/D ratio 18:1–22:1 and compression ratio 2.0:1–2.5:1 is commonly used for glass-filled PBT. Back pressure should be held at 3–5 bar (0.3–0.5 MPa) to homogenize glass distribution without excessive shear heating. Injection speed is part-specific: thin-wall connector housings may require fill times below 0.5 s to prevent freeze-off, but high injection speeds increase glass-fiber orientation and create anisotropic shrinkage. Mold temperature should be 60–90°C. The upper end of the range improves crystallinity and hydrolytic resistance, while the lower end may produce a faster cycle but with reduced dimensional stability. Hot-runner manifold temperatures should not exceed 275°C; dead spots in hot-runner channels can retain material longer than the permissible residence time and produce brown or black degradation specks. Screw recovery should be monitored because a sharp drop in screw torque or shot weight at constant settings may indicate hydrolysis or fiber breakage from excessive shear.

    Because black-pigmented grades contain carbon black, outdoor weathering and infrared absorption can raise surface temperature under direct solar load. This is relevant for components such as exterior charging inlets or underhood fuse covers that may see localized thermal spikes. Carbon black also influences surface appearance and can mask visual defects, but it is not a functional stabilizer against hydrolysis; the BK suffix identifies color, not UV or thermal resistance. For outdoor UV exposure, additional UV stabilizers may be required depending on the application. The black coloration nevertheless provides consistent color uniformity and is preferred for parts requiring low light transmission or a neutral aesthetic. Dimensional checks after molding should account for post-shrinkage in hot service: glass-fiber-reinforced PBT may continue to shrink by 0.05–0.15% during the first 48 h after molding if mold temperature is below 80°C. Post-molding annealing at 120°C for 2 h can stabilize dimensions for tight-tolerance assemblies.

    Accelerated Hydrolysis Testing Benchmarks Under Hot-Humid and Coolant Exposure Conditions

    Qualification of Chang Chun LONGLITE® PBT+GF-Hydrolytic 4820 BK for coolant-contacting parts should include hydrothermal aging in both distilled water and a 50/50 vol% water-ethylene glycol mixture at elevated temperature. Typical test conditions for automotive electrical connectors use 85°C/85% RH for 1,000 h following ISO 6270-2 or IEC 60068-2-78, with tensile strength and elongation retention measured to ISO 527-1/-2. For pump impellers and housings exposed to glycol-based coolants, immersion testing at 120°C in a sealed autoclave for 200–500 h is a more severe screening procedure. The acceptance criterion in many powertrain specifications is a minimum 50% retention of notched Charpy impact strength after aging, measured to ISO 179-1/1eA. Published data for hydrolysis-stabilized PBT grades in this test environment generally show significantly slower degradation than unstabilized PBT, but grade-specific values must be confirmed by the supplier’s technical report.

    Thermal cycling can interact with hydrolysis through microcracking at the glass-fiber interface. Slow temperature sweeps from −40°C to 125°C with 30 min dwells, as described in SAE USCAR-2 or ISO 16750-4, can reveal latent damage that static hydrothermal aging does not. Because the coefficient of linear thermal expansion differs between the PBT matrix and glass fibers, repeated cycling can initiate interfacial debonding; hydrolytic degradation then propagates along the damaged interface. This failure sequence is why tensile elongation after combined temperature-humidity cycling is a better quality gate than tensile strength alone. For molded parts with weld lines, the weld-line strength retention after hydrothermal aging may be 20–30% lower than in non-weld regions; gate and knit-line placement should be evaluated using short-shot studies and molded-in stress analysis.

    For supplier qualification, the following documentation matrix is commonly required. The listed standard designations represent the test methods, not guaranteed values for any specific lot.

    ParameterMethod / ConditionDocumentation
    Glass fiber contentISO 3451-120 wt% nominal
    DensityISO 1183-1Certificate of analysis
    Tensile strength, elongation at breakISO 527-1/-2, 23°CCertificate of analysis
    Charpy notched impact strengthISO 179-1/1eA, 23°CCertificate of analysis
    Heat deflection temperatureISO 75-1/-2, 1.8 MPaCertificate of analysis
    Flammability classUL 94Yellow Card
    RoHS compliance2011/65/EU + (EU) 2015/863Supplier declaration
    REACH SVHC statusRegulation (EC) No 1907/2006Supplier declaration

    For applications involving fuel vapor or aggressive alkaline cleaning solutions, chemical compatibility should be verified before production. PBT is resistant to many automotive fluids, but strong bases, hot amines, and concentrated phosphoric acid can attack the ester backbone even when hydrolytic stabilization is present. Avoid combination with amine-based additives or rich amine-containing overmolding compounds that can accelerate depolymerization and consume the stabilizer. This incompatibility is particularly important when black-pigmented parts are overmolded with thermoplastic elastomers containing amine-rich curatives or flame-retardant packages.

    When Coolant-Glycol Mixtures Dictate Material Selection for Pump Impellers and End Covers

    For coolant circulation pump impellers and end covers, hydrolytic stabilization is the primary material requirement, but it is not sufficient by itself. The component geometry must minimize high-shear regions where glass-fiber orientation creates weak planes. Impeller blades molded from 20 wt% glass-filled PBT can exhibit hub-to-tip tensile strength variations because flow converges at the hub and forms knit lines at the trailing edge. Production tooling should place gates at the impeller hub and use multiple valve-gated drops if necessary; melt temperature near 260°C, mold temperature 80–90°C, and holding pressure 60–80 MPa are typical process targets. In hydraulic pump applications, the presence of corrosion inhibitors, silicates, or organic acid-based coolant formulations influences the rate of hydrolysis. Long-term immersion screening in the specific coolant formulation at 120°C for 500 h is recommended before homologation.

    Compared with a PBT/PET blend, a hydrolysis-stabilized PBT retains a higher crystallization temperature and can provide more consistent crystallinity across variable mold temperatures. This matters for pump housings that combine thin walls and thick bosses: uneven crystallinity produces differential shrinkage and reduces dimensional accuracy. Compared with polyphenylene sulfide (PPS) grades, the PBT+GF-Hydrolytic grade offers lower melt temperature and better elongation but lower continuous-use temperature and solvent resistance. PPS remains preferred for service above 180°C or continuous contact with aggressive fuels, while the hydrolytic PBT is more cost-effective for water-glycol environments below 120°C.

    Top